6 resultados para LB

em ArchiMeD - Elektronische Publikationen der Universität Mainz - Alemanha


Relevância:

10.00% 10.00%

Publicador:

Resumo:

In the present work a series of thiophene oligomers of three and six thiophene units were synthesized, starting from thiophene, and characterized. Polymers containing these electroative side groups were then prepared by two strategies. The oligomers were attached to existing polymer systems and were connected to a polymerizable unit leading to monomer containing the oligothiophenes as side groups. Subsequently the properties of the monomers and the polymers were investigated. A butylcellulose derivative carrying terthienyl side chains (BCTTE, 26) was synthesized starting from cellulose acetate and 5-(2-chloroethyl)-2,2':5',2'-terthiophene (4). The polymer had a degree of substitution (DS) of the butyl and terthienyl side chains of DSbutyl = 1.9 and DSterth = 0.35, respectively. It was successfully spread on a Langmuir-Blodgett (LB) trough and then transferred to several solid substrates. X-rays reflectometry showed an ordered architecture of the cellulose backbones. However, the terthiophene side groups were found as isotropically aligned by polarized UV-Vis spectroscopy. When used as anode material in the electropolymerization of 3-pentylthiophene (28), polythiophene was grafted onto the cellulose backbone through the terthienyl side groups. The polythiophene chains showed an average anisotropic alignment of 20 % along the LB dipping direction, calculated by means of polarized UV-Vis spectroscopy. A second butylcellulose derivative carrying sexithienyl side chains (BCST) was synthesized and investigated, starting from butylcellulose and 2-[b ', b ''-dipentyl-5'''-(2-hydroxyethyl)-2,2': 5',2':5',2'':5'',2'':5'',2'''-sexithiophen-5-yl]-ethyl p-toluensulfonate (7). The polymer showed formation of stable LB monolayers at the air-water interface, but its transfer onto solid substrates was not successful. A poly(p-phenylene-ethynylene) bearing sexithienyl side chains (BzAcST, 31) was prepared by reaction of the two monomers 2-[b ', b ''-dipentyl-5'''-(2-hydroxyethyl)-2,2': 5',2':5',2'':5'',2'':5'',2'''-sexithiophen-5-yl]-ethyl 2,5-diiodobenzoate (15) and 2-[b', b ''-dipentyl-5'''-(2-hydroxyethyl)-2,2':5',2':5',2'':5'',2'':5'',2'''-sexithiophen-5-yl]-ethyl 2,5-diethynylbenzoate (18). The polymer was obtained as insoluble product. Upon oxidation with FeCl3 (doping) of the polymer suspension, BzAcST showed an electrical conductivity of ó = 2.5 . 10 -6 S/cm, a typical value for semiconductors. The IR spectrum of the doped polymer presented the diagnostic bands of oxidized sexithiophene in good agreement with literature results. Along with the monomer and polymer synthesis, an a,a '-disubstituted sexithiophene, b ', b ''-dipentyl-5,5'''-bis-(2-hydroxyethyl)-2,2':5',2':5',2'':5'',2'':5'',2'''-sexithiophene (6a),was synthesized and characterized. The UV-Vis absorption of the chromophore wasinvestigated as a function of temperature and different solvents, showing a blue-shift of the absorption maximum with increasing temperature and a red-shift changing the solvent from hexane to ethanol to toluene. Monitoring the change of the UV-Vis spectrum upon electrochemical oxidation, the oxidized chromophore showed a new broad absorption band, red shifted with respect to the p -p* transition of the neutral state. Upon reduction, the new band disappeared and the UV-Vis spectrum of the chromophore was restored. Such oxidation-reduction cycles were totally reversible. This feature, together with the absorption maximum falling in the visible region, makes this chromophore a suitable compound for the development of an electrochemical sensor.Attempts to polymerize acrylic monomers carrying sexythienyl side chains both via radical polymerization, as in the case of 2-[b ', b ''-dipentyl-5'''-(2-hydroxyethyl)-2,2': 5',2':5',2'':5'',2'':5'',2'''-sexithiophen-5-yl]-ethyl acrylate (8), and anionic polymerization, as in the case of 2-{b ', b ''-dipentyl-5'''-[2-(tertbutyldimethylsiloxy)ethyl]-2,2':5',2':5',2'':5'',2'': 5'',2''' -sexithiophen-5-yl}-ethylacrylate (29), were not successful, probably due to the steric hindrance of the oligothiophene side group. However, due to the time consuming and therefore restricted availability of the monomers, a screening of the polymerization conditions towards the formation of polymeric material was not possible.