Extração de ferro de esmectita brasileira com emprego do método ditionito-citrato-bicarbonato


Autoria(s): Leite,Sidnei Quezada M.; Colodete,Carlos Henrique A.; Dieguez,Lídia Chaloub; San Gil,Rosane A. S.
Data(s)

01/06/2000

Resumo

A natural clay from Campina Grande region (Paraíba, Brazil), with 8.57% of Fe2O3, was used to study the most appropriate condition to carry out the iron extraction, without altering the clay structure in a significant way. Samples were treated with the Dithionite-Citrate-Bicarbonate method (DCB) for 30 and 120 minutes (pH=9.1), and also with citric acid (pH=1.8; time=15min), at 75°C. Conductivity measurements, X-ray fluorescence, X-ray diffraction, energy-dispersive spectrometry, electron-diffraction with transmission electron microscopy and textural evaluation by nitrogen adsorption were done. The treatment in a basic medium was more selective for iron removal than in acid condition. The time of 30 minutes, with 1.6 g Na2S2O4/10 g clay, was the best condition for the iron extraction.

Formato

text/html

Identificador

http://www.scielo.br/scielo.php?script=sci_arttext&pid=S0100-40422000000300002

Idioma(s)

pt

Publicador

Sociedade Brasileira de Química

Fonte

Química Nova v.23 n.3 2000

Palavras-Chave #brazilian clay #smectite #iron extraction