The nonlinear (NL) response of lead-germanium oxide amorphous films was investigated using a Ti:saphire laser delivering pulses of approximate to 150 fs at 800 nm. The Kerr shutter technique was employed to reveal the time response of the nonlinearity that is smaller than 150 fs. The sign and magnitude of the nonlinearity were obtained using a novel technique called thermally managed eclipse Z scan which allows the simultaneous characterization of cumulative and noncumulative NL effects. The NL refractive index of electronic origin, n(2)approximate to 2x10(-17) m(2)/W, and the NL absorption coefficient, alpha(2)approximate to 3x10(3) cm/GW, were determined. (c) 2007 American Institute of Physics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A polymeric precursor method was used to synthesis PbTiO3 amorphous thin film processed at low temperature. The luminescence spectra of PbTiO3 amorphous thin films at room temperature revealed an intense single-emission band in the visible region, the visible emission band was found to be dependent on the thermal treatment history, Photoluminescence properties Versus different annealing temperatures were investigated. The experimental results (XRD, AFM, FL) indicate that the nature of photoluminescence (PL) must be related to the disordered structure of PbTiO3 amorphous thin films, Copyright (C) 2000 John Wiley & Sons, Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Ca0.95Sm0.05TiO3 (CT:Sm) powder was prepared by the polymeric precursor method (PPM). Order-disorder at short and long range has been investigated by means of Raman spectroscopy, X-ray diffraction (XRD), and photoluminescence emission (PL) experimental techniques. The broad PL band and the Sm emission spectrum measured at room temperature indicate the increase of structural order with annealing temperature. The measured PL emission reveals that the PL intensity changes with the degree of disorder in the CT: Sm. The electronic structures were performed by the ab initio periodic method in the DFT level with the hybrid nonlocal B3LYP approximation. Theoretical results are analyzed in terms of DOS, charge densities, and Mulliken charges. Localized levels into the band gap of the CT: Sm material favor the creation of the electron-hole pair, supporting the observed room-temperature PL phenomenon.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Amorphous and crystalline powder of PLT phase was synthesized by using the Pechini method. Infrared (FTIR) analysis of the polymeric resin shows intense bands of organic materials from 250 to 1620 cm(-1). X-ray diffraction (XRD) and Raman spectra of calcined powder at different temperatures show amorphous phase at 450 degrees C/3 h, semi-crystalline phase at 550 degrees C/3 h and a crystalline phase at 800 degrees C/3 h. Luminescence effect was observed in amorphous powder calcined from 300 to 350 degrees/3 h with broad absorption peaks in 579 nm at 300 degrees C/3 h and 603 rum at 350 degrees C/3 h, respectively. The photoluminescence effect is attributed to emissions of Ti -> 0 directly from the oxygen 2p orbital (valence band) to the titanate 3d orbital (conduction bands). (c) 2004 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Photoluminescence (PL) at room temperature has been achieved in amorphous thin films and powders of the TiO2-PbO system. They were prepared by the polymeric precursor method with [PbO]/[TiO2] molar ratios ranging from 0.0 to 1.0. The energy position of maximum PL emission and the PL intensity showed dependence on Pb concentration. The Pb addition suggests an increase in the number of nonbridging oxygens (NBO) in the amorphous TiO2 network. These results support the relationship between photoluminescence and structure in TiO2-based amorphous materials.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This work reports the changes in the optical properties produced by annealing of amorphous GaAs at temperatures smaller than or just sufficient to produce crystallization of the material. The films were grown by the flash evaporation technique on glass substrates at room temperature. Optical and structural changes of our samples were monitored through photothermal deflection spectroscopy, optical transmittance and reflectance and X-ray diffraction (XRD). The structural results from XRD detected no crystallization of the films for temperatures up to 240 degreesC. We have observed consistent changes in the optical gap and Urbach energy of the annealed film. The optical gap increases with increasing annealing temperature from 1.17 to 1.32 eV. The Urbach energy decrease from 120 meV (as-grown film) to 105 meV (anneal at 200 degreesC). We propose that these changes are due to a diminution of the tail state defects and/or the relaxation of strained bonds. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Amorphous and crystalline powder of PLZ was prepared by using the polymeric precursor method. TGA-DSC (Thermal analysis and Differential Scanning Calorimetry) shows the decomposition of polymeric resin, an amorphous phase and the crystallization of powder. Raman scattering of powder shows an amorphous and semicrystalline phase at 450 and 550 degreesC, respectively. XRD (X-ray diffraction pattern) of powder shows high crystallinity at 700 degreesC/3 h. PL (Photoluminescence) analysis of powder at 300 degreesC/3 h shows a broad asymmetric peak at 585 nm and increases of calcining time led to intense peaks of PL at 300 degreesC/6 h. This emission could be attributed to Zr --> O from the oxygen-2p orbitals to the zirconate-3d orbitals. (C) 2003 Elsevier Ltd and Techna S.r.l. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Indium-tin oxide nanostructures were deposited by excimer laser ablation in a nitrogen atmosphere using catalyst-free oxidized silicon substrates at 500 degrees C. Up to 1 mbar, nanowires grew by the vapor-liquid-solid (VLS) mechanism, with the amount of liquid material decreasing as the deposition pressure increased. The nanowires present the single-crystalline cubic bixbyite structure, oriented < 100 >. For the highest pressure used, pyramids were formed and no sign of liquid material could be observed, indicating that these structures grew by a vapor-solid mechanism. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The effects of bath composition and electroplating conditions on structure, morphology, and composition of amorphous Fe-Cr-P-Co deposits on AISI 1020 steel substrate, priorly plated with a thin Cu deposit, were investigated. The increase of charge density activates the inclusion of Cr in the deposit. However, above specific values of the charge density, which depend on the deposition current density, the Cr content in the deposit decreases. This Cr content decreasing is probably due to the significant hydrogen evolution with the increasing of deposition cur-rent and charge density. The effect of charge density on the content of Fe and Co is not clear. However, there is a tendency of increasing of Fe content and decreasing of Co content with the raising of current density. The Co is more easily deposited than the P, and its presence results in a more intense inhibition effect on the Cr deposition than the inhibition effect caused by P presence. Scanning electron microscope (SEM) analysis showed that Co increasing in the Fe-Cr-P-Co alloys analyzed does not promote the susceptibility to microcracks, which led to a good quality deposit. The passive film of the Fe-Cr-P-Co alloy shows a high ability formation and high protective capacity, and the results obtained by current density of corrosion, j(cor), show that the deposit with addition of Co, Fe31Cr11P28Co30, presents a higher corrosion resistance than the deposit with addition of Ni, Fe54Cr21P20Ni5. (C) 2004 Published by Elsevier B.V.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Pb1-XLaXTiO3 thin films, (X = 0.0; 13 and 0.27 mol%) were prepared by the polymeric precursor method. Thin films were deposited on Pt/Ti/SiO2/Si (1 1 1), Si (1 0 0) and glass substrates by spin coating, and annealed in the 200-300degreesC range in an O-2 atmosphere. X-ray diffraction, scanning electron microscopy and atomic force microscopy were used for the microstructural characterization of the thin films. Photoluminescence (PL) at room temperature has been observed in thin films of (PbLa)TiO3. The films deposited on Pt/Ti/SiO2/Si substrates present PL intensity greater than those deposited on glass and silicon substrates. The intensity of PL in these thin films was found to be dependent on the thermal treatment and lanthanum molar concentration. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Diverse amorphous hydrogenated carbon and similar films containing additional elements were produced by Plasma Enhanced Chemical Vapor Deposition (PECVD) and by Plasma Immersion Ion Implantation and Deposition (PIIID). Thus a-C:H, a-C:H:F, a-C:H:N, a-C:H:Cl and a-C:H:O:Si were obtained, starting from the same feed gases, using both techniques. The same deposition system supplied with radiofrequency (RF) power was used to produce all the films. A cylindrical stainless steel chamber equipped with circular electrodes mounted horizontally was employed. RF power was fed to the upper electrode; substrates were placed on the lower electrode. For PIIID negative high tension pulses were also applied to the lower electrode. Raman spectroscopy confirmed that all the films are amorphous. Chemical characterization of each pair of films was undertaken using Infrared Reflection Absorption Spectroscopy and X-ray Photoelectron Spectroscopy. The former revealed the presence of specific structures, such as C-H, C-O, O-H. The latter allowed calculation of the ratio of hetero-atoms to carbon atoms in the films, e. g. F:C, N:C, and Si:C. Only relatively small differences in elemental composition were detected between films produced by the two methods. The deposition rate in PIIID is generally reduced in relation to that of PECVD; for a-C:H:Cl films the reduction factor is almost four.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Conditions for as-quenched amorphous ribbon fabrication by a single roll-casting method are analyzed from a hydrodynamic standpoint. The analysis is based on the investigation of the processing conditions for Fe 4 0Ni 40P 14B 6 amorphous ribbons. It is shown that the dependence of ribbon thickness on the ejection pressure for different roll angular velocities and different dimensions of crucible and orifice can be obtained from general considerations on the melt flow regime.