98 resultados para Optical Properties and Phenomena.


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this work, we report on the synthesis of SrMoO4 powders by co-precipitation method and processed in a microwave-hydrothermal at 413 K for 5 h. These powders were analyzed by X-ray diffraction (XRD), Fourier transform Raman (FT-Raman), ultraviolet-visible (UV-vis) absorption spectroscopy and photoluminescence (PL). XRD analyses revealed that the SrMoO4 powders are free of secondary phases and crystallize in a tetragonal structure. FT-Raman investigations showed the presence of Raman-active vibration modes correspondent for this molybdate. UV-vis technique was employed to determine the optical band gap of this material. SrMoO4 powders exhibit an intense PL emission at room temperature with maximum peak at 540 nm (green region) when excited by 488 nm wavelength of an argon ion laser. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this work, GdAlO3:RE3+ (RE = Eu or Tb) was successfully prepared by the Pechini method at lower temperatures when compared to others methods as solid-state synthesis and sol-gel process. In accordance to the XRD data, the fully crystalline single-phase GdAlO3 could be obtained at 900 degrees C. The differential thermal analysis (DTA) shows a crystallization peak at 850 degrees C. The samples are composed by monocrystalline particles (50-120 nm) exhibiting the formation of aggregates among them, which indicates the beginning of the sinterization process. This feature indicates a strong tendency to the formation of aggregates, which is a suitable ability for the close-packing of particles, and hence a potential application in X-ray intensifying screens. Luminescence measurements indicate Gd3+ -> RE3+ energy transfer. The Eu3+ emission spectra exhibit all the characteristics D-5(0) -> F-7(j) transitions and the observed profile suggests that RE3+ ions occupy at least one site without center of symmetry. For terbium-doped samples, the D-5(3) -> F-7(j) (blue emission) and D-5(4) -> F-7(j) (green emission) transitions were observed and the ratio between them may depend on the Tb3+ content due to cross-relaxation processes. (C) 2009 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The synthesis and characterization of a new organic ligand monooctyldiphenylphosphinate (L) is described, as well as a new Eu(3+) diketonate complex [Eu(tta)(3)(L)(2)] (tta = thenoyltrifluoracetone). The ligand (L) was formed by substitution reaction (80% yield) and characterized by uni- and bidimensional (1)H, (13)C and (31)P NMR experiments, to confirm its molecular structure. The coordination of (L) to Eu(3+) in the complex [Eu(tta)(3)(L)(2)] was confirmed by FT-IR spectra. The emission spectra present the same profile when excited in Eu(3+) or in the ligands, suggesting an energy transfer from ligands to Eu(3+) ions. The emission spectra of the precursor [Eu(tta)(3)(H(2)O)(2)], and [Eu(tta)(3)(L(2))] present bands arising from f-f intra-configurational transitions. The only (5)D(0)-(7)F(0) transition shows the presence of at least one site without symmetry center. The FWHM of such transition is 7 cm(-1) and 57 cm(-1) for [Eu(tta)(3)(H(2)O)(2)] and [Eu(tta)(3)(L)(2)] complexes, respectively. This widening is provided by the presence of large groups around Eu(3+) ion. The calculated intensity parameters Omega(2) and Omega(4) show that the interaction features between center-ion and ligand are different; the small value of Omega(4) is related to long range effects of alkyl chain. The Langmuir isotherms of this ligand and complex have been investigated although their hydrolysis in water subphase does not allow stable monolayers. (C) 2009 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Crystalline lead-pyrophosphate precursor was prepared in aqueous solution from lead nitrate and phosphoric acid and characterized by X-ray diffraction, thermogravimetry and Raman scattering. This crystalline lead-phosphate was then used to prepare glass samples in the binary system Pb(2)P(2)O(7)-WO(3). Dependence of WO(3) content on thermal, structural and optical properties were investigated by thermal analysis (DSC), Raman spectroscopy, UV-visible and near-infrared absorption and M-Line technique to access refractive index values. Incorporation of WO(3) in the lead-pyrophosphate matrix enhances the glass transition temperature and thermal stability against devitrification, favors formation