898 resultados para BISMUTH MOLYBDATE


Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this work, we investigated the oxygen permeation properties of barium bismuth iron oxide within the family of [Ba2−3xBi3x−1][Fe2xBi1−2x]O2+3x/2 for x = 0.17–0.60. The structure changed progressively from cubic to tetragonal and then to hexagonal as function of x in accordance with the different relative amounts of bismuth on A-site and B-site of ABO3−δ perovskite lattices. We found that the oxygen flux and electrical conductivity correlated strongly, and it was prevalent for the cubic structure (x = 0.33–0.40) which conferred the highest oxygen flux of 0.59 ml min−1 cm−2 at 950 °C for a disk membrane x = 0.33 with a thickness of 1.2 mm. By reducing the thickness of the disk membrane to 0.8 mm, the oxygen flux increased to 0.77 ml min−1 cm−2, suggesting both surface kinetics and ion diffusion controlled oxygen flux, though the former was more prominent at higher temperatures. For disk membranes x = 0.45–0.60, the perovskite structure changed to tetragonal and hexagonal, and the oxygen flux was insignificant below 900 °C, clearly indicating electron conduction properties only. However, for two compositions with relatively high bismuth content, e.g. x = 0.55 and 0.60, there was a sudden and significant rise of oxygen permeability above 900 °C, by more than one order of magnitude. These materials changed conduction behavior from metallic to semiconductor at around 900 °C. These results suggest the advent of mixed ionic electronic conducting properties caused by the structure transition as bismuth ions changed their valence states to compensate for the oxygen vacancies formed within the perovskite lattices.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A simple and rapid flow-injection spectrophotometric method is reported for the determination of dipyrone in pharmaceutical formulations. The method is based on the reaction of dipyrone with ammonium molybdate in acidic medium to produce blue molybdenum, which was detected spectrophotometrically at 620 nm. The analyte was determined in a single-line flow system. The calibration curve obtained was linear in the range of 5x10(-4) to 8x10(-3) mol L-1 for dipyrone concentration and the precision ( s r =1.7%) was satisfactory. The method proved to be selective and adequately sensitive. Application of the method to the analysis of pharmaceutical samples resulted in excellent accuracy; the percent mean recoveries were in the range 95.3%-101% and relative errors less than 5.0% for five pharmaceutical formulations were found.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A strong greenish-light photoluminescence (PL) emission was measured at room temperature for disordered and ordered powders of CaMoO4 prepared by the polymeric precursor method. The structural evolution from disordered to ordered powders was accompanied by XRD. Raman spectroscopy, and TEM imagery. High-level quantum mechanical calculations in the density functional framework were used to interpret the formation of the structural defects of disorder powders in terms of band diagram and density of states. Complex cluster vacancies [MoO3 center dot V-O(z)] and [CaO7 center dot V-O(z)] (where V-O(z) = V-O(X), V-O(center dot), V-O(center dot center dot)) were suggested to be responsible to the appearance of new states shallow and deeply inserted in the band gap. These defects give rise to the PL in disordered powders. The natural PL emission of ordered CaMoO4 was attributed to an intrinsic slight distortion of the [MoO4] tetrahedral in the short range.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effect of film orientation on piezoelectric and ferroelectric properties of bismuth layered compounds deposited on platinum coated silicon substrates was investigated. Piezo-force microscopy was used to probe the local piezoelectric properties of Bi(4)Ti(3)O(12), CaBi(4)Ti(4)O(15) and SrBi(4)Ti(4)O(15) films. Our measurements on individual grains clearly reveal that the local piezoelectric properties are determined by the polarization state of the grain. A piezoelectric coefficient of 65 pm/V was attained after poling in a grain with a polar axis very close to the normal direction. The piezoelectric coefficient and the remanent polarization were larger for a-b axes oriented than for c-axis-oriented films. (c) 2007 Elsevier B.V All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Lanthanum-modified bismuth titanate, Bi4-xLaxTi3O12 (BLT), with x ranging from 0 to 0.75 was grown on Pt/Ti/SiO2/Si substrates using a polymeric precursor solution and spin-coating method. The dielectric constant of highly doped bismuth titanate was equal to 148 while dielectric losses remained low (tan delta = 0.0018), and the films showed well-saturated polarization-electric field curves (2P(r) = 40.6 muC/cm(2) and V-c = 0.99 V). The leakage current densities improve for the lanthanum-doped system. For five-layered BLT films with x = 0.75, a charge storage density of 35 fC/mum(2) and a thickness of 320 nm were found. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Crystalline molybdate thin films were prepared by the complex polymerization method. The AMoO(4) (A = Ca, Sr, Ba) films were deposited onto Si wafers by the spinning technique. The Mo-O bond in the AMoO(4) structure was confirmed by FTIR spectra. X-ray diffraction revealed the presence of crystalline scheelite-type phase. The mass, size, and basicity of A(2+) cations was found to be dependent on the intrinsic characteristics of the materials. The grain size increased in the following order: CaMoO4 < SrMoO4 < BaMoO4. The emission band wavelength was detected at around 576 nm. Our findings suggest that the material's morphology and photoluminescence were both affected by the variations in cations (Ca, Sr, or Ba) and in the thermal treatment.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Foram preparados os ditizonatos de Hg (I), Ag (I) e Bi (III). Termogravimetria (TG), termogravimetria derivada (DTG), calorimetria exploratória diferencial (DSC), difratometria de raios X pelo método do pó e análise elementar foram usados para caracterizar e para estudar a estabilidade térmica e a decomposição térmica da ditizona e destes ditizonatos.