Resumo:
This paper reports the details of an experimental study of cold-formed steel hollow section columns at ambient and elevated temperatures. In this study the global buckling behaviour of cold-formed Square Hollow Section (SHS) slender columns under axial compression was investigated at various uniform elevated temperatures up to 700℃. The results of these column tests are reported in this paper, which include the buckling/failure modes at elevated temperatures, and ultimate load versus temperature curves. Finite element models of tested columns were also developed and their behaviour and ultimate capacities at ambient and elevated temperatures were studied. Fire design rules given in European and American standards including the Direct Strength Method (DSM) based design rules were used to predict the ultimate capacities of tested columns at elevated temperatures. Elevated temperature mechanical properties and stress-strain models given in European steel design standards and past researches were used with design rules and finite element models to investigate their effects on SHS column capacities. Comparisons of column capacities from tests and finite element analyses with those predicted by current design rules were used to determine the accuracy of currently available column design rules in predicting the capacities of SHS columns at elevated temperatures and the need to use appropriate elevated temperature material stress-strain models. This paper presents the important findings derived from the comparisons of these column capacities.
Resumo:
Cold-formed steel members have many advantages over hot-rolled steel members. However, they are susceptible to various buckling modes at stresses below the yield stress of the member because of their relatively high width-to-thickness ratio. Web crippling is a form of localized failure mode that can occur when the members are subjected to transverse high concentrated loadings and/or reactions. The four common loading conditions are the end-one-flange (EOF), interior-one-flange (IOF), end-two-flange (ETF) and interior-two-flange (ITF) loadings. Recently a test method has been proposed by AISI to obtain the web crippling capacities under these four loading conditions. Using this test method 42 tests were conducted in this research to investigate the web crippling behaviour and strengths of unlipped channels with stocky webs under ETF and ITF cases. DuraGal sections having a nominal yield stress of 450 MPa were tested with different web slenderness and bearing lengths. The flanges of these channel sections were not fastened to the supports. In this research the suitability of the currently available design rules for unlipped channels subject to web crippling was investigated, and suitable modifications were proposed where necessary. In addition to this, a new design rule was proposed based on the direct strength method to predict the web crippling capacities of tested beams. This paper presents the details of this experimental study and the results.
Resumo:
Cold-formed steel members have been widely used in residential and commercial buildings as primary load bearing structural elements. They are often made of thin steel sheets and hence they are more susceptible to local buckling. The buckling behaviour of cold-formed steel compression members under fire conditions is not fully investigated yet and hence there is a lack of knowledge on the fire performance of cold-formed steel compression members. Current cold-formed steel design standards do not provide adequate design guidelines for the fire design of cold-formed steel compression members. Therefore a research project based on extensive experimental and numerical studies was undertaken to investigate the local buckling behaviour of light gauge cold-formed steel compression members under simulated fire conditions. First a series of 91 local buckling tests was conducted at ambient and uniform elevated temperatures up to 700oC on cold-formed lipped and unlipped channels. Suitable finite element models were then developed to simulate the behaviour of tested columns and were validated using test results. All the ultimate load capacity results for local buckling were compared with the predictions from the available design rules based on AS/NZS 4600, BS 5950 Part 5, Eurocode 3 Parts 1.2 and 1.3 and the direct strength method (DSM), based on which suitable recommendations have been made for the fire design of cold-formed steel compression members subject to local buckling at uniform elevated temperatures.
Resumo:
Cold water immersion and ice baths are popular methods of recovery used by athletes. From the simple wheelie bin with water and ice, to the inflatable baths with complex water cooling units to recovery sessions in the ocean, the practice of cold water immersion is wide and varied. Research into cold water immersion was conducted as early as 1963 when Clarke1 examined the influence of cold water on performance recovery after a sustained handgrip exercise. Research has been conducted to understand how cold water immersion might affect the body’s physiological systems and how factors such as water temperature and the duration of immersion might enhance recovery after training and/or competition. Despite this research activity, how are we to know if research is being put into practice? In more serious situations, where guidelines and policies need to be standardised for the safe use of a product, one would expect that there is a straight forward follow-on from research into practice. Although cold water immersion may not need the rigor of testing compared to drug treatments, for example, the decision on whether to use cold water immersion in specific situations (e.g. after training or competition) may rest with one or two of the staff associated with the athlete/team. Therefore, it would be expected that these staff are well-informed on the current literature regarding cold water immersion.
