268 resultados para titanate


Relevância:

10.00% 10.00%

Publicador:

Resumo:

The aim of this work is to investigate the structural properties of the (Pb1-xErx)TiO3 (PET) powders, with x varying from 0.01 to 0.08, prepared by the polymeric precursor method. Combined X-ray diffraction, Raman spectroscopy and ab initio calculation reveal a diffuse phase-transition of a tetragonal to a cubic phase. The crystalline models built allowed to calculate electronic properties and to analyze the behavior of the doping element in the structure of the material, which are consistent with the experimental results that indicate the beginning of phase-transition from tetragonal to cubic. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Conselho Nacional de Desenvolvimento Científico e Tecnológico (CNPq)

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this work we optimized conditions for aerosol deposition of homogeneous, nano-grained, smooth Ba0.8Sr0.2TiO3 thin films. Investigation involved optimization of deposition parameters, namely deposition time and temperature for different substrates. Solutions were prepared from titanium isopropoxide, strontium acetate and barium acetate. Films were deposited on Si (1 0 0) or Si covered by platinum (Pt (1 1 1) /Ti/SiO2/Si). Investigation showed that the best films were obtained at substrate temperature of 85 degrees C. After deposition films were slowly heated up to 650 degrees C, annealed for 30 min, and slowly cooled. Grain size of BST films deposited on Si substrate were in the range 40-70 nm, depending on deposition conditions, while the same films deposited on Pt substrates showed mean grain size in the range 35-50 nm. Films deposited under optimal conditions were very homogeneous, crack-free, and smooth with rms roughness lower than 4 nm for both substrates.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this article a new technique for thermal neutron detection using pyroelectric ceramics is described. The detector system is basically constituted of a PZT (lead zirconate titanate) ceramic attached to an uranium disk. The energy released in the uranium fission gives rise to an electrical signal in the detector which is amplified by a lock-in system. The neutron beam impinging on the uranium disk was modulated with a cadmium chopper. Thermal neutron fluxes within the interval of 103 to 106 n/cm2 s have been detected using a U3O8 pellet with 20% enrichment in 235U. © 1992.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This paper describes two simple thermal methods for measuring the energy fluence in J/cm 2 from a diagnostic x-ray exposure. Both detectors absorb essentially 100% of the radiation and give a signal that is directly proportional to the energy fluence of the x-ray beam. One detector measures the thermal effect when a pulse of x rays is totally absorbed in the pyroelectric detector of lead-zirconium-titanate (PZT). The other detector measures the expansion of a gas surrounding a lead disk detector in a photoacoustic chamber. The increased pressure of the gas is transmitted through a 1-mm duct to a sensitive microphone. Both detectors have previously been used to measure the energy fluence rate of continuous x-ray beams in the same energy region using a chopped beam and a lock-in amplifier. Measurement of the energy fluence of a pulse of radiation eliminates the need for the beam chopper and lock-in amplifier and results in a simple, rugged, and inexpensive dosimeter. Either method can be combined with the area of the beam to give an estimate of the imparted energy to the patient from a diagnostic x-ray exposure.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The phase formation mechanism, as well as the morphotropic phase boundary, of lead zirconate titanate (PZT) processed by a partial oxalate method was investigated by simultaneous thermal analysis (TG-DTA) and by qualitative and quantitative X-ray diffraction (XRD). The results show that the ZrxTi1-xO2 (ZT) phase reacts with PbO forming the PZT phase without intermediate phases. XRD analysis showed the coexistence of rhombohedral and tetragonal phases for 0.47 ≤ x ≤ 0.55 with the phase boundary composition for x = 0.51. For low calcination temperatures, preferential formation of the PZT rhombohedral phase was observed. A model for phase formation of PZT by the partial oxalate method is proposed based on the existence of two interfaces of reaction (PbO-PZT and PZT-ZT) and diffusion of cations.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

