Resumo:
The effect of magnesium addition on the phase formation, microstructure and electric and ferroelectric properties of LiNbO 3 thin films prepared through polymeric precursors was analyzed. By X ray diffraction no secondary phase was observed with the increase of magnesium concentration. Comparing to pure LiNbO 3, the addition of 0.5 and 1.0 mol% of Mg +2 increased of the dielectric constant, while 2.0 mol% decreased it. It was noticed that the increase in additive concentration decreases the ferroelectric remanent polarization and increases the coercive field. © 2002 Taylor & Francis.
Resumo:
Strontium-modified lead titanate thin films with composition Pb1-xSrxTiO3 were grown on Pt/Ti/SiO2/Si substrates using the polymeric precursor method. The structural phase evolution as a function of the Sr contents was studied using micro-Raman scattering, specular reflectance infrared Fourier transform spectroscopy, and x-ray diffraction. The results showed a gradual change from tetragonal to cubic structure, the transition occurring at about x = 0.58. The infrared reflectance spectra showed that the frequency of several peaks decreases as the strontium concentration increases. These features are correlated with a decrease in the tetragonal distortion of the TiO6 octahedra as the strontium concentration increases.
Resumo:
Lead zirconate titanate (PZT) solutions were prepared using a polymeric precursor method, Zr n-propoxide and Ti i-propoxide were used as starting materials with ethylene glycol and water as solvents. The PZT solution was spin-coated on Pt/Ti/SiO2/Si substrates, baked on a hot plate, and finally heat-treated in a tube furnace between 400 and 800°C. The surface morphology and grain size of the films were characterized by atomic force microscopy (AFM), using a tapping mode with amplitude modulation. The films, thermal annealed at temperatures higher than 500°C, exhibited a dense microstructure, without noticeable cracks or voids. Electrical properties were investigated as a function of composition and annealing temperature.
Resumo:
Thin films of lithium niobate were deposited on the Pt/Ti/SiO2 (111) substrates by the polymeric precursor method (Pechini process). Annealing in static air and oxygen atmosphere was performed at 500°C for 3 hours. The films obtained were characterized by X-ray diffraction, scanning electron microscopy and transmission electron microscopy. The dielectric constant, dissipation factor and resistance were measured in frequency region from 10 Hz to 10 MHz. Electrical characterizations of the films pointed to ferroelectricity via hysteresis loop. The influence of oxygen atmosphere on crystallization and properties of LiNbO3 thin films is discussed.
Resumo:
It is very important for the building of the SAW devices to study dielectric and ferroelectrics properties because every SAW device is based in piezoelectric effect that it is made up to transform an electric sign in the mechanical or acoustic sign and a mechanical or acoustic sign in an electric sign. Thus, the purpose of the present work is to prepare PbZr 0,53Ti0.47O3 (PZT) and PbTiO3 (PT) thin films on the Si (100) substrates across spin-coating using a chemical method based in polymeric precursors. After conventional treatment in the furnace, the films were characterized by impedance spectroscopy and hysteresis loops to know its dielectric and ferroelectric properties.
Resumo:
Pure and scandium doped-TiO2 thin films were prepared by the sol-gel process and coated by dip coating. The effects of scandium on the phase formation, optical properties and photoactivity of the TiO2 thin films were investigated. The lattice parameters and the crystallinity of the anatase phase, characterized by the Rietveld method, demonstrated that scandium doping affected the structural parameters and crystallinity of the films, modifying the absorption edge. A direct correlation was found between band gap energy and photodegradation efficiency, with lower values of band gap energy augmenting this efficiency. Moreover, a significant improvement in the catalyst's photodegradation efficiency was attained with a scandium concentration of 5.0 mol%. © 2007 Springer Science+Business Media, LLC.
Resumo:
Optical excitation of Ce3+-doped SnO2 thin films, obtained by the sol-gel-dip-coating technique, is carried out and the effects on electrical transport are evaluated. Samples are doped with O. lat% of Ce, just above the saturation limit. The excitation is done with an intensity-controlled halogen-tungsten lamp through an interference filter, yielding an excitation wavelength of 513nm, 9 nm wide (width at half intensity peak). Irradiation at low temperature (25K) yields a conductivity increase much lower than above bandgap light. Such a behavior assures the ionization of intra-bandgap defect levels, since the filter does not allow excitation of electron-hole pairs, what would happen only in the UV range (below about 350nm). The decay of intra-bandgap excited levels in the range 250-320 K is recorded, leading to a temperature dependent behavior related to a thermally excited capture cross section for the dominating defect level. © 2008 American Institute of Physics.
