952 resultados para dussertite, arsenate, crandallite group, Raman spectroscopy, infrared spectroscopy, hydroxyl ions, molecular water, adsorbed water
Resumo:
The mineral dussertite, a hydroxy-arsenate mineral of formula BaFe3+3(AsO4)2(OH)5, has been studied by Raman complimented with infrared spectroscopy. The spectra of three minerals from different origins were investigated and proved quite similar, although some minor differences were observed. In the Raman spectra of Czech dussertite, four bands are observed in the 800 to 950 cm-1 region. The bands are assigned as follows: the band at 902 cm-1 is assigned to the (AsO4)3- ν3 antisymmetric stretching mode, at 870 cm-1 to the (AsO4)3- ν1 symmetric stretching mode, and both at 859 cm-1 and 825 cm-1 to the As-OM2+/3+ stretching modes/and or hydroxyls bending modes. Raman bands at 372 and 409 cm-1 are attributed to the ν2 (AsO4)3- bending mode and the two bands at 429 and 474 cm-1 are assigned to the ν4 (AsO4)3- bending mode. An intense band at 3446 cm-1 in the infrared spectrum and a complex set of bands centred upon 3453 cm-1 in the Raman spectrum are attributed to the stretching vibrations of the hydrogen bonded (OH)- units and/or water units in the mineral structure. The broad infrared band at 3223 cm-1 is assigned to the vibrations of hydrogen bonded water molecules. Raman spectroscopy identified Raman bands attributable to (AsO4)3- and (AsO3OH)2- units.
Resumo:
Raman and infrared spectra of two polymorphous minerals with the chemical formula Fe3+(SO4)(OH)•2H2O, monoclinic butlerite and orthorhombic parabutlerite, are studied and the spectra assigned. Observed bands are attributed to the (SO4)2- stretching and bending vibrations, hydrogen bonded water molecules, stretching and bending vibrations of hydroxyl ions, water librational modes, Fe-O and Fe-OH stretching vibrations, Fe-OH bending vibrations and lattice vibrations. The O-H...O hydrogen bond lengths in the structures of both minerals are calculated from the wavenumbers of the stretching vibrations. One symmetrically distinct (SO4)2- unit in the structure of butlerite and two symmetrically distinct (SO4)2- units in the structure of parabutlerite are inferred from the Raman and infrared spectra. This conclusion agrees with the published crystal structures of both mineral phases.
Resumo:
Some minerals are formed which show poorly defined X-ray diffraction patterns. Vibrational spectroscopy offers one of the few methods for the assessment of the structure of the oxyanions in such minerals. Among this group of minerals is mallestigite with formula Pb3Sb5+(SO4)(AsO4)(OH)6•3H2O. The objective of this research is to determine the molecular structure of the mineral mallestigite using vibrational spectroscopy. Raman and infrared bands are attributed to the AsO43- , SO42- and water stretching vibrations. Mallestigite is a mineral formed in ancient waste dumps such as occurs at Mallestiger, Carinthia, Austria and as such is a mineral of archaeological significance.
Resumo:
The presence of arsenic in the environment is a hazard. The accumulation of arsenate by a range of cations in the formation of minerals provides a mechanism for the accumulation of arsenate. The formation of the tsumcorite minerals is an example of a series of minerals which accumulate arsenate. There are about twelve examples in this mineral group. Raman spectroscopy offers a method for the analysis of these minerals. The structure of selected tsumcorite minerals with arsenate and sulphate anions were analysed by Raman spectroscopy. Isomorphic substitution of sulphate for arsenate is observed for gartrellite and thometzekite. A comparison is made with the sulphate bearing mineral natrochalcite. The position of the hydroxyl and water stretching vibrations are related to the strength of the hydrogen bond formed between the OH unit and the AsO43- anion. Characteristic Raman spectra of the minerals enable the assignment of the bands to specific vibrational modes.
