66 resultados para Thickness.


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Lead zirconate titanate Pb(Zr 0.50Ti 0.50)O 3 (PZT) thin films were deposited by a polymeric chemical method on Pt(111)/Ti/SiO2/Si substrates to understand the mechanisms of phase transformations and the effect of film thickness on the structure, dielectric and piezoelectric properties in these films. PZT films pyrolyzed at temperatures higher than 350 °C present a coexistence of pyrochlore and perovskite phases, while only perovskite phase grows in films pyrolyzed at temperatures lower than 300 °C. For pyrochlore-free PZT thin films, a small (100) orientation tendency near the film-substrate interface was observed. Finally, we demonstrate the existence of a self-polarization effect in the studied PZT thin films. Results suggest that Schottky barriers and/or mechanical coupling near the filmsubstrate interface are not primarily responsible for the observed self-polarization effect in our films. © 2012 IEEE.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The purpose of this study was to evaluate the correlation between the hybrid layer thickness, resin tag length and resin bond strength of a self-etching adhesive system to sound dentin tissue in vivo. After performing restorative procedures and tooth extractions, ten specimens were sectioned in a mesiodistal direction. One dental section was used for light microscope analysis, in which both the resin tag length and hybrid layer thickness were measured, while the other section was analyzed using a microtensile test (0.5 mm/min). The fractured surface of the latter section was characterized using a stereoscopic magnifying glass (40x magnifcation). The results were subject to statistical analysis using the Pearson Correlation Test (a = 0.05). The hybrid layer thickness, resin tag length and resin bond strength mean values were 2.19 microm (0.34), 4.34 microm (0.28) and 9.73 MPa (5,55), respectively. In addition, correlation tests between the resin tag length and the resin bond strength (r=0.014) and also between the hybrid layer thickness and bond strength (r=0.43), showed no statistically significant correlation. The microtensile bond strength of Adper Prompt L Pop self-etching adhesive system does not depend on hybrid layer thickness or resin tag length.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This study evaluated whether periodontal ligament (PL) thickness varied with root size and examined the possible influence of this variation on orthodontic mechanics. Measurements were taken of the maxillary left first molar in 54 male Wistar rats. Mean mesial and distal PL thicknesses were compared between the intermediate buccal and mesiobuccal roots using paired Student's t-tests with a 5% significance level. Mean values differed significantly between roots (p < 2.2 × 10-16). PL thickness in rats is directly proportional to root dimensions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background: Among adults, obesity has been positively related to bone mineral density. However, recent findings have pointed out that abdominal obesity could be negatively related to bone density. The above mentioned relationship is not clear among pediatric populations. Therefore, this cross-sectional study analyzed the relationship between thickness of abdominal adipose tissue and bone mineral variables in sedentary obese children and adolescents.Methods: One hundred and seventy five obese children and adolescents (83 male and 92 female) with ages ranging from 6 to 16 years-old were analyzed. Bone mineral content and density were estimated by dual-energy X-ray absorptiometry and ultrasound equipment which estimated the thickness of the abdominal adipose tissue. Pubertal stage was self-reported by the participants.Results: The mean age was 11.1 (SD = 2.6). Thickness of the abdominal adipose tissue was negatively related to bone mineral density (r = -0.17 [r95%CI: -0.03;-0.32]), independent of gender, pubertal stage and other confounders (β = -0.134 ± 0.042 [β95%CI: -0.217; -0.050]).Conclusions: In sedentary obese children and adolescents abdominal obesity is negatively related to bone mineral density, suggesting a potential link between abdominal obesity and osteoporosis. © 2013 Júnior et al.; licensee BioMed Central Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Lead zirconate titanate Pb(Zr0.50Ti0.50)O3 (PZT) thin films were deposited by a polymeric chemical method on Pt(111)/Ti/SiO2/Si substrates to understand the mechanisms of phase transformations and the effect of film thickness on the structure, dielectric, and piezoelectric properties in these films. PZT films pyrolyzed at temperatures higher than 350 °C present a coexistence of pyrochlore and perovskite phases, while only perovskite phase grows in films pyrolyzed at temperatures lower than 300 °C. For pyrochlore-free PZT thin films, a small (100)-orientation tendency near the film-substrate interface was observed. Finally, we demonstrate the existence of a self-polarization effect in the studied PZT thin films. The increase of self-polarization with the film thickness increasing from 200 nm to 710 nm suggests that Schottky barriers and/or mechanical coupling near the film-substrate interface are not primarily responsible for the observed self-polarization effect in our films. © 2013 AIP Publishing LLC.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background: Meat quality involves many traits, such as marbling, tenderness, juiciness, and backfat thickness, all of which require attention from livestock producers. Backfat thickness improvement by means of traditional selection techniques in Canchim beef cattle has been challenging due to its low heritability, and it is measured late in an animal's life. Therefore, the implementation of new methodologies for identification of single nucleotide polymorphisms (SNPs) linked to backfat thickness are an important strategy for genetic improvement of carcass and meat quality.Results: The set of SNPs identified by the random forest approach explained as much as 50% of the deregressed estimated breeding value (dEBV) variance associated with backfat thickness, and a small set of 5 SNPs were able to explain 34% of the dEBV for backfat thickness. Several quantitative trait loci (QTL) for fat-related traits were found in the surrounding areas of the SNPs, as well as many genes with roles in lipid metabolism.Conclusions: These results provided a better understanding of the backfat deposition and