31 resultados para Material science


Relevância:

30.00% 30.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Pós-graduação em Ciências Sociais - FFC

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Pós-graduação em Educação - FFC

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This work describes the production and characterization of a selective membrane useful for electronic devices. The membrane was a composite made by a thin film of plasma-polymerized HFE (methyl nonafluoro(iso)butyl ether) immersed in plasma-polymerized HMDS (hexamethyldisilazane) film, a third phase being 5 µm starch particles included in this matrix. The film was deposited on silicon substrates and its physical, chemical and adsorption characteristics were determined. Infrared and x-ray photoelectron spectroscopy analyses showed fluorine and carboxyl groups on the bulk and the surface, respectively. SEM results indicate the film is conformal even if starch is present. Optical microscopy analysis showed good resistance toward acid and base solutions. Quartz crystal microbalance indicated adsorption of polar organic compounds on ppm range. This thin film is environment-friendly and can be used as a protective layer or in electronic devices due to adsorption of volatile organic compounds.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This work evaluates fluorinated thin films and their composites for sensor development. Composites were produced using 5 µm starch particles and plasma films obtained from organic fluorinated and silicon compounds reactants. Silicon wafers and aluminum trenches were used as substrates. Film thickness, refractive index and chemical structure were also determined. Scanning electron microscopy shows conformal deposition on aluminum trenches. Films deposited on silicon were exposed to vapor of volatile organic compounds and CV curves were obtained. A qualitative model (FemLab 3.2® program) was proposed for the electronic behavior. These environmentally correct films can be used in electronic devices and preferentially reacted to polar compounds. Nonetheless, due to the difficulty in signal recovery, these films are more effective in one-way sensors, in sub-ppm range.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The ability to integrate multiple materials into miniaturized fiber structures enables the realization of novel biomedical textile devices with higher-level functionalities and minimally-invasive attributes. In this work, we present novel textile fabrics integrating unobtrusive multi-material fibers that communicate through 2.4 GHz wireless networks with excellent signal quality. The conductor elements of the textiles are embedded within the fibers themselves, providing electrical and chemical shielding against the environment, while preserving the mechanical and cosmetic properties of the garments. These multi-material fibers combine insulating and conducting materials into a well-defined geometry, and represent a cost-effective and minimally-invasive approach to sensor fabrics and bio-sensing textiles connected in real time to mobile communications infrastructures, suitable for a variety of health and life science applications.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This article describes a new approach of recycling the leather waste (shavings) using it as filler in natural rubber foams composites. The foams were prepared using different amounts of leather waste (0-60 parts per hundred of rubber) and submitted to morphological (SEM microscopy) and mechanical analyses (cyclic stress-strain compression). The increase of leather shavings on the composite causes an increase of viscosity in the mixture, which reflects in the foaming process. This results in smaller and fairly uniform cells. Furthermore, expanded rubber has the biggest cell size, with more than 70% of cell with 1000 mu m, while the composite with the higher concentration of leather has around 80% of total number of cells with 100-400 mu m. The mechanical parameters were found to depend on the leather dust concentration. Moreover, the stiffness rises with the increase of leather shavings; consequently, the compression force for expanded rubber was 0.126 MPa as well as the composite with higher concentration of leather was 7.55 MPa. (c) 2014 Wiley Periodicals, Inc. J. Appl. Polym. Sci. 2015, 132, 41636.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The aim of this study was to evaluate the deformation suffered by cantilevered implant-supported fixed prostheses frameworks cast in silver-palladium alloy and coated with two occlusal veneering materials: acrylic resin or porcelain. Material and Methods: Two strain gauges were bonded to the inferior surface of the silver-palladium framework and two other were bonded to the occlusal surface of the prosthesis framework covered with ceramic and acrylic resin on each of its two halves. The framework was fixed to a metallic master model and a 35.2 N compression force was applied to the cantilever at 10, 15 and 20 mm from the most distal implant. The measurements of deformation by compression and tension were obtained. The statistical 2-way ANOVA test was used for individual analysis of the experiment variables and the Tukey test was used for the interrelation between all the variables (material and distance of force application). Results: The results showed that both variables had influence on the studied factors (deformation by compression and tension). Conclusion: The ceramic coating provided greater rigidity to the assembly and therefore less distortion compared with the uncoated framework and with the resin-coated framework. The cantilever arm length also influenced the prosthesis rigidity, causing higher deformation the farther the load was applied from the last implant.