Resumo:
We have studied the mineral goyazite using Raman and infrared spectroscopy. Goyazite is a member of the crandallite subgroup of the alunite supergroup. The crystal structure is of the alunite-type and consists of sheets of corner-sharing AlO6 octahedra parallel to (0001). The octahedrally coordinated Sr2+ cations occupy cavities between pairs of octahedral sheets and are surrounded by six oxygen atoms from the (Al3+)O6 octahedra. The very intense sharp band at 983 cm-1 is assigned to the ν1 PO43- symmetric stretching mode. The observation of a single band supports the concept that all the phosphate units are equivalent in the structure of goyazite. Raman bands observed at 1029 cm-1 and 1037 cm-1 are assigned to the to the ν3 PO43- antisymmetric stretching vibrations. Two Raman bands at 895 and 927 cm-1 are attributed to the stretching vibrations of H2PO4; thus indicating some hydrogen phosphate units in the structure of goyazite. Raman bands at 556, 581, 596 and 612 cm-1 are assigned to the ν4 PO43- bending modes, suggesting a reduction of symmetry of phosphate units. Two sharp Raman bands at 3609 and 3631 cm-1 are attributed to OH stretching vibrations from the goyazite hydroxyl units. Broad Raman bands at 2924, 3043, 3210, 3429 and 3511 cm-1 are assigned to water stretching vibrations. Vibrational spectroscopy enables subtle details of the molecular structure of goyazite to be determined.
Resumo:
The kaolinite-like phyllosilicate minerals bismutoferrite BiFe3+2Si2O8(OH) and chapmanite SbFe3+2Si2O8(OH) have been studied by Raman spectroscopy and complemented with infrared spectra. Tentatively interpreted spectra were related to their molecular structure. The antisymmetric and symmetric stretching vibrations of the Si-O-Si bridges, SiOSi and OSiO bending vibrations, (Si-Oterminal)- stretching vibrations, OH stretching vibrations of hydroxyl ions, and OH bending vibrations were attributed to observed bands. Infrared bands 3289-3470 cm-1 and Raman bands 1590-1667 cm-1 were assigned to adsorbed water. O-H...O hydrogen bond lengths were calculated from the Raman and infrared spectra.
Resumo:
The stratum corneum (SC) barrier typically consists of layers of corneocytes embedded in a lipid continuum that regulates barrier function. The lipid domain containing ceramides, cholesterol, and free fatty acids provides the major pathway for most drugs permeating across SC. Penetration enhancers diminish the SC barrier function. The classic enhancer is dimethyl sulfoxide (DMSO). Its mechanisms of action remain unclear, although DMSO disrupts lipid organisation and may displace protein-bound water. Here we use confocal Raman spectroscopy to probe molecular interactions between a finite (depleting) dose of DMSO and SC, as functions of depth and time, providing novel information about residence time and location of DMSO in human SC in vivo
Resumo:
In archaeometry, the advantages of a combined use of Raman spectroscopy and X-ray fluorescence spectroscopy are extensively discussed for applications such as the analysis of paintings, manuscripts, pottery, etc. Here, we demonstrate for the first time the advantage of using both techniques for analysing glyptics. These engraved gemstones or glass materials were originally used as stamps, to identify the owner, for instance on letters, but also on wine vessels. For this research, a set of 64 glyptics (42 Roman glass specimens and 22 modern ones), belonging to the collection of the museum ‘Quinta das Cruzes’ in Funchal (Madeira, Portugal), was analysed with portable Raman spectroscopy and handheld X-ray fluorescence (hXRF). These techniques were also used to confirm the gemological identification of these precious objects and can give extra information about the glass composition. Raman spectroscopy identifies the molecular composition as well as on the crystalline phases present. On the other hand, hXRF results show that the antique Roman glass samples are characterised with low Pb and Sn levels and that the modern specimens can be discriminated in two groups: lead-based and non-lead-based ones.
