Resumo:
Glass samples with the composition (mol%) 80TeO(2)-10Nb(2)O(5)-5K(2)O-5Li(2)O, stable against crystallization, were prepared containing Yb3+, Tm3+ and Ho3+. The energy transfer and energy back transfer mechanisms in samples containing 5% Yb3+-5% Tm3+ and 5% Yb3+-5% Tm3+-0.5% Ho3+ were estimated by measuring the absorption and fluorescence spectra together with the time dependence of the Yb3+ F-2(5/2) excited state. A good fit for the luminescence time evolution was obtained with the Yokota-Tanimoto's diffusion-limited model. The up-conversion fluorescence was also studied in 5% Yb-5% Tm. 5% Yb-0.5% Ho and 5% Yb-5% Tm-0.5% Ho tellurite glasses under laser excitation at 975 nm. Strong emission was observed from (1)G(4) and F-3(2) Tm3+ energy levels in all samples. The S-5(2) Ho3+ emission was observed only in Yb3+Ho3+ samples being completely quenched in Yb3+/Tm3+/Tm3+ samples. (C) 2001 Elsevier B.V. B.V. All rights reserved.
Resumo:
The compounds [Fe(ch)(CO)(2)PP3] (1) (ch = chalcone) and [Fe(sba)(CO)(2)PPh3] (2) (sba = sorbic acid) were prepared by irradiating the tetracarbonyltriphenylphosphineiron(0) complex in benzene in the presence of ch or sba. The compounds were characterized by infrared and P-31 NMR spectroscopies. Their electrochemical behavior was investigated by cyclic voltammetry and the results suggest that their oxidations occur by more than one electrochemical step, producing free ch and sba, free PPh3 and solvated Fe(III). It was observed that sba ligand contributes more effectively to the stabilization of metal center in these complexes, the X-ray crystal and molecular structures of 1 and 2 were determined; it was shown that the Fe atom adopts a distorted octahedral coordinated geometry in which three of the sites are occupied by the ch or sba ligand. The [Fe(ch)(CO)(2)PPh3] complex is a monomer and the unit cell of complex 2 contains exist two identical and crystallographically independent molecules of [Fe(sba)(CO)(2)PPh3] which are linked by short hydrogen bonds O-H . . .O (C) 2001 Published by Elsevier B.V. Ltd.
Resumo:
This work deals with the synthesis, spectroscopic and structural investigation of pyrazolyl complexes of the type trans-[M(NCS)(2)(HPz)(4)] {M=Co (1), Ni (2); HPz=pyrazole}. Single crystal X-ray studies on 1 and 2 reveal the formation of similar supramolecular arrangements derived from self-assembly of monomers linked together through intermolecular N-H center dot center dot center dot SCN hydrogen bonds, C-H center dot center dot center dot pi interactions and pi-pi stacking. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
A tungsten carbide coating on the integrated platform of a transversely heated graphite atomizer (THGA((R))) used together with Pd(NO3)(2) + Mg(NO3)(2) as modifier is proposed for the direct determination of lead in vinegar by graphite furnace atomic absorption spectrometry. The optimized heating program (temperature, ramp time, hold time) of atomizer involved drying stage (110 degrees C, 5 s, 30 s; 130 degrees C, 5 s, 30 s), pyrolysis stage (1000 degrees C, 15 s, 30 s), atomization stage (1800 degrees C, 0 s, 5 s) and clean-out stage (2450 degrees C, I s, 3 s). For 10 mu L of vinegar delivered into the atomizer and calibration using working standard solutions (2.5-20.0 mu g L-1 Pb) in 0.2% (v/v) HNO3, analytical curve with good linear correlation (r = 0.9992) was established. The characteristic mass was 40 pg Pb and the lifetime of the tube was around 730 firings. The limit of detection (LOD) was 0.4 mu g L-1 and the relative standard deviations (n = 12) were typically <8% for a sample containing 25 pg L-1 Pb. Accuracy of the proposed method was checked after direct analysis of 23 vinegar samples. A paired t-test showed that results were in agreement at 95% confidence level with those obtained for acid-digested vinegar samples. The Pb levels varied from 2.8 to 32.4 pg L-1. Accuracy was also checked by means of addition/recovery tests and recovered values varied from 90% to 110%. Additionally, two certified reference materials were analyzed and results were in agreement with certified values at a 95% confidence level. (C) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Reactions of Hg(CH3COO)(2) with [Fe(CO)(5)] in MeOH and EtOH lead to the compounds Hg[Fe(COOR)(CO)(4)](2) (I for R = CH3 and II for R = C2H5). Crystals of I are triclinic, P (1) over bar, with a = 6.272(2), b = 6.441(3), c = 11.703(4) Angstrom, a = 92.94(3)degrees, beta = 103.77(3)degrees, gamma = 96.10(2)degrees, and Z = 1. Crystals of II are tetragonal, I4(1)/a, with a = 17.906(3) Angstrom, c = 12.756(2) Angstrom, and Z = 8. The geometry around Hg is linear for compound I and approximately linear for compound II. The Hg-Fe distances are 2.5716(8) and 2.575(4) Angstrom for compounds I and II, respectively. The geometry around the Fe in both compounds is approximately octahedral. The carboalkoxy group is cis to Hg in both compounds with Fe-C distances equal to 2.034(6) and 2.05(4) Angstrom for compounds I and II, respectively.
