36 resultados para Dielectric relaxation


Relevância:

30.00% 30.00%

Publicador:

Resumo:

A side-chain methacrylate copolymer functionalized with the nonlinear optical chromophore 4-[N-ethyl-N-(2-hydroxyethyl)]amino-2'-chloro-4'-nitroazobenzene, disperse red-13, was prepared and characterized. The chromophore relaxation was investigated measuring the decay of the electrooptic coefficient r(13) and the complex dielectric constant at different temperatures. Results obtained below and above T-g were analyzed using the Kohlrausch-Williams-Watts(KWW) equation, through the study of the temperature dependence of the KWW parameters. Above T-g the relaxation time experimental data were fitted to the Williams-Landel-Ferry (WLF) equation and its parameters determined. Chromophore relaxation leading to the decrease of electrooptic properties was found associated with a primary alpha relaxation. The obtained WLF equation parameters were introduced into the Adam-Gibbs-Tool-Narayanaswamy-Moynihan equation, and the overall relaxation time temperature dependence was successfully obtained in terms of the fictive temperature, accounting for the sample thermal treatment and allowing optimized thermal treatment to be found. The copolymer KWW stretching parameter at the glass transition temperature lies close to the limit value for short-range interactions, i.e., 0.6, suggesting that the chromophore group is participating in primary a relaxation.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The complex analysis of dielectric/capacitance is a very useful approach to separate different polarization contributions existing in polycrystalline ceramics. In this letter, the authors use this type of spectroscopic analysis to separate the bulk's dielectric dipolar relaxation contributions from the polarization contribution due to space charge in the grain boundaries of a CaCu3Ti4O12/CaTiO3 polycrystalline composite system. The bulk dielectric dipolar relaxation was attributed to the self-intertwined domain structures from the CaCu3Ti4O12 phase coupled to the dipole relaxation from the CaTiO3 phase, while the space charge relaxation was attributed to the Schottky-type potential barrier responsible for the highly non-Ohmic properties observed in this composite polycrystalline system.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this work fresh cables were laboratory aged under multi-stressing conditions at room temperature. Foils were peeled from cables, with approximately 150 ?m thickness, from the outer, middle and inner positions of the XLPE cable insulating layer. For samples obtained from the outer cable layer position, an increasing near-permanent electrical conduction process with aging time was observed. At the middle and inner cable layer positions a flat-loss relaxation process was observed becoming a dominating process on the ageing. In addition, PEA results confirmed that degradation in the outer region of the XLPE cables arises from the simultaneous presence of dipoles and injected space charge that distorts the internal electric field on the ageing.