Resumo:
The Raman spectrum of bukovskýite, Fe3+2(OH)(SO4)(AsO4)•7H2O has been studied and compared with the Raman spectrum of an amorphous gel containing specifically Fe, As and S elements and is understood as an intermediate product in the formation of bukovskýite. Observed bands are assigned to the stretching and bending vibrations of (SO4)2- and (AsO4)3- units, stretching and bending vibrations and librational modes of hydrogen bonded water molecules, stretching and bending vibrations of hydrogen bonded (OH)- ions and Fe3+-(O,OH) units. Approximate range of O-H...O hydrogen bond lengths is inferred from the Raman spectra. Raman spectra of crystalline bukovskýite and of the amorphous gel differ in that the bukovskýite spectrum is more complex, observed bands are sharp, the degenerate bands of (SO4)2- and (AsO4)3- are split and more intense. Lower wavenumbers of H2O bending vibration in the spectrum of the amorphous gel may indicate the presence of weaker hydrogen bonds compared with those in bukovskýite.
Resumo:
Shattuckite Cu5(SiO3)4(OH)2 is a copper hydroxy silicate and is commonly known as a ‘healing’ mineral. Three shattuckite mineral samples from three different origins were analysed by Raman spectroscopy. Some Raman bands are common in the spectra of the minerals. Raman bands at around 890, 1058 and 1102 are described as the ν3 –SiO3 antisymmetric stretching vibrations. The Raman band at 670 cm-1 is assigned to the ν4 bending modes of the -SiO3 units and the band at around 785 cm-1is due to Si-O-Si chain stretching mode. Raman (and infrared) spectroscopy proves that water is in the molecular structure of shattuckite; thus the formula is better written as Cu5(SiO3)4(OH)2•xH2O.
Resumo:
Raman spectrum of callaghanite, Cu2Mg2(CO3)(OH)6⋅2H2O, was studied and compared with published Raman spectra of azurite, malachite and hydromagnesite. Stretching and bending vibrations of carbonate and hydroxyl units and water molecules were tentatively assigned. Approximate O–H…O hydrogen bond lengths were inferred from the spectra. Because of the high content of hydroxyl ions in the crystal structure in comparison with low content of carbonate units, callaghanite should be better classified as a carbonatohydroxide than a hydroxycarbonate.
Resumo:
Raman spectrum of burgessite, Co2(H2O)4[AsO3OH]2.H2O was studied, interpreted and compared with its infrared spectrum. The stretching and bending vibrations of (AsO3) and As-OH units together with the stretching, bending and libration modes of water molecules and hydroxyl ions were assigned. The range of O-H...O hydrogen bond lengths was inferred from the Raman and infrared spectra of burgessite. The presence of (AsO3OH)2- units in the crystal structure of burgessite was proved in agreement with its recently solved crystal structure. Raman and infrared spectra of erythrite inferred from the RRUFF database are used for comparison.
Resumo:
Raman spectra of two well-defined types of koritnigite crystals from the Jáchymov ore district, Czech Republic, were recorded and interpreted. No substantial differences were observed between both crystal types. Observed Raman bands were attributed to the (AsO3OH)2- stretching and bending vibrations, stretching and bending vibrations of water molecules and hydroxyl ions. Non-interpreted Raman spectra of koritnigite from the RRUFF database, and published infrared spectra of cobaltkoritnigite were used for comparison. The O-H...O hydrogen bond lengths in the crystal structure of koritnigite were inferred from the Raman spectra and compared with those derived from the X-ray single crystal refinement. The presence of (AsO3OH)2- units in the crystal structure of koritnigite was proved from the Raman spectra which supports the conclusions of the X-ray structure analysis.
Resumo:
Raman microscopy of two mixite minerals BiCu6(AsO4)3(OH)6.3H2O from Jáchymov and from Smrkovec (both Czech Republic) has been used to study their molecular structure, which is interpreted and the presence of (AsO4)3-, (AsO3OH)2-, (PO4)3- and (PO3OH)2- units, molecular water and hydroxyl ions were inferred. O-H…O hydrogen bond lengths were calculated from the Raman and infrared spectra using Libowitzky’s empirical relation. Small differences in the Raman spectra between both samples were observed and attributed to compositional and hydrogen bonding network differences.