Resumo:
In strengthening systems, the CFRP (Carbon Fibre Reinforced Polymer) materials typically have excellent resistance against environmental conditions; however, the performance of adhesives between CFRP and steel is generally affected by various environmental conditions such as marine environment, cold and hot weather. This paper presents the comparative durability study of CFRP strengthened tubular steel structures by using two different adhesives such as MBrace saturant and Araldite K630 under four-point bending. The program consisted of testing twelve CFRP strengthened specimens having treated with epoxy based adhesion promoter, untreated surface and one unstrengthened specimen and conditioned under cold weather for 3 and 6 months to determine the environmental durability. The beams were then loaded to failure in quasi-static manner under four-point bending. The structural responses of CFRP strengthened tubular steel beams were compared in terms of failure load, stiffness and modes of failure. The research findings show that the cold weather immersion had adversely affected the durability of CFRP strengthened steel members. Design factor is also proposed to address the short-terms durability performance under cold weather.
Resumo:
We investigated functional, morphological and molecular adaptations to strength training exercise and cold water immersion (CWI) through two separate studies. In one study, 21 physically active men strength trained for 12 weeks (2 d⋅wk–1), with either 10 min of CWI or active recovery (ACT) after each training session. Strength and muscle mass increased more in the ACT group than in the CWI group (P<0.05). Isokinetic work (19%), type II muscle fibre cross-sectional area (17%) and the number of myonuclei per fibre (26%) increased in the ACT group (all P<0.05) but not the CWI group. In another study, nine active men performed a bout of single-leg strength exercises on separate days, followed by CWI or ACT. Muscle biopsies were collected before and 2, 24 and 48 h after exercise. The number of satellite cells expressing neural cell adhesion molecule (NCAM) (10−30%) and paired box protein (Pax7)(20−50%) increased 24–48 h after exercise with ACT. The number of NCAM+ satellitecells increased 48 h after exercise with CWI. NCAM+- and Pax7+-positivesatellite cell numbers were greater after ACT than after CWI (P<0.05). Phosphorylation of p70S6 kinaseThr421/Ser424 increased after exercise in both conditions but was greater after ACT (P<0.05). These data suggest that CWI attenuates the acute changes in satellite cell numbers and activity of kinases that regulate muscle hypertrophy, which may translate to smaller long-term training gains in muscle strength and hypertrophy. The use of CWI as a regular post-exercise recovery strategy should be reconsidered.
Resumo:
Cold water immersion (CWI) and active recovery (ACT) are frequently used as post-exercise recovery strategies. However, the physiological effects of CWI and ACT after resistance exercise are not well characterized. We examined the effects of CWI and ACT on cardiac output (Q), muscle oxygenation (SmO2) and blood volume (tHb), muscle temperature (Tmuscle ) and isometric strength after resistance exercise. On separate days, 10 men performed resistance exercise, followed by 10 min CWI at 10°C or 10 min ACT (low-intensity cycling). Q (7.9±2.7 l) and Tmuscle (2.2±0.8ºC) increased, whereas SmO2 (-21.5±8.8%) and tHb (-10.1±7.7 μM) decreased after exercise (p<0.05). During CWI, Q ̇(-1.1±0.7 l) and Tmuscle (-6.6±5.3ºC) decreased, while tHb (121±77 μM) increased (p<0.05). In the hour after CWI, Q ̇and Tmuscle remained low, while tHb also decreased (p<0.05). By contrast, during ACT, Q ̇(3.9±2.3 l), Tmuscle (2.2±0.5ºC), SmO2 (17.1±5.7%) and tHb (91±66 μM) all increased (p<0.05). In the hour after ACT, Tmuscle and tHb remained high (p<0.05). Peak isometric strength during 10 s maximum voluntary contractions (MVCs) did not change significantly after CWI, whereas it decreased after ACT (-30 to -45 Nm; p<0.05). Muscle deoxygenation time during MVCs increased after ACT (p<0.05), but not after CWI. Muscle reoxygenation time after MVCs tended to increase after CWI (p=0.052). These findings suggest firstly that hemodynamics and muscle temperature after resistance exercise are dependent on ambient temperature and metabolic demands with skeletal muscle, and secondly, that recovery of strength after resistance exercise is independent of changes in hemodynamics and muscle temperature.
Resumo:
Light gauge Steel Frame (LSF) walls are extensively used in the building industry due to the many advantages they provide over other wall systems. Although LSF walls have been used widely, fire design of LSF walls is based on approximate prescriptive methods based on limited fire tests. Also these fire tests were conducted using the standard fire curve [1] and the applicability of available design rules to realistic design fire curves has not been verified. This paper investigates the accuracy of existing fire design rules in the current cold-formed steel standards and the modifications proposed by previous researchers. Of these the recently developed design rules by Gunalan and Mahendran [2] based on Eurocode 3 Part 1.3 [3] and AS/NZS 4600 [4] for standard fire exposure [1] were investigated in detail to determine their applicability to predict the axial compression strengths and fire resistance ratings of LSF walls exposed to realistic design fire curves. This paper also presents the fire performance results of LSF walls exposed to a range of realistic fire curves obtained using a finite element analysis based parametric study. The results from the parametric study were used to develop a simplified design method based on the critical hot flange temperature to predict the fire resistance ratings of LSF walls exposed to realistic fire curves. Finally, the stud failure times (fire resistance rating) obtained from the fire design rules and the simplified design method were compared with parametric study results for LSF walls lined with single and double plasterboards, and externally insulated with rock fibres under realistic fire curves.
