993 resultados para Ti : sapphire laser


Relevância:

30.00% 30.00%

Publicador:

Resumo:

K alpha radiation generated by interaction of an ultrashort (1 ps) laser with thin (25 mu m) Ti foils at high intensity (2x10(16) W/cm(2)) is analyzed using data from a spherical Bragg crystal imager and a single hit charge-coupled device spectrometer together with Monte Carlo simulations of K alpha brightness. Laser to K alpha and electron conversion efficiencies have been determined. We have also measured an effective crystal reflectivity of 3.75 +/- 2%. Comparison of imager data with data from the relatively broadband single hit spectrometer has revealed a reduction in crystal collection efficiency for high K alpha yield. This is attributed to a shift in the K-shell spectrum due to Ti ionization. (c) 2005 American Institute of Physics.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Saturation of a low pump energy x-ray laser utilizing a transient inversion mechanism on the 3p-3s transition at 32.63 nm in Ne-like Ti has been demonstrated. A close to saturation amplification was simultaneously achieved for the 3d-3p, J=1-->1 transition at 30.15 nm. Small signal effective transient gain coefficients of g similar to 46 and similar to 35 cm(-1) and gain-length products of 16.7 and 16.9 for these lines were obtained. Experiments demonstrate that it is possible to achieve saturated laser action in a transient regime with Ne-like Ti for a pump energy as low as similar to 5 J.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Aims - To study the interchangeability of the measurements of the optic disc topography obtained by one computerised image analyser and one confocal laser tomographic scanner. Methods - One eye of 28 patients with glaucoma or glaucoma suspects was studied. All cases had simultaneous stereoscopic disc photographs taken with the fundus camera Topcon TRC-SS and optic disc examination with the Heidelberg retina tomograph (HRT) during the same visit. The optic disc photographs were digitised and analysed with the Topcon ImageNet (TI) system. Three variables of the optic disc topography provided by the TI and the HRT were compared - cup volume (CV), rim area (RA), and cup area to disc area ratio (CA/DA). Results - The mean values of CV and RA provided by the TI (0.52 (SD 0.32) mm and 1.58 (0.39) mm , respectively) were greater (p <0.01) than the mean values of CV and RA determined by the HRT (0.32 (0.25) mm , and 1.33 (0.47) mm , respectively). The mean value of CA/DA provided by the TI (0.42 (0.14)) and the HRT (0.42 (0.18)) was similar (p = 0.93). Correlation coefficients between measurements obtained by the two methods ranged from 0.53 to 0.73. Conclusion - There was a significant discrepancy in the measurements of rim area and cup volume of the optic disc obtained by a computerised image analyser and a laser scanning tomograph.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The biocompatibility of NiTi after laser welding was studied by examining the in vitro (mesenchymal stem cell) MSC responses at different sets of time varying from early (4 to 12 h) to intermediate phases (1 and 4 days) of cell culture. The effects of physical (surface roughness and topography) and chemical (surface Ti/Ni ratio) changes as a consequence of laser welding in different regions (WZ, HAZ, and BM) on the cell morphology and cell coverage were studied. The results in this research indicated that the morphology of MSCs was affected primarily by the topographical factors in the WZ: the well-defined and directional dendritic pattern and the presence of deeper grooves. The morphology of MSCs was not significantly modulated by surface roughness. Despite the possible initial Ni release in the medium during the cell culture, no toxic effect seemed to cause to MSCs as evidenced by the success of adhesion and spreading of the cells onto different regions in the laser weldment. The good biocompatibility of the NiTi laser weldment has been firstly reported in this study.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Post-weld heat-treatment (PWHT) was applied to NiTi weldments to improve the corrosion behaviour by modifying the microstructure and surface composition. The surface oxide film on the weldments is principally TiO2, together with some Ti, TiO, and Ti2O3. The surface Ti/Ni ratio of the weldments after PWHT is increased. The oxide film formed in Hanks’ solution is thicker on the weldments after PWHT. The pitting resistance of the weldments is increased by PWHT. The galvanic effect in the weldments is very small. The weldment with PWHT at 350 °C shows the best corrosion resistance among other heat-treated weldments in this study.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this study, two L27 Taguchi experiments were carried out to study the effect of fibre laser welding parameters and their interactions upon the weld bead aspect ratio of nickel–titanium thin foil. The optimum parameters to produce full penetrated weld with the largest aspect ratio and desirable microstructure were successfully obtained by the Taguchi experimental design. The corrosion property of the optimized NiTi weld in Hank’s solution at 37.5 °C was studied and compared with the as-received NiTi. To improve the corrosion properties of the weld, the effect of post-weld-heat-treatments ranging from 573 to 1173 K was investigated. The corrosion properties, surface morphology, microstructure and Ti/Ni ratio of the heat-treated NiTi weld were analysed. It was found that a post-weld heat treatment at 573 K for 1 h provided the best pitting corrosion resistance at the weld zone.