Resumo:
Using pump-probe reflectometry, we study the ultrafast excited-state dynamics in thin films of BuPTCD, an organic semiconductor, deposited on gold nanoparticles. We observe depletion of the ground state and excited state absorption after photo-excitation. © 2008 Optical Society of America.
Resumo:
This paper focuses on the magnetoelectric coupling (ME) at room temperature in lanthanum modified bismuth ferrite thin film (BLFO) deposited on SrRuO 3-buffered Pt/TiO 2/SiO 2/Si(100) substrates by the soft chemical method. BLFO film was coherently grown at a temperature of 500 °C. The magnetoelectric coefficient measurement was performed to evidence magnetoelectric coupling behavior. Room temperature magnetic coercive field indicates that the film is magnetically soft. The maximum magnetoelectric coefficient in the longitudinal direction was close to 12 V/cmOe. Dielectric permittivity and dielectric loss demonstrated only slight dispersion with frequency due the less two-dimensional stress in the plane of the film. Polarization reversal was investigated by applying dc voltage through a conductive tip during the area scanning. We observed that various types of domain behavior such as 71 ° and 180° domain switching, and pinned domain formation occurred. Copyright © 2009 American Scientific Publishers All rights reserved.
Resumo:
We present a study on the thin film morphology and the optical properties of eumelanin resulting from different synthesis routes: the oxidation of tyrosine with hydrogen peroxide, the auto-oxidation of dihydroxyphenylanaline in water and its auto-oxidation in dimethyl sulfoxid. Atomic Force Microscopy images indicate that the presence of holes and particles depends on the eumelanin synthesis route and the substrate employed. Smooth films with very few defects could be obtained with eumelanin synthesized in dimethyl sulfoxide deposited on glass substrates. Our study shows that all eumelanin preparations are comparable in terms of thin film morphology on the submicrometer scale and UV-visible transmission properties. ©The Electrochemical Society.
Resumo:
CCTO thin films were deposited on Pt(111)/Ti/SiO 2/Si substrates using a chemical (polymeric precursor) and pressure method. The pressure effects on the CCTO thin films were evaluated by XRD, FEG-SEM and optical properties. Pressure films were found to be more homogeneous and dense than chemical deposition films. Pressure also leaded to an increase in the photoluminescence emission; it is suggested that the displacement of Ti in the titanate clusters, favors the charge transference from TiO 6 to [TiO 5V o z], TiO 5V o z] to [CaO 11V o z] and [TiO 5V o z] to [CuO 4] x. The low synthesis temperature used in the pressure method allows the deposition of films on less expensive substrates (i.e. glass, aluminum, polymer and others).
Resumo:
Lead zirconate titanate Pb(Zr 0.50Ti 0.50)O 3 (PZT) thin films were deposited by a polymeric chemical method on Pt(111)/Ti/SiO2/Si substrates to understand the mechanisms of phase transformations and the effect of film thickness on the structure, dielectric and piezoelectric properties in these films. PZT films pyrolyzed at temperatures higher than 350 °C present a coexistence of pyrochlore and perovskite phases, while only perovskite phase grows in films pyrolyzed at temperatures lower than 300 °C. For pyrochlore-free PZT thin films, a small (100) orientation tendency near the film-substrate interface was observed. Finally, we demonstrate the existence of a self-polarization effect in the studied PZT thin films. Results suggest that Schottky barriers and/or mechanical coupling near the filmsubstrate interface are not primarily responsible for the observed self-polarization effect in our films. © 2012 IEEE.
Resumo:
The influence of benzoyl peroxide (BPO) on the synthesis of polysiloxane thin films doped with Ce(III) deposited onto Sn coated steel as well as their anticorrosion properties are reported. The addition of BPO, whose role is polymerize the film, showed an increase in |Z| values due to the fact that augments the crossed link bonds and therefore improves the protective feature of the film. Ce(III) does not act in the polymerization process and thus is essential the addition of BPO to obtain more resistant polysiloxane films. ©The Electrochemical Society.
Resumo:
ZnO thin films were prepared by the polymeric precursor method. The films were deposited on silicon substrates using the spin-coating technique, and were annealed at 330°C for 32h under pressure-assisted thermal annealing and under ambient pressure. Their structural and optical properties were characterized, and the phases formed were identified by X-ray diffraction. No secondary phase was detected. The ZnO thin films were also characterized by field-emission scanning electron microscopy, Fourier transform infrared spectroscopy, photoluminescence and ultraviolet emission intensity measurements. The effect of pressure on these thin films modifies the active defects that cause the recombination of deep level states located inside the band gap that emit yellow-green (575nm) and orange (645nm) photoluminescence. © 2012 John Wiley & Sons, Ltd.