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Tethered bilayer lipid membranes provide an efficient, stable and versatile platform for the investigation of integrated membrane proteins. However, the incorporation of large proteins, as well as of proteins with a large submembrane part is still a very critical issue and therefore, further optimisation of the system is necessary. The central element of a tBLM is a lipid bilayer. Its proximal leaflet is, at least to some extend, covalently attached to a solid support via a spacer group. The anchor lipid consists of three distinct parts, a lipid headgroup, a spacer group and an anchor. All parts together influence the final bilayer properties. In the frame of this work, the synthesis of new thiolipids for tBLMs on gold has been investigated. The aim was to obtain molecules with longer spacers in order to increase the submembrane space. The systems obtained have been characterized using SPR and EIS. The results obtained during this study are multiple. First, the synthesis of a previously synthesized architecture was successfully scaled up in an industrial lab using a new synthetic approach. The synthesis of large amounts is now feasible. Then, the synthesis of the new thiolipids was carried out taking into account the following requirements: the increase of the submembrane space by having longer ethyleneglycol spacers, the attachment of the molecules to a gold substrate via a thiol bond, and the tunability of the lateral mobility by changing the lipid headgroup. Three different synthetic strategies have been investigated. The polymeric approach did not prove to be successful, merely because of the broad molecular weight distribution. The synthesis of heterofunctionally protected oligoethyleneglycols allowed to obtain ethyleneglycol moieties with 6 and 8 units, but the tedious purification steps gave very low yields. Finally, the block by block synthesis using ethyleneglycol precursors proved to be an efficient and fast method to synthesize the target molecules. Indeed, these were obtained with very high yields, and the separation was very efficient. A whole family of new compounds was obtained, having 6, 8 and 14 ethyleneglycol units and with mono- or diphytanyl lipid headgroups. This new pathway is a very promising synthetic strategy that can be used further in the development of new compounds of the tether system. The formation of bilayers was investigated for the different thiolipids mainly by using EIS. The electrical properties of a bilayer define the quality of the membrane and allow the study of the functionality of proteins embedded in such a system. Despite multiple trials to improve the system using self assembly, Langmuir Blodgett transfer, and detergent mixed vesicles, the new polymer thiolipids did not show as high electrical properties as tBLMs reported in the literature. Nevertheless, it was possible to show that a bilayer could be obtained for the different spacer lengths. These bilayers could be formed using self assembly for the first monolayer, and two different methods for bilayer formation, namely vesicle fusion and solvent exchange. We could furthermore show functional incorporation of the ion carrier valinomycin: the selective transport of K+ ions could be demonstrated. For DPHL, it was even possible to show the functional incorporation of the ion channel gramicidin. The influence of the spacer length is translated into an increase of the spacer capacitance, which could correspond to an increase in the capacity of charge accumulation in the submembrane space. The different systems need to be further optimised to improve the electrical properties of the bilayer. Moreover, the incorporation of larger proteins, and proteins bearing submembrane parts needs to be investigated.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Tethered bilayer lipid membranes (tBLMs) are a promising model system for the natural cell membrane. They consist of a lipid bilayer that is covalently coupled to a solid support via a spacer group. In this study, we developed a suitable approach to increase the submembrane space in tBLMs. The challenge is to create a membrane with a lower lipid density in order to increase the membrane fluidity, but to avoid defects that might appear due to an increase in the lateral space within the tethered monolayers. Therefore, various synthetic strategies and different monolayer preparation techniques were examined. Synthetical attempts to achieve a large ion reservoir were made in two directions: increasing the spacer length of the tether lipids and increasing the lateral distribution of the