156 resultados para plasma treatment
em Repositório Institucional UNESP - Universidade Estadual Paulista "Julio de Mesquita Filho"
Resumo:
Mechanical strength of polyethylene terephthalate (PET) fibres and polymethyl methacrylate (PMMA) matrix composites were studied with particular interest on the effects of oxygen and argon plasma treated fibres. PET. fibres were treated in a radio frequency plasma reactor using argon or oxygen for different treatment times to increase the interface adhesion. Fibre volume fraction was measured through digital image analysis. Elastic moduli resulted between 3 GPa for untreated to 6 GPa for treated composites. Tensile tests on PET fibres showed that plasma treatment caused a decrease in average tensile strength compared to untreated fibres. Fracture analysis confirmed the increase in interfacial adhesion due to plasma treatment. (c) 2004 Elsevier Ltd. All rights reserved.
Resumo:
Polypropylene powder and sisal fibers were oxygen plasma treated, and the mechanical properties of their composites were tested. Two main effects were investigated: the incorporation of oxygen polar groups in the polypropylene surface and the surface degradation and chain scission of both polypropylene and sisal fibers. Prior to these treatments, three reactor configurations were tested to investigate the best condition for both effects to occur in PP film. Results showed that polypropylene-cellulose adhesion forces are about an order of magnitude higher for PP film treatments at 13.56 MHz than at 40 kHz owing to much higher chain scission at lower frequencies, although it probably also occurs at high frequency and high power. Polypropylene powder treated with oxygen plasma in optimum conditions for polar group incorporation did not result in improvement in any composite mechanical property, probably owing to the polymer melting. Sisal fibers and PP powder treated In conditions of surface degradation did not improve flexural or tensile properties but resulted in higher impact resistance, comparable to the improvement obtained with the addition of compatibilizer.
Resumo:
Plasma processing of carbon fibers (CFs) is aimed to provide better contact and adhesion between individual plies without decrease in the CF mechanical resistance. This paper deals with surface modification of CFs by an atmospheric pressure dielectric barrier discharge (DBD) for enhancing the adhesion between the CF and the polymeric matrix. The scanning electron microscopy of the treated samples revealed many small particles distributed over entire surface of the fiber. These particles are product of the fiber surface etching during the DBD treatment that removes the epoxy layer covering as-received samples. The alteration of the CF surface morphology was also confirmed by the Atomic force microscopy (AFM), which indicated that the CF roughness increased as a result of the plasma treatment. The analysis of the surface chemical composition provided by X-ray photoelectron spectroscopy showed that oxygen and nitrogen atoms are incorporated onto the surface. The polar oxygen groups formed on the surface lead to the increasing of the CF surface energy. The results of interlaminar shear strength test (short beam) of CFs/polypropylene composites demonstrated a greater shear resistance of the composites made with CFs treated by DBD than the one with untreated fibers. Both the increase in surface roughness and the surface oxidation contribute for the enhancement of CF adhesion properties. © 2012 IEEE.
Resumo:
Plasma treatments were applied on the surface of postconsumer polyethylene terephthalate (PET) bottles to increase their wettability and hasten the subsequent hydrolysis process. Sixty-four treatments were tested by varying plasma composition (oxygen and air), power (25-130 W), pressure (50-200 mTorr), and time (1 and 5 min). The best treatment was the one applied in air plasma at 130 W and 50 mTorr for 5 min, as it provided the lowest contact angle, 9.4°. Samples of PET before and after the optimized plasma condition were subjected to hydrolysis at 205°C. Although the treatment changed only a thin surface layer, its influence was evident up to relatively high conversion rates, as the treated samples presented more than 40% higher conversion rates than the untreated ones after 2 h of reaction. Infrared spectroscopy showed that the terephthalic acid obtained from 99% of depolymerization was similar to the commercial product used in PET synthesis. © 2012 Wiley Periodicals, Inc.
