Hafnium dioxide (HfO2) films, deposited using electron beam evaporation, are optimized for high performance back-gated graphene transistors. Bilayer graphene is identified on HfO2/Si substrate using optical microscope and subsequently confirmed with Raman spectroscopy. Back-gated graphene transistor, with 32 nm thick HfO2 gate dielectric, has been fabricated with very high transconductance value of 60 mu S. From the hysteresis of the current-voltage characteristics, we estimate the trap density in HfO2 to be in the mid 10(11)/cm(2) range, comparable to SiO2.
Resumo:
HfO2 thin films deposited on Si substrate using electron beam evaporation, are evaluated for back-gated graphene transistors. The amount of O-2 flow rate, during vaporation is optimized for 35 nm thick HfO2 films, to achieve the best optical, chemical and electrical properties. It has been observed that with increasing oxygen flow rate, thickness of the films increased and refractive index decreased due to increase in porosity resulting from the scattering of the evaporant. The films deposited at low O-2 flow rates (1 and 3 SCCM) show better optical and compositional properties. The effects of post-deposition annealing and post-metallization annealing in forming gas ambience (FGA) on the optical and electrical properties of the films have been analyzed. The film deposited at 3 SCCM O-2 flow rate shows the best properties as measured on MOS capacitors. To evaluate the performance of device properties, back-gated bilayer graphene transistors on HfO2 films deposited at two O-2 flow rates of 3 and 20 SCCM have been fabricated and characterized. The transistor with HfO2 film deposited at 3 SCCM O-2 flow rate shows better electrical properties consistent with the observations on MOS capacitor structures. This suggests that an optimum oxygen pressure is necessary to get good quality films for high performance devices.
Resumo:
We investigated the effect of oxygen flow rate during the reactive magnetron sputtering on the compositional, structural, optical and electrical properties of HfO2 films. We also studied the influence of annealing temperature on the structural and electrical properties of optimized HfO2 films of 25 to 30 nm thick. X-ray photoelectron study reveals that the films deposited at 15 SCCM of oxygen flow rate are stoichiometric and have an optical band gap of 5.86 eV. X-ray diffraction indicates that films without oxygen flow are amorphous, and beyond an oxygen flow rate of 5 SCCM exhibit polycrystalline monoclinic structure. At an annealing temperature of 600 degrees C, tetragonal phase was observed besides the monoclinic phase. The dielectric constant of 11 and low leakage currents of 1 x 10(-7) A/cm(2) were achieved for the stoichiometric films. As-deposited films show significant frequency dispersion due to the presence of defect states at the HfO2/Si interface, and it reduces after annealing.
Resumo:
This paper reports an improvement in Pt/n-GaN metal-semiconductor (MS) Schottky diode characteristics by the introduction of a layer of HfO2 (5 nm) between the metal and semiconductor interface. The resulting Pt/HfO2/n-GaN metal-insulator-semiconductor (MIS) Schottky diode showed an increase in rectification ratio from 35.9 to 98.9(@ 2V), increase in barrier height (0.52 eV to 0.63eV) and a reduction in ideality factor (2.1 to 1.3) as compared to the MS Schottky. Epitaxial n-type GaN films of thickness 300nm were grown using plasma assisted molecular beam epitaxy (PAMBE). The crystalline and optical qualities of the films were confirmed using high resolution X-ray diffraction and photoluminescence measurements. Metal-semiconductor (Pt/n-GaN) and metal-insulator-semiconductor (Pt/HfO2/n-GaN) Schottky diodes were fabricated. To gain further understanding of the Pt/HfO2/GaN interface, I-V characterisation was carried out on the MIS Schottky diode over a temperature range of 150 K to 370 K. The barrier height was found to increase (0.3 eV to 0.79 eV) and the ideality factor decreased (3.6 to 1.2) with increase in temperature from 150 K to 370 K. This temperature dependence was attributed to the inhomogeneous nature of the contact and the explanation was validated by fitting the experimental data into a Gaussian distribution of barrier heights. (C) 2015 Author(s).
Resumo:
Laser conditioning effects of the HfO2/SiO2 antireflective (AR) coatings at 1064 nm and the accumulation effects of multishot laser radiation were investigated. The HfO2/SiO2 AR coatings were prepared by E-beam evaporation (EBE). The singleshot and multi-shot laser induced damage threshold was detected following ISO standard 11254-1.2, and the laser conditioning was conducted by three-step raster scanning method. It was found that the single-shot LIDT and multi-shot LIDT was almost the same. The damage mostly > 80% occurred in the first shot under multi-shot laser radiation, and after that the damage occurring probability plummeted to < 5%. There was no obvious enhancement of the laser damage resistance for both the single-shot and multi-shot laser radiation of the AR coatings after laser conditioning. A Nomarski microscope was employed to map the damage morphology, and it found that the damage behavior is defect-initiated for both unconditioned and conditioned samples. © 2004 Elsevier B.V. All rights reserved.
