Thin films were prepared using glass precursors obtained in the ternary system NaPO(3)-BaF(2)-WO(3) and the binary system NaPO(3)-WO(3) with high concentrations of WO(3) (above 40% molar). Vitreous samples have been used as a target to prepare thin films. Such films were deposited using the electron beam evaporation method onto soda-lime glass substrates. Several structural characterizations were performed by Raman spectroscopy and X-ray Absorption Near Edge Spectroscopy (XANES) at the tungsten L(I) and L(III) absorption edges. XANES investigations showed that tungsten atoms are only sixfold coordinated (octahedral WO(6)) and that these films are free of tungstate tetrahedral units (WO(4)). In addition, Raman spectroscopy allowed identifying a break in the linear phosphate chains as the amount of WO(3) increases and the formation of P-O-W bonds in the films network indicating the intermediary behavior of WO(6) octahedra in the film network. Based on XANES data, we suggested a new attribution of several Raman absorption bands which allowed identifying the presence of W-O and W=O terminal bonds and a progressive apparition of W-O-W bridging bonds for the most WO(3) concentrated samples (above 40% molar) attributed to the formation of WO(6) clusters. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The use of internal standardization for simultaneous atomic absorption spectrometry (SIMAAS) was investigated for Cd and Pb determination in whole blood. The comparison of thermochemical and physicochemical parameters allowed the selection of Ag, Bi, and Tl as internal standard candidates. Correlation graphs, plotted from the normalized absorbance signals (n = 20) of internal standard (axis y) versus analyte ( axis x), precision and accuracy were used to select Ag as the most appropriate internal standard. Blood samples were diluted (1 + 9) with 0.11% (m/v) Triton X-100 + 1.1% (v/v) HNO3 + 0.28% (m/v) NH4H2PO4 + 10 mug L-1 Ag+. Pyrolysis and atomization temperatures for the optimized heating program were 550 and 1700 degreesC, respectively. Characteristic masses based on integrated absorbance were 1.68 +/- 0.01 pg for Cd and 30.3 +/- 0.1 pg for Pb. The detection limits (DL) were 0.095 +/- 0.001 mug L-1 and 0.86 +/- 0.01 mug L-1 for Cd and Pb, respectively. The mean RSD for all determinations was the same for Cd (13 +/- 9%) with or without Ag as internal standard ( IS). on the other hand, the use of Ag as IS improved the RSD for Pb from 3.6 +/- 4.0% to 2.2 +/- 2.0%. An effective contribution of the internal standard Ag was verified in the recoveries of spiked samples (0.5 mug L-1 Cd2+ and 5.0 mug L-1 Pb2+). The mean recoveries were 81 +/- 8% and 91 +/- 4% for Cd, and 80 +/- 11% and 93 +/- 6% for Pb without and with IS correction, respectively. This is the first application of IS for a simultaneous determination by SIMAAS.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Iridium-, Ru-, and W-coated platforms were prepared by thermal treatment of the transversely heated graphite atomizer and investigated for the simultaneous determination of As, Bi, Pb, Sb, and Se in tap water by electrothermal atomic absorption spectrometry. The maximum pyrolysis temperature for As and Bi increased in a modifier sequence W < Ru < Ir. For Pb, Sb, and Se, this sequence was W < Ru, It. Calculated characteristic masses in the presence of It, Ru, and W were 35, 33, and 35 pg for As; 63, 51, and 52 pg for Bi; 50, 32, and 34 pg for Pb; 40, 35, and 31 pg for Sb; and 39, 39, and 93 pg for Se, respectively. Ruthenium was elected as the optimum modifier.Repeatability of the measurements was typically < 6%. Recoveries of As, Bi, Pb, Sb, and Se added to tap water samples varied from 79 to 109%. Accuracy was also checked by analysis of five certified reference materials (CRMs) from the National Institute of Standards and Technology (NIST1640 - Trace Elements in Natural Water; NIST 1643d Trace Elements in Water) and High Purity Standards (Trace Metals in Drinking Water Standards, lots #812708, #591107, and #710710). A paired t-test showed that the results for the CRMs were in agreement at the 95% confidence level with the certified values. The graphite tube lifetime was about 650 firings. multi-element determination is particularly challenging due to the necessity of carefully optimizing compromise conditions.Based on the considerations listed above, the aim of this paper was to evaluate the behavior of Ir, Ru, and W as permanent modifiers for the simultaneous determination of As, Bi, Pb, Sb, and Se. The performance of the proposed procedure was also verified after the ETAAS analysis of tap waters and reference materials.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

