353 resultados para Ferroelectric and dielectric
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Piezoresponse Force Microscopy (PFM) is used to characterize the nanoscale electromechanical properties of centrosymmetric CaCu3Ti4O12 ceramics with giant dielectric constant. Clear PFM contrast both in vertical (out-of-plane) and lateral (in-plane) modes is observed on the ceramic surface with varying magnitude and polarization direction depending on the grain crystalline orientation. Lateral signal changes its sign upon 180 degrees rotation of the sample thus ruling out spurious electrostatic contribution and confirming piezoelectric nature of the effect. Piezoresponse could be locally reversed by suitable electrical bias (local poling) and induced polarization was quite stable showing long-time relaxation (similar to 3 hrs). The electromechanical contrast in unpoled ceramics is attributed to the surface flexoelectric effect (strain gradient induced polarization) while piezoresponse hysteresis and ferroelectric-like behavior are discussed in terms of structural instabilities due to Ti off-center displacements and structural defects in this material. (C) 2011 American Institute of Physics. [doi:10.1063/1.3623767]
Resumo:
Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)
Resumo:
Fundação de Amparo à Pesquisa do Estado de São Paulo (FAPESP)
Resumo:
Lead zirconate powder, with Zr/Ti ratio of 50/50 was prepared by polymeric precursor method and doped with 3, 5 and 7 mol% of Sr+2 Or Ba+2, as well as by 0.2 to 5 mol% of Nb+5. The powder was calcined at 750 degrees C by 4 hours and milled during 1.5 h in isopropilic alcohol. Powders were characterized by surface area measurements (BET method), by infrared spectroscopy and by X-ray diffraction to characterize the crystal structure. Isostatically pressed samples were sintered in a dilatometer furnace by using a constant heating rate of 10 degrees C/min from ambient to 1200 degrees C. Synthetic air and air with water vapor were used as atmospheres. Both Sr+2 and Ba+2 substitute Pb+2 and favor the formation of rhombohedral phase. Otherwise, Nb+5 substitute preferentially Zr+4 favoring tetragonal phase. The concentration of dopants and the atmosphere influence the densification and the microstructure of the PZT, which alters the dielectric and piezoelectric properties of the ceramics.
Resumo:
Ceramic samples of SrBi2(Nb1-xTax)O-9 (0 less than or equal to x less than or equal to 1) were prepared by the solid state reaction method in order to investigate their structural and electrical features as well as obtain useful information to improve the properties of SrBi2(Nb1-xTax)O-9 as a thin film. The X-ray diffraction patterns and the scanning electronic microscopy photomicrographs show no secondary phases but the formation of a solid-state solution for all the composition. The ac conductivity of the samples, measured at 25 degreesC and 100 kHz frequency, decreases with the increase of Ta content. Such results were explained by intrinsic conductivity of pure components.
Resumo:
Ferroelectric layefed-perovskite BaBi2Ta2O9 (BBT) has been prepared successfully by solid-state reaction. The influence of pressure and temperature/time annealing regime on the BBT phase formation was analyzed. The powders were characterized by thermal analysis and Xray diffraction and the sintered pellets by scanning electron microscopy. The crystalline BBT phase, free of secondary phases was obtained at 950 degreesC for 2 h. For an applied field strength of 380 kV/cm, a remnant polarization of 7.6 muC/cm(2) and an electric coercive field of 45.7 kV/cm were obtained. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Our efforts were directed to the preparation of bismuth titanate-Bi4Ti3O12 (BIT) by two procedures: mechanically assisted synthesis and polymeric precursor method to display a variety of their advantages. To follow the nucleation and phase formation of BIT, XRD and Rietveld refinement analysis were used and it was shown that Bi4Ti3O12 ceramic can been successfully prepared from nano-sized powders obtained by both methods. The ferroelectric properties were determined and the loops from BIT obtained by polymeric precursor method were not fully saturated with a remnant polarization of 20 mu C/cm(2) and coercitive field of 1500 kV/cm. BIT obtained from powders prepared by mechanically assisted synthesis shows a remnant polarization of 0.65 mu C/cm(2) and coercitive field of 1050 kV/cm. The grain morphology may be the factor causing the observed differences. (C) 2005 Published by Elsevier Ltd and Techna Group S.r.l.
Resumo:
Ferroelectric CaBi4Ti4O15 (CBTi144) thin films were deposited on Pt/Ti/SiO2/Si substrates by the polymeric precursor method. The films present a single phase of layered-structured perovskite with polar axis orientation after annealing at 700 degrees C for 2 h in static air and oxygen atmosphere. The a/b-axis orientation of the ferroelectric film is considered to be associated with the preferred orientation of the Pt bottom electrode. It is noted that the films annealed in static air showed good polarization fatigue characteristics at least up to 10(10) bipolar pulse cycles and excellent retention properties up to 10(4) s. on the other hand, oxygen atmosphere seems to be crucial in the decrease of both, fatigue and retention characteristics of the capacitors. Independently of the applied electric field, the retained switchable polarization approached a nearly steady-state value after a retention time of 10 s. (C) 2006 Elsevier B.V. All rights reserved.
