858 resultados para Titanium casting
Resumo:
Titaniuni and its alloys have many applications in aerospace, marine and other engineering industries. Titanium requires special melting techniques because of its high reactivity at elevated temperatures and needs special mould materials and methods for castings. This paper reviews the development of titanium casting technology.
Resumo:
Statement of problem. There are few studies on titanium casting shrinkage, and phosphate-bonded investments for titanium casting have not produced appropriate marginal fit.Purpose. The purpose of this study was to determine the thermal shrinkage of titanium and the setting and thermal expansion of 3 phosphate-bonded investments.Material and methods. The thermal shrinkage between the melting temperature and room temperature was calculated using a titanium thermal expansion coefficient. The thermal and setting expansion were measured for 3 phosphate bonded investments: Rematitan Plus (RP) specific for titanium, Rema Exakt (RE), and Castorit Super C (CA), using different special liquid concentrations (100%, 75%, and 50%). Setting expansion was measured for cylindrical specimens 50 mm long x 8 mm in diameter with a transducer. The heating and cooling curves were obtained with a dilatometer (DIL 402 PC). The total expansion curve was drawn using software, and temperatures to obtain expansion equivalent to titanium casting shrinkage were determined (n=5). In addition, the total expansion of the control group (RP at 430 degrees C) was measured, as well as the temperatures at which the other groups achieved equivalent total expansion (n=5). Data were analyzed by 1-way ANOVA and the Tukey HSD test (alpha=.05).Results. Titanium casting shrinkage was estimated as 1.55%. RP did not achieve this expansion. RE achieved expansion of 1.55% only with a special liquid concentration of 100% at 594 degrees C. CA with all special liquid concentrations attained this expansion (351 degrees C to 572 degrees C). Total expansion of the control group was 0.86%, and the other groups reached that expansion within the range of 70 degrees C to 360 degrees C.Conclusions. Only RE and CA demonstrated sufficient expansion to compensate for titanium casting shrinkage. All groups reached total expansion equivalent to that of the control group at significantly lower temperatures.
A Quality Assessment of Titanium Castings Produced in an Experimental Short-Heating-Cycle Investment
Resumo:
The aim of this study was to evaluate the quality of casting produced in an experimental short-term heating-cycle investment. Thus, reaction layer and castability of titanium casting using an experimental spinel-based investment (VR) with short heating cycle were compared with the commercial short-heating-cycle spinel-based investment Trinell (TR), the silica-phosphate-based investment Rematitan Plus ( RP), and the conventional spinel-based investment Rematitan Ultra (RU). VR has polymeric fibers added to inorganic particles. Reaction layer assessments were carried out using Vickers hardness and elemental analysis using dispersive X-ray microanalysis (EDX). Mesh patterns were used for castability test, and powder characterization was made by scanning electron microscopy (SEM). Hardness evaluation showed no difference among the investments between 100 and 200 mu m. The most important contaminant element for VR, TR, and RU was oxygen. Higher levels of mold filling were found for TR, VR, and RU compared with that obtained with RP. The quality of castings, characterized by means of the assessments of reaction layer and castability, made from the VR was similar to the commercial investments TR and RU but superior to the RP.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Objectives: To conduct a controlled study contrasting titanium surface topography after procedures that simulated 10 years of brushing using toothpastes with or without fluoride. Methods: Commercially pure titanium (cp Ti) and Ti-6Al-4V disks (6 mm circle divide x 4 mm) were mirror-polished and treated according to 6 groups (n = 6) as a function of immersion (I) or brushing (B) using deionised water (W), fluoride-free toothpaste (T) and fluoride toothpaste (FT). Surface topography was evaluated at baseline (pretreatment) and post-treatment, using atomic force microscope in order to obtain three-dimensional images and mean roughness. Specimens submitted to immersion were submerged in the vehicles without brushing. For brushed specimens, procedures were conducted using a linear brushing machine with a soft-bristled toothbrush. Immersion and brushing were performed for 244 h. IFT and BFT samples were analysed under scanning electron microscope with Energy-Dispersive X-ray Spectroscopy (EDS). Pre and post-treatment values were compared using the paired Student T-test (alpha = .05). Intergroup comparisons were conducted using one-way ANOVA with Tukey post-test (alpha = .05). Results: cp Ti mean roughness (in nanometers) comparing pre and post-treatment were: IW, 2.29 +/- 0.55/2.33 +/- 0.17; IT, 2.24 +/- 0.46/2.02 +/- 0.38; IFT, 2.22 +/- 0.53/1.95 +/- 0.36; BW, 2.22 +/- 0.42/3.76 +/- 0.45; BT, 2.27 +/- 0.55/16.05 +/- 3.25; BFT, 2.27 +/- 0.51/22.39 +/- 5.07. Mean roughness (in nanometers) measured in Ti-6Al-4V disks (pre/post-treatment) were: IW, 1.79 +/- 0.25/2.01 +/- 0.25; IT, 1.61 +/- 0.13/1.74 +/- 0.19; IFT, 1.92 +/- 0.39/2.29 +/- 0.51; BW, 2.00 +/- 0.71/2.05 +/- 0.43; BT, 2.37 +/- 0.86/11.17 +/- 2.29; BFT, 1.83 +/- 0.50/15.73 +/- 1.78. No significant differences were seen after immersions (p > .05). Brushing increased the roughness of cp Ti and of Ti-6Al-4V (p < .01); cp Ti had topographic changes after BW, BT and BFT treatments whilst Ti-6Al-4V was significantly different only after BT and BTF. EDS has not detected fluoride or sodium ions on metal surfaces. Conclusions: Exposure to toothpastes (immersion) does not affect titanium per se; their use during brushing affects titanium topography and roughness. The associated effects of toothpaste abrasives and fluorides seem to increase roughness on titanium brushed surfaces. (C) 2012 Elsevier Ltd. All rights reserved.
