272 resultados para TiO2-SnO2 composite
Resumo:
The oxidation of a reactive dye, Reactive Blue 4, RB4, (C.I. 61205), widely used in the textile industries to color natural fibers, was studied by electrochemical techniques. The oxidation on glassy carbon electrode and reticulated vitreous carbon electrode occurs in only one step at 2.0 < PH < 12 involving a two-electron transfer to the amine group leading to the imide derivative. Dye solution was not decolorized effectively in this electrolysis process. Nevertheless, the oxidation of this dye on Ti/SnO2/SbOx (3% mol)/RuO2 (1% mol) electrode showed 100% of decolorization and 60% of total organic carbon removal in Na2SO4 0.2 M at PH 2.2 and potential of +2.4 V. Experiments on degradation photoelectrocatalytic were also carried out for RB4 degradation in Na2SO4 0.1 K PH 12, using a Ti/TiO2 photoanode biased at +1.0 V and UV light. After 1 h of electrolysis the results indicated total color removal and 37% of mineralization. (c) 2004 Elsevier Ltd. All rights reserved.
Resumo:
The electrical and microstructural properties of SnO2-based varistors with the addition of 0.025 and 0.050 mol% of Fe2O3 have been characterised. Electric field (E) versus current density (J) curves showed that the effect of Fe2O3 addition is to increase both the non-linear coefficient and the breakdown voltage. Variations in the potential barrier height were inferred from impedance spectroscopy (IS) analysis. Through transmission electron microscopy (TEM), the presence of precipitates of secondary phases was confirmed. Samples with precipitates displayed poor electrical properties. (c) 2004 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
Resumo:
This paper reports a study of influence of Cr concentration on the electrical properties and microstructure of SnO2-based powders doped with Mn and Nb, prepared by an organic route (Pechini method). All the samples were compacted into discs and sintered at 1300 degrees C for 3h, resulting in ceramics with relative density varying between 78% and 98%. The powders were characterized by X-ray diffraction analysis. Impedance spectroscopy characterization indicated that the conductivity decreases as Cr concentration increases, probably due to Cr segregation at grain boundaries, which reduces grain size, increasing the number of resistive boundaries.
Resumo:
The influence of yttrium oxide, Y2O3, on the microstructure development of the SnO(2)center dot Co(3)O(4)center dot Nb2O5 typical varistor system was studied with scanning (SEM) and transmission (TEM) electron microscopies. The different phases present in the studied samples were characterized through XRD, EDS and selected area diffraction patterns (SAD). Particles of Co2SnO4 were observed with TEM in every sample, whereas clusters of the pyrochlore phase T2Sn2O7 were observed with SEM in samples with 0.05, 0.10 and 0.25 mol% of Y2O3. The higher non-linearity (a = 16) was achieved with the addition of 0.05 mol% of Y2O3. The influence of the secondary phases on the electrical properties is also addressed in this work. (c) 2005 Published by Elsevier B.V.
Resumo:
The preparation of the ZrO(2):8 mol % Y(2)O(3)/NiO (YSZ/NiO) composites by a modified liquid mixture technique is reported. Nanometric NiO particles dispersed over the yttria-stabilized zirconia (YSZ) were prepared, resulting in dense sintered specimens with no solid solution formation between the oxides. Such a feature allowed for the electrical characterization of the composites in a wide range of relative volume fraction, temperature, and oxygen partial pressure. The main results indicate that the composites have high electrical conductivity, and the transport properties in these mixed ionic-electronic (MIEC) composites are strongly dependent on the relative volume fraction of the phases, microstructure, and temperature. These parameters should hence be taken into consideration for the optimized design of MIEC composites for electrochemical applications. In this context, the composite was reduced under H(2) for the preparation of high-conductivity YSZ/Ni cermets for use as solid oxide fuel cell anode material with relatively low metal content. (c) 2005 the Electrochemical Society. [DOI:10.1149/1.2149312] All rights reserved.
Resumo:
Addition of 0.5 mol% of CoO into SnO2 promotes densification of this oxide to 99% of the theoretical density during sintering. TEM in this system reveals that after sintering at 1210 degrees C a secondary phase of Co2SnO4 is precipitated at the SnO2 grain boundaries during cooling. This phase is formed by diffusion of Co ions from the bulk to the grain boundary during sintering leaving needle-like defects at the grain bulk. The high resolution TEM micrograph of this system sintered at 1210 degrees C and 1400 degrees C showed an amorphous grain boundary region low in cobalt, indicating that the Co2SnO4 phase is precipitated from this region. (C) 1999 Elsevier B.V. Limited and Techna S.r.l. All rights reserved.
Resumo:
Suspensions of undoped SnO2 nanoparticles and containing Eu3+ ions were prepared by a sol-gel procedure. Using the classical synthesis method ( precipitation), the particles tend to grow by a coarsening process in order to minimize the surface free energy. This effect can strongly be reduced by the addition of an amide and surfactant during the synthesis, which decreases the surface free energy of the colloidal particles. These additives promote the formation of powders composed of very small primary particles formed by a crystallite of 10 Angstrom, and exhibit good redispersion properties. The local and long order structures of the redispersible powder were studied by X-rays absorption spectroscopy at Sn L-I edge and X-rays diffraction, respectively. The structure of the colloidal aggregates in suspension was investigated by small angle X-rays scattering (SAXS). SAXS results indicate the sol are composed by a polidisperse system of hard spheres resulting of agglomeration of the primary particles and their size increasing by agglomeration for progressively higher Eu3+ content.
Resumo:
Photoconductivity of SnO2 sol-gel films is excited, at low temperature, by using a 266 nm line-fourth harmonic-of a Nd:YAG laser. This line has above bandgap energy and promotes generation of electron-hole pairs, which recombines with oxygen adsorbed at grain boundary. The conductivity increases up to 40 times. After removing the illumination on an undoped SnO2 film, the conductivity remains unchanged, as long as the temperature is kept constant. Adsorbed oxygen ions recombine with photogenerated holes and are continuously evacuated from the system, leaving a net concentration of free electrons into the material, responsible for the increase in the conductivity. For Er doped SnO2, the excitation of conductivity by the laser line has similar behavior, however after removing illumination, the conductivity decreases with exponential-like decay. (C) 2003 Elsevier Ltd. All rights reserved.
Resumo:
The thermal decomposition of ammonium perchlorate (AP)/hydroxyl-terminated-polybutadiene (HTPB), the AP/HTPB solid propellant, was studied at different heating rates in dynamic nitrogen atmosphere. The exothermic reaction kinetics was studied by differential scanning calorimetry (DSC) in non-isothermal conditions. The Arrhenius Parameters were estimated according to the Ozawa method. The calculated activation energy was 134.5 W mol(-1), the pre-exponential factor, A, was 2.04.10(10) min(-1) and the reaction order for the global composite decomposition was estimated in 0.7 by the kinetic Shimadzu software based on the Ozawa method. The Kissinger method for obtaining the activation energy value was also used for comparison. These results are discussed here.