Resumo:
Dielectric spectroscopy was used in this study to examine CaCu3Ti4O12 polycrystalline samples. The analysis involved systems presenting low non-Ohmic properties, and the grain's internal domain was evaluated separately from the contribution of barrier-layer capacitances associated with Schottky-type barriers in this type of material. The effect of oxygen-rich atmosphere and high cooling rate was evaluated, revealing a strong increase in the dielectric properties of the CaCu3Ti4O12 system under these conditions. This effect was attributed to a chemical change in the grain's internal domain, which may be considered an internal barrier-layer capacitance of the polycrystalline material. (c) 2006 American Institute of Physics.
Resumo:
The dielectric properties of (Ba, Sr)TiO3 films were found to be remarkably sensitive to the postannealing treatment atmosphere. This study demonstrates that postannealing in an oxygen atmosphere increases the dielectric relaxation phenomenon and that postannealing in a nitrogen atmosphere produces a slight dielectric relaxation. Such dependence of the dielectric relaxation was related both to oxygen vacancies and to the presence of negatively charged oxygen, trapped at the grain boundary and/or at the electrode/dielectric film interface. (C) 2000 American Institute of Physics. [S0003-6951(00)00817-2].
Resumo:
Composites, made of lead zirconate titanate (PZT) ceramic powder and castor oil-based polyurethane (PU), were prepared in the film form. The films were obtained in the thickness range 100-300 mum using up to 50/50 vol.% of ceramic. Another composite (PZT/C/PU) was obtained by adding a small amount (1.0 vol.%) of graphite (C) to the PZT/PU composite. By increasing the conductivity of PU-containing graphite, polarization of PZT could be carried out with better efficiency. A comparison of piezo- and pyroelectric activities and spatial distribution of polarization between graphite doped and undoped composites reveal the advantages of using semiconductor filler. These composites were used as sensors to detect acoustic emission (AE). The detection was made using two simulated sources of AE, i.e., ball bearing drop and pencil lead break. PZT/C/PU composite was able to detect both flexural and extensional components of wave vibration. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
SrBi2Nb2O9 (SBN) thin films were prepared by the polymeric precursors method and deposited by dip coating onto Pt/Ti/SiO2/Si(100) substrates. The dip-coated films were specular and crack-free and crystallized during firing at 700 degrees C. Microstructure and morphological evaluation were followed by grazing incident X-ray diffraction (GIXRD), scanning electron microscopy (SEM) and atomic force microscopy (AFM). The films exhibited somewhat porous grain structure with rounded grains of about 100 nm. For the electrical measurements, gold electrodes of 300 mu m in diameter were sputter deposited on the top surface, forming a metal-ferroelectric-metal (MFM) configuration. The remanent polarization (P-r) and coercive field (E-c) were 5.6 mu C/cm(2) and 100 kV/cm, respectively. (C) 1999 Elsevier B.V. B.V. All rights reserved.
Resumo:
Pure and lanthanum-doped Bi4Ti3O12 thin films were deposited on Pt/Ti/SiO2/Si substrate using a polymeric precursor solution. The spin-coated films were specular and crack-free and crystalline after annealing at 700 degreesC for 2 h. Crystallinity and morphological evaluation were examined by X-ray diffraction (XRD), scanning electron microscopy (SEM), and atomic force microscopy (AFM). Multilayered films obtained using the intermediate-crystalline layer route present a dense microstructure with spherical grains. Films obtained using the intermediate-amorphous layer, present elongated grains around 250 nm in size. The dielectric and ferroelectric properties of the lanthanum-doped Bi4Ti3O12 films are strongly affected by the crystallization route. The hysteresis loops are fully saturated with a remnant polarization and drive voltage of the films, heat-treated by the intermediate-crystalline (P-r = 20.2 muC/cm(2) and V = 1.35 V) and for the film heat-treated by amorphous route (P-r = 22.4 muC/cm(2) and V = 2.99 V). (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
Morphology of three samples of alumina are investigated. Infrared spectra are analysed by use of their morphology through the theory of average dielectric constant. Crystal shape is obtained from X-ray diffraction patterns by reflection intensity ratio. In the case of electron scanning microscopy, shape factor was obtained by an average axial ratio of the particles. Comparison of results show that there is agreement among these techniques and infrared spectra can be used to determine the morphology of alumina particles from 2.7 to 10 mu m, even for heterogeneous samples. (C) 1999 Elsevier B.V. B.V. All rights reserved.