Nonisothermal crystallization behaviors of PVA and poly (vinyl alcohol) and Silica (PVA/SiO2) nanocomposites prepared via a self-assembly monolayer (SAM) technique are investigated in this study. Differential scanning calorimetry (DSC) is used to measure the crystallization temperature and enthalpy of PVA and nanocomposites in nitrogen at various cooling rate. The results show that the degree of crystallinity of PVA and nanocomposites decreases when the SiO2 content increases but increases with an increasing cooling rate. The peak crystallization temperature decreases with an increasing cooling rate.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The phase behavior, morphology and crystallization in blends of a low-molecular-weight (Mn = 1400) double-crystalline polyethylene-block-poly(ethylene oxide) (PE-PEO) diblock copolymer with poly(hydroxyether of bisphenol A) (PH) were investigated by differential scanning calorimetry, transmission electron microscopy and small-angle X-ray scattering. The symmetric PE-PEO diblock copolymer consists of a PH-miscible PEO block and a PH-immiscible PE block. However, PH only exhibits partial miscibility with the PEO block of the copolymer in the PH/PE-PEO blends; both macrophase and microphase separations took place. There existed two macrophases in the PH/PE-PEO blends, i.e., a PH-rich phase and a PE-PEO copolymer-rich phase. The PE block of the copolymer in the blends exhibited fractionated crystallization behavior by homogeneous nucleation. There appeared three crystallization exotherms related to the crystallization of the PE block within three different microenvironments in the PH/PE-PEO blends.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

In this study, a novel method for manufacturing composite tubes utilizing the QuickstepTM process has been developed. Tubes manufactured from `quick-cure' Toray G83C prepreg have demonstrated highly repeatable axial crush behavior with an average specific energy absorption (SEA) of 86 kJ/kg. The cure cycle is optimized by comparing the results from compression, dynamic mechanical thermal analysis (DMTA), differential scanning calorimetry (DSC), and porosity testing. The tube lay-up is optimized using compression and porosity test results. The effect of changes in fiber-orientation on SEA is also investigated. Process development has resulted in a robust manufacturing method capable of producing fully cured, high performance composite tubes with a cure cycle of 7 min. This corresponds to a 95% reduction in time compared to an equivalent autoclave cycle.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Thermosetting polymer blends of poly(ethylene oxide) (PEO) and bisphenol-A-type epoxy resin (ER) were prepared using 4,4′-methylenebis(3-chloro-2,6-diethylaniline) (MCDEA) as curing agent. The miscibility and crystallization behavior of MCDEA-cured ER/PEO blends were investigated by differential scanning calorimetry (DSC). The existence of a single composition-dependent glass transition temperature (Tg) indicates that PEO is completely miscible with MCDEA-cured ER in the melt and in the amorphous state over the entire composition range. Fourier-transform infrared (FTIR) investigations indicated hydrogen-bonding interaction between the hydroxyl groups of MCDEA-cured ER and the ether oxygens of PEO in the blends, which is an important driving force for the miscibility of the blends. The average strength of the hydrogen bond in the cured ER/PEO blends is higher than in the pure MCDEA-cured ER. Crystallization kinetics of PEO from the melt is strongly influenced by the blend composition and the crystallization temperature. At high conversion, the time dependence of the relative degree of crystallinity deviated from the Avrami equation. The addition of a non-crystallizable ER component into PEO causes a depression of both the overall crystallization rate and the melting temperature. The surface free energy of folding σe displays a minimum with variation of composition. The spherulitic morphology of PEO in the ER/PEO blends exhibits typical characteristics of miscible crystalline/amorphous blends, and the PEO spherulites in the blends are always completely volume-filling. Real-time small-angle X-ray scattering (SAXS) experiments reveal that the long period L increases drastically with increasing ER content at the same temperatures. The amorphous cured ER component segregates interlamellarly during the crystallization process of PEO because of the low chain mobility of the cured ER. A model describing the semicrystalline morphology of MCDEA-cured ER/PEO blends is proposed based on the SAXS results. The semicrystalline morphology is a stack of crystalline lamellae; the amorphous fraction of PEO, the branched ER chains and imperfect ER network are located between PEO lamellae.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Nanostructured thermoset blends of bisphenol A-type epoxy resin (ER) and amphiphilic poly(ethylene oxide)-block-poly(propylene oxide)-block-poly(ethylene oxide) (PEO-PPO-PEO) triblock copolymers were successfully prepared. Two samples of PEO-PPO-PEO triblock copolymer with different ethylene oxide (EO) contents, denoted as EO30 with 30 wt % EO content and EO80 with 80 wt % EO content, were used to form the self-organized thermoset blends of varying compositions using 4,4'-methylenedianiline (MDA) as curing agent. The phase behavior, crystallization, and morphology were investigated by differential scanning calorimetry (DSC), transmission electron microscopy (TEM), atomic force microscopy (AFM), and small-angle X-ray scattering (SAXS). It was found that macroscopic phase separation took place in the MDA-cured ER/EO30 blends containing 60-80 wt % EO30 triblock copolymer. The MDA-cured ER/EO30 blends with EO30 content up to 50 wt % do not show macroscopic phase separation but exhibit nanostructures on the order of 10-30 nm as revealed by both the TEM and SAXS studies. The AFM study further shows that the ER/EO30 blend at some composition displays structural inhomogeneity at two different nanoscales and is hierarchically nanostructured. The spherical PPO domains with an average size of about 10 nm are uniformly dispersed in the 80/20 ER/EO30 blend; meanwhile, a structural inhomogeneity on the order of 50-200 nm is observed. The ER/EO80 blends are not macroscopically phase-separated over the entire composition range because of the much higher PEO content of the EO80 triblock copolymer. However, the ER/EO80 blends show composition-dependent nanostructures on the order of 10-100 nm. The 80/20 ER/EO80 blend displays hierarchical structures at two different nanoscales, i.e., a bicontinuous microphase structure on the order of about 100 nm and spherical domains of 10-20 nm in diameter uniformly dispersed in both the continuous microphases. The blends with 60 wt % and higher EO80 content are completely volume-filled with spherulites. Bundles of PEO lamellae with spacing of 20-30 nm interwoven with a microphase structure on the order of about 100 nm are revealed by AFM study for the 30/70 ER/EO80 blend.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

