2 resultados para solo-fibra
em Universidade Federal do Rio Grande do Norte(UFRN)
Resumo:
To take care of to the demand of the new constructions in the low income communities and to develop the production of a strengthened alternative brick with staple fibers of coconut, capable to contribute mainly with the recycling of the green and mature coconut in the urban and agricultural lexes, this research was developed, to confection bricks of soil-cement with coconut fiber. Ecologically correct material and of low cost, since the greenhouse use of or oven for burning will be manufactured without. The study it presents a set of tables and graphs that prove good indices found in the values of the density, water absorption, axial compressive strength and isolation term acoustics, with evidential results that make possible the production in industrial character with press mechanics or the place of the workmanship with manual form. The preparation of coconut staple fibers was made of natural form without use of chemical products not to deprive of characteristics the properties mechanical physicist-chemistries and of the same ones. The sixty bricks produced in simple and manual press had been carried through in four lots of fifteen units. The mixture of aggregates was made in four different traces composites for: ground erinaceous, cement, fiber of dry coconut and water; the bricks had been compact in the press and cured in natural way under an area covered during the minimum time of seven days
Resumo:
In this work the use of coconut fiber (coir) and bamboo shafts as reinforcement of soil-cement was studied, in order to obtain an alternative material to make stakes for fences in rural properties. The main objective was to study the effect of the addition of reinforcement to the soil-cement matrix. The effect of humidity on the mechanical properties was also analyzed. The soil-cement mortar was composed by a mixture, in equal parts, of soil and river sand, 14% in weight of cement and 10 % in weight of water. As reinforcement, different combinations of (a) coconut fiber with 15 mm mean length (0,3 %, 0,6 % and 1,2 % in weight) and (b) bamboo shafts, also in crescent quantities (2, 4 and 8 shafts per specimen) were used. For each combination 6 specimens were made and these were submitted to three point flexural test after 28 days of cure. In order to evaluate the effect of humidity, 1 specimen from each of the coconut fiber reinforced combination was immersed in water 24 hours prior to flexural test. The results of the tests carried out indicated that the addition of the reinforcement affected negatively the mechanical resistance and, on the other hand, increased the tenacity and the ductility of the material.