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The dielectric properties of BaTiO3 thin films and multilayers are different from bulk materials because of nanoscale dimensions, interfaces, and stress-strain conditions. In this study, BaTiO3/SrTiO3 multilayers deposited on SrTiO3 substrates by pulsed laser deposition have been investigated by high-energy-resolution electron energy-loss spectroscopy. The fine structures in the spectra are discussed in terms of crystal-field splitting and the internal strain. The crystal-field splitting of the BaTiO3 thin layer is found to be a little larger than that of bulk BaTiO3, which has been interpreted by the presence of the internal strain induced by the misfit at the interface. This finding is consistent with the lattice parameters of the BaTiO3 thin layer determined by the selected area diffraction pattern. The near-edge structure of the oxygen K edge in BaTiO3 thin layers and in bulk BaTiO3 are simulated by first-principle self-consistent full multiple-scattering calculations. The results of the simulations are in a good agreement with the experimental results. Moreover, the aggregation of oxygen vacancies at the rough BaTiO3/SrTiO3 interface is indicated by the increased [Ti]/[O] element ratio, which dominates the difference of dielectric properties between BaTiO3 layer and bulk materials.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Epitaxial thin films Of various bismuth-layered perovskites SrBi(2)Ta(2)O(9), Bi(4)Ti(3)O(12), BaBi(4)Ti(4)O(15), and Ba(2)Bi(4)Ti(5)O(18) were deposited by pulsed laser deposition onto epitaxial conducting LaNiO(3) or SrRuO(3) electrodes on single crystalline SrTiO(3) substrates with different crystallographic orientations or on top of epitaxial buffer layers on (100) silicon. The conductive perovskite electrodes and the epitaxial ferroelectric films are strongly influenced by the nature of the substrate, and bismuth-layered perovskite ferroelectric films with mixed (100), (110)- and (001)-orientations as well as with uniform (001)-, (116)- and (103)- orientations have been obtained. Structure and morphology investigations performed by X-ray diffraction analysis, scanning probe microscopy, and transmission electron microscopy reveal the different epitaxial relationships between films and substrates. A clear correlation of the crystallographic orientation of the epitaxial films with their ferroelectric properties is illustrated by macroscopic and microscopic measurements of epitaxial bismuth-layered perovskite thin films of different crystallographic orientations.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The relatively high elastic modulus coupled with the presence of toxic vanadium (V) in Ti6Al4 V alloy has long been a concern in orthopaedic applications. To solve the problem, a variety of non-toxic and low modulus beta-titanium (beta-Ti) alloys have been developed. Among the beta-Ti alloy family, the quaternary Ti-Nb-Zr-Ta (TNZT) alloys have received the highest attention as a promising replacement for Ti6Al4 V due to their lower elastic modulus and outstanding long term stability against corrosion in biological environments. However, the inferior wear resistance of TNZT is still a problem that must be resolved before commercialising in the orthopaedic market. In this work, a newly-developed laser surface treatment technique was employed to improve the surface properties of Ti-35.3Nb-7.3Zr-5.7Ta alloy. The surface structure and composition of the laser-treated TNZT surface were examined by grazing incidence x-ray diffraction (GI-XRD) and x-ray photoelectron spectroscopy (XPS). The wear and corrosion resistance were evaluated by pin-on-plate sliding test and anodic polarisation test in Hanks’ solution. The experimental results were compared with the untreated (or base) TNZT material. The research findings showed that the laser surface treatment technique reported in this work can effectively improve the wear and corrosion resistance of TNZT.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This work deals with the optical properties of supported noble metal nanoparticles, which are dominated by the so-called Mie resonance and are strongly dependent on the particles’ morphology. For this reason, characterization and control of the dimension of these systems are desired in order to optimize their applications. Gold and silver nanoparticles have been produced on dielectric supports like quartz glass, sapphire and rutile, by the technique of vapor deposition under ultra-high vacuum conditions. During the preparation, coalescence is observed as an important mechanism of cluster growth. The particles have been studied in situ by optical transmission spectroscopy and ex situ by atomic force microscopy. It is shown that the morphology of the aggregates can be regarded as oblate spheroids. A theoretical treatment of their optical properties, based on the quasistatic approximation, and its combination with results obtained by atomic force microscopy give a detailed characterization of the nanoparticles. This method has been compared with transmission electron microscopy and the results are in excellent agreement. Tailoring of the clusters’ dimensions by irradiation with nanosecond-pulsed laser light has been investigated. Selected particles are heated within the ensemble by excitation of the Mie resonance under irradiation with a tunable laser source. Laser-induced coalescence prevents strongly tailoring of the particle size. Nevertheless, control of the particle shape is possible. Laser-tailored ensembles have been tested as substrates for surface-enhanced Raman spectroscopy (SERS), leading to an improvement of the results. Moreover, they constitute reproducible, robust and tunable SERS-substrates with a high potential for specific applications, in the present case focused on environmental protection. Thereby, these SERS-substrates are ideally suited for routine measurements.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

