Resumo:
Lanthanum-modified bismuth titanate, Bi4-xLaxTi3O12 (BLT), thin films with a La concentration of 0.75 was grown on Pt/Ti/SiO2/Si substrates by using the polymeric precursor solution and spin-coating method. The scanning electron microscopy (SEM) showed rounded grains, which is not typical for these system. The BLT films showed well-saturated polarization-electric field curve which 2P(r) = 41.4 muC/cm(2) and V-c = 0.99 V. The capacitance dependence on the voltage is strongly nonlinear, confirming the ferroelectric properties of the film resulting from the domains switching. These properties make BLT a promising material for FERAM applications.
High Curie point CaBi2Nb2O9 thin films: A potential candidate for lead-free thin-film piezoelectrics
Resumo:
CaBi2Nb2O9 (CBNO) thin films deposited on platinum coated silicon substrates by the polymeric precursor method exhibited good structural, dielectric, and piezoelectric characteristics. Capacitance-voltage measurements indicated good ferroelectric polarization switching characteristics. Remanent polarization and drive voltage values were 4.2 mu C/cm(2) and 1.7 V for a maximum applied voltage of 10 V. The film has a piezoelectric coefficient d(33) equal to 60 pm/V, current density of 0.7 mu A/cm(2), and Curie temperature of 940 degrees C. The polar-axis-oriented CBNO is a promising candidate for use in lead-free high Curie point in ferroelectric and piezoelectric devices. (c) 2006 American Institute of Physics.
Resumo:
The gap between the bulk materials and thin films can be filled with thick films suitably designed and appropriate processed. Thick films of complex system like lead-lanthanum-zirconium titanate (PLZT) is difficult to produce by simple solid-state reaction keeping compositional homogeneity and optimal grain size distribution. In the present work, PLZT thick films were fabricated by screen-printing technique from nanosized powders obtained through soft chemistry by polymeric precursor method. Thick film paste was obtained by mixing PLZT fine powders and organic vehicle. The upper and bottom electrodes based on Ag-Pd and functional component based on PLZT were screen-printed on alumina substrate and after that annealed in air atmosphere. The powder morphology, microstructure, dielectric and ferroelectric properties of 9.5/65/35 PLZT thick films were analysed. (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
Polycrystalline or single-crystal ferroelectric materials present dielectric dispersion in the frequency range 100 MHz-1 GHz that has been attributed to a dispersive ( relaxation-like) mechanism as well as a resonant mechanism. Particularly in 'normal' ferroelectric materials, a dielectric response that is indistinguishable from dispersion or a resonance has been reported. Nevertheless, the reported results are not conclusive enough to distinguish each mechanism clearly. A detailed study of the dielectric dispersion phenomenon has been carried out in PbTiO3-based ferroelectric ceramics, with the composition Pb1-xLaxTiO3 (x = 0.15), over a wide range of temperatures and frequencies, including microwave frequencies. The dielectric response of La-modified lead titanate ferroelectric ceramics, in 'virgin' and poled states, has been investigated in the temperature and frequency ranges 300-450 K and 1 kHz-2 GHz, respectively. The results revealed that the frequency dependence of the dielectric anomalies, depending on the measuring direction with respect to the orientation of the macroscopic polarization, may be described as a general mechanism related to an 'over-damped' resonant process. Applying either a uniaxial stress along the measurement field direction or a poling electric field parallel and/or perpendicular to the measuring direction, a resonant response of the real and imaginary components of the dielectric constant is observed, in contrast to the dispersion behavior obtained in the absence of the stress, for the 'virgin' samples. Both results, resonance and/or dispersion, can be explained by considering a common mechanism involving a resonant response (damped and/or over-damped) which is strongly affected by a ferroelastic-ferroelectric coupling, contributing to the low-field dielectric constant.
