966 resultados para OPTICAL PROPERTIES
Resumo:
Multilayer InGaN/GaN quantum dots (QDs) were grown on sapphire substrates through a three-dimensional growth mode, which was initiated by a special passivation processing introduced into the normal growth procedure. Surface morphology and photoluminescence properties of QDs with different stacking periods (from one to four) were investigated. The temperature dependences of the PL peak energies were found to show a great difference between two-layer and three-layer QDs. The fast redshift and the reversed sigmoidal temperature dependences of the PL energies for the former were attributed to the thermally activated carrier transfer from small to large dots. However, the increase of both the dot size and the spatial space among dots with the growing stacking periods reduced the carrier escape and retrapping. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
InGaN/GaN multiple quantum wells (MQWs) are grown by metal-organic chemical vapour deposition on (0001) sapphire substrates. Triple-axis X-ray diffraction (TXRD) and photoluminescence (PL) spectra are used to assess the influence of trimethylgallium (TMGa) flow on structural defects, such as dislocations and interface roughness, and the optical properties of the MQWs. In this paper, a method, involving an ! scan of every satellite peak of TXRD, is presented to measure the mean dislocation density of InGaN/GaN MQWs. The experimental results show that under certain conditions which keep the trimethlyindium flow constant, dislocation density and interface roughness decrease with the increase of TMGa flow, which will improve the PL properties. It can be concluded that dislocations, especially edge dislocations, act as nonradiative recombination centres in InGaN/GaN MQWs. Also noticed is that changing the TMGa flow has more influence on edge dislocations than screw dislocations.
Resumo:
Raman scattering and photoluminescence (PL) of boron-doped silicon nanowires have been investigated. Raman spectra showed a band at 480 cm(-1), indicating that the crystallinity of the nanowires was suppressed by boron doping. PL taken from B-doped SiNWS at room temperature exhibited three distinct emission peaks at 1.34, 1.42. and 1.47 eV and the PL intensity was much stronger than that of undoped SiNWS. The increased PL intensity should be very profitable for nano-optoelectronics. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
InGaN/GaN multiquantum-well (MQW) structures grown by metalorganic chemical-vapor deposition on n-type GaN and capped by p-type GaN were investigated by cross-sectional transmission electron microscopy, double crystal x-ray diffraction, and temperature-dependent photoluminescence. For the sample with strained-layer thicknesses greater than the critical thicknesses, a high density of pure edge type threading dislocations generated from MQW layers and extended to the cap layer was observed. These dislocations result from a relaxation of the strained layers when their thicknesses are beyond the critical thicknesses. Because of indium outdiffusion from the well layers due to the anneal effect of Mg-doped cap layer growth and defects generated from strain relaxation, the PL emission peak was almost depressed by the broad yellow band with an intensity maximum at 2.28 eV. But for the sample with strained-layer thicknesses less than the critical thicknesses, it has no such phenomenon. The measured critical thicknesses are consistent with the calculated values using the model proposed by Fischer, Kuhne, and Richter. (C) 2004 American Institute of Physics.
Resumo:
The effects of pre-TMIn flow prior to QW growth and TMIn flow rates during QW growth on the interface and optical properties of InGaN/GaN MQWs were investigated. Pre-depositing indium prior to QW growth and an appropriate TMIn flow rate can improve the interface abruptness and increase the EL intensity. InGaN/GaN MQWs with improved interface abruptness have increasing emission intensity and wavelength. We attribute the interface improvement and the increase of EL intensity to the improvement of the indium compositional profiles. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
AlInGaN quaternary epilayers have been grown with various TMGa flows by metalorganic chemical vapor deposition to investigate the influence of growth rate on the structural and optical properties. Triple-axis X-ray diffraction measurements show AlInGaN epilayers have good crystalline quality. Photolummescence (PL) measurements show that the emission intensity of AlInGaN epilayers is twenty times stronger than that of AlGaN epilayer with comparable Al content. V-shaped pits are observed at the surface of AlInGaN epilayers by atomic force microscopy (AFM) and transmission electron microscopy (TEM). High growth rate leads to increased density and size of V-shaped pits, but crystalline quality is not degraded. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
The optical properties of quantum rods in the absence and presence of the magnetic field are studied in the framework of effective-mass envelope function theory. The two-dimensional (2D) and 1D transition dipoles of wurtzite quantum rods are investigated. It is found that the transition dipoles change from 2D to 1D as the aspect ratio of the ellipsoid increases, in agreement with the experimental results. The linear polarization factors of optical transitions of quantum rods with critical aspect ratio are zero at every orientation of the wave propagation. So quantum rods with critical aspect ratio have isotropic transition dipoles. Due to the 2D or 1D transition dipoles, the linear polarization factors of optical transitions of quantum rods change from negative or positive values to zero as the orientation of the wave propagation changes from the x axis of the crystal structure to the z axis, in agreement with the experimental results. Under magnetic field applied along the z axis of the crystal structure, the negative linear polarization factors in the 2D transition dipole case decrease as the magnetic field increases, while under magnetic field applied along the x axis, the negative linear polarization factors increase as the magnetic field increases. The antisymmetric Hamiltonian is very important to these effects of the magnetic field. It is found that quantum rods with a given radius at a given temperature have dark excitons in a range of aspect ratio. The dimensions along the x, y axes of the crystal structure play opposite roles to the dimension along the z axis on the dark exciton phenomenon. Dark excitons become bright under appropriate magnetic field.
