Huntington’s disease (HD) is a fatal autosomal dominant neurodegenerative disease. HD has no cure, and patients pass away 10-20 years after the onset of symptoms. The causal mutation for HD is a trinucleotide repeat expansion in exon 1 of the huntingtin gene that leads to a polyglutamine (polyQ) repeat expansion in the N-terminal region of the huntingtin protein. Interestingly, there is a threshold of 37 polyQ repeats under which little or no disease exists; and above which, patients invariably show symptoms of HD. The huntingtin protein is a 350 kDa protein with unclear function. As the polyQ stretch expands, its propensity to aggregate increases with polyQ length. Models for polyQ toxicity include formation of aggregates that recruit and sequester essential cellular proteins, or altered function producing improper interactions between mutant huntingtin and other proteins. In both models, soluble expanded polyQ may be an intermediate state that can be targeted by potential therapeutics.

In the first study described herein, the conformation of soluble, expanded polyQ was determined to be linear and extended using equilibrium gel filtration and small-angle X-ray scattering. While attempts to purify and crystallize domains of the huntingtin protein were unsuccessful, the aggregation of huntingtin exon 1 was investigated using other biochemical techniques including dynamic light scattering, turbidity analysis, Congo red staining, and thioflavin T fluorescence. Chapter 4 describes crystallization experiments sent to the International Space Station and determination of the X-ray crystal structure of the anti-polyQ Fab MW1. In the final study, multimeric fibronectin type III (FN3) domain proteins were engineered to bind with high avidity to expanded polyQ tracts in mutant huntingtin exon 1. Surface plasmon resonance was used to observe binding of monomeric and multimeric FN3 proteins with huntingtin.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Entre os polímeros considerados promissores para a remoção seletiva de CO2, destacam-se aqueles que contêm os grupos glicol etilênico (EG). Nesta dissertação, foram obtidos filmes a partir de dispersões aquosas de poliuretano (PU), sintetizadas em trabalho anterior, à base de poli(glicol propilênico) (PPG), copolímero em bloco à base de poli(glicol etilênico) (PEG) e PPG (EG-b-PG), ácido dimetilolpropiônico (DMPA), diisocianato de isoforona (IPDI) e etilenodiamina (EDA). PPG, EG-b-PG e DMPA formaram as regiões flexíveis nas proporções de: PPG 100% e 0% EG-b-PG, PPG 75% e 25% EG-b-PG, PPG 50% e 50% EG-b-PG e PPG 25% e 75% EG-b-PG em termos de equivalentes-gramas. A influência da quantidade dos segmentos de PEG foi avaliada por ensaios de permeação com os gases CO2, CH4 e N2. Os filmes obtidos das dispersões foram caracterizados por espectrometria de infravermelho com transformadas de Fourier (FTIR), análise termogravimétrica (TGA), difração de raios x (DRX) e espalhamento de raios X a baixo ângulo (SAXS). Espectros de FTIR mostraram que os segmentos de EG influenciaram a frequência da banda de carbonila. Curvas de perda de massa (TG) mostraram perfis semelhantes de degradação, enquanto que as curvas derivadas apresentaram diferenças. DRX e SAXS mostraram que os segmentos de PEG promoveram uma maior ordenação na estrutura da membrana. Testes de permeação de gases mostraram que o aumento do teor de PEG aumentou o valor da permeabilidade para o CO2, indicando que os segmentos de PEG interagiram favoravelmente com este gás. Em relação ao CH4 e N2, houve uma diminuição na permeabilidade quando comparados com os valores encontrados para o CO2, sendo atribuído a perda de mobilidade segmental. Em termos de seletividade, para o par CO2/CH4 foi obtido um valor médio de 61,7 para a membrana contendo o maior teor de PEG, e o par CO2/N2 um valor médio de 121,5, sendo superior aos valores encontrados na literatura, tornando o material promissor

Relevância:

100.00% 100.00%

Publicador:

Resumo:

用磁控溅射法分别制备了以Mo膜层和Si膜层为顶层的Mo/Si多层膜系列,利用小角X射线衍射确定了各多层膜的周期厚度。以不同周期数的Mo/Si多层膜的新鲜表面近似等同于同一多层膜的内界面,通过原子力显微镜研究了多层膜界面粗糙度随膜层数的变化规律。并在国家同步辐射实验室测量了各多层膜的软X射线反射率。研究表明:随着膜层数的增加,Mo膜层和Si膜层的界面粗糙度先减小后增加然后再减小,多层膜的峰值反射率先增加后减小。

Relevância:

100.00% 100.00%

Publicador:

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A facile, efficient way to fabricate macroscopic soft colloidal crystals with fiber symmetry by drying a latex dispersion in a tube is presented. A transparent, stable colloidal crystal was obtained from a 25 wt % latex dispersion by complete water evaporation for 4 days. The centimeter-long sample was investigated by means of synchrotron small-angle X-ray diffraction (SAXD). Analysis of a large number of distinct Bragg peaks reveals that uniaxially oriented colloidal crystals with face-centered cubic lattice structure were formed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The microstructure and mechanical properties of beta-nucleated iPP before and after being annealed at different temperatures (90-160 degrees C) have been analyzed, Annealing induced different degrees of variation in fracture toughness of beta-nucleated iPP samples. namely, slight enhancement at relatively low annealing temperatures (< 110 degrees C) and great improvement at moderate temperatures (120-130 degrees C), whereas dramatic deterioration at relatively high temperatures ( > 140 degrees C) has been observed. The variation of fracture toughness of beta-nucleated iPP is observed to be dependent on the content of beta-NA. Experiments, including scanning electronic microscope (SEM), wide-angle X-ray diffraction (WAXD), differential scanning calorimetry (DSC), small-angle X-ray scattering (SAXS), and dynamic mechanical analysis (DMA), are performed to study the variations of microstructures as well as the toughening mechanism of the beta-nucleated iPP after being annealed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Poly(epsilon-caprolactone)-based segmented polyurethanes (PCLUs) were prepared from poly(epsilon-caprolactone) diol, diisocyanates (DI), and 1,4-butanediol. The DIs used were 4,4'-diphenylmethane diisocyanate (MDI), 2,4-toluenediisocyanate (TDI), iso-phorone diisocyanate (IPDI), and hexamethylene diisocyanate (HDI). Differential scanning calorimetry, small-angle X-ray scattering, and dynamic mechanical analysis were employed to characterize the two-phase structures of all PCLUs. It was found that HDI- and MDI-based PCLUs had higher degree of microphase separation than did IPDI- and TDI-based PCLUs, which was primarily due to the crystallization of HDI- and MDI-based hard-segments. As a result, the HDI-based PCLU exhibited the highest recovery force up to 6 MPa and slowest stress relaxation with increasing temperature. Besides, it was found that the partial damage in hard-segment domains during the sample deformation was responsible for the incomplete shape-recovery of PCLUs after the first deformation, but the damage did not develop during the subsequent deformation.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The crystallization kinetics and the development of lamellar structure during the isothermal crystallization of poly (epsilon-caprolactone) (PCL) were investigated by means of differential scanning calorimetry (DSC) and real-time synchrotron small angle X-ray scattering (SR-SAXS) techniques, respectively. The Avrami analysis was performed to obtain the kinetics parameters. The value of Avrami index, n, is about 3, demonstrating a three-dimensional spherulitic growth on heterogeneous nuclei in the process of isothermal crystallization. The activation energy and the surface free energy of chain folding for isothermal crystallization were determined according to the Arrhenius equation and Hoffman-Lauritzen theory, respectively. In the process of nonisothermal crystallization of PCL, the value of Avrami index, n, is about 4, which demonstrates a three-dimensional spherulitic growth on homogeneous nuclei. In addition, lamellar parameters were obtained from the analysis of SR-SAXS data.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Differential scanning calorimeter (DSC), wide-angle X-ray diffraction (WAXD), small-angle X-ray scattering (SAXS), and density techniques have been used to investigate the structural parameters of the solid state of Nylon 11 annealed at different temperatures. The equilibrium heat of fusion Delta H-m(0) and equilibrium melting temperature T-m(0) were estimated to be 189.05 J g(-1) and 202.85 degrees C respectively by using the Hoffman-Weeks approach. The degree of crystallinity (W-c,W-x) ranged approximately 24-42% was calculated by WAXD and compared with those by calorimetry (W-c,W-h) and density (W-c,W-d) measurements. The radius of gyration R-g, crystalline thickness L-c, noncrystalline thickness L-a, long period L, semiaxes of the particles (a, b), electron-density difference between the crystalline and noncrystalline regions eta(c) - eta(a), and the invariant Q increased with increasing annealing temperature. The analysis of the SAXS data was based upon the particle characteristic function and the one-dimensional electron-density correlation function. An interphase region existed between the crystalline and noncrystalline region with a clear dimension of about 2 nm for semicrystalline Nylon 11. Instead of the traditional two-phase model, a three-phase model has been proposed to explain these results by means of SAXS.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The miscibility, spherulite growth kinetics, and morphology of binary blends of poly(beta-hydroxybutyrate) (PHB) and poly(methyl acrylate) (PMA) were studied with differential scanning calorimetry, optical microscopy, and small-angle X-ray scattering (SAXS). As the PMA content increases in the blends, the glass-transition temperature and cold-crystallization temperature increase, but the melting point decreases. The interaction parameter between PHB and PMA, obtained from an analysis of the equilibrium-melting-point depression, is -0.074. The presence of an amorphous PMA component results in a reduction in the rate of spherulite growth of PRE. The radial growth rates of spherulites were analyzed with the Lauritzen-Hoffman model. The spherulites of PHB were volume-filled, indicating the inclusion of PMA within the spherulites. The long period obtained from SAXS increases with increased PMA content, implying that the amorphous PMA is entrapped in the interlamellar region of PHB during the crystallization process of PHB. All the results presented show that PHB and PMA are miscible in the melt. (C) 2000 John Wiley & Sons, Inc.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