Resumo:
The influence of subacute and chronic lead intoxication on the responsiveness of the rat vas deferens was investigated by determining pD2 and relative responsiveness ratio (p) values for noradrenaline and for acetylcholine. Thus, the pD2 values of noradrenaline and acetylcholine from vas deferens of lead-treated rats were greater than those from normal rats, indicating that lead, in the dose and periods of treatment utilized, provoked a rise in vas deferens sensibility to noradrenaline and acetylcholine. Since it is known that the cirurgical or chemical denervation of the sexual ducts also provokes hypersensitivity, it may be suggested that this would be a possible mechanism for the observed alterations. A local lead toxic effect on the smooth muscle or at the level of androgen receptors should also be considered.
Resumo:
A new lead fluoroborate glass (PbO-PbF2-B2O3) doped with ytterbium (Yb:PbFB) is presented. Samples with different concentrations of Yb3+ were produced and had their emission cross-sections, fluorescence lifetimes and minimum pump intensities determined. They have high refractive index of 2.2 and a density of 4.4 g/cm(3). For a doping level of 1.153x10(20) ions/cm(3), the fluorescence lifetime, after excitation at 968 nm, is 0.81 ms, which is comparable to Yb:tellurite laser glass. Also, an emission band at 1022 nm is measured with emission cross-section of approximately 1.07x10(-20) cm(2) and fluorescence effective linewidth of 60 nm, which is comparable to Yb:phosphate laser glass. (C) 2001 Optical Society of America.
Resumo:
Lead toxicity was studied in rats exposed from conception until weaning and assessed by monitoring offspring behavior in both the open field and elevated plus maze and by determining tissue lead in an assessment schedule extended to first (F1) and second (F2) generations. Dams utilized for the F1 generation were submitted to 750 ppm of lead (acetate) in drinking water during pregnancy and lactation. For F1 pups, behavioral alterations were not detected in the elevated plus maze, while in the open field, spontaneous locomotor activity as well as time of both grooming and rearing increased, while freezing time decreased in 30- and 90-day-old rats. Lead content was higher in tissues of 1- and 30-day-old pups. However, in 90-day-old rats, lead was detected only in the femur. F2 generation was lead-free but still presented alterations in both locomotor activity and grooming in 30- and 90-day-old pups. It appears that developmental lead exposure may cause behavioral effects during the developmental stage of the F1 generation, which remains throughout the animal's adult life as a sequel, regardless of lead accumulation, and is extended to the F2 generation of rats. (C) 2001 Elsevier B.V. All rights reserved.
Resumo:
Diode-pumped Yb-doped glass lasers have received considerable attention for applications such as high-power beam production or femtosecond pulses generation. In this paper, we evaluate the laser potential of three different glass families doped with Yb3+ : alkali lead fluorborate (PbO-PbF2-B2O3), heavy metal oxide (Bi2O3-PbO-Ga2O3) and niobium tellurite (TeO2-Nb2O5-K2O-Li2O). Spectroscopic properties were studied for the samples and calculations of the minimum laser pump intensity (I-min), saturation fluence (U-sat) and the theoretical limit of peak power (P-max) are also presented. A comparison of laser properties of these three different glasses and their importance is shown and analyzed. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
Lanthanum-modified bismuth titanate, Bi4-xLaxTi3O12 (BLT), thin films with a La concentration ranging from 0 to 0.75 were grown on Pt/Ti/SiO2/Si substrates using a polymeric precursor solution and spin-coating method. The scanning electron microscopy shows a change of morphology with increasing the lanthanum concentration. The BLT films show well-saturated polarization-electric field curves whit remnant polarizations of 14.7, 20.5, 21.5, and 20.4 muC/cm(2) for x = 0, 0.25, 0.50 and 0.75, respectively. The dielectric constant of BLT (x = 0.75 mol% La) is equal to 158 while dielectric loss remain low (tandelta = 0.0018).
Resumo:
The family of bismuth titanate, Bi(4)Ti(3)O(12) (BIT) layered-structured ferroelectrics materials is attractive from the viewpoint of such as their application as electronic materials dielectrics, piezoelectrics and pyroelectrics, because they are characterized by good stability of piezoelectric properties, a high Curie temperature and a good resistance vs temperature. Bismuth titanate (Bi(4)Ti(3)O(12)) powders can be prepared using different methods, depending if the creation will be film coating or ceramics. The structure and properties of bismuth titanate materials show a significance dependence on the applied synthesis method. In this review paper, we made an attempt to give an approach to analyszing the structure, synthesis methods and properties of bismuth titanate ferroelectrics materials.