lipids in the monolayer. The first resulted in the synthesis of a small library of tether lipids (DPTT, DPHT and DPOT) characterized by 1H and 13C NMR, FD-MS, ATR, DSC and TGA. The synthetic strategy for their preparation includes synthesis of precursor with a double bond anchor that can be easily modified for different substrates (e.g. metal and metaloxide). Here, the double bond was modified into a thiol group suitable for gold surface. Another approach towards the preparation of homogeneous monolayers with decreased two-dimensional packing density was the synthesis of two novel anchor lipids: DPHDL and DDPTT. DPHDL is “self-diluted” tether lipid containing two lipoic anchor moieties. DDPTT has an extended lipophylic part that should lead to the preparation of diluted, leakage free proximal layers that will facilitate the completion of the bilayer. Our tool-box of tether lipids was completed with two fluorescent labeled lipid precursors with respectively one and two phytanyl chains in the hydrophobic region and a dansyl group as a fluorophore. The use of such fluorescently marked lipids is supposed to give additional information for the lipid distribution on the air-water interface. The Langmuir film balance was used to investigate the monolayer properties of four of the synthesized thiolated anchor lipids. The packing density and mixing behaviour were examined. The results have shown that mixing anchor with free lipids can homogeneously dilute the anchor lipid monolayers. Moreover, an increase in the hydrophylicity (PEG chain length) of the anchor lipids leads to a higher packing density. A decrease in the temperature results in a similar trend. However, increasing the number of phytanyl chains per lipid molecule is shown to decrease the packing density. LB-monolayers based on pure and mixed lipids in different ratio and transfer pressure were tested to form tBLMs with diluted inner layers. A combination of the LB-monolayer transfer with the solvent exchange method accomplished successfully the formation of tBLMs based on pure DPOT. Some preliminary investigations of the electrical sealing properties and protein incorporation of self-assembled DPOT and DDPTT-based tBLMs were conducted. The bilayer formation performed by solvent exchange resulted in membranes with high resistances and low capacitances. The appearance of space beneath the membrane is clearly visible in the impedance spectra expressed by a second RC element. The latter brings the conclusion that the longer spacer in DPOT and the bigger lateral space between the DDPTT molecules in the investigated systems essentially influence the electrical parameters of the membrane. Finally, we could show the functional incorporation of the small ion carrier valinomycin in both types of membranes.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Im Rahmen dieser Arbeit wurden drei neue Modelle zur funktionellen Mimiese biologischer Membranen im Bereich der Bionanotechnologie entwickelt. Um den Rahmen der notwendigen Faktoren und Komponenten für biomimetische Membranmodelle abzustecken, wurde das biologische Vorbild im Bezug auf Zusammensetzung, Organisation und Funktion analysiert. Die daraus abgeleiteten Erkenntnisse erlauben das Erreichen von biologisch relevanten Membranwiderständen im Bereich von mehreren MOhm cm2 und eine gute lokale Fluidität. Ein weiteres Ziel dieser Arbeit war die Entwicklung einer Hierachie unterschiedlich stark von der Festkörperoberfläche entkoppelter Membranen zur Vergrößerung des submembranen Raumes. Diese Ziele konnten realisiert werden. Das auf archaealen Etherlipiden basierende DPTL-System wurde analog dem biologischen Vorbild stereoselektiv synthetisiert und ist in der Lage die Membran bei maximaler Elongation des TEG-Spacers mit mehr als 2 nm von der Oberfläche zu entkoppeln. Die erzielten Wiederstände liegen im hohen ein- bis zweistelligen MOhm-Bereich, die Kapazität entspricht mit 0,5 µF cm-2 ebenfalls dem Wert biologischer Membranen. Die Membraneigenschaften wurden mit Hilfe von SPS, EIS, IR-Spektroskopie, QCM, AFM und Kontaktwinkelmessungen charakterisiert. Die Funktionalität und lokale Fluidität der DPTL-Membran konnte anhand des Valinomycin vermittelten K+-Transports über die Membran gezeigt werden. Fluide Elektroden oder laterale Verdünnung mit TEGL erlauben den Einbau größerer Ionenkanäle. Lipo-Glycopolymere (LGP) mit unterschiedlichen Kettenlängen wurden mit Hilfe der kontrollierten radikalischen Polymerisation mit einer PD < 1.2 synthetisiert. Es zeigte sich, daß die Vororientierung der LGPs auf dem LB-Trog, gefolgt von einem LB-Übertrag auf einen funktionalisierten Träger mit photoreaktivem SAM, nach Belichten des Systems zu einer verlässlichen kovalenten Anbindung der supramolekularen LGP-Architektur führt. Da die Lipo-Glycopolymerketten am Glycopolymerterminus nur mit oberflächennahen Repetiereinheiten an die photoaktivierte Oberfläche binden, sind sie in der Lage Oberflächenrauhigkeiten des Festkörpersubstrates auszugleichen. Die photochemische Immobilisierung von funktionell orientierten supramolekularen LGP-Architekturen auf Goldoberflächen resultiert in tBLMs mit großen vertikalen Enkopplungen der Membran von der Festkörperoberfläche (>8 nm). Der funktionelle Ionentransport von Kaliumionen durch Valinomycin zeigt eine ausreichende lokale Fluidität der Membran die mit einem guten Membranwiderstand (mehrere MOhm) kombiniert ist. Große Membran-Oberflächenentkopplungen konnten mit Hilfe plasmapolymerisierter elektrophiler Polymere erreicht werden. Filmdicken von 50 nm sind mit homogener Oberfläche und Rauhigkeiten im Bereich von Nanometern möglich. Das System zeigt interessante fluide Eigenschaften mit guten Erholungsraten bei FRAP-Experimenten (Diffusionskonstanten von etwa 17 mikro m2 s-1). Die elektrischen Eigenschaften liegen mit Widerständen von wenigen kOhm unterhalb der für gute Membranmimikrie notwendigen Werte. Erstmalig konnte gezeigt werden, daß mit Hilfe dieser Methode inerte Polymere/Plastikträger (zum Beispiel Polypropylen und TOPAS) in effizienter Weise kovalent mit reaktiven Polymeroberflächen modifiziert werden können (Anwendung als DNA-Chip ist beschrieben).

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The collapse of linear polyelectrolyte chains in a poor solvent: When does a collapsing polyelectrolyte collect its counter ions? The collapse of polyions in a poor solvent is a complex system and is an active research subject in the theoretical polyelectrolyte community. The complexity is due to the subtle interplay between hydrophobic effects, electrostatic interactions, entropy elasticity, intrinsic excluded volume as well as specific counter-ion and co-ion properties. Long range Coulomb forces can obscure single molecule properties. The here presented approach is to use just a small amount of screening salt in combination with a very high sample dilution in order to screen intermolecular interaction whereas keeping intramolecular interaction as much as possible (polyelectrolyte concentration cp ≤ 12 mg/L, salt concentration; Cs = 10^-5 mol/L). This is so far not described in literature. During collapse, the polyion is subject to a drastic change in size along with strong reduction of free counterions in solution. Therefore light scattering was utilized to obtain the size of the polyion whereas a conductivity setup was developed to monitor the proceeding of counterion collection by the polyion. Partially quaternized PVP’s below and above the Manning limit were investigated and compared to the collapse of their uncharged precursor. The collapses were induced by an isorefractive solvent/non-solvent mixture consisting of 1-propanol and 2-pentanone, with nearly constant dielectric constant. The solvent quality for the uncharged polyion could be quantified which, for the first time, allowed the experimental investigation of the effect of electrostatic interaction prior and during polyion collapse. Given that the Manning parameter M for QPVP4.3 is as low as lB / c = 0.6 (lB the Bjerrum length and c the mean contour distance between two charges), no counterion binding should occur. However the Walden product reduces with first addition of non solvent and accelerates when the structural collapse sets in. Since the dielectric constant of the solvent remains virtually constant during the chain collapse, the counterion binding is entirely caused by the reduction in the polyion chain dimension. The collapse is shifted to lower wns with higher degrees of quaternization as the samples QPVP20 and QPVP35 show (M = 2.8 respectively 4.9). The combination of light scattering and conductivity measurement revealed for the first time that polyion chains already collect their counter ions well above the theta-dimension when the dimensions start to shrink. Due to only small amounts of screening salt, strong electrostatic interactions bias dynamic as well as static light scattering measurements. An extended Zimm formula was derived to account for this interaction and to obtain the real chain dimensions. The effective degree of dissociation g could be obtained semi quantitatively using this extrapolated static in combination with conductivity measurements. One can conclude the expansion factor a and the effective degree of ionization of the polyion to be mutually dependent. In the good solvent regime g of QPVP4.3, QPVP20 and QPVP35 exhibited a decreasing value in the order 1 > g4.3 > g20 > g35. The low values of g for QPVP20 and QPVP35 are assumed to be responsible for the prior collapse of the higher quaternized samples. Collapse theory predicts dipole-dipole attraction to increase accordingly and even predicts a collapse in the good solvent regime. This could be exactly observed for the QPVP35 sample. The experimental results were compared to a newly developed theory of uniform spherical collapse induced by concomitant counterion binding developed by M. Muthukumar and A. Kundagrami. The theory agrees qualitatively with the location of the phase boundary as well as the trend of an increasing expansion with an increase of the degree of quaternization. However experimental determined g for the samples QPVP4.3, QPVP20 and QPVP35 decreases linearly with the degree of quaternization whereas this theory predicts an almost constant value.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

DNA block copolymer, a new class of hybrid material composed of a synthetic polymer and an oligodeoxynucleotide segment, owns unique properties which can not be achieved by only one of the two polymers. Among amphiphilic DNA block copolymers, DNA-b-polypropylene oxide (PPO) was chosen as a model system, because PPO is biocompatible and has a Tg < 0 °C. Both properties might be essential for future applications in living systems. During my PhD study, I focused on the properties and the structures of DNA-b-PPO molecules. First, DNA-b-PPO micelles were studied by scanning force microscopy (SFM) and fluorescence correlation spectroscopy (FCS). In order to control the size of micelles without re-synthesis, micelles were incubated with template-independent DNA polymerase TdT and deoxynucleotide triphosphates in reaction buffer solution. By carrying out ex-situ experiments, the growth of micelles was visualized by imaging in liquid with AFM. Complementary measurements with FCS and polyacrylamide gel electrophoresis (PAGE) confirmed the increase in size. Furthermore, the growing process was studied with AFM in-situ at 37 °C. Hereby the growth of individual micelles could be observed. In contrast to ex-situ reactions, the growth of micelles adsorbed on mica surface for in-situ experiments terminated about one hour after the reaction was initiated. Two reasons were identified for the termination: (i) block of catalytic sites by interaction with the substrate and (ii) reduced exchange of molecules between micelles and the liquid environment. In addition, a geometrical model for AFM imaging was developed which allowed deriving the average number of mononucleotides added to DNA-b-PPO molecules in dependence on the enzymatic reaction time (chapter 3). Second, a prototype of a macroscopic DNA machine made of DNA-b-PPO was investigated. As DNA-b-PPO molecules were amphiphilic, they could form a monolayer at the air-water interface. Using a Langmuir film balance, the energy released owing to DNA hybridization was converted into macroscopic movements of the barriers in the Langmuir trough. A specially adapted Langmuir trough was build to exchange the subphase without changing the water level significantly. Upon exchanging the subphase with complementary DNA containing buffer solution, an increase of lateral pressure was observed which could be attributed to hybridization of single stranded DNA-b-PPO. The pressure versus area/molecule isotherms were recorded before and after hybridization. I also carried out a series of control experiments, in order to identify the best conditions of realizing a DNA machine with DNA-b-PPO. To relate the lateral pressure with molecular structures, Langmuir Blodgett (LB) films were transferred to highly ordered pyrolytic graphite (HOPG) and mica substrates at different pressures. These films were then investigated with AFM (chapter 4). At last, this thesis includes studies of DNA and DNA block copolymer assemblies with AFM, which were performed in cooperation with different group of the Sonderforschungsbereich 625 “From Single Molecules to Nanoscopically Structured Materials”. AFM was proven to be an important method to confirm the formation of multiblock copolymers and DNA networks (chapter 5).