After isothermal crystallization of the amorphous poly(ether ether ketone), double endothermic behaviour can be found through differential scanning calorimetry experiments. During the heating scan of semicrystalline PEEK, a metastable melt, which comes from the melt of the thinner lamellar crystal populations, can be obtained between these two endotherms. The metastable melt can recrystallize immediately just above the lower melting temperature and form slightly thicker lamellae than the original ones. The thickness and the perfection depend upon the crystallization time and the crystallization temperature. By comparing the TEM morphological observations of the samples before and after partial melting, it can be shown that lamellar crystals, having different thermodynamic stability, form during isothermal crystallization. After partial melting, only the type of lamellar crystal exhibiting the higher thermodynamic stability remains. Wide angle X-ray diffraction measurements shows a slightly change in the crystallinity of the samples before and after the partial melting. Small angle X-ray scattering results exhibit a change in the long period of the lamellar crystals before and after the partial melting process. The crystallization kinetics of the metastable melt can be determined by means of differential scanning calorimetry. The kinetic analysis showed that the isothermal crystallization of the metastable PEEK melt proceeds with an Avrami exponent of n = 1.0 similar to 1.4, reflecting that probably one-dimensional or an irregular line growth of the crystal occurred between the existing main lamellae with heterogeneous nucleation. (C) 1998 Elsevier Science Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The positive temperature coefficient (PTC) and negative temperature coefficient (NTC) effect of carbon black (CB) filled low density polyethylene (LDPE) composites was studied using electrical resistivity spectra, DSC, tensile mechanical analysis (TMA) and small-angle X-ray scattering (SAXS) techniques. The three LDPEs used have a similar crystallinity and different melting index (MI). The experimental results indicate that the CB has no significant effect on the crystallinity and the long spacing of crystalline domains of LDPE. Based upon the TMA and dynamic elastic modulus spectra, it can be concluded that the PTC effect is related to the thermal expansion of the polymer matrix, and the NTC effect is caused by a decrease of the elastic modulus of the polymer at high temperatures. The NTC effect can be reduced by enhancing either the elastic modulus or the interaction between carbon black and matrix. (C) 1997 Elsevier Science Ltd.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The polycrystalline powder of para- and meta-dimethyl ester of pyromellitic acid (PMDE) have been prepared by fractional crystallization, and their crystal structures have been determined by Wide-Angle X-ray Diffraction (WAXD). Both p-PMDE and m-PMDE was found to be orthorhombic crystal system, and their unit cell parameters a = 0.840 nm, b = 0.707 nm, c = 1.136 nm and a = 1.032 nm; b = 0.835 nm, c = 0.714 nm, respectively. Space group all belongs to P-mmm. p-PMDE has two molecules per unit cell with crystal density 1.388 g . cm(-3), while m-PMDE has two molecules per unit cell with crystal density 1.522 g . cm(-3). Indices of crystal diffraction peaks are also detailed in the present work. The difference in crystal structures between p-PMDE and m-PMDE has thus been used to explain the curing behavior of isomerically pyromellitic dianhydride-based poly(amic ester)s.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The polycrystalline powder of the cyclic tetramer based on bisphenol A and o-phthaloyldichloride has been prepared by recrystallization from nitrobenzene and its crystal structure has been determined by Wide-Angle X-ray Diffraction (WAXD). The unit cell is orthorhombic and its dimensions a = 0.967 6 nm, b = 0.869 9 nm, c = 2.085 9 nm, Space group belongs to Pmmm, With two tetramers per unit cell,the crystal density is 1.36 g . cm(-3), Indices of crystal diffraction peaks are also detailed in the present work.