Resumo:
The erbium-based manganite ErMnO3 has been partially substituted at the manganese site by the transition-metal elements Ni and Co. The perovskite orthorhombic structure is found from x(Ni) = 0.2-0.5 in the nickel-based solid solution ErNixMn1-xO3, while it can be extended up to x(Co) = 0.7 in the case of cobalt, provided that the synthesis is performed under oxygenation conditions to favor the presence of Co3+. Presence of different magnetic entities (i.e., Er3+, Ni2+, Co2+, Co3+, Mn3+, and Mn4+) leads to quite unusual magnetic properties, characterized by the coexistence of antiferromagnetic and ferromagnetic interactions. In ErNixMn1-xO3, a critical concentration x(crit)(Ni) = 1/3 separates two regimes: spin-canted AF interactions predominate at x < x(crit), while the ferromagnetic behavior is enhanced for x > x(crit). Spin reversal phenomena are present both in the nickel- and cobalt-based compounds. A phenomenological model based on two interacting sublattices, coupled by an antiferromagnetic exchange interaction, explains the inversion of the overall magnetic moment at low temperatures. In this model, the ferromagnetic transition-metal lattice, which orders at T-c, creates a strong local field at the erbium site, polarizing the Er moments in a direction opposite to the applied field. At low temperatures, when the contribution of the paramagnetic erbium sublattice, which varies as T-1, gets larger than the ferromagnetic contribution, the total magnetic moment changes its sign, leading to an overall ferrimagnetic state. The half-substituted compound ErCo0.50Mn0.50O3 was studied in detail, since the magnetization loops present two well-identified anomalies: an intersection of the magnetization branches at low fields, and magnetization jumps at high fields. The influence of the oxidizing conditions was studied in other compositions close to the 50/50 = Mn/Co substitution rate. These anomalies are clearly connected to the spin inversion phenomena and to the simultaneous presence of Co2+ and Co3+ magnetic moments. Dynamical aspects should be considered to well identify the high-field anomaly, since it depends on the magnetic field sweep rate. (C) 2006 Elsevier B.V. All rights reserved.
Resumo:
This paper describes a simple method to co-precipitate CeO2 and Ce0.8Gd0.2O1.9-delta with ammonium hydroxide from solvents such as: water, ethylene glycol, ethyl alcohol and isopropyl alcohol. Characterization by Raman spectroscopy and XRD evidenced the formation of a solid solution of gadolinium-doped ceria at room temperature. Nanometric particles with crystallite size of 3.1 nm were obtained during synthesis using ethyl alcohol as solvent. This is a promising result compared with those mentioned in the literature, in which the smallest crystallite size reported was, 6.5 nm. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
Bismuth was evaluated as an internal standard for the direct determination of Pb in vinegar by graphite furnace atomic absorption spectrometry using Ru as a permanent modifier with co-injection of Pd/Mg(NO3)(2). The correlation coefficient of the graph plotted from the non-nalized absorbance signals of Bi versus Pb was r=0.989. Matrix effects were evaluated by analyzing the slope ratios between the analytical curve, and analytical curves obtained from Pb additions in red and white wine vinegar obtained from reference solutions prepared in 0.2% (v/v) HNO3, samples. The calculated ratios were around 1.04 and 1.02 for analytical curves established applying an internal standard and 1.3 and 1.5 for analvtical curves without. Analytical curves in the 2.5-15 pg L-1 Pb concentration interval were established using the ratio Pb absorbance to Bi absorbance versus analvte concentration, and typical linear correlations of r=0.999 were obtained. The proposed method was applied for direct determination of Pb in 18 commercial vinegar samples and the Pb concentration varied from 2.6 to 31 pg L-1. Results were in agreement at a 95% confidence level (paired t-test) with those obtained for digested samples. Recoveries of Pb added to vinegars varied from 96 to 108% with and from 72 to 86% without an internal standard. Two water standard reference materials diluted in vinegar sample were also analyzed and results were in agreement with certified values at a 95% confidence level. The characteristic mass was 40 pg Pb and the useful lifetime of the tube was around 1600 firings. The limit of detection was 0.3 mu g L-1 and the relative standard deviation was <= 3.8% and <= 8.3% (n = 12) for a sample containing, 10 mu L-1 Pb with and without internal standard, respectively. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