Resumo:
By analysis of impurity elements in HfO2 coating material, the influence of main impurity elements on the characteristic of coatings were studied. The results indicate that the metal elements and absorptive dielectric elements damage the HfO2 coatings. The more the Zr element content is, the more the absorption is for the coatings in ultraviolet wave. The negative ion element will become the gas source center and form an ejection in the process of evaporation of coating material, so decrease the damage threshold of the coatings.
Resumo:
Negative ion element impurities breakdown model in HfO2 thin film was reported in this paper. The content of negative ion elements were detected by glow discharge mass spectrum analysis (GDMS); HfO2 thin films were deposited by the electron-beam evaporation method. The weak absorption and laser induced damage threshold (LIDT) of HfO2 thin films were measured to testify the negative ion element impurity breakdown model. It was found that the LIDT would decrease and the absorption would increase with increasing the content of negative ion element. These results indicated that negative ion elements were harmful impurities and would speed up the damage of thin film. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
We prepare HfO2 thin films by electron beam evaporation technology. The samples are annealed in air after deposition. With increasing annealing temperature, it is found that the absorption of the samples decreases firstly and then increases. Also, the laser-induced damage threshold (LIDT) increases firstly and then decreases. When annealing temperature is 473K, the sample has the highest LIDT of 2.17J/cm(2), and the lowest absorption of 18 ppm. By investigating the optical and structural characteristics and their relations to LIDT, it is shown that the principal factor dominating the LIDT is absorption.
Resumo:
采用电子束蒸发沉积方法在BK7玻璃基底和熔融石英基底上沉积了HfO2薄膜,研究了不同沉积温度下的应力变化规律。利用ZYGO干涉仪测量了基片镀膜前后曲率半径的变化,计算了薄膜应力。结果发现在所考察的实验条件下HfO2薄膜的残余应力均为张应力,应力值随沉积温度的升高先增大后减小。两种基底上薄膜的残余应力的主要产生机制不同。对于BK7玻璃基底HfO2薄膜的残余应力起决定作用的是内应力,熔融石英基底上HfO2薄膜的残余应力在较低沉积温度下制备的薄膜起决定作用的是热应力,在沉积温度进一步升高后内应力开始起决定作用。
Resumo:
The single- and multi-shot damage behaviors of HfO2/SiO2 high-reflecting (HR) coatings under Nd:YAG laser exposure were investigated. Fundamental aspects of multi-shot laser damage, such as the instability due to pulse-to-pulse accumulation of absorption defect and structural defect effect, and the mechanism of laser induced defect generation, are considered. It was found in multi-shot damage, the main factors influencing laser-induced damage threshold (LIDT) are accumulation of irreversible changes of structural defects and thermal stress that induced by thermal density fluctuations.
Resumo:
利用蒸发氧化铪和离子辅助蒸发金属铪反应沉积氧化铪薄膜,对两种工艺下制备的氧化铪薄膜进行光学和结构以及激光损伤特性的研究,实验结果表明,用金属铪反应沉积的氧化铪薄膜不仅结构均匀,并且具有较高的激光损伤阈值.文章对损伤阈值和薄膜的结构及光学特性之间的关系进行了讨论。
Resumo:
HfO2 films were deposited by electron beam evaporation with different deposition parameters. The properties such as refractive index, weak absorption, and laser induced damage thresholds (LIDTs) of these films have been investigated. It was found that when pulsed Nd:YAG 1064 nm laser is used to investigate LIDT of films: Metallic character is the main factor that influences LIDTs of films obtained from Hf starting material by ion-assisted reaction, and films prepared with higher momentum transfer parameter P have fewer metallic character; The ion-assisted reaction parameters are key points for preparing high LIDT films and if the parameters are chose properly, high LIDT films can be obtained. (c) 2004 Elsevier B.V. All rights reserved.
Resumo:
用电子柬蒸发方法制备了HfO2薄膜,根据镀膜前后基片曲率半径的变化,用Stoney公式计算了薄膜应力。讨论了沉积温度对薄膜残余应力的影响。结果发现,HfO2薄膜的残余应力均为张应力,应力值随沉积温度的升高先增大后减小,在280℃左右出现极大值。对样品进行了XRD测试,从微观结构上对实验结果进行了分析,发现微结构演变引起的内应力变化是引起薄膜残余应力改变的主要因素,HfO2薄膜在所选沉积温度60~350℃内出现了晶态转变,堆积密度随温度升高而增大。
Resumo: