273 resultados para Óxidos de ferro
Resumo:
A natural clay from Campina Grande region (Paraíba, Brazil), with 8.57% of Fe2O3, was used to study the most appropriate condition to carry out the iron extraction, without altering the clay structure in a significant way. Samples were treated with the Dithionite-Citrate-Bicarbonate method (DCB) for 30 and 120 minutes (pH=9.1), and also with citric acid (pH=1.8; time=15min), at 75°C. Conductivity measurements, X-ray fluorescence, X-ray diffraction, energy-dispersive spectrometry, electron-diffraction with transmission electron microscopy and textural evaluation by nitrogen adsorption were done. The treatment in a basic medium was more selective for iron removal than in acid condition. The time of 30 minutes, with 1.6 g Na2S2O4/10 g clay, was the best condition for the iron extraction.
Resumo:
Independent of the sample form (powder or film), XRD analysis of Ir0,3Ti(0,7-x)Ce xO2, (nominal) mixtures, for x=0, shows the formation of a solid solution phase between IrO2 and TiO2, as well as the rutile phases of IrO2 and TiO2. The presence of the anatase phase of TiO2 is also confirmed. The introduction of 30 mol% CeO2 in the mixture reveals the presence of the CeO2 and Ce2O3 phases, besides the already mentioned ones, in the powder. In the film form, however, an amorphous phase is identified. When all of the TiO2 is substituded by CeO2, for both sample forms, the only phases found are IrO2, CeO2 and Ce2O3. This result suggests cerium oxides are not capable of forming solid solutions with either IrO2 or (Ir,Ti)O2 acting solely as a dispersant matrix for these phases. These results are consistent with the much higher electrochemically active surface area when CeO2 is introduced in the binary Ti/Ir0,3Ti0,7O2 mixture. It was possible to establish a relationship between the electrochemical stability of the supported films and their crystalline structure. The unexpected presence of TiO2 and Ti2O3 in the Ti/Ir0,3Ce0,7O2 (film sample) is attributed to oxidation of the Ti support during the calcination step.
Resumo:
In the present work four different analytical methodologies were studied for the determination of iron and titanium in Portland cement. The cement samples were dissolved with hot HCl and HF, being compared Fe and Ti concentrations through four analytical methods: molecular absorption spectrophotometry using the reagents 1,2-hydroxybenzene-3,5-disulfonic acid (Tiron) and the 5-chloro-salicylic acid (CSA), inductively coupled plasma atomic emission spectrometry (ICP-AES) and flame atomic absorption spectrophotometry (FAAS). In the spectrophotometric determinations were studied pH conditions, reagents addition order, interferences, amount of reagents, linear range and stability of the system. In the techniques of ICP-AES and FAAS were studied the best lines, interferences, sensibility and linear range. The obtained results were compared and the agreement was evaluated among the methods for the determination of the metals of interest.
Resumo:
Copper, aluminum and iron concentrations were determined in four geochemical fractions of three different basaltic soils from the northwest region of the Parana State, Brazil. The fractions examined were the reducible manganese dioxide and amorphous iron oxide, crystaline iron oxide, organic and residual. Metal concentrations were determined in the extracts by flame atomic absorption spectrophotometry. High Fe concentrations were extracted from the crystalline iron oxide (>20%), as well as the amorphous iron oxide (>12%). Copper was extracted from the amorphous and crystalline iron oxides in the range 5 to 12%, but low concentrations were bound to organic matter. Low concentrations of aluminum were extracted (<8%) from the amorphous and crystaline iron oxides, and organic matter. High concentrations of aluminum were found in the residual fraction.
Resumo:
Particles of porous silica or other solvent resistent inorganic oxides can be functionalized by aliphatic (e.g., C-8 or C-18) or other groups to give stationary phases for use in reversed phase HPLC. The functionalization can be done by bonding of individual groups to the surface of the support particles, by producing an organic polymeric film from pre-polymers, or by adsorbing/immobilizing pre-formed polymers on the surfaces. These three types of functionalization are reviewed.
Resumo:
Bottom ash has been used as raw material to glass and glass ceramic production because it is a source of SiO2 and Al2O3. However, the high concentration of iron (about 10% wt.) difficulty the control of the nucleation and the crystallization processes. The iron content was reduced by magnetic process, where the magnetite phase was mainly removed. In order to compare glass ceramics obtained from original and low iron bottom ashes, microstructural and dilatometric characterizations were performed.
Influência da calcinação sobre a remoção de ferro da caulinita e ilita e seus efeitos sobre a acidez
Resumo:
Samples of natural clay composed by kaolinite, illite, goethite and quartz, were calcinated and submitted to lixiviation with citrate and chloridric acid in order to remove iron. Investigation due to extraction consequences was carried cut by analyzing its acid properties using ammonia gas as probe in infrared spectrophotometry analysis. The sample that were treated with citrate followed by acid lixiviation yield materials twice more acid than samples treated with acid only.