Resumo:
The surface energy of the implant surface has an impact on osseointegration. In this study, 2 surfaces: nonwashed resorbable blasting media (NWRBM; control) and Ar-based nonthermal plasma 30 days (Plasma 30 days; experimental), were investigated with a focus on the surface energy. The surface energy was characterized by the Owens-Wendt-Rabel-Kaelble method and the chemistry by X-ray photoelectron spectroscopy (XPS). Five adult beagle dogs received 8 implants (n = 2 per surface, per tibia). After 2 weeks, the animals were euthanized, and half of the implants (n = 20) were removal torqued and the other half were histologically processed (n = 20). The bone-to-implant contact (BIC) and bone area fraction occupancy (BAFO) were evaluated on the histologic sections. The XPS analysis showed peaks of C, Ca, O, and P for the control and experimental surfaces. While no significant difference was observed for BIC parameter (P > 0.75), a higher level for torque (P < 0.02) and BAFO parameter (P < 0.01) was observed for the experimental group. The surface elemental chemistry was modified by the plasma and lasted for 30 days after treatment resulting in improved biomechanical fixation and bone formation at 2 weeks compared to the control group. © 2013 Fernando P. S. Guastaldi et al.
Resumo:
This study evaluated the potential of plasma treatments to modify the surface chemistry and hydrophobicity of a denture base acrylic resin to reduce the Candida glabrata adhesion. Specimens (n=54) with smooth surfaces were made and divided into three groups (n=18): control - non-treated; experimental groups - submitted to plasma treatment (Ar/50W; AAt/130W). The effects of these treatments on chemical composition and surface topography of the acrylic resin were evaluated. Surface free energy measurements (SFE) were performed after the treatments and after 48h of immersion in water. For each group, half (n=9) of the specimens were preconditionated with saliva before the adhesion assay. The number of adhered C. glabrata was evaluated by cell counting after crystal violet staining. The Ar/50W and AAt/130W treatments altered the chemistry composition, hydrophobicity and topography of acrylic surface. The Ar/50W group showed significantly lower C. glabrata adherence than the control group, in the absence of saliva. After preconditioning with saliva, C. glabrata adherence in experimental and control groups did not differ significantly. There were significant changes in the SFE after immersion in water. The results demonstrated that Ar/50W treated surfaces have potential for reducing C. glabrata adhesion to denture base resins and deserve further investigation, especially to tailor the parameters to prolong the increased wettability. © 2012 Blackwell Verlag GmbH.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Statement of problem. Surface transformation with nonthermal plasma may be a suitable treatment for dental ceramics, because it does not affect the physical properties of the ceramic material.Purpose. The purpose of this study was to characterize the chemical composition of lithium disilicate ceramic and evaluate the surface of this material after nonthermal plasma treatment.Material and methods. A total of 21 specimens of lithium disilicate (10 mm in diameter and 3 mm thick) were fabricated and randomly divided into 3 groups (n=7) according to surface treatment. The control group was not subjected to any treatment except surface polishing with abrasive paper. In the hydrofluoric acid group, the specimens were subjected to hydrofluoric acid gel before silane application. Specimens in the nonthermal plasma group were subjected to the nonthermal plasma treatment. The contact angle was measured to calculate surface energy. In addition, superficial roughness was measured and was examined with scanning electron microscopy, and the chemical composition was characterized with energy-dispersive spectroscopy analysis. The results were analyzed with ANOVA and the Tukey honestly significant difference test (alpha=.05).Results. The water contact angle was decreased to 0 degrees after nonthermal plasma treatment. No significant difference in surface roughness was observed between the control and nonthermal plasma groups. Scanning electron microscopy and energy-dispersive spectroscopy images indicated higher amounts of oxygen (O) and silicon (Si) and a considerable reduction in carbon (C) in the specimens after nonthermal plasma treatment.Conclusions. Nonthermal plasma treatment can transform the characteristics of a ceramic surface without affecting its surface roughness. A reduction in C levels and an increase in 0 and Si levels were observed with the energy-dispersive spectroscopy analysis, indicating that the deposition of the thin silica film was efficient.