of P-O-W bonds and WO(6) clusters. In addition, optical properties are strongly modified with a redshift of the optical bandgap with WO(3) incorporation as well as an increase of the refractive index from 1.89 to 2.05 in the visible. (C) 2011 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Organic-inorganic hybrids were prepared using ureapropyltriethoxysilane, methacryloxypropyltrimethoxysilane and acrylic acid modified zirconium(IV) n-propoxide precursors and were characterized by small angle X-ray scattering, X-ray diffraction and photoluminescence spectroscopy. The results indicate an effective interaction between the zirconium-based nanoparticles and the siliceous nanodomains that induces changes in the hybrids' emission features. Planar waveguides were obtained by spin-coating of the prepared sols on sodalime and silica substrates. Refractive index, thickness, number of propagating modes, and attenuation coefficient were measured at 543.5, 632.8 and 1550 nm by the prism coupling technique. The synergism between the two hybrid precursors resulted in monomode planar waveguides with low losses in the infrared ( from 0.6-1.1 dB cm(-1)) which also support a number of propagating modes in the visible ( losses from 0.4-1.5 dB cm(-1)). Channel waveguides were also obtained by UV photopatterning using amplitude or phase masks and propagating modes were observed at 1550 nm.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Tungstate fluorophosphate glasses of good optical quality were synthesized by fusion of the components and casting under air atmosphere. The absorption spectra from near-infrared to visible were obtained and the Judd-Ofelt parameters determined from the absorption bands. Transition probabilities, excited state lifetimes and transition branching ratios, were, determined from the measurements. Pumping with a 354.7 nm beam from a pulsed laser. resulted in emission at 450 nm. due to transition D-1(2)-->F-3(4) in Tm3+ ions and a broadband emission centered at approximate to 550 nm attributed to the glass matrix. When pumping at 650 nm, two emission bands at 450 nm (D-1(2)-->F-3(4)) and at 790 nm (H-3(4)-->H-3(6)) were observed. Excitation spectra were also obtained in order to understand the origin of both emissions. Theoretical and experimental lifetimes were determined and,the results were explained in terms of multiphonon relaxation. (C) 2003 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Barium strontium titanate (Ba0.8Sr0.2TiO3) thin films have been prepared on Pt/Ti/SiO2/Si substrates using a soft solution processing. X-ray diffraction and also micro-Raman spectroscopy showed that the Ba0.8Sr0.2TiO3 thin films exhibited a tetragonal structure at room temperature. The presence of Raman active modes was clearly shown at the 299 and 725 cm(-1) peaks. The tetragonal-to-cubic phase transition in the Ba0.8Sr0.2TiO3 thin films is broadened, and suppressed at about 35 degreesC, with a maximum dielectric constant of 948 (100 kHz). Electrical measurements for the prepared Ba0.8Sr0.2TiO3 thin films showed a remnant polarization (P-r) of 6.5 muC/cm(2), a coercive field (E-c) of 41 kV/cm, and good insulating properties. The dispersion of the refractive index is interpreted in terms of a single electronic oscillator at 6.97 eV. The direct band gap energy (E-g) and the refractive index (n) are estimated to be 3.3 eV and n = 2.27-2.10, respectively. (C) 2002 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Polymer films were grown in rf discharges containing different proportions of C2H2 and SF6. Quantitative optical emission spectrometry (actinometry) was used to follow the trends in the plasma concentrations of the species H and F, and more tentatively, of CH, CF, and CF2, as a function of the feed composition. Infrared spectroscopy revealed the density of CH and CF bonds in the deposited material. As the partial pressure of SF6 in the feed was increased, the degree of fluorination of the polymer also rose. The form of the dependency of the deposition rate on the proportion of SF6 in the feed was in good qualitative agreement with the activated growth model. From transmission ultraviolet visible spectroscopy data the refractive index and the absorption coefficient of the polymers were calculated as a function of the deposition parameters. Since the optical gap depended to some extent upon the degree of fluorination, it could, within limits, be determined by a suitable choice of the proportion of SF6 in the feed. A qualitative explanation of this relationship is given.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

