17 resultados para silicate and luminescence

em Doria (National Library of Finland DSpace Services) - National Library of Finland, Finland


Relevância:

90.00% 90.00%

Publicador:

Resumo:

The objective of the thesis was to develop methods to manufacture and control calcium carbonate crystal nucleation and growth in precipitation process. The work consists of experimental part and literature part that addresses theory of nucleation, crystallization and precipitation. In the experimental part calcium carbonate was precipitated using carbonization reaction. Precipitation was carried out in presence of known morphology controlling agents (anionic polymers and sodium silicate) and by using different operation conditions. Formed material was characterized using SEM images, and its thermal stability was assessed. This work demonstrates that carbon dioxide feeding rate and concentrations of calcium hydroxide and additives can be used to control size, shape and amount of precipitating calcium carbonate.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

Cellulose fiber-silica nanocomposites with novel mechanical, chemical and thermal properties have potential to be widely applied in different area. Monodispered silica nanoparticles play an important role in enhancing hybrids properties of hardness, strength, thermal stability etc. On the other hand, cellulose is one of the world’s most abundant and renewable polymers and possesses several unique properties required in many areas and biomedicine. The aim of this master thesis is to study if silica particles from reaction of sodium silicate and sulphuric acid can be adsorbed onto cellulose fiber surfaces via in situ growth. First, nanosilica particles were synthesized. Effect of pH and silica contents were tested. In theoretical part, introduction of silica, methods of preparation of nanosilica from sodium silicate, effect factors and additives were discussed. Then, cellulose fiber-silica nanocomposites were synthesis via route from sodium silicate and route silicic acid. In the experiment of route from sodium silicate, the effects of types of sodium silicate, pH and target ratio of silica to fiber were investigated. From another aspect, the effects of types of sodium silicate, fiber concentration in mixture solution and target ratio of silica to fiber were tested in the experiment of route from silicic acid. Samples were investigated via zeta potential measurement, particle size distribution, ash content measurement and Scanning Electron Microscopy (SEM). The Results of the experiment of preparing silica sol were that the particle size of silica sol was smaller prepared in pH 11.7 than that prepared in pH 9.3. Then in the experiment of synthesis of cellulose fiber-silica nanocomposites, it was concluded that the zeta potential of all the samples were around -16 mV and the highest ash content of all the samples was only 1.4%. The results of SEM images showed only a few of silica particles could be observed on the fiber surface, which corresponded to the value of ash content measurement.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Tässä työssä tutkittiin natriumsilikaatin (vesilasi) liuotukseen ja suodatukseen vaikuttavia tekijöitä. Työssä pyrittiin optimoimaan natriumsilikaatin liuotus- ja suodatuskapasiteetti J. M. Huber Finland Oy:n Haminan tehtaan liuotuslaitoksella. Kirjallisuusosassa perehdyttiin kiinteän natriumsilikaatin ja natriumsilikaatin vesiliuoksen ominaisuuksiin, sekä käsiteltiin soveltuvin osin liuotuksen ja suodatuksen teoriaa. Kokeellisessa osassa vertailtiin kahden eri valmistajan natriumsilikaatteja toisiinsa, sekä pyrittiin löytämään molemmille laseille optimaalisimmat prosessiparametrit liuotus- ja suodatuskokeiden avulla. Erilaisia prosessiparametreja ja ajotapoja testattiin tehdasmittakaavan koeajoilla todellisilla prosessilaitteilla. Eri natriumsilikaattien vertailu tehtiin tehdasmittakaavan koeajojen sekä laboratorioanalyysien avulla. Koeajojen tulosten perusteella Taavetista toimitettu vesilasi liukenee nopeammin kuin Puolasta toimitettu ostolasi, mutta puolalaisesta lasista liuotettu silikaatti suodattuu helpommin kuin Taavetin lasista liuotettu silikaatti. Liukenemisnopeuden eroon selitettävissä Taavetin lasin suuremmalla ominaispinta-alalla sekä hauraammalla rakenteella. Suodatuseroon ei löytynyt yksiselitteistä syytä, joten sen löytämiseksi vaadittaisiin jatkotutkimuksia. Kokeiden perusteellaparas keino puolalaisen lasin liuotuksen nopeuttamiseen olisi pitää liuotussäiliön lasiylimäärä mahdollisimman korkeana jokaisessa panoksessa ja nopeuttaa liuotussäiliön panostusta lasin ja veden yhtäaikaisella annostelulla. Tulosten perusteella paras keino Taavetin lasista liuotetun silikaatin suodatuksen helpottamiseen olisi laskea liuoksen tavoitetiheyttä nykyisestä arvostaan, jolloin viskositeetti pienenee merkittävästi ja suodatus onnistuu liuotuslaitoksen kapasiteetin kannalta paremmin. Edellä mainituilla ajotavoilla tehtyjen koeajojen perusteella, molemmilla laseilla on mahdollista päästä 150 MT/d tavoitekapasiteettiin, mutta varmin tapa kyseisen kapasiteetin saavuttamiseksi olisi lisätä suodatuskapasiteettia investoimalla toiseen silikaattisuodattimeen.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Selostus: Pohjois-Euroopan silikaattisten kalkitusaineiden reaktiivisuus astiakoemenetelmällä ja kahdella pH-staattisella menetelmällä arvioituna