El vello facial no deseado es un problema común en las mujeres, los tratamientos láser han mostrado efectividad para su manejo. Objetivo: Evaluar los resultados de la depilación láser en cara de las pacientes tratadas a largo plazo (20 sesiones o más ) luego de un seguimiento de 6 meses durante los años 1997 y 2012. Metodología: 55 mujeres que con tipo de piel II a V recibieron 20 o más sesiones de láser con seguimiento mayor a 6 meses posterior al la última sesión. Resultados: la edad promedio fue (32 ± 9,3 años), el 18,2 % presentaban SOP o Hiperandrogenismo el número de sesiones en cara fue de (30,84 ± 12,132), un promedio de disparos de (6,330 ± 7,804), los Kilojulios acumulados tuvieron un promedio de (126,5 ± 161,4) la fluencia promedio fue (18,5 ± 3,2 Julios/cm2), el láser de Alexandrita fue utilizado en el 98% de las pacientes. Se encontró cambios significativos entre el conteo inicial y el final de vello facial (484,9 ± 568.9 (med=300) vs. 103,33± 138,63 (med=60), p<0.001, Test de Wilcoxon). El 32.7% mostraron reducción > 90% (5,5% reducción del 100%). Conclusión : El tratamiento con de depilación con láser mostro una reducción significativa del vello facial, en mujeres mayores de 14 años con un tratamiento a largo plazo (20 sesiones o más), con una tasa de reducción mayor del 90% en 32.7% de las pacientes y un promedio de reducción del grupo de 79,36 ±15,51 %, similar a lo reportado en los diferentes estudios (77%).

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Laser beam spot-welding is widely applied to join sheet metals for automotive components especially for thinsheet components in automotive industries. The spot welds in such metallic structures contribute a lot to the integrated strength and fatigue life for the whole structures and they are responsible for their damage or collapse in some loading cases. In this paper, the 2-D hybrid special finite elements each containing an edge crack are employed to study the fracture behaviors of laser beam spot-welds. Hence the calculation accuracy in the vicinity of crack tips is ensured, and a better description of stress singularity with only one hybrid element surrounding one crack is provided. The numerical modeling for laser beam spot-welds subjected to three typical modes ofloadings including tension-lap, shear-lap and angle-clip can be greatly simplified with the applications of such elements. Three specimens under lap-shear, lap-tension and angle clip are devised and analyzed respectively, and main fracture parameters such as stress intensity factors and the initial direction of crack growth are obtained through tinite element analyses. The computed results ti'om numerical examples demonstrate the validity and versatility of the proposed modeling.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Titanium alloys are widely used in various engineering design application due to its superior material properties. The traditional manufacturing of titanium products is always difficult, time consuming, high material wastage and manufacturing costs. Selective laser melting (SLM), an additive manufacturing technology has widely gained attention due to its capability to produce near net shape components with less production time. In this technical paper,microstructure,chemical composition,tensile properties and hardness are studied for the wrought and additive manufactured SLM cylindrical bar. Microstructure,mechanical properties and hardness were studied in both the longitudinal and transverse directions of the bar to study the effect of orientation. It was found that additive manufactured bar have higher yield strength, ultimate tensile strength and hardness than the wrought bar. For both conventional and SLM test samples, the yield strength, ultimate tensile strength and hardness was found to be high in the transverse direction. The difference in the properties can be attributed to the difference in microstructure as a result of processing conditions. The tensile fracture area was quantified by careful examination of the fracture surfaces in the scanning electron microscope.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This study compared the tensile strength and fracture mechanism of tungsten inert gas (TIG) welds in cylindrical rods of commercially pure titanium (cp Ti) with those of laser welds and intact samples. Thirty dumbbell-shaped samples were developed by using brass rods as patterns. The samples were invested in casings, subjected to thermal cycles, and positioned in a plasma arc welding machine under argon atmosphere and vacuum, and titanium was injected under vacuum/pressure. The samples were X-rayed to detect possible welding flaws and randomly assigned to three groups to test the tensile strength and the fracture mechanism: intact, laser welding, and TIG welding. The tensile test results were investigated using ANOVA, which indicated that the samples were statistically similar. The fracture analysis showed that the cpTi samples subjected to laser welding exhibited brittle fracture and those subjected to TIG welding exhibited mixed brittle/ductile fracture with a predominance of ductile fracture with the presence of microcavities and cleavage areas. Intact samples presented the characteristic straightening in the fracture areas, indicating the ductility of the material.