Resumo:
Quasi-aligned Eu2+-doped wurtzite ZnS nanowires on Au-coated Si wafers have been successfully synthesized by a vapor deposition method under a weakly reducing atmosphere. Compared with the undoped counterpart, incorporation of the dopant gives a modulated composition and crystal structure, which leads to a preferred growth of the nanowires along the [0110] direction and a high density of defects in the nanowire hosts. The ion doping causes intense fluorescence and persistent phosphorescence in ZnS nanowires. The dopant Eu2+ ions form an isoelectronic acceptor level and yield a high density of bound excitions, which contribute to the appearance of the radiative recombination emission of the bound excitons and resonant Raman scattering at higher pumping intensity. Co-dopant Cl- ions can serve not only as donors, producing a donor-acceptor pair transition with the Eu2+ acceptor level, but can also form trap levels together with other defects, capture the photoionization electrons of Eu2+, and yield long-lasting (about 4 min), green phosphorescence. With decreasing synthesis time, the existence of more surface states in the nanowires forms a higher density of trap centers and changes the crystal-field strength around Eu2+. As a result, not only have an enhanced Eu2+ -4f(6)5d(1)-4f(7) intra-ion transition and a prolonged afterglow time been more effectively observed (by decreasing the nanowires' diameters), but also the Eu2+ related emissions are shifted to shorter wavelengths.
Resumo:
Six-stacked InAs/In0.52Al0.48As self-assembled quantum wires (QWRs) on InP(001) by molecular-beam epitaxy (MBE) have been studied by high-resolution transmission electron microscopy (HRTEM) and polarized PL measurements. We obtained the chemical lattice fringe (CLF) image of InAs self-assembled QWRs embedded in the In0.52Al0.48As matrix by the interference between the (002)-diffracted beam and the transmitted beam in the image plane of the objective lens. The results show that the InAs QWRs were bounded by (113), (001) and (114) facets. Both the size and strain distribution in QWRs were determined. It was found that with the growth of successive periods, the height and height fluctuation of InAs QWRs decreased from the bottom period to the upper one. Some suggestions are put forward for further improving the uniformity of the stacked InAs QWRs. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Thermal annealing effect on InAs quantum dots grown on vicinal (100) GaAs substrates is studied in comparison with dots on exact (100) GaAs substrates. We find that annealing acts stronger effect on dots with vicinal substrates by greatly accelerating the degradation of material quality. as well as slightly increasing the blueshift of the emission wavelength and the narrowing of PL linewidth. It is attributed to the higher strain in the dots formed on the vicinal substrates.
Resumo:
GaN epilayers were grown on Si (111) substrates by MOCVD. The optical properties of the samples under different growth conditions were characterized The abnormal peaks of excitonic emissions related to cubic-GaN were observed on the samples under improper growth conditions based on the LT PL measurements. Also the peak intensity is much higher than that of hexagonal-GaN. The higher intensity of exciton peaks is attributed to the local quantum well formed between the hexagonal- and cubic-GaN. No exciton peaks of cubic-GaN were found on the sample using the optimal growth conditions.
Resumo:
Based on the results of the temperature-dependent photoluminescence (PL) measurements, the broad PL emission in the phase-separated GaNP alloys with P compositions of 0.03, 0.07, and 0.15 has investigated. The broad PL peaks at 2.18, 2.12 and 1.83 eV are assigned to be an emission from the optical transitions from several trap levels, possibly the iso-electronic trap levels related to nitrogen. With the increasing P composition (from 0.03 to 0.15), these iso-electronic trap levels are shown to become resonant with the conduction band of the alloy and thus optically inactive, leading to the apparent red shift (80-160meV) of the PL peak energy and the trend of the red shift is strengthened. No PL emission peak is observed from the GaN-rich GaNP region, suggesting that the photogenerated carriers in the GaN-rich GaNP region may recombine with each other via non-radiation transitions.
Resumo:
Optical properties of highly strained GaInAs/GaAs quantum wells (QWs) grown by molecular beam epitaxy with Sb assistance are investigated. The samples grown by Sb incorporation and Sb pre-deposition methods display high room-temperature photoluminescence (PL) intensity at extended long wavelength. This result is explained by the surfactant effects of Sb during the growth of GaInAs/GaAs QW systems. An abnormal S-shaped temperature dependence of the PL peak position is found in the In0.42Ga0.58As/GaAs triple QWs sample grown with Sb pre-deposition. By investigating the transmission electron microscope images and time-resolved PL spectra, it is found that the S-shaped temperature dependence of the PL peak position originates from the exciton localization effect brought by the Sb-rich clusters on the QW interface.
Resumo:
GaNAs/GaAs single quantum wells (SQWs) and dilute GaNAs bulk grown by molecular beam epitaxy(MBE) were studied by photoluminescence (PL), selectively-excited PL, and time-resolved PL. Exciton localization and delocalization were investigated in detail. Under short pulse laser excitation, the delocalization exciton emission was revealed in GaNAs/GaAs SQWs. It exhibits quite different optical properties from N-related localized states. In dilute GaNAs bulk, a transition of alloy band related recombination was observed by measuring the PL dependence on temperature and excitation intensity and time-resolved PL, as well. This alloy-related transition presents intrinsic optical properties. These results are very important for realizing the abnomal features of III-V-N semiconductors.
Resumo:
Microscopic luminescence and Raman scattering study was carried on AIInGaN quaternary alloy. Based on the analyses of SEM image and cathodoluminescence spectra measured around V-defects, the correlation between V-defect formation and indium segregation was clarified. Raman scattering of thin AlInGaN epilayers was investigated by using the short wavelength excitation of 325nm laser line. The frequency shift of A(1)(LO) phonon induced by the change of Al composition in alloy was observed. The Raman scattering of LO phonons was found to be resonantly enhanced with outgoing resonance, and it is attributed to the cascade-like electron-multiphonon interaction mechanism.