985 resultados para silicate-based ceramics
Resumo:
Transparent glasses in the system (1−x)Li2B4O7–xBi2WO6 (0≤x≤0.35) were prepared via melt quenching technique. Differential thermal analysis was employed to characterize the as-quenched glasses. Glass-ceramics with high optical transparency were obtained by controlled heat-treatment of the glasses at 720 K for 6 h. The amorphous nature of the as-quenched glass and crystallinity of glass-ceramics were confirmed by X-ray powder diffraction studies. High resolution transmission electron microscopy (HRTEM) shows the presence of nearly spherical nanocrystallites of Bi2WO6 in Li2B4O7 glass matrix. Capacitance and dielectric loss measurements were carried out as a function of temperature (300–870 K) in the frequency range 100 Hz–40 MHz. Impedance spectroscopy employed to rationalize the electrical behavior of glasses and glass-ceramics suggest the coexistence of electronic and ionic conduction in these materials. The thermal activation energies for the electronic conduction and ionic conduction were also estimated based on the Arrhenius plots.
Resumo:
The objective of this paper is to discuss the results of the ballistic testing of spark plasma sintered TiB2-Ti based functionally graded materials (FGMs) with an aim to assess their performance in defeating small-calibre armor piercing projectiles. We studied the efficacy of FGM design and compared its ballistic properties with those of TiB2-based composites as well as other competing ceramic armors. The ballistic properties are critically analyzed in terms of depth of penetration, ballistic efficiency, fractographs of fractured surfaces as well as quantification of the shattered ceramic fragments. It was found that all the investigated ceramic compositions exhibit ballistic efficiency (eta) of 5.1 -5.9. We also found that by increasing the thickness of FGM from 5 mm to 7.8 mm, the ballistic property of the composite degraded. Also, the strength of the ceramic compositions studied is sufficient to completely fracture the nose of the pointed projectile used. Analysis of the ceramic fragments (2 mu m-10 mm) showed that harder the ceramic, coarser were the fragments formed. On comparing the results with available armor systems, it has been concluded that TiB2 based composites can show better ballistic properties, except B4C. SEM analysis of the fragments obtained after testing with FGM showed formation of cleavage steps as well as presence of intergranular cracks, indicating that the FGM fractured by mixed mode of failure. It can be concluded that the FGM developed has lower ballistic properties compared to its monolith TiB2-20 wt.% Ti.
Resumo:
Giant grained (42 mu m) translucent Ba5Li2Ti2Nb8O30 ceramic was fabricated by conventional sintering technique using the powders obtained via solid state reaction route. These samples were confirmed to possess tetragonal tungsten bronze structure (P4bm) at room temperature. The scanning electron microscopy established the average grain size to be close to 20 mu m. The photoluminescence studies carried out on these ceramics indicated sharp emission bands around 433 and 578 nm at an excitation wavelength of 350 nm which were attributed to band-edge emission as the band gap was 2.76 eV determined by Kubelka-Munk function. The dielectric properties of these ceramics were studied over wide frequency range (100-1 MHz) at room temperature. The decrease in dielectric constant with frequency could be explained on the basis of Koops theory. The dielectric constant and the loss were found to decrease with increasing frequency. The Curie temperature was confirmed to be similar to 370 A degrees C based on the dielectric anomaly observed when these measurements were carried out over a temperature range of 30-500 A degrees C. This shows a deviation from Curie-Weiss behaviour and hence an indicator of the occurrence of disordering in the system, the gamma = 1.23 which confirms the diffuse ferroelectric transition. These ceramics at room temperature exhibited P-E hysteresis loops, though not well saturated akin to that of their single crystalline counterparts. These are the suitable properties for ferroelectric random access memory applications.
