53 resultados para ZNO NANOWIRES


Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nanosized ZnO was prepared by polyol synthesis. Fluorescence spectrum of the ZnO colloid at varying pump intensities was studied. The powder was extracted and characterized by XRD and BET. The extracted powder was screen printed on glass substrates using ethyl cellulose as binder and turpinol as solvent. Coherent back scattering studies were performed on the screen printed sample which showed evidence of weak localization. The screen printed pattern showed strong UV emission.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In the present work, we report the third order nonlinear optical properties of ZnO thin films deposited using self assembly, sol gel process as well as pulsed laser ablation by z scan technique. ZnO thin films clearly exhibit a negative nonlinear index of refraction at 532 nm and the observed nonlinear refraction is attributed to two photon absorption followed by free carrier absorption. Although the absolute nonlinear values for these films are comparable, there is a change in the sign of the absorptive nonlinearity of the films. The films developed by dip coating and pulsed laser ablation exhibit reverse saturable absorption whereas the self assembled film exhibits saturable absorption. These different nonlinear characteristics in the self assembled films can be mainly attributed to the saturation of linear absorption of the ZnO defect states.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We have investigated the third-order nonlinearity in ZnO nanocolloids with particle sizes in the range 6-18 nm by the z-scan technique. The third-order optical susceptibility χ(3) increases with increasing particle size (R) within the range of our investigations. In the weak confinement regime, an R2 dependence of χ(3) is obtained for ZnO nanocolloids. The optical limiting response is also studied against particle size.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report enhanced back scattering in nanometer-sized ZnO colloids prepared in two different media, by different methods. The FWHM of the back scattered cone and hence the mean free path varied with concentration of ZnO as well as particle size. The Lorentzian profile of backscattered cone indicates the presence of coherence.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We present the spectral and nonlinear optical properties of ZnO-SiO2 nanocomposites prepared by colloidal chemical synthesis. Obvious enhancement of ultraviolet (UV) emission of the samples is observed, and the strongest UV emission of a typical ZnO-SiO2 nanocomposite is over three times stronger than that of pure ZnO. The nonlinearity of the silica colloid is low, and its nonlinear response can be improved by making composites with ZnO. These nanocomposites show self-defocusing nonlinearity and good nonlinear absorption behavior. The observed nonlinear absorption is explained through two photon absorption followed by weak free carrier absorption and nonlinear scattering. The nonlinear refractive index and the nonlinear absorption increase with increasing ZnO volume fraction and can be attributed to the enhancement of exciton oscillator strength. ZnO-SiO2 is a potential nanocomposite material for the UV light emission and for the development of nonlinear optical devices with a relatively small limiting threshold.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this article we present size dependent spectroscopic observations of nanocolloids of ZnO. ZnO is reported to show two emission bands, an ultraviolet (UV) emission band and another in the green region. Apart from the known band gap 380 nm and impurity 530 nm emissions, we have found some peculiar features in the fluorescence spectra that are consistent with the nanoparticle size distribution. Results show that additional emissions at 420 and 490 nm are developed with particle size. The origin of the visible band emission is discussed. The mechanism of the luminescence suggests that UV luminescence of ZnO colloid is related to the transition from conduction band edge to valence band, and visible luminescence is caused by the transition from deep donor level to valence band due to oxygen vacancies and by the transition from conduction band to deep acceptor level due to impurities and defect states. A correlation analysis between the particle size and spectroscopic observations is also discussed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In the present work we report the preparation details studies on ZnO thin films. ZnO thin films are prepared using cost effective deposition technique viz., Chemical Spray Pyrolysis (CSP). The method is very effective for large area preparation of the ZnO thin film. A new post-deposition process could also be developed to avoid the adsorption of oxygen that usually occurs after the spraying process i.e., while cooling. Studies were done by changing the various deposition parameters for optimizing the properties of ZnO thin film. Moreover, different methods of doping using various elements are also tried to enhance the conductivity and transparency of the film to make these suitable for various optoelectronic applications.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Magnetic nanowires (NWs) are ideal materials for the fabrication of various multifunctional nanostructures which can be manipulated by an external magnetic fi eld. Highly crystalline and textured nanowires of nickel (Ni NWs) and cobalt (Co NWs) with high aspect ratio (~330) and high coercivity have been synthesized by electrodeposition using nickel sulphate hexahydrate (NiSO4·6H2O) and cobalt sulphate heptahydrate (CoSO4·7H2O) respectively on nanoporous alumina membranes. They exhibit a preferential growth along〈110〉. A general mobility assisted growth mechanism for the formation of Ni and Co NWs is proposed. The role of the hydration layer on the resulting one-dimensional geometry in the case of potentiostatic electrodeposition is verified. A very high interwire interaction resulting from magnetostatic dipolar interactions between the nanowires is observed. An unusual low-temperature magnetisation switching for fi eld parallel to the wire axis is evident from the peculiar high fi eld M(T) curve