PbMg1/3Nb2/3O3 (PMN) prepared by organic solution of citrates was analyzed by the Rietveld method to determine the influence of seeds and dopants on the perovskite and pyrochlore phase formation. It was observed that pyrochlore phase formation increases with an increase in calcination time when no additives are included during the preparation. It was also observed that a greater amount of perovskite phase appeared in doped or seeded samples. The fraction of perovskite phase increased from 88 mol % in pure sample to ∼95 mol % in doped and seeded samples calcined at 800°C for 1 h. It is clear that the addition of dopants or seeds during PMN preparation can enhance the formation of perovskite phase.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The use of polymeric precursors was employed in preparing SrTiO3 thin films by dip coating using Si (111) as substrate. Crack free films were obtained after sintering at temperatures ranging from 550 to 1000°C. The microstructure, characterized by SEM, shows the development of dense polycrystalline films with smooth surface and mean grain size of 52 nm, for films sintered at 1000°C. Grazing incident angle XRD characterization of these films shows that the SrTiO3 phase crystallizes from an inorganic amorphous matrix. No intermediate crystalline phase was identified.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The particle-growth kinetics of sodium niobate and zirconium titanate powders that were processed by the polymeric precursors method were studied. The growth kinetics that were studied for the particle, in the final stage of crystallization, showed that the growth process occurs in two different stages. For temperatures <800°C, the particle-growth mechanism is associated with surface diffusion, with an activation energy in the range of 40-80 KJ/mol. For temprratures >800°C, particle growth is controlled by densification of the nanometric particle cluster and by a neck-size-controlled particle-growth mechanism. The results suggest that this behavior was typical of the synthesis method, because two different polycation oxides presented the same behavior.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Lead titanate powders were synthesized through the use of polymeric precursors according to the Pechini Process. The polymeric precursor was calcined at temperatures ranging from 300 to 600°C for 1 or 2 h. X-ray diffraction (XRD) showed that lead titanate crystallizes from the precursor at temperatures as low as 400°C. No intermediate carbonate phase was detected by Fourier transform infrared spectroscopy (FTIR) or by XRD. A powder with mean particle size of 150 nm was obtained after calcination of the precursor at 600°C for 1 h. © 1998 Elsevier Science B.V. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Ferroelectric ceramic particles based on lead titanate zirconate (PZT) were dispersed in a polymer matrix based on castor oil. After the poling process, the pyroelectric activity of this composite was measured using a direct method in which a linear heating rate was applied to the pre-poled samples. The pyroelectric coefficient at 343 K is comparable with that of a PZT-poly(vinylidene fluoride) (PVDF) composite and significantly higher than that of PVDF. © 1998 Kluwer Academic Publishers.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Flexible and free-standing films of piezoelectric composites made up of lead zirconate titanate (PZT) ceramic powder dispersed in a castor oil-based polyurethane (PU) matrix were obtained by spin coating and characterized as materials for sensor applications. The piezoelectric coefficients d 31 and d 33 were measured with the usual technique. The piezoelectric charge constant d 33 yields values up to ≤24 pC/N, even at lower PZT content (33 vol%). Some desirable properties like piezoelectricity, flexibility and good mechanical resistance show this new material to be a good alternative for use as sensors and actuators.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Ferroelectric barium titanate thin films were produced by the polymeric precursor method. In this technique, the desired metal cations are chelated in a solution using a hydroxycarboxylic acid as the chelating agent. Barium carbonate and titanium IV isopropoxide were used as precursors for the citrate solution. Ethylene glycol and citric acid were used as polymerization/complexation agents for the process. The crystalline structure of the film annealed at 700 °C had a single perovskite phase with a tetragonal structure. The BaTiO3 film showed good P-E hysteresis loops and C-V characteristics due to the switched ferroelectric domains.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Lead lanthanum zirconate titanate (PLZT) thin films with (9/65/35) stoichiometry were prepared by dip coating from polymeric precursor method. The films deposited on silicon (100) substrates, were thermally treated from 450° to 700°C for 6 hours in order to study the influence of thermal treatment on the crystallinity, microstructure, grain size and roughness of the final film. X-ray diffraction results showed that PLZT phase crystallizes at low temperature (500°C) and present preferential orientation. It was observed by scanning electron microscopy (SEM) that it is possible to obtain dense thin films at temperatures around 650°C. The atomic force microscopy (AFM) studies showed that the grain size and roughness are strongly influenced by the annealing temperature.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this study the preparation of 9.5/65/35 PLZT ceramic powders were investigated. The powders with the formula Pb0.905La0.095(Zr0.65 Ti0.35)0.976O3 + 3.5 w% PbO were prepared using Pechini process and partial oxalate method. The powder phase formation, powder morphology, and green density of PLZT were shown.