28 resultados para plasma polymers
Resumo:
Amorphous hydrogenated chlorinated carbon (a-C:H:Cl) films were produced by the plasma polymerization of chloroform-acetylene-argon mixtures in a radiofrequency plasma enhanced chemical vapor deposition system. The main parameter of interest was the proportion of chloroform in the feed, R(C), which was varied from 0 to 80%. Deposition rates of 80 nm min (1) were typical for the chlorinated films. Infrared reflection-absorption spectroscopy revealed the presence of C-Cl groups in all the films produced with chloroform in the feed. X-ray photoelectron spectroscopy confirmed this finding, and revealed a saturation of the chlorine content at similar to 47 at.% for R(C)>= 40%. The refractive index and optical gap, E(04), of the films were roughly in the 1.6 to 1.7, and the 2.8 to 3.7 eV range. These values were calculated from transmission ultraviolet-visible-near infrared spectra. Chlorination leads to an increase in the water surface contact angle from similar to 40 degrees to similar to 77 degrees. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
This paper deals with the study of optical, structural and biocompatible properties of PEO-like plasma polymerized films resulting from RF excited diethylene glycol dimethyl ether (CH3O(CH2CH2O)(2)CH3 diglyme) glow discharges. The study was carried out using visible-ultraviolet and FTIR spectroscopies and contact angle measurements. FTIR spectra of plasma polymerized diglyme showed a stronger presence of ethylene glycol groups in film structure for lower RF power levels. The contact angle measurements for water revealed an increasing from 30degrees to 62,5degrees when the RF power was varied from 2 to 45 W, indicating the decreasing of the hydrophilic character of diglyme films with the increasing of RF power. This trend is in agreement with FTIR results. The data from visible-ultraviolet reflectance and transmittance spectra revealed alterations on optical properties of plasma polymerized diglyme films. The film's optical gap varied from 3.8 to 3 eV for RF power running from 5 to 45 W.
Resumo:
Benzene plasma polymer films were bombarded with Ar ions by plasma immersion ion implantation. The treatments were performed using argon pressure of 3 Pa and 70 W of applied power. The substrate holder was polarized with high voltage negative pulses (25 kV, 3 Hz). Exposure time to the immersion plasma, t, was varied from 0 to 9000 s. Optical gap and chemical composition of the samples were determined by ultraviolet-visible and Rutherford backscattering spectroscopies, respectively. Film wettability was investigated by the contact angle between a water drop and the film surface. Nanoindentation technique was employed in the hardness measurements. It was observed growth in carbon and oxygen concentrations while there was decrease in the concentration of H atoms with increasing t. Furthermore, film hardness and wettability increased and the optical gap decreased with t. Interpretation of these results is proposed in terms of the chain crosslinking and unsaturation. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
The effects of ion irradiation on fluorinated plasma polymer films are investigated using profilometry, surface contact-angle measurements, infrared reflection absorption spectroscopy (IRRAS) and X-ray photoelectron spectroscopy (XPS). Remarkably, helium plasma immersion ion implantation (PIII) of several amorphous hydrogenated fluorinated plasma polymers deposited from C(2)H(2)-SF(6), C(6)H(6)-SF(6) or C(6)F(6) produces film compactions of up to 40%, and modifies the surface energy in the 35 to 65 dyn cm(-1) range. As revealed by IRRAS and XPS, the films contain C-H, C-C, C=C, C=O, O-H and C-F groups. XPS spectra confirm the presence of N (typically similar to 5%). The films produced from SF(6)-containing plasmas also contain S. For irradiation times of 80 min, the film carbon content is increased, and the fluorine content is greatly reduced, by factors of about 3 to 15, depending on the initial film composition. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Novel brominated amorphous hydrogenated carbon (a-C:H:Br) films were produced by the plasma polymerization of acetylene-bromoform mixtures. The main parameter of interest was the degree of bromination, which depends on the partial pressure of bromoform in the plasma feed, expressed as a percentage of the total pressure, R-B. When bromoform is present in the feed, deposition rates of up to about 110 nm min(-1) may be obtained. The structure and composition of the films were characterized by Transmission Infrared Reflection Absorption Spectroscopy (IRRAS) and X-ray Photo-electron Spectroscopy (XPS). The latter revealed that films with atomic ratios Br:C of up to 0.58 may be produced. Surface contact angles, measured using goniometry, could be increased from similar to 63 degrees (for an unbrominated film) to similar to 90 degrees for R-B of 60 to 80%. Film surface roughness, measured using a profilometer, does not depend strongly on R-B. Optical properties the refractive index, n, absorption coefficient, alpha(E), where E is the photon energy, and the optical gap, E-g, were determined from film thicknesses and data obtained by Transmission Ultraviolet-Visible Near Infrared Spectroscopy (UVS). Control of n was possible via selection of R-B. The measured optical gap increases with increasing F-BC, the atomic ratio of Br to C in the film, and semi-empirical modeling accounts for this tendency. A typical hardness of the brominated films, determined via nano-indentation, was similar to 0.5 GPa. (C), 2013 Elsevier B.V. All rights reserved.