Resumo:
One of the desired properties for any new biomaterial composition is its long-term stability in a suitable animal model and such property cannot be appropriately assessed by performing short-term implantation studies. While hydroxyapatite (HA) or bioglass coated metallic biomaterials are being investigated for in vivo biocompatibility properties, such study is not extensively being pursued for bulk glass ceramics. In view of their inherent brittle nature, the implant stability as well as impact of long-term release of metallic ions on bone regeneration have been a major concern. In this perspective, the present article reports the results of the in vivo implantation experiments carried out using 100% strontium (Sr)-substituted glass ceramics with the nominal composition of 4.5 SiO2-3Al(2)O(3)-1.5P(2)O(5)-3SrO-2SrF(2) for 26 weeks in cylindrical bone defects in rabbit model. The combination of histological and micro-computed tomography analysis provided a qualitative and quantitative understanding of the bone regeneration around the glass ceramic implants in comparison to the highly bioactive HA bioglass implants (control). The sequential polychrome labeling of bone during in vivo osseointegration using three fluorochromes followed by fluorescence microscopy observation confirmed homogeneous bone formation around the test implants. The results of the present study unequivocally confirm the long-term implant stability as well as osteoconductive property of 100% Sr-substituted glass ceramics, which is comparable to that of a known bioactive implant, that is, HA-based bioglass. (c) 2014 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater, 103B: 1168-1179, 2015.
Designing Novel Sulphate-based Ceramic Materials as Insertion Host Compounds for Secondary Batteries
Resumo:
Rechargeable batteries have propelled the wireless revolution and automobiles market over the past 25 years. Developing better batteries with improved energy density demands unveiling of new cathode ceramic materials with suitable diffusion channels and open framework structure. In this pursuit of achieving higher energy density, one approach is to realize enhanced redox voltage of insertion of ceramic compounds. This can be accomplished by incorporating highly electronegative anions in the cathode ceramics. Building on this idea, recently various sulphate- based compounds have been reported as high voltage cathode materials. The current article highlights the use of sulphate (SO4) based cathodes to realize the highest ever Fe3+/Fe2+ redox potentials in Li-ion batteries (LiFeSO4F fluorosulphate: 3.9V vs Li/Li+) and Na-ion batteries (Na2Fe2(SO4)(3) polysulphate: 3.8V vs Na/Na+). These sulphate-based cathode ceramic compounds pave way for newer avenues to design better batteries for future applications.
Resumo:
The objective of the article is to present a unified model for the dynamic mechanical response of ceramics under compressive stress states. The model incorporates three principal deformation mechanisms: (i) lattice plasticity due to dislocation glide or twinning; (ii) microcrack extension; and (iii) granular flow of densely packed comminuted particles. In addition to analytical descriptions of each mechanism, prescriptions are provided for their implementation into a finite element code as well as schemes for mechanism transitions. The utility of the code in addressing issues pertaining to deep penetration is demonstrated through a series of calculations of dynamic cavity expansion in an infinite medium. The results reveal two limiting behavioral regimes, dictated largely by the ratio of the cavity pressure p to the material yield strength σY. At low values of p/σY, cavity expansion occurs by lattice plasticity and hence its rate diminishes with increasing σY. In contrast, at high values, expansion occurs by microcracking followed by granular plasticity and is therefore independent of σY. In the intermediate regime, the cavity expansion rate is governed by the interplay between microcracking and lattice plasticity. That is, when lattice plasticity is activated ahead of the expanding cavity, the stress triaxiality decreases (toward more negative values) which, in turn, reduces the propensity for microcracking and the rate of granular flow. The implications for penetration resistance to high-velocity projectiles are discussed. Finally, the constitutive model is used to simulate the quasi-static and dynamic indentation response of a typical engineering ceramic (alumina) and the results compared to experimental measurements. Some of the pertinent observations are shown to be captured by the present model whereas others require alternative approaches (such as those based on fracture mechanics) for complete characterization. © 2011 The American Ceramic Society.
Resumo:
Many experimental observations have shown that a single domain in a ferroelectric material switches by progressive movement of domain walls, driven by a combination of electric field and stress. The mechanism of the domain switch involves the following steps: initially, the domain has a uniform spontaneous polarization; new domains with the reverse polarization direction nucleate, mainly at the surface, and grow though the crystal thickness; the new domain expands sideways as a new domain continues to form; finally, the domain switch coalesces to complete the polarization reversal. According to this mechanism, the volume fraction of the domain switching is introduced in the constitutive law of the ferroelectric material and used to study the nonlinear constitutive behavior of a ferroelectric body in this paper. The principle of stationary total potential energy is put forward in which the basic unknown quantities are the displacement u(i), electric displacement D-i and volume fraction rho(I) of the domain switching for the variant I. The mechanical field equation and a new domain switching criterion are obtained from the principle of stationary total potential energy. The domain switching criterion proposed in this paper is an expansion and development of the energy criterion established by Hwang et al. [ 1]. Based on the domain switching criterion, a set of linear algebraic equations for determining the volume fraction rho(I) of domain switching is obtained, in which the coefficients of the linear algebraic equations only contain the unknown strain and electric fields. If the volume fraction rho(I) of domain switching for each domain is prescribed, the unknown displacement and electric potential can be obtained based on the conventional finite element procedure. It is assumed that a domain switches if the reduction in potential energy exceeds a critical energy barrier. According to the experimental results, the energy barrier will strengthen when the volume fraction of the domain switching increases. The external mechanical and electric loads are increased step by step. The volume fraction rho(I) of domain switching for each element obtained from the last loading step is used as input to the constitutive equations. Then the strain and electric fields are calculated based on the conventional finite element procedure. The finite element analysis is carried out on the specimens subjected to uniaxial coupling stress and electric field. Numerical results and available experimental data are compared and discussed. The present theoretic prediction agrees reasonably with the experimental results.
