59 resultados para Potentiodynamic polarisation
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Pós-graduação em Química - IQ
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Pós-graduação em Engenharia Mecânica - FEG
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The aim of this work was to evaluate the corrosion resistance of AuPdAgIn alloy, submitted to laser beam welding, in 0.9% NaCl solution, using electrochemical techniques. Measures of the open circuit potential (OCP) versus time were applied to electrochemical experiments, as well as potentiodynamic direct scanning (PDS) and electrochemical impedance spectroscopy (EIS) on AuPdAgIn alloy, submitted to laser beam welding in 0.9% NaCl solution. Some differences observed in the microstructure can explain the results obtained for corrosion potential, Ecorr, and corrosion resistance, Rp. EIS spectra have been characterized by distorted capacitive components, presenting linear impedance at low frequencies, including a non-uniform diffusion. The area of the laser weld presented corrosion potential slightly superior when compared to the one of the base metal. The impedance results suggest the best resistant corrosion behavior for laser weld than base metal region. This welding process is a promising alternative to dental prostheses casting.
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
The electrochemical behaviour of copper in 6.0 mol 1-1 sulfuric acid at 30°C, was studied by means of the potentiodynamic method. At low potential sweep rates, v < 200 m V s-1, the data reveal that the anodic process is basically constituted of copper dissolution and a film formation which inhibits further metal oxidation and which may undergo further dissolution. For higher potential sweep rates, a modification in the passivation region of the voltammogram is observed. It can be ascribed to a change in the passivation mechanism which possibly involves different surface species. The kineticrelationships derived from the potentiodynamic I/E curves obtained at low v suggest a film formation via a dissolution/precipitation mechanism. © 1993.
Resumo:
Several alloys have been used for prosthodontics restorations in the last years. These alloys have a number of metals that include gold, palladium, silver, nickel, cobalt, chromium and titanium and they are used in oral cavity undergo several corrosion. Corrosion can lead to poor esthetics, compromise of physical properties, or increased biological irritation. The objective of this study was evaluated corrosion resistance of two alloys Ni-Cr and Ni-Cr-Ti in three types of mouthwashes with different active ingredients: 0.5g/l cetylpyridinium chloride + 0.05% sodium fluoride, 0.05% sodium fluoride + 0.03% triclosan (with fluor) and 0.12% chlorohexidine digluconate. The potentiodynamic curves were performed by means of an EG&G PAR 283 potentiostat/galvanostat. The counter electrode was a platinum wire and reference electrode was an Ag/AgCl, KCl saturated. Before each experiment, working electrodes were mechanically polished with 600 and 1200 grade papers, rinsed with distilled water and dried in air. All experiments were carried out at 37.0oC in conventional three-compartment double wall glass cell containing mouthwashes. The microstructures of two alloys were observed in optical microscopy. Analysis of curves showed that Ni-Cr alloy was less reactive in the presence of 0.12% chlorohexidine digluconate while Ni-Cr-Ti alloy was more sensitive for others two types of mouthwashes (0.5g/l cetylpyridinium chloride + 0.05% sodium fluoride and 0.05% sodium fluoride + 0.03% triclosan). This occurred probably due presence of titanium in this alloy. Microstructural analysis reveals the presence of dendritic and eutectic microstructures for NiCr and Ni-Cr-Ti, respectively.