SnO2:Sb multi-layer coatings were prepared by the Pechini method. An investigation was made of the influence of the concentration of Sb2O3 and the viscosity of the precursor solution on the electrical and optical properties of SnO2 thin films. The use of a multi-layer system as an alternative form of increasing the packing and. thus. decreasing porosity proved to be efficient, decreasing the system's resistivity without altering its optical properties. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The influence of the substrate temperature on the structural features and opto-electrical properties of undoped and indium-doped ZnO thin films deposited by pyrosol process was investigated. The addition of indium induces a drastic decrease (by a factor approximate to 10(10) for samples deposited at 300 degreesC) in the electrical resistivity of films, the lowest electrical resistivity (6 mOmega-cm) being observed for the film deposited at 450 degreesC. Films are highly transparent (>80%) in the Vis-NIR ranges, and the optical band gap exhibits a blue shift (from 3.29 to 3.33 eV) for the In-doped films deposited at increasing temperature. Preferential orientation of the ZnO crystallites with the c-axis perpendicular to the substrate surface and an anisotropic morphology of the nanoporous structure was observed for films growth at 300 and 350 degreesC. (C) 2002 Elsevier B.V. B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The refractive index and the temperature coefficient of the optical path length change of tellurite (80TeO(2):20Li(2)O) and chalcogenide glasses (72.5Ga(2)S(3):27.5La(2)O(3)) were determined as a function of temperature (up to 150 degrees C) and wavelength (in the range between 454 and 632.8 nm). The tellurite glass exhibits the usual refractive index dispersion in the wavelength range analyzed, while anomalous refractive index dispersion was observed for the chalcogenide glass between 454 and 530 nm. The dispersion parameters were determined by means of the single-effective oscillator model. In addition, a strong dependence of the temperature coefficient of the optical path length on the photon energy and temperature was found for the chalcogenide glass. The latter was correlated to the shift of the optical band gap (or electronic edge) with temperature, which was interpreted by the electron-phonon interaction model. (C) 2007 American Institute of Physics.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

This work reports the preparation and characterization of (SnO2) thin films doped with 7 mol% Sb2O3. The films were prepared by the polymeric precursor method, and deposited by spin-coating, all of them were deposited on amorphous silica substrate. Then, we have studied the thickness effect on the microstrutural, optical and electric properties of these samples. The microstructural characterization was carried out by X-ray diffraction (XRD) and scanning tunneling microscopy (STM). The electrical resistivity measurements were obtained by the van der Pauw four-probe method. UV-visible spectroscopy and ellipsometry were carried out for the optical characterization. The films present nanometric grains in the order of 13 nm, and low roughness. The electrical resistivity decreased with the increase of the film thickness and the smallest measured value was 6.5 x 10(-3) Omega cm for the 988 nm thick film. The samples displayed a high transmittance value of 80% in the visible region. The obtained results show that the polymeric precursor method is effective for the TCOs manufacturing.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Gallium-doped zinc oxide (ZnO:Ga 1, 2 3, 4 and 5 at%) samples were prepared in powder form by modifying the Pechini method. The formation of zinc gallate (ZnGa2O4) With the spinel crystal structure was observed even in ZnO:Ga 1 at% by X-ray diffraction. The presence of ZnGa2O4 in ZnO:Ga samples was also evidenced by luminescence spectroscopy through its blue emission at 430 nm, assigned to charge transfer between Ga3+ at regular octahedral symmetry and its surrounding O2- ions. The amount of ZnGa2O4 increases as the dopant concentration increases, as observed by the quantitative phase analysis by the Rietveld method. (C) 2006 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)