This work reports the first instance of self-organized thermoset blends containing diblock copolymers with a crystallizable thermoset-immiscible block. Nanostructured thermoset blends of bisphenol A-type epoxy resin (ER) and a low-molecular-weight (Mn = 1400) amphiphilic polyethylene-block-poly(ethylene oxide) (EEO) symmetric diblock copolymer were prepared using 4,4'-methylenedianiline (MDA) as curing agent and were characterized by transmission electron microscopy (TEM), atomic force microscopy (AFM), small-angle X-ray scattering (SAXS), and differential scanning calorimetry (DSC). All the MDA-cured ER/EEO blends do not show macroscopic phase separation but exhibit microstructures. The ER selectively mixes with the epoxy-miscible PEO block in the EEO diblock copolymer whereas the crystallizable PE blocks that are immiscible with ER form separate microdomains at nanoscales in the blends. The PE crystals with size on nanoscales are formed and restricted within the individual spherical micelles in the nanostructured ER/EEO blends with EEO content up to 30 wt %. The spherical micelles are highly aggregated in the blends containing 40 and 50 wt % EEO. The PE dentritic crystallites exist in the blend containing 50 wt % EEO whereas the blends with even higher EEO content are completely volume-filled with PE spherulites. The semicrystalline microphase-separated lamellae in the symmetric EEO diblock copolymer are swollen in the blend with decreasing EEO content, followed by a structural transition to aggregated spherical micellar phase morphology and, eventually, spherical micellar phase morphology at the lowest EEO contents. Three morphological regimes are identified, corresponding precisely to the three regimes of crystallization kinetics of the PE blocks. The nanoscale confinement effect on the crystallization kinetics in nanostructured thermoset blends is revealed for the first time. This new phenomenon is explained on the basis of homogeneous nucleation controlled crystallization within nanoscale confined environments in the block copolymer/thermoset blends.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

In this paper, sereval varieties of animal fibres including cashmere and Australian fine Merino wool have been analysed by Fourier transform infrared microscope and differential scanning calorimeter. The results showed that both Chinese and Australian cashmere fibres started absorbing heat at a relatively higher temperature but were thermally degraded quicker than other animal fibres tested. However, the mass changes (within the temperature range of 200oC to 350oC) and associated onset temperatures varied among fibre varieties. From the attenuated total reflectance spectra, the Chinese cashmere was clearly different from Australian cashmere and wool in a peak near 1040 cm-1 wavelength for S-O stretching of cysteic acid residues. The Chinese cashmere presented a stronger absorption at 1019 cm-1 wavelength, while Australian cashmere and wool peaked at 1079 cm-1 wavelength and had a weaker absorption. Combined with thermal analysis, the normalised R-SO3 - content of cysteic acid residues to the amide II peak of the protein backbone may have potential use in identifying Australian fine Merino wool from Chinese cashmere.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

