893 resultados para Boron Solubility
Resumo:
Immersion in various media has different effect on the properties of dental composites, such as sorption, solubility, elution of unreacted monomers, flexural strength, and flexural elastic modulus. In the present work, the effect of immersion in various media and the relationship between the variation of these properties and the components of dental composite were investigated.
Resumo:
The substantial crystallization suppression of poly(3-hexylthiophene) (P3HT) in the untreated P3HT:C60 composite film prepared from o-dichlorobenzene (ODCB) solution has been revealed. Besides, the effective conjugation length of P3HT in this composite has been nearly maintained to that in the solution. The different crystallization behaviors of P3HT in its composites with C60 and [6,6]-phenyl C-61 butyric acid methyl ester (PCBM) are mainly attributed to the relative solubility of C60 and PCBM with respect to P3HT in ODCB. The solution to overcome this disadvantage of chain conformation and crystallinity of P3HT in the composite with C60 is thus proposed and finalized by resorting to the addition of low volatile solvent with much higher solubility of C60 than P3HT into the main solvent used, so as P3HT can crystallize before C60 forms crystallites in the solution. The feasibility of this approach has been proven by the improved efficiency of devices based on composites of P3HT and the low cost C60 without resorting to post-treatments.
Resumo:
Four diboron-contained ladder-type pi-conjugated compounds 1-4 were designed and synthesized. Their thermal, photophysical, electrochemical properties, as well as density functional theory calculations, were fully investigated. The single crystals of compounds 1 and 3 were grown, and their crystal structures were determined by X-ray diffraction analysis. Both compounds have a ladder-type g-conjugated framework. Compounds I and 2 possess high thermal stabilities, moderate solid-state fluorescence quantum yields, as well as stable redox properties, indicating that they are possible candidates for emitters and charge-transporting materials in electroluminescent (EL) devices. The double-layer device with the configuration of [ITO/NPB (40 nm)/1 or 2 (70 nm)/LiF (0.5 nm)/Al (200 nm)] exhibited good EL performance with the maximum brightness exceeding 8000 cd/m(2).
Resumo:
The relationship between structure, ionic radius and electronegativity and solubility of the various rare-earth elements in Mg was studied. It is found that light RE(La-Sm, Eu, Yb) have more complicated phase relation with Mg but the heavy RE(Gd-Lu, Sc) have the similar crystal structure with magnesium. Also it is found that the less electronegativity difference between Mg and RE is, the more solubility limit of RE in Mg is. The fact of the RE solubility decreased in magnesium with lowering temperature suggests that there is a possibility of Mg supersaturated solid solution formation and it will decomposition during aging. According to the rule, an megnesium alloy with higher strength feature was developed. Their mechanical properties are UTS 347MPa, YTS 290MPa and elongation 12.5% at room temperature.
Resumo:
A bright blue boron complex BPh2(pybm) containing 2-(2-pyridyl)benzimidazole ligand was designed and synthesized by using N, N-bidentate ligand instead of N, O-bidentate one such as 8-quinolinol. For three-layer LED devices with the configuration of ITO/NPB/BPh2(pybm)/Alq(3)/LiF/Al, the white light emission covering the whole visible region from 400 to 750 nm with the maximum brightness of 110 cd/m(2) and the luminous efficiency of 0.8 cd/A was observed.
Resumo:
A series of homopolyimides and copolyimides was synthesized by the solution condensation of biphenyltetracarboxylic dianhydride (BPDA) isomers and various diamines followed by chemical imidization. These polyimides had intermediate to high molecular weights with inherent viscosities of 0.34-1.01 dL/g for homopolyimides and 0.48-1.02 dL/g for copolyimides. Thermogravimetric analysis indicated that the aromatic polyimides were stable up to 500degreesC, and the 5% weight loss temperatures were recorded in the range of 506-597degreesC in an air atmosphere and in the range of 517-601degreesC in a nitrogen atmosphere, depending on the diamines used. The glass transition temperatures of aromatic homopolyimides were above 271degreesC, while the glass transition temperatures of the copolyimides increased with an increase in the 2, 2', 3, 3'-BPDA-component. The effects of the chemical structure of the polymer chain on the solubility were investigated. It was found that the solubility of BPDA-based polyimides could be improved by the introduction of flexible units, nonlinear and non-coplanar units, and copolymerization. The polyimides with nonlinear and non-coplanar units derived from 2, 2', 3, 3'-BPDA appeared to have prominently enhanced solubility in polar aprotic solvents and polychlorocarbons when compared with the homopolyimide derived from 3, 3', 4, 4'-BPDA.
Resumo:
Endohedral metallofullerenes Tm@C-2n were synthesized with the carbon-arc discharge method of activating the Tm2O3-containing graphite anode in situ and back-burning technique, Toluene soxhlet extraction, toluene and pyridine high-temperature and high-pressure extraction technique were employed for the effective extraction of Tm@C-2n. The formation of Tm@C-2n was confirmed by LD-TOF and DEIMS characterization. The mass spectrometric results indicate that Tm@C-2n have a better solubility in toluene and worse solubility in pyridine than other metallofullerenes.
Resumo:
A series of narrow molecular weight distribution fractions of phenolphthalein polyarylether sulfone(PES-C) had been prepared, The <(M) over bar (w)> of these fractions were determined by conventional light scattering method. The [eta] and the Huggins slope constant k' in DMF, CHCl3 and 1,2-dichloroethane were also determined. The Huggins constants are greater than 0.5 in all of these solvents showing a special solubility behavior. The Mark-Houwink equations of PES-C in these solvents at 25 degrees C are [eta] = 2.79 x 10(-2) <(M) over bar (0.615)(w)> (DMF); [eta] = 3.96 x 10(-2) <(M) over bar (0.58)(w)> (CHCl3); [eta] = 7.40 x 10(-2) <(M) over bar (0.52)(w)> (CH2ClCH2Cl).
Resumo:
The effects of mechanical alloying on the solubility in a Ag-Gd solid solution have been investigated. The study shows that the solubility of Gd in Ag can be extended to about 5 at. % Gd by mechanical alloying from the equilibrium solubility of less than 0.95 at. % Gd. Ag85Gd15 prepared by mechanical alloying exhibits a spin-glass-type transition at similar to 5 K. A Curie-Weiss behavior at higher temperatures and x-ray patterns of the material indicate that Gd atoms are either dissolved in the Ag matrix or in the form of small clusters of diameters of a few nanometers;