Resumo:
Based on a constitutive law which includes the shear components of transformation plasticity, the asymptotic solutions to near-tip fields of plane-strain mode I steadity propagating cracks in transformed ceramics are obtained for the case of linear isotropic hardening. The stress singularity, the distributions of stresses and velocities at the crack tip are determined for various material parameters. The factors influencing the near-tip fields are discussed in detail.
Resumo:
The speciation of water in a variety of hydrous silicate glasses, including simple and rhyolitic compositions, synthesized over a range of experimental conditions with up to 11 weight percent water has been determined using infrared spectroscopy. This technique has been calibrated with a series of standard glasses and provides a precise and accurate method for determining the concentrations of molecular water and hydroxyl groups in these glasses.
For all the compositions studied, most of the water is dissolved as hydroxyl groups at total water contents less than 3-4 weight percent; at higher total water contents, molecular water becomes the dominant species. For total water contents above 3-4 weight percent, the amount of water dissolved as hydroxyl groups is approximately constant at about 2 weight percent and additional water is incorporated as molecular water. Although there are small but measurable differences in the ratio of molecular water to hydroxyl groups at a given total water content among these silicate glasses, the speciation of water is similar over this range of composition. The trends in the concentrations of the H-bearing species in the hydrous glasses included in this study are similar to those observed in other silicate glasses using either infrared or NMR spectroscopy.
The effects of pressure and temperature on the speciation of water in albitic glasses have been investigated. The ratio of molecular water to hydroxyl groups at a given total water content is independent of the pressure and temperature of equilibration for albitic glasses synthesized in rapidly quenching piston cylinder apparatus at temperatures greater than 1000°C and pressures greater than 8 kbar. For hydrous glasses quenched from melts cooled at slower rates (i.e., in internally heated or in air-quench cold seal pressure vessels), there is an increase in the ratio of molecular water to hydroxyl group content that probably reflects reequilibration of the melt to lower temperatures during slow cooling.
Molecular water and hydroxyl group concentrations in glasses provide information on the dissolution mechanisms of water in silicate liquids. Several mixing models involving homogeneous equilibria of the form H_2O + O = 20H among melt species have been explored for albitic melts. These models can account for the measured species concentrations if the effects of non-ideal behavior or mixing of polymerized units are included, or by allowing for the presence of several different types of anhydrous species.
A thermodynamic model for hydrous albitic melts has been developed based on the assumption that the activity of water in the melt is equal to the mole fraction of molecular water determined by infrared spectroscopy. This model can account for the position of the watersaturated solidus of crystalline albite, the pressure and temperature dependence of the solubility of water in albitic melt, and the volumes of hydrous albitic melts. To the extent that it is successful, this approach provides a direct link between measured species concentrations in hydrous albitic glasses and the macroscopic thermodynamic properties of the albite-water system.
The approach taken in modelling the thermodynamics of hydrous albitic melts has been generalized to other silicate compositions. Spectroscopic measurements of species concentrations in rhyolitic and simple silicate glasses quenched from melts equilibrated with water vapor provide important constraints on the thermodynamic properties of these melt-water systems. In particular, the assumption that the activity of water is equal to the mole fraction of molecular water has been tested in detail and shown to be a valid approximation for a range of hydrous silicate melts and the partial molar volume of water in these systems has been constrained. Thus, the results of this study provide a useful thermodynamic description of hydrous melts that can be readily applied to other melt-water systems for which spectroscopic measurements of the H-bearing species are available.