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZnO nanoflowers were synthesized by the hydrothermal process at an optimized growth temperature of 200 ◦C and a growth/reaction time of 3 h. As-prepared ZnO nanoflowers were characterized by x-ray diffraction, scanning electron microscopy, UV–visible and Raman spectroscopy. X-ray diffraction and Raman studies reveal that the as-synthesized flower-like ZnO nanostructures are highly crystalline with a hexagonal wurtzite phase preferentially oriented along the (1 0 1 1) plane. The average length (234–347 nm) and diameter (77–106 nm) of the nanorods constituting the flower-like structure are estimated using scanning electron microscopy studies. The band gap of ZnO nanoflowers is estimated as 3.23 eV, the lowering of band gap is attributed to the flower-like surface morphology and microstructure of ZnO. Room temperature photoluminescence spectrum shows a strong UV emission peak at 392 nm, with a suppressed visible emission related to the defect states, indicating the defect free formation of ZnO nanoflowers that can be potentially used for UV light-emitting devices. The suppressed Raman bands at 541 and 583 cm−1 related to defect states in ZnO confirms that the ZnO nanoflowers here obtained have a reduced presence of defects

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The magnetic properties of Mn-doped ZnO (ZnO:Mn) nanorods grown by hydrothermal process at a temperature of 200 8C and a growth time of 3 h have been studied. The samples were characterized by using powder X-ray diffraction with Rietveld refinement, scanning electron microscopy, energy-dispersive X-ray analysis and SQUID magnetometry. Mn (3 wt%) and (5 wt%)-doped ZnO samples exhibit paramagnetic and ferromagnetic behavior, respectively, at room temperature. The spin-glass behavior is observed from the samples with respect to the decrease of temperature. At 10 K, both samples exhibit a hysteresis loop with relatively low coercivity. The room-temperature ferromagnetism in 5 wt% Mn-doped ZnO nanorods is attributed to the increase in the specific area of grain boundaries, interaction between dopant Mn2þ ions substituted at Zn2þ site and the interaction between Mn2þ ions and Zn2þ ions from the ZnO host lattice

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZnO thin films were coated on amorphous glass substrate at various temperatures in the range 160-500 0C by spray pyrolysis method. The as deposited films were characterised by using XRD and SEM. Wurtzite phase of ZnO was formed at a substrate temperature of 400 0C, highly oriented (002) phase was developed with respect to increase of substrate temperature from 450 to 500 0C. Morphological and growth mode of these films were analyzed with respect to structural orientation of films from wurtzite to highly (002) oriented phase. Present study reveals that substrate temperature was one of the important parameters which determine the crystalline quality, population of defects, grain size, orientation and morphology of the films

Relevância:

20.00% 20.00%

Publicador:

Resumo:

ZnO micro particles in the range 0.4-0.6 μm were synthesized by microwave irradiation method. The XRD analysis reveals that the sample is in the wurtzite phase with orientation along the (101) plane. SAED pattern of the sample reveals the single crystalline nature of the micro grains. TEM images show the formation of cylindrical shaped ZnO micro structures with hexagonal faces. The optical phonon modes were slightly shifted in the Raman spectrum,attributed to the presence of various crystalline defects and laser induced local heating at the grain boundaries. A broad transmission profile was observed in the FTIR spectrum from 1550-3400 cm-1 which falls in the atmospheric transparency window region. PL spectrum centered at 500 nm with a broad band in the region 420-570 nm comprised of different emission peaks attributed to transition between defect levels. Various emission levels in the sample were expliained with a band diagram

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The objective of the present study is the formation of single phase Zn1−xTMxO thin films by PLD and increase the solubility limit of TM dopants. The TM doped ZnO nanostructures were also grown by hydrothermal method. The structural and morphological variation of ZnO:TM thin films and nanostructures with TM doping concentration is also investigated. The origin and enhancement of ferromagnetism in single phase Zn1−xTMxO thin films and nanostructures using spectroscopic techniques were also studied. The dependence of ablation parameters on the structural and optical properties of ZnO thin films were studied

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Effect of varying spray rate on the structure and optoelectronic properties of spray pyrolysed ZnO film is analysed. ZnO films were characterised using different techniques such as X-ray diffraction (XRD), photoluminescence, electrical resistivity measurement, and optical absorption. The XRD analysis proved that, with the increase in spray rate, orientation of the grains changed from (1 0 1) plane to (0 0 2) plane. The films exhibited luminescence in two regions—one was the ‘near band-edge’ (NBE) (∼380 nm) emission and the other one was the ‘blue-green emission’ (∼503 nm). Intensity of the blue-green emission decreased after orientation of grains shifted to (0 0 2) plane. Scanning electron microscope (SEM) analysis of the films asserts that spray rate has major role in improving the crystallographic properties of the films. Moreover resistivity of the films could be lowered to 2.4×10−2 cm without any doping or post-deposition annealing

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This work projects photoluminescence (PL) as an alternative technique to estimate the order of resistivity of zinc oxide (ZnO) thin films. ZnO thin films, deposited using chemical spray pyrolysis (CSP) by varying the deposition parameters like solvent, spray rate, pH of precursor, and so forth, have been used for this study. Variation in the deposition conditions has tremendous impact on the luminescence properties as well as resistivity. Two emissions could be recorded for all samples—the near band edge emission (NBE) at 380 nm and the deep level emission (DLE) at ∼500 nm which are competing in nature. It is observed that the ratio of intensities of DLE to NBE ( DLE/ NBE) can be reduced by controlling oxygen incorporation in the sample. - measurements indicate that restricting oxygen incorporation reduces resistivity considerably. Variation of DLE/ NBE and resistivity for samples prepared under different deposition conditions is similar in nature. DLE/ NBE was always less than resistivity by an order for all samples.Thus from PL measurements alone, the order of resistivity of the samples can be estimated.