37 resultados para TM3
Resumo:
Conselho Nacional de Desenvolvimento CientÃfico e Tecnológico (CNPq)
Resumo:
Energy transfer processes between Er3+ and Tm3+ were investigated examining the frequency upconversion emissions in a fluoroindate glass pumped at 790 nm. A 60-fold enhancement in the emission at ≈670 nm originating from Er3+ was observed when Tm3+ at concentration of 2% was introduced in a sample containing 2% of Er3+. The results are explained considering the influence of cross-relaxation processes between the active ions. © 2002 Elsevier Science B.V. All rights reserved.
Resumo:
Optical absorption and fluorescence were investigated in Tm3+ doped fluoroindate glass. The spectroscopic parameters for transitions in the 4f11 configuration were determined. The fluorescence study revealed the origin of the frequency upconversion process as well as allowed to quantify the interaction between Tm3+ ions.
Resumo:
The spectroscopic properties of Tm3+-doped fluoroindate glasses (FIG) were described by single wavelength pumping in the red region. The Judd-Ofelt (J-O) theory was used to obtain the quantum efficiency of the 4f-4f transitions and other spectroscopic parameters. The dynamics of the fluorescence was investigated and energy transfer (ET) processes among Tm3+ ions were studied. The results indicate that a two-step one-photon absorption process is responsible for the ultraviolet upconversion (UC) emissions, and dipole-dipole interaction provides the main contribution for ET rate is equal to the decay rate of noninteracting among active ions.
Resumo:
Two series of glasses with composition (mol%) 70PbGeO3- 15PbF2-15CdF2, the first one with different Tm 3+ contents (0.2, 0.4, 0.6 and 0.8 mol%) and the second one with 0.2 mol% Tm3+ and different Ho3+ contents (0.1, 0.5, 1.0 and 1.5 mol%), have been prepared and some of their spectroscopic properties studied. Absorption in the visible-near infrared and emission in the near infrared region of the electromagnetic spectrum have been obtained. Concerning emission at the 1.4-1.5 μm region, optimization of rare earth ions content leads to 0.2 and 0.5 mol% for Tm3+ and Ho3+, respectively. We discuss potential application of these compositions. © 2005 Elsevier B.V. All rights reserved.
Resumo:
Fabrication and optical characterization of Tm3+/Yb3+ codoped PbO-GeO2 (PGO) pedestal-type waveguides are investigated in this work. It is important to mention that, to the best of authors' knowledge, the use of PGO pedestal-type waveguide has not been studied before. PGO thin films codoped with Tm3+ and Yb3+ were obtained through RF magnetron sputtering technique. The pedestal profile was obtained using conventional optical lithography procedures, followed by plasma etching and sputtering deposition. The profile of Tm3+/Yb3+ codoped PGO waveguides was observed by means of Scanning Electron Microscopy (SEM) measurements. Also the infrared and infrared-to-visible frequency upconversion luminescences of Tm3+ ions were measured exciting the samples with a cw 980 nm diode laser. Propagation losses around 11 dB/cm and 9 dB/cm were obtained at 630 and 1050 nm, respectively, for waveguides in the 20-100 μm width range. Single-mode propagation was observed for waveguides width up to 12 μm and 7 μm, at 1050 nm and 630 nm, respectively; larger waveguides width provided multi-mode propagation. The present results corroborate the possibility of using Tm3+/Yb3+ codoped PGO thin films as active waveguide for photonic applications. © 2013 Elsevier B.V. All rights reserved.
Resumo:
Conselho Nacional de Desenvolvimento CientÃfico e Tecnológico (CNPq)
Resumo:
Conselho Nacional de Desenvolvimento CientÃfico e Tecnológico (CNPq)
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de NÃvel Superior (CAPES)
Resumo:
New Yb3+, Er3+ and Tm3+ doped fluoro-phosphate glasses belonging to the system NaPO3–YF3–BaF2–CaF2 and containing up to 10 wt% of rare-earth ion fluorides were prepared and characterized by differential scanning calorimetry, absorption spectroscopy and up-conversion emission spectroscopy under excitation with a 975 nm laser diode. Transparent and homogeneous glass-ceramics have been reproducibly obtained with a view to manage the red, green and blue emission bands and generate white light. X-ray diffraction as well as electron microscopy techniques have confirmed the formation of fluorite-type cubic nanocrystals at the beginning of the crystallization process while complex nanocrystalline phases are formed after a longer heat-treatment. The prepared glass-ceramics exhibit high optical transparency even after 170 h of thermal treatment. An improvement of up-conversion emission intensity – from 10 to 160 times larger – was measured in the glass-ceramics when compared to the parent glass, suggesting an important incorporation of the rare-earth ions into the crystalline phase(s). The involved mechanisms and lifetime were described in detail as a function of heat-treatment time. Finally, a large range of designable color rendering (from orange to turquoise through white) can be observed in these materials by controlling the laser excitation power and the crystallization rate.