regulation pathways, and can be considered a starting point for future implementation of a genomic selection program for backfat thickness in Canchim beef cattle. © 2013 Mokry et al.; licensee BioMed Central Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Examining three bleaching systems, this in vivo clinical trial evaluated the relationship among tooth sensitivity, light activation, and agent concentration, and it correlated dental sensitivity with tooth thickness.Materials and Methods: Eighty-seven volunteer patients were included. Inclusion criteria were the presence of anterior teeth without restorations as well as the absence of a previous bleaching experience and absence of non-carious cervical lesions or dental pain. Exclusion criteria included pregnancy or breastfeeding, a maximum of TF3 hypoplasia, tetracycline-fluorosis stains, malpositioned teeth, orthodontic treatment, periodontal disease, and/or analgesic/anti-inflammatory intake. Patients were randomly assigned to three bleaching groups: Group A (n=25) was treated with 15% H2O2 and nitrogenous-titanium-dioxide and was light activated (Lase Peroxide Lite, DMC, SaoCarlos, Sao Paulo, Brazil); Group B (n=27) was treated with 35% H2O2 and was light activated (Lase Peroxide Sensy, DMC); and Group C (n=35) was treated with 35% H2O2 (White Gold Office, Dentsply, 38West Clark Ave., Milford, USA) without light activation. Tooth sensitivity (TS) was self-reported by the patients using the visual analog scale (VAS) at baseline (TSO), immediately after treatment (TSI), and at seven days after treatment (TS7). In 46 patients, tooth thickness was determined by computed tomography. TSO, TSI, and TS7 were compared between the A and B groups to determine the effect of concentration and between the B and C groups to determine the effect of light using analysis of covariance. The correlation between tooth thickness and TSI was determined by Spearman Rho test (SPSS 15).Results: Eighty-seven patients were evaluated at baseline, and 61 were evaluated at seven days. Separated by groups, tooth sensitivity, expressed as VAS value at the time points TS0, TS1, and TS7, respectively, were as follows: Group A: 13.76 +/- 13.53, 24.40 +/- 25.24, and 5.94 +/- 5.5; Group B: 15.07 +/- 18.14, 42.4 +/- 31.78, and 8.68 +/- 17.99; and Group C: 10.80 +/- 14.83, 31.51 +/- 29.34, and 7.24 +/- 9.2. Group A showed significantly lower tooth sensitivity than group B at TSI (p=0.032). No differences were observed in the tooth sensitivities between groups B and C. No correlation was encountered between tooth thickness and tooth sensitivity immediately after treatment (Rho=-0.088,p=0.563). The median tooth thickness was 2.78 +/- 0.21 mm.Conclusions: Increases in the concentration of bleaching agents directly affect tooth sensitivity, and LED/laser activation and tooth thickness are not correlated with tooth sensitivity after dental bleaching.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Adhesive restorations have increasingly been used in dentistry, and the adhesive system application technique may determine the success of the restorative procedure. The aim of this study was to evaluate the influence of the application technique of two adhesive systems (Clearfil SE Bond and Adper Scotchbond MultiPurpose) on the bond strength and adhesive layer of composite resin restorations. Eight human third molars were selected and prepared with Class I occlusal cavities. The teeth were restored with composite using various application techniques for both adhesives, according to the following groups (n = 10): group 1 (control), systems were applied and adhesive was immediately light activated for 20 seconds without removing excesses; group 2, excess adhesive was removed with a gentle jet of air for 5 seconds; group 3, excess was removed with a dry microbrush-type device; and group 4, a gentle jet of air was applied after the microbrush and then light activation was performed. After this, the teeth were submitted to microtensile testing. For the two systems tested, no statistical differences were observed between groups 1 and 2. Groups 3 and 4 presented higher bond strength values compared with the other studied groups, allowing the conclusion that excess adhesive removal with a dry micro-brush could improve bond strength in composite restorations. Predominance of adhesive fracture and thicker adhesive layer were observed via scanning electron microscopy (SEM) in groups 1 and 2. For groups 3 and 4, a mixed failure pattern and thinner adhesive layer were verified. Clinicians should be aware that excess adhesive may negatively affect bond strength, whereas a thin, uniform adhesive layer appears to be favorable. (Quintessence Int 2013;44:9-15)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Purpose: This study aimed to investigate the influence of ceramic thickness and shade on the Knoop hardness and dynamic elastic modulus of a dual-cured resin cement.Materials and Methods: Six ceramic shades (Bleaching, A1, A2, A3, A3.5, B3) and two ceramic thicknesses (1 mm, 3 mm) were evaluated. Disk specimens (diameter: 7 mm; thickness: 2 mm) of the resin cement were light cured under a ceramic block. Light-cured specimens without the ceramic block at distances of 1 and 3mm were also produced. The Knoop hardness number (KHN), density, and dynamic Young's moduli were determined. Statistical analysis was conducted using ANOVA and a Tukey B rank order test (p = 0.05).Results: The bleaching 1-mm-thick group exhibited significantly higher dynamic Young's modulus. Lower dynamic Young's moduli were observed for the 3-mm-thick ceramic groups compared to bleaching 3-mm-thick group, and no difference was found among the other 3-mm groups. For the KHN, when A3.5 3-mm-thick was used, the KHN was significantly lower than bleaching and A1 1-mm-thick ceramic; however, no difference was exhibited between the thicknesses of the same shade.Conclusions: The dual-cured resin cement studied irradiated through the 1-mm-thick ceramic with the lightest shade (bleaching ceramic) exhibited a better elastic modulus, and there was no effect in KHN of the resin cement when light cured under different ceramic shades and thicknesses (1 and 3 mm), except when the A3.5 3-mm-thick ceramic was used.Clinical Significance: Variolink II irradiated through ceramic with the lowest chroma exhibited the highest elastic modulus; therefore, the light activation method might not be the same for all clinical situations.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)