Resumo:
Polymer films, deposited from acetylene and argon plasma mixtures, were bombarded with 150 keV He+ ions, varying the fluence, Phi, from 10(18) to 10(21) ions/m(2). Molecular structure and optical gap of the samples were investigated by infrared and ultraviolet-visible spectroscopies, respectively. Two-point probe was employed to determine the electrical resistivity while hardness was measured by nanoindentation technique. It was verified modification of the molecular structure and composition of the films. There was loss of H and increment in the concentration of unsaturated carbon bonds with Phi. Optical gap and electrical resistivity decreased while hardness increased with Phi. Interpretation of these results is proposed in terms of chain crosslinking and unsaturation. (C) 2002 Elsevier B.V. B.V. All rights reserved.
Resumo:
Coordenação de Aperfeiçoamento de Pessoal de Nível Superior (CAPES)
Resumo:
Highly fluorinated plasma polymers are chemically inert,acid resistant and have low friction coefficients, thereby being useful in chemical laboratories and for tribological applications. Here we report the plasma polymerization of ethylene-hexafluorobenzene mixtures by PECVD. The principal parameter of interest is the proportion of C(6)F(6) in the feed, R(F). Films were analyzed using near-normal and grazing-angle Infrared Reflection Absorption Spectroscopy (IRRAS), the latter being particularly useful for detecting modes not usually observed at near-normal incidence. The presence of CH and CF(x) (x=1 to 2) groups was thus confirmed in films deposited with R(F)>= 40%. Depending on R(F) IRRAS also revealed the presence of -CH(x) (x=1 to 3) -C=C, -C=O and phenyl rings. Deconvolution of C is spectra obtained by X-ray Photoelectron Spectroscopy (XPS) confirmed the presence of CH, CF and CF(2) groups in films deposited with R(F)>= 40%. Atomic ratios of F:C calculated from the XPS spectral data show that the degree of fluorination rises with increasing RF Some unbound fluorine is present in the films. Post-deposition reactions account for the presence of oxygen (similar to 5%) in the films. Surface energies, determined from contact angle measurements, fall with increasing R(F). (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
Plasma treatments are frequently employed to modify surface properties of materials such as adhesivity, hydrophobicity, oleophobicity etc. Present work deals with surface modification of common commercial polymers such as polyethylene terephthalate (PET) and polyurethane (PU) by an air dielectric barrier discharge (DBD) at atmospheric pressure. The DBD treatment was performed in a plain reactor in wire-duct geometry (non-uniform field reactor), which was driven by a 60 Hz power supply. Material characterization was carried out by water contact angle measurements, atomic force microscopy (AFM) and X-ray photoelectron spectroscopy (XPS). The plasma-induced modifications are associated with incorporation of polar oxygen and nitrogen containing groups on the polymer surface. The AFM analysis reveals that the plasma treatment roughens the material surface. Due to these structural and morphological changes the surface of DBD-treated polymers becomes more hydrophilic resulting in enhanced adhesion properties. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
In this work it was investigated the effect of the exposure to different plasmas on the wettability of silicone samples. We have observed that oxygen. argon, and hydrogen glow discharges are quite effective in reducing the water contact angle of such polymer. However, indifferently to efficiency of the treatment, practically all the modified surfaces recovered great part of their original hydrophobicity. We have investigated this hydrophobic recovery using surface energy measurements and theoretical simulations based on the exponential decay of the population of polar groups on the surface. According to our results such recovery can be attributed to the decrease of polar species at the interface water-polymer surface.