Resumo:
The preparation of Tm3+/Yb3+/Ho3+ co-doped CeO2 prepared by the precipitation method using ammonium hydroxide as a precursor is presented. By X-ray diffraction the materials show the phase-type of fluorite structure and the crystallite sizes were calculated by the Scherrer's equation. No other phase was observed evincing that the rare earth ions were inserted into the fluorite phase as substitutional or interstitial dopants. The microstrain calculated by the Williamson-Hall method do not show significant changes in their values, indicating that the inclusion of rare earths does not causes structural changes in the CeO2 used as a host matrix. All material showed intense upconversion emission at red and green region under excitation with diode laser at 980 nm. The color of emission changes from green to red with increasing excitation power pump. The materials showed suitable photoluminescent properties for applications as a laser source, solar cells, and great emitter at 800 nm. (C) 2014 Elsevier B.V. All rights reserved.
Resumo:
The mechanism involved in the Tm3+ (F-3(4))-->Ho3+ (I-5(7)) energy transfer and Tm3+ (H-3(4), H-3(6))-->Tm3+ (F-3(4), F-3(4)) cross relaxation as a function of the donor and acceptor concentrations was investigated in Tm-Ho-codoped fluorozirconate glasses. The experimental transfer rates were determined for the Tm-->Ho energy transfer from the best fit of the acceptor luminescence decay using an expression which takes into account the Inokuti-Hirayama model and localized donor-to-acceptor interaction solution. The original acceptor solution derived from the Inokuti-Hirayama model fits well the acceptor luminescence transient only for low-concentrated systems. The results showed that a fast excitation diffusion that occurs in a very short time (t<<gamma(-2)) reduces the mean distance between an excited donor (D-*) and the acceptor (A). A localized donor-to-acceptor interaction takes place, leading to an exponential decay of donors as an average of the microscopic rate equation solution of each D-*-A pair separated by distance R that contributes in addition to the Inokuti-Hirayama solution. The observation that the experimental transfer rates were always much bigger than the one predicted by the diffusion model, in which the energy transfer process is assisted by excitation migration among donors state, reinforces the existence of a fast excitation diffusion among donor ions before the energy transfer to acceptor already observed in Yb:Er:ZBLAN. The fast excitation diffusion effect was observed to dominate both the Tm-->Tm cross relaxation and Tm-->Ho energy transfer ions from H-3(4) and F-3(4) thulium states, respectively. (C) 2004 American Institute of Physics.
Resumo:
Fluoroindate glasses of the following compositions: (40-x)InF3-20ZnF(2)-16BaF(2)-20SrF(2)-2GdF(3)-2NaF-xTmF(3) with x = 1,3 mol% were prepared in a dry box under an argon atmosphere. The absorption spectra at room temperature in the spectral range 350-2200 nm were obtained. The spectra obtained for each sample had similar absorption and only the amplitude of the different bands changed as the concentration of Tm3+. The experimental oscillator strengths were determined from the areas under the absorption bands. Using the standard and modified Judd-Ofelt theory, intensity parameters Ohm(lambda) (lambda = 2,4,6) and (lambda = 2,3,4,5,6), respectively for f-f transitions of Tm3+ ions as well as transition probabilities, branching ratios and radiative lifetimes for each band were determined. The results are compared with those of other glasses described in the literature. (C) 1999 Elsevier B.V. B.V. All rights reserved.
Resumo:
Strong interest in developing technology for visual information. stimulates research for thin film electroluminescent devices. Here, for the first time, we report that thulium- and terbium-doped zinc-oxide films are suitable for electroluminescence applications. Two different devices were assembled as lTO/LiF/ZnO:RE/LiF/Al or ITO/SiO2/ZnO:RE/SiO2/Al, where ZnO:RE is a film of zinc oxide containing 10 at% of Tb3+ or Tm3+. Electroluminescence spectra show that besides a broad emission band with maximum around 650 nm assigned to ZnO, also emission lines from Tb3+ at 484 nm (D-5(4) -> F-7(6)), 543 nm (D-5(4) -> F-7(6)), and 589 nm (D-5(4) -> F-7(4)), or from Tm3+ at 478 nm ((1)G(4) -> H-3(6)), and 511 mn (D-1(2) -> H-3(5)) were detected. Intensity of emission as function of applied voltage and current-voltage characteristic are shown and discussed. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Infrared-to-visible and infrared-to-infrared frequency upconversion processes in Yb3+-Tm3+ doped PbO-GeO2 glasses containing silver nanoparticles (NPs) were investigated. The experiments were performed by exciting the samples with a diode laser operating at 980 nm (in resonance with the Yb3+ transition F-2(7/2)-> F-2(5/2)) and observing the photoluminescence (PL) in the visible and infrared regions due to energy transfer from Yb3+ to Tm3+ ions followed by excited state absorption in the Tm3+ ions. The intensified local field in the vicinity of the metallic NPs contributes for enhancement in the PL intensity at 480 nm (Tm3+ :(1)G(4)-> H-3(6)) and at 800 nm (Tm3+ : H-3(4) -> H-3(6)). (C) 2009 American Institute of Physics. [doi:10.1063/1.3211300]