Resumo:
Objective. The aim of this study was to evaluate the castability of CP titanium and Ti-6Al-4V alloy castings into Rematitan Plus investment at three different mold temperatures.Methods. A nylon mesh pattern (20 mm with 64 squares and wire of 0.7 mm in diameter) was used for the castability testing. Initially, an image of the wax pattern was obtained by means of a digital camera and the total extension of filaments (mm) was then measured, using the Leica Qwin image analysis system. The mesh sprued was placed in the Rematitan Plus investment material and the castings were made in a Discovery Plasma machine at three different mold temperatures: 430 degrees C (control group), 480 degrees C or 530'C. Ten castings were made for each temperature. The images of the castings were analyzed (Leica Qwin) and the castability index determined by the number of the completely cast segments as a percentage of the wax pattern. Data were analyzed by two-way ANOVA and Tukey's multiple comparison test (a = 0.05) using materials and temperatures as discriminating variables.Results. The Ti-6Al-4V alloy (60.86%) presented a better castability index than CP Ti (48.44%) (p < 0.000001). For CP Ti, the temperature of 530 degrees C (23.96%) presented better castability than at other temperatures, 480 degrees C (14.66%) and 430 degrees C (12.54%), with no difference between them (p < 0.001). For Ti-6Al-4V alloy, there was a statistically significant difference among the three temperatures: 530 degrees C (28.36%) > 480 degrees C (19.66%) > 430 degrees C (15.97%) (p < 0.002).Significance. Within the limitations of this study, the increase in the mold temperature of the Rematitan Plus investment resulted in a better castability index for both materials, and Ti-6Al-4V presented a better castability index than CP Ti. (c) 2005 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Resumo:
The aim of the work was to evaluate the influence of the temperature of investment healting on the tensile strength and Vickers hardness of CP Ti and Ti-6Al-4V alloy casting. Were obtained for the tensile strength test dumbbell rods that were invested in the Rematitan Plus investment and casting in the Discovery machine cast. Thirty specimens were obtained, fiftten to the CP Titanium and fifteen to the Ti-6Al-4V alloy, five samples to each an of the three temperatures of investment: 430°C (control group), 480°C and 530°C. The tensile test was measured by means of a universal testing machine, MTS model 810, at a strain of 1.0 mm/min. After the tensile strenght test the specimens were secctioned, embedded and polished to hardness measurements, using a Vickers tester, Micromet 2100. The means values to tensile tests to the temperatures 430°C, 480 and 530: CP Ti (486.1 - 501.16 - 498.14 -mean 495.30 MPa) and Ti-6Al-4V alloy (961.33 - 958.26 - 1005.80 - mean 975.13 MPa) while for the Vickers hardness the values were (198.06, 197.85, 202.58 - mean 199.50) and (352.95, 339.36, 344.76 - mean 345.69), respectively. The values were submitted to Analysis of Variance (ANOVA) and Tukey' s Test that indicate differences significant only between the materials, but not between the temperature, for both the materias. It was conclued that increase of the temperature of investment its not chance the tensile strength and the Vickers hardness of the CP Titanium and Ti-6Al-4V alloy.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Pós-graduação em Reabilitação Oral - FOAR
On the evaluation of stability of rare earth oxides as face coats for investment casting of titanium
Resumo:
Attempts have been made to evaluate the thermal stability of rare earth oxide face coats against liquid titanium. Determination of microhardness profiles and concentration profiles of oxygen and metallic constituents of oxide in investment cast titanium rods has allowed grActation of relative stability of rare earth oxides. The relative stability of evaluated oxides in the order of increasing stability follows the sequence CeO2 — ZrO2 — Gd2O3 — didymium oxide — Sm2O3 —Nd2O3 — Y2O3. The grading does not follow the free energy data of the formation of these oxides. A better correlation with the experimental observations is obtained when the solubility of the metallic species in titanium is also taken into consideration.