Resumo:
Cold-formed steel wall frame systems using lipped or unlipped C-sections and gypsum plasterboard lining are commonly utilised in the construction of both the load bearing and non-load bearing walls in the residential, commercial and industrial buildings. However, the structural behaviour of unlined and lined stud wall frames is not well understood and adequate design rules are not available. A detailed research program was therefore undertaken to investigate the behaviour of stud wall frame systems. As the first step in this research, the problem relating to the degree of end fixity of stud was investigated. The studs are usually connected to the top and bottom tracks and the degree of end fixity provided by these tracks is not adequately addressed by the design codes. A finite element model of unlined frames was therefore developed, and validated using full scale experimental results. It was then used in a detailed parametric study to develop appropriate design rules for unlined wall frames. This study has shown that by using appropriate effective length factors, the ultimate load and failure modes of the unlined studs can be accurately predicted using the provisions of Australian or American cold-formed steel structures design codes. This paper presents the details of the finite element analyses, the results and recommended design rules for unlined wall frames.
Resumo:
Light gauge cold-formed steel sections have been developed as more economical building solutions to the alternative heavier hot-rolled sections in the commercial and residential markets. Cold-formed lipped channel beams (LCB), LiteSteel beams (LSB) and triangular hollow flange beams (THFB) are commonly used as flexural members such as floor joists and bearers while rectangular hollow flange beams (RHFB) are used in small scale housing developments through to large building structures. However, their shear capacities are determined based on conservative design rules. For the shear design of cold-formed steel beams, their elastic shear buckling strength and the potential post-buckling strength must be determined accurately. Hence experimental and numerical studies were conducted to investigate the shear behaviour and strength of LCBs, LSBs, THFBs and RHFBs. Improved shear design rules including the direct strength method (DSM) based design equations were developed to determine the ultimate shear capacities of these open and hollow flange steel beams. An improved equation for the higher elastic shear buckling coefficient of cold-formed steel beams was proposed based on finite element analysis results and included in the design equations. A new post-buckling coefficient was also introduced in the design equations to include the available post-buckling strength of cold-formed steel beams. This paper presents the details of this study on cold-formed steel beams subject to shear, and the results. It proposes generalised and improved shear design rules that can be used for any type of cold-formed steel beam.
Resumo:
Background Recovery strategies are often usedwith the intention of preventing orminimisingmuscle soreness after exercise. Whole-body cryotherapy, which involves a single or repeated exposure(s) to extremely cold dry air (below -100 °C) in a specialised chamber or cabin for two to four minutes per exposure, is currently being advocated as an effective intervention to reduce muscle soreness after exercise. Objectives To assess the effects (benefits and harms) of whole-body cryotherapy (extreme cold air exposure) for preventing and treating muscle soreness after exercise in adults. Search methods We searched the Cochrane Bone, Joint and Muscle Trauma Group Specialised Register, the Cochrane Central Register of Controlled Trials, MEDLINE, EMBASE, CINAHL, the British Nursing Index and the Physiotherapy Evidence Database. We also searched the reference lists of articles, trial registers and conference proceedings, handsearched journals and contacted experts. The searches were run in August 2015. Selection criteria We aimed to include randomised and quasi-randomised trials that compared the use of whole-body cryotherapy (WBC) versus a passive or control intervention (rest, no treatment or placebo treatment) or active interventions including cold or contrast water immersion, active recovery and infrared therapy for preventing or treating muscle soreness after exercise in adults. We also aimed to include randomised trials that compared different durations or dosages of WBC. Our prespecified primary outcomes were muscle soreness, subjective recovery (e.g. tiredness, well-being) and adverse effects. Data collection and analysis Two review authors independently screened search results, selected studies, assessed risk of bias and extracted and cross-checked data. Where appropriate, we pooled results of comparable trials. The random-effects model was used for pooling where there was substantial heterogeneity.We assessed the quality of the evidence using GRADE. Main results Four laboratory-based randomised controlled trials were included. These reported results for 64 physically active predominantly young adults (mean age 23 years). All but four participants were male. Two trials were parallel group trials (44 participants) and two were cross-over trials (20 participants). The trials were heterogeneous, including the type, temperature, duration and frequency of WBC, and the type of preceding exercise. None of the trials reported active surveillance of predefined adverse events. All four trials had design features that carried a high risk of bias, potentially limiting the reliability of