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Resonance energy transfer (RET) is a non-radiative transfer of the excitation energy from the initially excited luminescent donor to an acceptor. The requirements for the resonance energy transfer are: i) the spectral overlap between the donor emission spectrum and the acceptor absorption spectrum, ii) the close proximity of the donor and the acceptor, and iii) the suitable relative orientations of the donor emission and the acceptor absorption transition dipoles. As a result of the RET process the donor luminescence intensity and the donor lifetime are decreased. If the acceptor is luminescent, a sensitized acceptor emission appears. The rate of RET depends strongly on the donor–acceptor distance (r) and is inversely proportional to r6. The distance dependence of RET is utilized in binding assays. The proximity requirement and the selective detection of the RET-modified emission signal allow homogeneous separation free assays. The term lanthanide-based RET is used when luminescent lanthanide compounds are used as donors. The long luminescence lifetimes, the large Stokes’ shifts and the intense, sharply-spiked emission spectra of the lanthanide donors offer advantages over the conventional organic donor molecules. Both the organic lanthanide chelates and the inorganic up-converting phosphor (UCP) particles have been used as donor labels in the RET based binding assays. In the present work lanthanide luminescence and lanthanide-based resonance energy transfer phenomena were studied. Luminescence lifetime measurements had an essential role in the research. Modular frequency-domain and time-domain luminometers were assembled and used successfully in the lifetime measurements. The frequency-domain luminometer operated in the low frequency domain ( 100 kHz) and utilized a novel dual-phase lock-in detection of the luminescence. One of the studied phenomena was the recently discovered non-overlapping fluorescence resonance energy transfer (nFRET). The studied properties were the distance and temperature dependences of nFRET. The distance dependence was found to deviate from the Förster theory and a clear temperature dependence was observed whereas conventional RET was completely independent of the temperature. Based on the experimental results two thermally activated mechanisms were proposed for the nFRET process. The work with the UCP particles involved the measurement of the luminescence properties of the UCP particles synthesized in our laboratory. The goal of the UCP particle research is to develop UCP donor labels for binding assays. In the present work the effect of the dopant concentrations and the core–shell structure on the total up-conversion luminescence intensity, the red–green emission ratio, and the luminescence lifetime was studied. Also the non-radiative nature of the energy transfer from the UCP particle donors to organic acceptors was demonstrated for the first time in aqueous environment and with a controlled donor–acceptor distance.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Measuring protein biomarkers from sample matrix, such as plasma, is one of the basic tasks in clinical diagnostics. Bioanalytical assays used for the measuring should be able to measure proteins with high sensitivity and specificity. Furthermore, multiplexing capability would also be advantageous. To ensure the utility of the diagnostic test in point-of-care setting, additional requirements such as short turn-around times, ease-ofuse and low costs need to be met. On the other hand, enhancement of assay sensitivity could enable exploiting novel biomarkers, which are present in very low concentrations and which the current immunoassays are unable to measure. Furthermore, highly sensitive assays could enable the use of minimally invasive sampling. In the development of high-sensitivity assays the label technology and affinity binders are in pivotal role. Additionally, innovative assay designs contribute to the obtained sensitivity and other characteristics of the assay as well as its applicability. The aim of this thesis was to study the impact of assay components on the performance of both homogeneous and heterogeneous assays. Applicability of two different lanthanide-based label technologies, upconverting nanoparticles and switchable lanthanide luminescence, to protein detection was explored. Moreover, the potential of recombinant antibodies and aptamers as alternative affinity binders were evaluated. Additionally, alternative conjugation