Resumo:
Chromium and potassium-doped iron oxides are widely used as industrial catalysts in the dehydrogenation of ethylbenzene to produce styrene. They have several advantages but deactivate with time, because of the loss of potassium. Also, they are toxic due to chromium compounds. Therefore there is a need for developing alternative non toxic catalysts without potassium. Then, iron and aluminum compounds were prepared by different methods in this work. Different phases were produced depending on the preparation method. Aluminum-doped hematite was more active and selective to styrene than the aluminum ferrite. Aluminum acts both as textural and structural promoter in the catalysts.
Resumo:
Sequential extraction is not totally effective to dissolve distinct forms of trace elements. The extractive solution, for example, can dissolve less of the target fraction and more than another not wished fraction. The goal of this work is to compare the extraction of native iron with three sequential extraction methods of the heavy metals, using three soils with different physical chemistry characteristics: a histosol, an oxisol, and a mollisol. The results obtained in this work demonstrate that a smaller relation soil/extractor results in a larger extraction in almost all phases. The use of many stages of the sequential extraction, with the purpose of more association of the metal with different components of the soil, can result, among other things, in modification of the substratum by the action of the reagents used, besides reducing the selectivity of the more specific extractors. Readsorption and redistribution of the heavy metals could have happened with larger intensity in the fraction where hidroxilamine was used with higher temperature. Sequential extraction of iron, without enrichment of soil samples, in the respective fractions in each method, it was important to better understand the behavior of the reagents considered specific to each form of the metal in soil.
Resumo:
Tungsten oxide thin films with three different compositions were deposited by reactive sputtering in an oxygen-argon plasma. In a system composed of a home made photochemical reactor coupled with an optic fiber spectrophotometer, the photochromic effect was studied in these oxide films as function of UV irradiation time, in ethanol, methanol and formaldehyde atmospheres. It was observed that the photochromic efficiency depends on the vapor chemical nature where the film is irradiated as well as the film composition. Kinetic analysis suggest that two kinds of optical absorption centers should respond by the photochromic effect in these films, one generated at film surface and other inside it, which one presenting a different time constant.
Resumo:
Simultaneous oxidation/co-precipitation of an equimolar mixture of La(III) and Co(II) nitrates and La(III) nitrate and Mn(II) chloride afforded a hydroxide gel, which was converted to LaCoO3 and LaMnO3 on calcination at 600 °C. After calcination, the obtained perovskites have been characterised by X-ray diffraction (XRD), X- ray photoelectron spectroscopy (XPS), thermogravimetric analysis (DTA - TGA) and BET specific surface determination. Specific surface areas of perovskites were 12 - 60 m²/g. XRD analysis showed that LaCoO3 and LaMnO3 are simple phase perovskite - type oxides. Traces of LaOCl, in addition to the perovskite were detected in the LaMnO3. The catalytic behavior was examined in the propane and CO oxidation. The LaCoO3 catalyst was more active to CO2 than the LaMnO3 catalyst.
Resumo:
Contaminant gases in the atmosphere constitute an important problem to be solved in the world. The NOx gases produced as a consequence of engine high temperatures are deleterious to environment and human health, as they promote acid rain and can act in the same way as freons in the destruction of the ozone layer in the stratosphere. In this review, three way and selective reduction catalysts for decomposition of these contaminant gases are described. Details about conditions and problems, such as catalyst poisoning, and the search for new catalysts are shown.
Resumo:
Anthropogenic pollution of groundwater and surface water has become a very serious environmental problem around the world. A wide range of toxic pollutants is recalcitrant to the conventional treatment methods, thus there is much interest in the development of more efficient remediation processes. Degradation of organic pollutants by zero-valent iron is one of the most promising approaches for water treatment, mainly because it is of low cost, easy to obtain and effective. After a general introduction to water pollution and current treatments, this work highlights the advances, applications and future trends of water remediation by zero-valent iron. Special attention is given to degradation of organochloride and nitroaromatic compounds, which are commonly found in textile and paper mill effluents.
Resumo:
In this work the degradation of aqueous solutions of reactive azo-dyes is reported using a combined reductive/advanced oxidative process based in the H2O2/zero-valent iron system. At optimized experimental conditions (pH 7, H2O2 100 mg L-1, iron 7 g L-1) and using a continuous system containing commercial iron wool, the process afforded almost total discolorization of aqueous solutions of three reactive azo-dyes (reactive orange 16, reactive black 5 and brilliant yellow 3G-P) at a hydraulic retention time of 2.5 min. At these conditions the hydrogen peroxide is almost totally consumed while the released total soluble iron reaches a concentration compatible with the current Brazilian legislation (15 mg L-1).
Resumo:
Two samples of residues from iron mining plants have been investigated for their retention capacity of As, Cu, Cr, and Pb. The sample with the higher content of iron oxides showed the highest capacity to retain metals. The adsorption affinity series changes from Pb>Cu>Cr~As to As>Pb>Cu>Cr or As>Cu>Cr>Pb, depending on the material and the concentration of the initial solution. In the competitive environment, the Pb adsorption decreases and the As, Cu and Cr adsorption increases. Sequential extraction procedures, carried out after adsorption batch experiments, showed that the most important adsorption process occurs in the oxide fraction and that the major part of the absorbed metal is remobilized from exchangeable and oxide fractions.