Resumo:
A methodology for evaluating the reactivity of titanium with mould materials during casting has been developed. Microhardness profiles and analysis of oxygen contamination have provided an index for evaluation of the reactivity of titanium. Microhardness profile delineates two distinct regions, one of which is characterised by a low value of hardness which is invariant with distance. The reaction products are uniformly distributed in the metal in this region. The second is characterised by a sharp decrease in microhardness with distance from the metal-mould interface. It represents a diffusion zone for solutes that dissolve into titanium from the mould. The qualitative profiles for contaminants determined by scanning electron probe microanalyser and secondary ion mass spectroscopy in the as-cast titanium were found to be similar to that of microhardness, implying that microhardness can be considered as an index of the contamination resulting from metal-mould reaction.
Resumo:
Metal-mold reaction during Ti casting in zircon sand molds has been studied using scanning electron microscope, energy and wave length dispersive analysis of X-rays, X-ray diffraction, microhardness measurements, and chemical analysis. Experimental results suggest that oxides from the mold are not fully leached out by liquid Ti, but oxygen is preferentially transferred to liquid Ti, leaving behind metallic constituents in the mold as lower oxides or intermetallics of Ti. The electron microprobe analysis has revealed the depth profile of contaminants from the mold into the cast Ti metal. The elements Si, Zr and O were found to have diffused to a considerable distance within the Ti metals. A possible mechanism has now been evolved in regard to the reactions that occur during casting of Ti in zircon sand molds.
Resumo:
TiAl castings are prone to various defects including bubbles entrained during the turbulent filling of moulds. The present research has exploited the principles of the Durville tilt casting technique to develop a novel process in which the Induction Skull Melting (ISM) of TiAl alloys in a vacuum chamber has been combined with controlled tilt pouring to achieve the tranquil transfer of the metal into a hot ceramic shell mould. Practical casting equipment has been developed to evaluate the feasibility of this process in parallel with the development of novel software to simulate and optimize it. The PHYSICA CFD code was used to simulate the filling, heat transfer and solidification during tilt pouring using a number of free surface modelling techniques, including the novel Counter Diffusion Method (CDM). In view of the limited superheat, particular attention was paid to the mould design to minimize heat loss and gas entrainment caused by interaction between the counter-flowing metal and gas streams. The model has been validated against real-time X-ray movies of the tilt casting of aluminium and against TiAl blade castings. Modelling has contributed to designing a mould to promote progressive filling of the casting and has led to the use of a parabolic tilting cycle to balance the competing requirements for rapid filling to minimize the loss of superheat and slow filling minimize the turbulence-induced defects.
Resumo:
The tilt-casting method is used to achieve tranquil filling of gamma-TiAl turbine blades. The reactive alloy is melted in a cold crucible using an induction coil and then the complete crucible-mould- running system assembly is rotated through 180degrees to transfer the metal into the mould. The induction current is ramped down gradually as the rotation starts and the mould is preheated to maintain superheat. The liquid metal then enters the mould and the gas within it (argon) escapes through the inlet aperture and through auxiliary vents. Solidification starts as soon the metal enters the mould and it is important to account for this effect to predict and prevent misruns. The rotation rate has to be controlled carefully to allow sufficient time for gas evacuation, but at the same time preserve superheat. This 3-phase system is modelled using the FV method, with a fast implicit numerical scheme used to capture the transient liquid free surface. The enthalpy method is used to model solidification and predict defects such as trapped bubbles, macro-porosity or surface connected porosity. Modeling is used to support an experimental program for the development of a production method for gamma-TiAl blades, with a target length of 40cm. The experiments provide validation for the model and the model in turn optimizes the tilt-casting process. The work is part of the EU project IMPRESS.
Resumo:
This study compared the vertical misfit of 3-unit implant-supported nickel-chromium (Ni-Cr) and cobalt-chromium (Co-Cr) alloy and commercially pure titanium (cpTi) frameworks after casting as 1 piece, after sectioning and laser welding, and after simulated porcelain firings. The results on the tightened side showed no statistically significant differences. On the opposite side, statistically significant differences were found for Co-Cr alloy (118.64 mu m [SD: 91.48] to 39.90 mu m [SD: 27.13]) and cpTi (118.56 mu m [51.35] to 27.87 mu m [12.71]) when comparing 1-piece to laser-welded frameworks. With both sides tightened, only Co-Cr alloy showed statistically significant differences after laser welding. Ni-Cr alloy showed the lowest misfit values, though the differences were not statistically significantly different. Simulated porcelain firings revealed no significant differences.