X-ray absorption spectroscopy was used to study the local environment of tungsten atoms in NaPO3-BaF2,-WO3 glasses and the results were compared with crystalline references Na2WO4 and WO3. XANES measurements at the W-L-1 edge allowed to determine a distorted octahedral environment of tungsten atoms in these glasses similar to the local order of tungsten in monoclinic WO3. Extended X-ray absorption fine structure (EXAFS) has been used as a local probe to monitor the effect of WO3 concentration on the tungsten environment. Based on an analysis of the EXAFS data, we proposed a three-shell model of oxygen atoms around tungsten as in monoclinic WO3. With increasing WO3 concentration, it was found that R-2 decreases from 1.96 to 1.92 angstrom whereas R-3 increases from 2.07 to 2.12 angstrom. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Bismuth was evaluated as an internal standard for the direct determination of Pb in vinegar by graphite furnace atomic absorption spectrometry using Ru as a permanent modifier with co-injection of Pd/Mg(NO3)(2). The correlation coefficient of the graph plotted from the non-nalized absorbance signals of Bi versus Pb was r=0.989. Matrix effects were evaluated by analyzing the slope ratios between the analytical curve, and analytical curves obtained from Pb additions in red and white wine vinegar obtained from reference solutions prepared in 0.2% (v/v) HNO3, samples. The calculated ratios were around 1.04 and 1.02 for analytical curves established applying an internal standard and 1.3 and 1.5 for analvtical curves without. Analytical curves in the 2.5-15 pg L-1 Pb concentration interval were established using the ratio Pb absorbance to Bi absorbance versus analvte concentration, and typical linear correlations of r=0.999 were obtained. The proposed method was applied for direct determination of Pb in 18 commercial vinegar samples and the Pb concentration varied from 2.6 to 31 pg L-1. Results were in agreement at a 95% confidence level (paired t-test) with those obtained for digested samples. Recoveries of Pb added to vinegars varied from 96 to 108% with and from 72 to 86% without an internal standard. Two water standard reference materials diluted in vinegar sample were also analyzed and results were in agreement with certified values at a 95% confidence level. The characteristic mass was 40 pg Pb and the useful lifetime of the tube was around 1600 firings. The limit of detection was 0.3 mu g L-1 and the relative standard deviation was <= 3.8% and <= 8.3% (n = 12) for a sample containing, 10 mu L-1 Pb with and without internal standard, respectively. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The local and medium-range structures of siloxane-POE hybrids doped with Fe(III) ions and prepared by the sol-gel process were investigated by X-ray absorption near-edge structure (XANES)/extended X-ray absorption fine structure (EXAFS) and small-angle X-ray scattering (SAXS), respectively. The experimental results show that the structure of these composites depends on the doping level. EXAFS data reveal that, for low doping levels ([O]/[Fe] > 40, oxygens being of the ether-type of the POE chains), Fe(III) ions are surrounded essentially by a shell of chlorine atoms, suggesting the formation of FeCl4- anions. At high doping levels ([O]/[Fe] < 20), Fe(III) ions interacts mainly with oxygen atoms and form FeOx species. The relative proportion of FeOx species increases with iron concentration, this result being consistent with the results of SAXS measurements showing that increasing iron doping induces the formation of iron-rich nanodomains embedded in the polymer matrix.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The electronic structure of Pb1-xLaxTiO3 (PLT) compounds for x ranging from 0 to 30 at. % of La is investigated by means of soft x-ray absorption near edge structure (XANES) at the Ti L-3,L-2 and O K edges. The greatest modification in the structure of the Ti 2p XANES spectra of the PLT compounds is observed in the region of the high energy peak of the L-3 edge (e(g) states), which exhibits a splitting in the undoped sample. As the amount of lanthanum increases, this splitting becomes less pronounced. This modification is interpreted as a decrease in the degree of disorder of titanium atoms, which is correlated to the substitution of Pb by La atoms. The structural changes observed at the low energy peaks of the O K-edge XANES spectra of the PLT compounds may be interpreted in terms of hybridization between O 2p, Ti 3d, and Pb 6p orbitals. A decrease in the degree of hybridization observed as Pb atoms are replaced by La atoms may be related to the differences in the ferroelectric properties observed between x=0.0 and x=0.30 compounds. (c) 2006 American Institute of Physics.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Transparent glasses were synthesized in the NaPO3-BaF2 WO3 tertiary system and several structural characterizations were performed by X-ray absorption spectroscopy (XANES) at the tungsten L-I and L-III absorption edges and by Raman spectroscopy. Special attention was paid to the coordination state of tungsten atoms in the vitreous network.XANES investigations showed that tungsten atoms are only six-fold coordinated (octahedra WO6) and that these glasses are free of tungstate tetrahedra (WO4).In addition, Raman spectroscopy allowed to identify a break in the linear phosphate chains as the amount of WO3 increases and the formation of P-O-W bonds in the vitreous network indicating the modifier behavior of WO6 octahedra in the glass network. Based on XANES data, we suggested a new attribution of several Raman absorption bands which allowed to identify the presence of W-O- and W=O terminal bonds and a progressive apparition of W-O-W bridging bonds for the most WO3 concentrated samples (&GE; 30% molar) due to the formation of WO6 clusters. © 2004 Elsevier B.V. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Different kinds of modifiers and coatings on the integrated platform of transversely heated graphite atomizer (THGA) have been tested for the simultaneous determination of two group of elements: the first, the more volatile, formed by arsenic, bismuth, lead, antimony and selenium; the second, the less volatile, formed by cobalt, chromium, cupper, iron and manganese in milk by electrothermal atomic absorption spectrometry. Different Rh-modifiers were studied, such as Rh-coated platforms (Rh), carbide plus rhodium coated platforms (W-Rh, Zr-Rh), carbide-coated platforms (W and Zr) with co-injection of RhCl3, solutions and uncoated platforms with injection of solutions of Pd(NO3)(2), Mg(NO3)(2), and RhCl3. Milk samples were diluted 1:10 in 1.0% HNO3 and injected into the tube. The mass of modifier deposited and co-injected in the tube and the use of end capped tubes were also evaluated in order to improve the electrothermal behavior of analytes. Integrated platform pretreated with W plus co-injection RhCl3 for first group and pretreated with W-Rh for second group were elected. For 20 mu L injected samples the analytical curves in the 5.0-20.0 mu g L-1 concentration range have good linear correlation coefficients (r > 0.998). Relative standard deviations (n = 12) are < 6% and the calculated characteristic masses are between 5 pg and 62 pg.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The combination of x-ray absorption spectroscopy (XAS) with UV-Vis and Raman spectroscopies or with Differential Scanning Calorimetry (DSC) has been recently carried out on the D44 beamline of DCI-LURE. The different set-ups used to perform such combinations are described and examples of combined investigations belonging to different field of materials science (coordination chemistry, sol-gel and catalysis) are presented. © Physica Scripta 2005.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Different modifiers (IrCl3, W+IrCl3, Zr+IrCl 3) and coatings (Ir, W-Ir, Zr-Ir) were evaluated for the simultaneous determination of arsenic, bismuth, lead, antimony, and selenium in milk by graphite furnace atomic absorption spectrometry using the 'end-capped' transversely heated graphite atomizer (THGA). Integrated platform, pretreated with Zr-Ir as permanent modifier, was elected as the optimum surface modification resulting in up to 250 firings. Two additional recoatings were possible without significant changes in the analytical performance (750 firings). For 20 μL of matrix-matched standard solutions using diluted (1:10) milk samples, typical correlation coefficients between integrated absorbance and analyte concentration (5.00-20.0 μg/L) was always better than 0.999. The levels of the analytes found in commercial milk samples were lower than the limit of detection: 2.9 μg/L As, 2.9 μg/L Bi, 1.8 μg/L Pb, 1.9 μg/L Sb, and 2.5 μg/L Se. Recoveries were found within the following intervals: 88-114% for As, 89-118% for Bi, 89-113% for Pb, 91-115% for Sb, and 92-115% for Se. The relative standard deviations (n = 12) were ≤2% (As), ≤ 5% (Bi), ≤ 1.4% (Pb), ≤ 3% (Sb), and 5% (Se), and the respective calculated characteristic masses were 54 pg As, 55 pg Bi, 40 pg Pb, 56 pg Sb, and 51 pg Se.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Lead-free solid solutions (1-x)Bi0.5Na0.5TiO 3 (BNT)-xBaZr0.25Ti0.75O3 (BZT) (x=0, 0.01, 0.03, 0.05, and 0.07) were prepared by the solid state reaction method. X-ray diffraction (XRD) and Rietveld refinement analyses of 1-x(BNT)-x(BZT) solid solution ceramic were employed to study the structure of these systems. A morphotropic phase boundary (MPB) between rhombohedral and cubic structures occured at the composition x=0.05. Raman spectroscopy exhibited a splitting of the (TO3) mode at x=0.05 and confirmed the presence of MPB region. Scanning electron microcopy (SEM) images showed a change in the grain shape with the increase of BZT into the BNT matrix lattice. The temperature dependent dielectric study showed a gradual increase in dielectric constant up to x=0.05 and then decrease with further increase in BZT content. Maximum coercive field, remanent polarization and high piezoelectric constant were observed at x=0.05. Both the structural and electrical properties show that the solid solution has an MPB around x=0.05. © 2012 Elsevier Ltd and Techna Group S.r.l.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

This paper reports on the structural characterization of Pb 1-xLaxZr0.40Ti0.60O3 (PLZT) ferroelectric ceramic compositions prepared by the conventional solid state reaction method. X-ray absorption spectroscopy (XAS) and Raman spectroscopy were used to probe the local structure of PLZT samples that exhibits a normal and relaxor ferroelectric behavior. From the Zr K-edge and Pb LIII-edge EXAFS spectra, a considerable dissymmetry of Zr and Pb sites was observed in all samples, including those showing a long-range order cubic symmetry and a relaxor behavior. The Raman spectroscopy results confirmed the existence of a local disorder in all PLZT samples through the observation of Raman active vibrational modes. The variation in the intensity of the E(TO 3) mode in the PLZT relaxor samples indicates that the process of correlation between nanodomains stabilizes at temperatures lower than T m. © 2013 Elsevier B.V. All rights reserved.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)