(1) C6H2N3O7- center dot C5H12NO2+, Mr = 346.26, P2(1)/c, a = 7.2356(6), b = 10.5765(9), c = 19.593(2) angstrom, 3 beta=95.101(6)degrees, V = 1493.5(2) angstrom(3), Z = 4, R-1 = 0.0414; (2) C6H2N3O7- center dot C6H8NO+, Mr = 38.24, P2(1)/n, a = 7.8713(5), b = 6.1979(7), c = 28.697(3) angstrom, beta = 90.028(7)degrees, V = 1400.0(2) angstrom(3), Z = 4, R-1 = 0.0416. The packing units in both compounds consist of hydrogen bonded cation-anion pairs. The (hyper)polarizabilities have been calculated for the crystallographic and optimized molecules, by AM1 and at the DFT/B3LYP(6-31G**) level.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Coorden§Ã£o de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Crystalline lead-pyrophosphate precursor was prepared in aqueous solution from lead nitrate and phosphoric acid and characterized by X-ray diffraction, thermogravimetry and Raman scattering. This crystalline lead-phosphate was then used to prepare glass samples in the binary system Pb(2)P(2)O(7)-WO(3). Dependence of WO(3) content on thermal, structural and optical properties were investigated by thermal analysis (DSC), Raman spectroscopy, UV-visible and near-infrared absorption and M-Line technique to access refractive index values. Incorporation of WO(3) in the lead-pyrophosphate matrix enhances the glass transition temperature and thermal stability against devitrification, favors formation of P-O-W bonds and WO(6) clusters. In addition, optical properties are strongly modified with a redshift of the optical bandgap with WO(3) incorporation as well as an increase of the refractive index from 1.89 to 2.05 in the visible. (C) 2011 Elsevier B.V. All rights reserved.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Thin films of potassium niobate were deposited on MgO (100) substrates by the polymeric precursor method and annealing in static air at 600 degreesC for 20 h. The obtained films were characterized by X-ray diffraction, atomic force microscopy (AFM) and the prism coupling method. The phi-scan diffraction evidenced the growth of the films with fourfold symmetry. AFM study shows that the films are homogeneous, dense and present a smooth surface. The refractive index and optical losses were strongly influenced by the degree of crystallinity. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Coorden§Ã£o de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Coorden§Ã£o de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

70.00% 70.00%

Publicador:

Resumo:

Coorden§Ã£o de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

70.00% 70.00%

Publicador:

Resumo:

We report, for the first time to our knowledge, experimental results on pedestal waveguides produced with Yb3+/Er3+ codoped Bi2O3-WO3-TeO2 thin films deposited by RF Sputtering for photonic applications. Thin films were deposited using Ar/O-2 plasma at 5 mTorr pressure and RF power of 40 W on substrates of silicon wafers. The definition of the pedestal waveguide structure was made using conventional optical lithography followed by plasma etching. Propagation losses around 2.0 dB/cm and 2.5 dB/cm were obtained at 633 and 1050 nm, respectively, for waveguides in the 20-100 mu m width range. Single-mode propagation was measured for waveguides width up to 10 mu m and 12 mu m, at 633 nm and 1050 nm, respectively; for larger waveguides widths multi-mode propagation was obtained. Internal gain of 5.6 dB at 1530 nm, under 980 nm excitation, was measured for 1.5 cm waveguide length (similar to 3.7 dB/cm). The present results show the possibility of using Yb3+/Er3+ codoped Bi2O3-WO3-TeO2 pedestal waveguide for optical amplifiers. (C) 2014 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coorden§Ã£o de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

In the present work, tellurite 20Li(2)O-80TeO(2) glasses were prepared with identical nominal composition under different glass-forming histories to produce a stressed and stress-free samples. X-ray Diffraction (XRD) and Differential Scanning Calorimetry (DSC) techniques were used to study the effects of the glass-forming histories on the thermal and structural properties of these glasses. The gamma-TeO2 (metastable), alpha-TeO2 and alpha-Li2Te2O5 phases were identified during the controlled devitrification in these glasses. The mestastable character of the gamma-TeO2 phase was clearly observed in the glass under stress but this effect is not so clear in the stress-free glass. The gamma-TeO2 and alpha-TeO2 phases crystallizes during the initial stages of crystallization in both studied glasses while the alpha-Li2Te2O5 phase crystallize in the final stages of the crystallization. The activation energies and Avrami exponent were calculated for both studied glasses with different particle size leading to E-3 > E-2 > E-1 for stressed glass and E-3 > E-2 approximate to E-1 for stress-free glass, where E-1, E-2 and E-3 were associated to the gamma-TeO2, alpha-TeO2 and alpha-Li2Te2O5 phases, respectively. The observed distinct (n) over bar (1) < <(n)over bar>(2) < <(n)over bar>(3) in both glasses is an indicative that nucleation and growth takes place by more than one mechanism in the early stages of the crystallization. (C) 2011 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Coorden§Ã£o de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Visible photoluminescence (PL) was observed for the first time at room temperature in structurally disordered calcium strontium tungstate powder, Ca0.60Sr0.40WO4 (CSW), obtained by the polymeric precursor method. The PL behavior of CSW powders has been analyzed as a function of the disorder rate, based on experimental and theoretical studies. Quantum mechanical theory based on density functional theory at the B3LYP level has been employed to study the electronic structure of two periodic models representing both crystalline and disordered powders. Their electronic structures have been analyzed in terms of density of states, band dispersion and charge densities. The calculations indicate a break in symmetry when passing from crystalline to disordered models, creating localized electronic levels above the valence band. Moreover, a negative charge transfer process takes place from the [WO3] cluster to the [WO4] cluster. The polarization induced by the break in symmetry and the existence of localized levels favors the creation of trapped holes and electrons, originating the PL phenomenon. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The correlation between experimental data and theoretical calculations have been investigated to explain the photoluminescence at room temperature of Ba(Ti0.75Zr0.25)O-3 (BTZ) thin films prepared by the polymeric precursor method. The degree of structural order-disorder was investigated by X-ray diffraction, Fourier transform infrared spectroscopy, ultraviolet-visible absorption spectroscopy and photoluminescence (PL) measurements. First-principles quantum mechanical calculations based on density functional theory (B3LYP level) were employed to study the electronic structure of ordered and deformed asymmetric models. The electronic properties are analyzed and the relevance of the present theoretical and experimental results on the PL behavior is discussed. The presence of localized electronic levels and a charge gradient in the band gap due to a break in symmetry, are responsible for the PL in disordered BTZ lattice. (c) 2007 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.