Resumo:
Plasma treatments are frequently employed to modify surface properties of materials such as adhesivity, hydrophobicity, oleophobicity etc. Present work deals with surface modification of common commercial polymers such as polyethylene terephthalate (PET) and polyurethane (PU) by an air dielectric barrier discharge (DBD) at atmospheric pressure. The DBD treatment was performed in a plain reactor in wire-duct geometry (non-uniform field reactor), which was driven by a 60 Hz power supply. Material characterization was carried out by water contact angle measurements, atomic force microscopy (AFM) and X-ray photoelectron spectroscopy (XPS). The plasma-induced modifications are associated with incorporation of polar oxygen and nitrogen containing groups on the polymer surface. The AFM analysis reveals that the plasma treatment roughens the material surface. Due to these structural and morphological changes the surface of DBD-treated polymers becomes more hydrophilic resulting in enhanced adhesion properties. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
This article reports on a series of experiments with polyethylene terepthalate (PET) treated in a radio frequency plasma reactor using argon and oxygen as a gas fuel, for treatment times equal to 5 s, 20 s, 30 s, and 100 s. The mechanical strength modification of PET fibers, evaluated by tensile tests on monofilaments, showed that oxygen and argon plasma treatment resulted in a decrease in the average tensile strength compared with the untreated fibers. This reduction in tensile strength is more significant for argon plasma and is very sensitive to the treatment time for oxygen plasma. Scanning electron microscopy (SEM) used to analyze the effects of cold plasma treatment on fiber surfaces indicates differences in roughness profiles depending on the type of treatments, which were associated with variations in mechanical strength. Differences in the roughness profile, surveyed through an image analysis method, provided the distance of roughness interval, D-ri. This parameter represents the number of peaks contained in a unit length and was introduced to correlate fiber surface condition, before and after cold plasma treatments, and average tensile strength. Statistical analysis of experimental data, using Weibull cumulative distribution and linear representation, was performed to explain influences of treatment time and environmental effects on mechanical properties. The shape parameter, alpha, and density parameter, beta, from the Weibull distribution function were used to indicate the experimental data range and to confirm the mechanical performance obtained experimentally.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Prosthetic composite is a widely used biomaterial that satisfies the criteria for application as an organic implant without adverse reactions. Polyethylene therephthalate (PET) fiber-reinforced composites have been used because of the excellent cell adhesion, biodegradability and biocompatibility. The chemical inertness and low surface energy of PET in general are associated with inadequate bonds for polymer reinforcements. It is recognized that the high strength of composites, which results from the interaction between the constituents, is directly related to the interfacial condition or to the interphase. A radio frequency plasma reactor using oxygen was used to treat PET fibers for 5, 20, 30 and 100 s. The treatment conditions were 13.56 MHz, 50 W, 40 Pa and 3.33 x 10(-7) m(3)/s. A Rame-Hart goniometer was used to measure the contact angle and surface energy variation of fibers treated for different times. The experimental results showed contact angle values from 47degrees to 13degrees and surface energies from 6.4 x 10(-6) to 8.3 x 10(-6) J for the range of 5 to 100 s, respectively. These results were confirmed by the average ultimate tensile strength of the PET fiber/polymethylmethacrylate (PMMA) matrix composite tested in tensile mode and by scanning electron microscopy. (C) 2003 Elsevier B.V. All rights reserved.
Resumo:
This work was performed to verify the chemical structure, mechanical and hydrophilic properties of amorphous hydrogenated carbon films prepared by plasma enhanced chemical vapor deposition, using acetylene/argon mixture as monomer. Films were prepared in a cylindrical quartz reactor, fed by 13.56 MHz radiofrequency. The films were grown during 5 min, for power varying from 25 to 125 W at a fixed pressure of 9.5 Pa. After deposition, all samples were treated by SF(6) plasma with the aim of changing their hydrophilic character. Film chemical structure investigated by Raman spectroscopy, revealed the increase of sp(3) hybridized carbon bonds as the plasma power increases. Hardness measurements performed by the nanoindentation technique showed an improvement from 5 GPa to 14 GPa following the increase discharge power. The untreated films presented a hydrophilic character, which slightly diminished after SF(6) plasma treatment.
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)