This work reports on the study about the luminescence behavior of Eu3+-O2- associates in Sr2SiO4 doped with Eu3+, or simultaneously doped with Eu3+ and Zn2+ ions, where the Zn2+ doping ion acts as a charge compensating agent. Both Sr2SiO4:Eu3+ and Sr2SiO4:Eu3+,Zn2+ emission spectra show two types D-5(0)-->F-7(0) type transitions, one type related to Eu3+ in the Sr2+ Site, at 577 and 580 nm and the other one related to Eu3+-O2- associates, at 574 nm. Excitation spectra present two CT bands at 275 and 324 nm related to each emission center, respectively. Comparing the relative intensities between the emission spectra, the 0-->0 transition at 574 nm assigned to Eu3+-O2- associates in the Sr2SiO4:Eu3+ emission spectrum is much more intense than the same transition in the Sr2SiO4:Eu3+,Zn2+ emission spectrum. Moreover, in the Sr2SiO4:Eu3+ excitation spectrum, the intensity ratio between the CT band related to the Eu3+-O2- emission center and Eu3+ F-7-->L-5(6) transition is also larger than in the Sr2SiO4:Eu3+,Zn2+ one. Therefore, the presence of Zn2+ species provides an extra charge compensating mechanism, which decreases the formation of Eu3+-O2- associates. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
The magnetic moment using self-consistent spin-polarized energy band calculations of Fe3Al and Fe2CoAl Heusler phases are presented. These results are compared with the experimental values obtained from the magnetization curves of these materials. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
In this article we present a concise report on our studies on the magnetic behavior and structural arrangements of the inverse spinel Zn7-xMxSb2O12 system (M = Ni, Co). Studies on the temperature dependence of the magnetization (M) of several samples in this system showed the occurrence of a spin-glass-like state in temperatures around 10 K. The capability of this system to hold magnetic ions in either octahedral and/or tetrahedral positions is responsible for the occurrence of competing ferromagnetic and antiferromagnetic interactions. This condition is likely to cause the appearance of the observed spin-glass-like behavior. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
This paper presents a methodology for the study of a molten carbonate fuel cell co-generation system. This system is applied to a dairy industry of medium size that typically demands 2100 kW of electricity, 8500 kg/h of saturated steam (P = 1.08 MPa) and 2725 kW of cold water production. Depending on the associated recuperation equipment, the co-generation system permits the recovery of waste heat, which can be used for the production of steam, hot and cold water, hot and cold air. In this study, a comparison is made between two configurations of fuel cell co-generation systems (FCCS). The plant performance has been evaluated on the basis of fuel utilisation efficiency and each system component evaluated on the basis of second law efficiency. The energy analysis presented shows a fuel utilisation efficiency of about 87% and exergy analysis shows that the irreversibilities in the combustion chamber of the plant are significant. Further, the payback period estimated for the fuel cell investment between US$ 1000 and US$ 1500/k-W is about 3 and 6 years, respectively. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
We report on the use of dynamic scale theory and fractal analyses in the Study of distinct growth stages of layer-by-layer (LBL) films of poly(allylamine hydrochloride) (PAH) and a side-chain-substituted azobenzene copolymer (Ma-co-DR13). The LBL films were adsorbed oil glass substrates and characterized with atomic force microscopy with the Ma-co-DR13 at the top layer. The ganular morphology exhibited by the films allowed the observation of the growth process inside and outside the grains. The growth outside the grains was found to follow the Kardar-Parisi-Zhang model, with fractal dimensions of ca. 2.6. One could expect that inside the grains the morphology would be close to a Euclidian surface with fractal dimension of ca. 2 for any growth stage. The latter, however, was observed only for thicker films containing more than 10 bilayers. For thinner films the morphology was well described by a self-affine fractal. Such dependence of the growth behavior with the film thickness is associated with a more complete coverage of adsorption sites in thicker films due to diffusion of polymer molecules. (c) 2004 Elsevier B.V. All rights reserved.