Resumo:
This work describes an XPS investigation of plasma-deposited polysiloxane films irradiated with 170 keV He+ ions at fluences, Phi, ranging from 1 x 10(14) to 1 x 10(16) cm(-2). Modifications in the atomic concentrations of the surface atoms with (D were revealed by changes in the [O]/[Si], [O]/[C] and [C]/[Si] atomic ratios. Surface chemical structure modifications were evidenced by the increasing C1s peak width and asymmetry as Phi was increased, due to the formation of ether and carboxyl functionalities. Moreover, structural transformations were indicated by the positive binding energy shift of the Si2p peaks, due to the increasing Si oxidation. Correlations of the XPS data with other results from previous work on polysiloxanes illustrate the role of ion beam-induced bond breaking on the structural modifications.
Resumo:
Polymer films were grown in rf discharges containing different proportions of C2H2 and SF6. Quantitative optical emission spectrometry (actinometry) was used to follow the trends in the plasma concentrations of the species H and F, and more tentatively, of CH, CF, and CF2, as a function of the feed composition. Infrared spectroscopy revealed the density of CH and CF bonds in the deposited material. As the partial pressure of SF6 in the feed was increased, the degree of fluorination of the polymer also rose. The form of the dependency of the deposition rate on the proportion of SF6 in the feed was in good qualitative agreement with the activated growth model. From transmission ultraviolet visible spectroscopy data the refractive index and the absorption coefficient of the polymers were calculated as a function of the deposition parameters. Since the optical gap depended to some extent upon the degree of fluorination, it could, within limits, be determined by a suitable choice of the proportion of SF6 in the feed. A qualitative explanation of this relationship is given.
Resumo:
Commercial polyvinylchloride (PVC) sheets were treated by plasma immersion ion implantation, PIII. Samples were immersed in argon glow discharges and biased with 25 kV negative pulses. Exposure time to the bombardment plasma changed from 900 to 10,800 s. Through contact angle measurements, the effect of the exposure time on the PVC wettability was investigated. Independent of t, all samples presented contact angles, theta, equal to zero after the treatment. However, in some cases, surface hydrophilization was not stable, as revealed by the temporal evolution of theta. Samples bombarded for shorter periods recovered partially or totally the hydrophobic character while the one exposed for the longest time stayed highly hydrophilic. These modifications are ascribed to the Cl loss and O incorporation as shown by XPS measurements. Furthermore, the mobility of surface polar groups and the variation in the cross-linking degree can also affect the PVC wettability.
Resumo:
Thin polymer films were grown in radio frequency discharges containing C2H2. Actinometry revealed the trend in the plasma concentration of the CH species as a function of the operating pressure. The C-H bond density in the films, revealed by infrared analysis, was found to increase with the pressure of C2H2 in a similar way to that of the concentration of the CH species in the discharge. From transmission ultraviolet-visible spectroscopy data, optical parameters of the polymers, namely, the refractive index and the optical gap, were calculated. For the range of pressure studied, the refractive index decreased from 1.73 to 1.63 and the optical gap increased from 2.4 to 3.3 eV. Finally, measurements of the residual stress of the polymer films were carried out by the bending beam method, using a He-Ne laser, yielding values from 0.05 to 0.3 GPa. (C) 1995 American Vacuum Society.
Resumo:
Ag-containing polyethyleneoxide (FEO)-like thin films have been deposited in Radio Frequency Glow Discharges fed with vapors of diethyleneglycol-dimethyl-ether and argon. Proper experimental conditions have been utilized in order to fragment the monomer in the glow and, at the same time, sputter Ag from the silver RF cathode of the reactor, in a way that polyethyleneoxide(PEO)-like coatings with embedded Ag clusters have been deposited at the ground electrode. The composition of the coatings has been investigated by means of different techniques; the plasma process has been investigated by means of Actinometric Optical Emission Spectroscopy. A correlation has been found between the amount of silver embedded in the coatings and that sputtered in the discharge, monitored by actinometry, that could eventually be utilized to control in situ the deposition process.