A novel polyvinylalcohol/silica (PVA/SiO2) nano-composite is prepared with the self-assembly monolayer (SAM) technique. The SiO2 nano-particles are homogenously distributed throughout the PVA matrixes as nano-clusters with an average diameter ranged from 15 to 240 nm depending on the SiO2 contents. Using differential scanning calorimetry (DSC), the non-isothermal crystallisation behaviour and kinetics of the PVA/SiO2 nano-composites are investigated and compared to those of the pure PVA. There are strong dependences of the degree of crystallinity (Xc), peak crystallisation temperature (Tp), half time of crystallisation (t1/2), and Ozawa exponent (m) on the SiO2 content and cooling rate. The crystallisation activation energy (E) calculated with the Kissinger model is markedly lower when a small amount of SiO2 is added, then gradually increases and finally becomes higher than that of the pure PVA when there is more than 10% SiO2 in the composite.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

In this study, we have electrospun poly(vinyl alcohol)(PVA) nanofibres and PVA composite nanofibres containing multi-wall carbon nanotubes (MWNTs) (4.5 wt%), and examined the effect of the carbon nanotubes and the PVA morphology change induced by post-spinning treatments on the tensile properties, surface hydrophilicity and thermal stability of the nanofibres. Through differential scanning calorimetry (DSC) and wide-angle x-ray diffraction (WAXD) characterizations, we have observed that the presence of the carbon nanotubes nucleated crystallization of PVA in the MWNTs/PVA composite nanofibres, and hence considerably improved the fibre tensile strength. Also, the presence of carbon nanotubes in PVA reduced the fibre diameter and the surface hydrophilicity of the nanofibre mat. The MWNTs/PVA composite nanofibres and the neat PVA nanofibres responded differently to post-spinning treatments, such as soaking in methanol and crosslinking with glutaric dialdehyde, with the purpose of increasing PVA crystallinity and establishing a crosslinked PVA network, respectively. The presence of carbon nanotubes reduced the PVA crystallization rate during the methanol treatment, but prevented the decrease of crystallinity induced by the crosslinking reaction. In comparison with the crosslinking reaction, the methanol treatment resulted in better improvement in the fibre tensile strength and less reduction in the tensile strain. In addition, the presence of carbon nanotubes reduced the onset decomposition temperature of the composite nanofibres, but stabilized the thermal degradation for the post-spinning treated nanofibres. The MWNTs/PVA composite nanofibres treated by both methanol and crosslinking reaction gave the largest improvement in the fibre tensile strength, water contact angle and thermal stability.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

A simple sol–gel method was developed for hydroxyapatite/titania (HA/TiO2) coatings on non-toxic titanium–zirconium (TiZr) alloy for biomedical applications. The HA/TiO2-coated TiZr alloy displayed excellent bioactivity when soaked in a simulated body fluid (SBF) for an appropriate period. Differential scanning calorimetry, thermogravimetric analysis, X-ray diffraction and scanning electron microscopy-energy dispersive spectrometry were used to characterize the phase transformations and the surface structures and to assess the in vitro tests. The HA/TiO2 layers were spin-coated on the surface of TiZr alloy at a speed of 3000 rpm for 15 s, followed by a heat treatment at 600 °C for 20 min in an argon atmosphere sequentially. The TiO2 layer exhibited a cracked surface and an anatase structure and the HA layer displayed a uniform dense structure. Both the TiO2 and HA layers were 25 μm thick, and the total thickness of the HA/TiO2 coatings was 50 μm. The TiZr alloy after the above HA/TiO2 coatings displayed excellent bone-like apatite-forming ability when soaked in SBF and can be anticipated to be a promising load-bearing implant material.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Two amorphous ribbons with the compositions of Al88Ni6La6 and Al86Ni6La6Cu2 were made using the meltspun method, and their thermal response and electrochemical behavior were studied comparatively. Differential scanning calorimetry (DSC) and electrochemical polarization measurements indicated that Al86Ni6La6Cu2 exhibited slightly higher crystallization temperature (Tx), lower melting point (T1) and better corrosion resistance in 0.01 mol · L−1 NaCl alkaline solution. These results demonstrated that Cu (2%) addition could slightly promote the glass forming ability, but it could greatly improve the corrosion resistance of Al88Ni6La6 alloy in 0.01 mol · L−1 NaCl alkaline solution.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The effect of the heat treatment on the corrosion behaviour of amorphous Al88Ni6La6 made by melt-spun has been investigated by electrochemical measurements. Heat treatment was carried out at 523 K and 673 K for 4 min and 15 min respectively. The evolution of the crystallization process after annealing was identified by differential scanning calorimeter (DSC) as well as X-ray diffraction. The XRD patterns show that the structure of samples heat-treated at higher temperature changes towards a crystal state. The results obtained from the polarization curves reveal that all Al88Ni6La6 alloys exhibit spontaneously passivated behaviour. Furthermore, it is noted that the partially crystallized alloy has the best corrosion resistance in comparison with as-spun amorphous and fully crystallized alloys, while the fully crystallized sample shows deterioration in the corrosion resistance.