their findings. The evidence for all outcomes was classified as ’very low’ quality based on the GRADE criteria. Two comparisons were tested: WBC versus control (rest or no WBC), tested in four studies; and WBC versus far-infrared therapy, also tested in one study. No studies compared WBC with other active interventions, such as cold water immersion, or different types and applications of WBC. All four trials compared WBC with rest or no WBC. There was very low quality evidence for lower self-reported muscle soreness (pain at rest) scores after WBC at 1 hour (standardised mean difference (SMD) -0.77, 95% confidence interval (CI) -1.42 to -0.12; 20 participants, 2 cross-over trials); 24 hours (SMD -0.57, 95%CI -1.48 to 0.33) and 48 hours (SMD -0.58, 95% CI -1.37 to 0.21), both with 38 participants, 2 cross-over studies, 1 parallel group study; and 72 hours (SMD -0.65, 95% CI -2.54 to 1.24; 29 participants, 1 cross-over study, 1 parallel group study). Of note is that the 95% CIs also included either no between-group differences or a benefit in favour of the control group. One small cross-over trial (9 participants) found no difference in tiredness but better well-being after WBC at 24 hours post exercise. There was no report of adverse events. One small cross-over trial involving nine well-trained runners provided very low quality evidence of lower levels of muscle soreness after WBC, when compared with infrared therapy, at 1 hour follow-up, but not at 24 or 48 hours. The same trial found no difference in well-being but less tiredness after WBC at 24 hours post exercise. There was no report of adverse events. Authors’ conclusions There is insufficient evidence to determine whether whole-body cryotherapy (WBC) reduces self-reportedmuscle soreness, or improves subjective recovery, after exercise compared with passive rest or no WBC in physically active young adult males. There is no evidence on the use of this intervention in females or elite athletes. The lack of evidence on adverse events is important given that the exposure to extreme temperature presents a potential hazard. Further high-quality, well-reported research in this area is required and must provide detailed reporting of adverse events.
Resumo:
Fire safety plays a vital role in building design because appropriate level of fire safety is important to safeguard lives and property. Cold-formed steel channel sections along with fire-resistive plasterboards are used to construct light-gauge steel frame (LSF) floor systems to provide adequate fire resistance ratings (FRR). It is common practice to use lipped channel sections (LCS) as joists in LSF floor systems, and past research has only considered such systems. This research focuses on adopting improved joist sections such as hollow flange channel (HFC) sections to improve the structural performance and FRR of cold-formed LSF floor systems under standard fire conditions. The structural and thermal performances of LSF floor systems made of a welded HFC, LiteSteel Beams (LSB), with different plasterboard and insulation configurations, were investigated using four full-scale fire tests under standard fires. These fire tests showed that the new LSF floor system with LSB joists improved the FRR in comparison to that of conventional LCS joists. Fire tests have provided valuable structural and thermal performance data of tested floor systems that included time-temperature profiles and failure times, temperatures, and modes. This paper presents the details of the fire tests conducted in this study and their results along with some important findings.
Resumo:
Much compelling evidence has emerged over the last two decades demonstrating the importance of Australia’s creative industries. In 2014, the Australian Bureau of Statistics confirmed that culture is ‘big business’ in this country. Yet despite this, interest by policy makers at all levels of government has been intermittent, at best. This chapter gives a brief history of policy development, and offers a number of reasons for why policy and politics have not focussed more resolutely on Australia’s creative economy. It finishes with a discussion of Australia’s ‘unfinished agenda’, one which demands attention not only by government, but also industry and higher education, if we are to properly meet both the challenges and opportunities before us.
Resumo:
Bearing failure is a form of localized failure that occurs when thin-walled cold-formed steel sections are subjected to concentrated loads or support reactions. To determine the bearing capacity of cold-formed channel sections, a unified design equation with different bearing coefficients is given in the current North American specification AISI S100 and the Australian/New Zealand standard AS/NZS 4600. However, coefficients are not available for unlipped channel sections that are normally fastened to supports through their flanges. Eurocode 3 Part 1.3 includes bearing capacity equations for different load cases, but does not distinguish between fastened and unfastened support conditions. Therefore, an experimental study was conducted to determine the bearing capacities of these sections as used in floor systems. Twenty-eight web bearing tests on unlipped channel sections with restrained flanges were conducted under End One Flange (EOF) and Interior One Flange (IOF) load cases. Using the results from this study, a new equation was proposed within the AISI S100 and AS/NZS 4600 guidelines to determine the bearing capacities of cold-formed unlipped channels with flanges fastened to supports. A new design rule was also proposed based on the direct strength method.