Resumo:
Transparent Ni2+-doped beta-Ga2O3 glass-ceramics were synthesized. The nanocrystal phase in the glass-ceramics was identified to be beta-Ga2O3 and its size was about 3.6 nm. It was confirmed from the absorption spectra that the ligand environment of Ni2+ ions changed from the trigonal bi-pyramid fivefold sites in the as-cast glass to the octahedral sites in the glass-ceramics. The broadband infrared emission centering at 1270 nm with full width at half maximum (FWHM) of more than 250 nm was observed. The fluorescence lifetime was about 1.1 mu s at room temperature. The observed infrared emission could be attributed to the T-3 (2g) (F-3) -> (3)A (2g) (F-3) transition of octahedral Ni2+ ions. It is suggested that the Ni2+-doped transparent beta-Ga2O3 glass-ceramics with broad bandwidth and long lifetime have a potential as a broadband amplification medium.
Resumo:
The fluorescence and up-conversion spectral properties of Er3+-doped TeO2-ZnO and TeO2-ZnO-PbCl2 glasses suitable for developing optical fiber amplifier and laser have been fabricate and characterized. Strong green (around 527-550 nm) and red (around 661 nm) up-conversion emissions under 977 nm laser diode excitation were investigated, corresponding to H-2(11/2), S-4(3/2), --> I-4(15/2) and F-4(9/2) --> I-4(15/2) transitions of Er3+ ions respectively, have been observed and the involved mechanisms have been explained. The dependence of up-converted fluorescence intensity versus laser power confirm that two-photons contribute to up-conversion of the green-red emissions. The novelty of this kind of optical material has been its ability in resisting devitrification, and its promising optical properties strongly encourage for their further development as the rare-earth doped optical fiber amplifiers and upconversion fiber laser systems.
Resumo:
We report on the fabrication and characterization of low-loss planar and stripe waveguides in a Nd3+-doped glass by 6 MeV oxygen-ion implantation at a dose of 1x10(15) ions/cm(2). The dark mode spectroscopy of the planar waveguide was measured using a prism coupling arrangement. The refractive index profile of the planar waveguide was reconstructed from a code based on the reflectivity calculation method. The results indicate that a refractive index enhanced region as well as an optical barrier have been created after the ion beam processing. The near-field mode profiles of the stripe waveguide were obtained by an end-fire coupling arrangement, by which three quasitransverse electric modes were observed. After annealing, the propagation losses of the planar and stripe waveguides were reduced to be similar to 0.5 and similar to 1.8 dB/cm, respectively. (c) 2007 American Institute of Physics.
Resumo:
Er3+ doped multicomponent fluoride based glass was prepared. These precursor fluoride glass samples were then heated using different schedules. Crystalline phase particles were successfully precipitated in the multicomponent fluoride glass samples after heat treatment. The influence of heat treatment on the spectroscopic properties of Er3+ in multicomponent fluoride based glass samples were discussed. Small changes of the Judd-Ofelt parameters Omega(i) (i = 2,4,6) were found in multicomponent fluoride glass samples before and after heat treatment compared to oxyfluoride telluride glass. Preparation conditions used to produce transparent multicomponent fluoride glass ceramics doped with rare-earth ions are discussed. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Low loss index enhanced planar waveguides in Nd3+-doped silicate glass were fabricated by 3.0 MeV C+ ion implantation. The enhancement of the refractive index confined the light propagating in the waveguide. The prism-coupling method was used to measure dark modes in the waveguide. The effective refractive indices of the waveguide were obtained based on the dark modes. The moving fiber method was applied to measure the waveguide propagation loss. Loss measured in non-annealed samples is about 0.6 dB/cm. And the waveguide mode optical near-field output at 633 nm was presented. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Broadband neat-infrared emission from transparent Ni2+-doped sodium aluminosilicate glass-cermaics is observed. The broad emission is centered at 1290 nm and covers the whole telecommunication wavelength region (1100-1700 nm) with full width at half maximum of about 340 nm. The observed infrared emission could be attributed to the T-3(2)(F) -> (3)A(2)(F) transition of octahedral Ni2+ ions that occupy high-field sites in nanocrystals. The product of the lifetime and the stimulated emission cross section is 2.15 x 10(-24) cm(2)s. It is suggested that Ni2+-doped sodium aluminosilicate glass ceramics have potential applications in tunable broadband light sources and broadband amplifiers.