Resumo:
This study was aimed at investigating the in vitro biocompatibility of a novel membrane of the composite poly(vinylidene-trifluoroethylene)/barium titanate (P(VDF-TrFE)/BT). Osteoblastic cells were obtained from human alveolar bone fragments and cultured under standard osteogenic condition until subconfluence. First passaged cells were cultured on P(VDF-TrFE)/BT and expanded polytetrafluoroethylene (e-PTFE - control) membranes in 24-well plates. Cell adhesion and spreading were evaluated at 30 min, and 4 and 24 h. For proliferation assay, cells were cultured for 1, 7, and 10 days. Cell viability was detected by trypan blue at 7 and 10 days. Total protein content and alkaline phosphatase (ALP) activity were measured at 7, 14, and 21 days. Cultures were stained with Alizarin red at 21 days, for detection of mineralized matrix. Data were compared by ANOVA and Student t test. Cell attachment (p = 0.001), cell number (p = 0.001), and ALP activity (p = 0.0001) were greater on P(VDF-TrFE)/BT. Additionally, doubling time was greater on P(VDF-TrFE)/BT (p = 0.03), indicating a decreased proliferation rate. Bone-like nodule formation took place only on P(VDF-TrFE)/BT. The present results showed that both membranes are biocompatible. However, P(VDF-TrFE)/BT presented a better in vitro biocompatibility and allowed bone-like nodule formation. Therefore, P(VDF-TrFE)/BT could be an alternative membrane to be used in guided tissue regeneration. (c) 2006 Wiley Periodicals, Inc.
Resumo:
Bismuth titanate (Bi4Ti3O12-BIT) films were evaluated for use as lead-free piezoelectric thin-films in micro-electromechanical systems. The films were grown by the polymeric precursor method on Pt/Ti/SiO2/Si (1 0 0) (Pt) bottom electrodes at 700 degrees C for 2 h in static air and oxygen atmospheres. The domain structure was investigated by piezoresponse force microscopy (PFM). Annealing in static air leads to better ferroelectric properties, higher remanent polarization, lower drive voltages and higher piezoelectric coefficient. on the other hand, oxygen atmosphere favors the imprint phenomenon and reduces the piezoelectric coefficient dramatically. Impedance data, represented by means of Nyquist diagrams, show a dramatic increase in the resistivity for the films annealed in static air atmopshere. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
Lanthanum doped bismuth titanate thin films (Bi3.25La0.75Ti3O12-BLT) were produced by the polymeric precursor method and crystallized in a domestic microwave oven and in conventional furnace. Using platinum coated silicon substrates configuration, ferroelectric properties of the films were determined with remanent polarization P-r and a coercive field E-c of 3.9 mu C/cm(2) and 70 kV/cm for the film annealed in the microwave oven and 20 mu C/cm(2) and 52 kV/cm for the film annealed in conventional furnace, respectively. The films annealed in conventional furnace exhibited excellent retention-free characteristics at low infant periods indicating that BLT thin films can be a promise material for use in nonvolatile memories. on the other hand, the pinning of domains wall causes a strong decay at low infant periods for the films annealed in the microwave furnace which makes undesireable the application for future FeRAMS memories. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
A powder mixture of BaO and TiO2, was mechanochemically treated in a planetary ball mill in an air atmosphere for up to 4 h, using zirconium oxide vial and zirconium oxide balls as the milling medium. Mechanochemical reaction leads to the gradual formation of BaTiO3 phase. Phase evolution during synthesis and changes in powder size and morphology were monitored by XRD, DSC, IR and TEM analysis and it was shown that the formation of BaTiO3 phase was initiated after 60 min. Extended time of milling directed to formation of higher amount of BaTiO3 perovskite phase. Barium titanate with good crystallinity was formed after 240 min sintering without pre-calcination step was performed at 1330 degrees C for 2 It within heating rate 10 degrees C/min. (c) 2005 Elsevier Ltd. All rights reserved.