chemistries for production of the labeled binders were studied. Different assay concepts were also evaluated with respect to their applicability to point-of-care testing, which requires simple yet sensitive methods. The applicability of upconverting nanoparticles to the simultaneous quantitative measurement of multiple analytes using imaging-based detection was demonstrated. Additionally, the required instrumentation was relatively simple and inexpensive compared to other luminescent lanthanide-based labels requiring time-resolved measurement. The developed homogeneous assays exploiting switchable lanthanide luminescence were rapid and simple to perform and thus applicable even to point-ofcare testing. The sensitivities of the homogeneous assays were in the picomolar range, which are still inadequate for some analytes, such as cardiac troponins, requiring ultralow limits of detection. For most analytes, however, the obtained limits of detection were sufficient. The use of recombinant antibody fragments and aptamers as binders allowed site-specific and controlled covalent conjugation to construct labeled binders reproducibly either by using chemical modification or recombinant technology. Luminescent lanthanide labels were shown to be widely applicable for protein detection in various assay setups and to contribute assay sensitivity.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Since the discovery of the up-conversion phenomenon, there has been an ever increasing interest in up-converting phosphors in which the absorption of two or more low energy photons is followed by emission of a higher energy photon. Most up-conversion luminescence materials operate by using a combination of a trivalent rare earth (lanthanide) sensitizer (e.g. Yb or Er) and an activator (e.g. Er, Ho, Tm or Pr) ion in a crystal lattice. Up-converting phosphors have a variety of potential applications as lasers and displays as well as inks for security printing (e.g. bank notes and bonds). One of the most sophisticated applications of lanthanide up-conversion luminescence is probably in medical diagnostics. However, there are some major problems in the use of photoluminescence based on the direct UV excitation in immunoassays. Human blood absorbs strongly UV radiation as well as the emission of the phosphor in the visible. A promising way to overcome the problems arising from the blood absorption is to use a long wavelength excitation and benefit from the up-conversion luminescence. Since there is practically no absorption by the whole-blood in the near IR region, it has no capability for up-conversion in the excitation wavelength region of the conventional up-converting phosphor based on the Yb3+ (sensitizer) and Er3+ (activator) combination. The aim of this work was to prepare nanocrystalline materials with high red (and green) up-conversion luminescence efficiency for use in quantitative whole-blood immunoassays. For coupling to biological compounds, nanometer-sized (crystallite size below 50 nm) up-converting phosphor particles are required. The nanocrystalline ZrO2:Yb3+,Er3+, Y2O2S:Yb3+,Er3+, NaYF4:Yb3+,Er3+ and NaRF4-NaR’F4 (R: Y, Yb, Er) materials, prepared with the combustion, sol-gel, flux, co-precipitation and solvothermal synthesis, were studied using the thermal analysis, FT-IR spectroscopy, transmission electron microscopy, EDX spectroscopy, XANES/EXAFS measurements, absorption spectroscopy, X-ray powder diffraction, as well as up-conversion and thermoluminescence spectroscopies. The effect of the impurities of the phosphors, crystallite size, as well as the crystal structure on the up-conversion luminescence intensity was analyzed. Finally, a new phenomenon, persistent up-conversion luminescence was introduced and discussed. For efficient use in bioassays, more work is needed to yield nanomaterials with smaller and more uniform crystallite sizes. Surface modifications need to be studied to improve the dispersion in water. On the other hand, further work must be carried out to optimize the persistent up-conversion luminescence of the nanomaterials to allow for their use as efficient immunoassay nanomaterials combining the advantages of both up-conversion and persistent luminescence.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Escherichia coli K-12 (pEGFPluxABCDEAmp) (E. coli-lux), constitutively emitting bioluminescence (BL), was constructed and its BL emitting properties tested in different growth and killing conditions. The BL emission directly correlated with the number of viable E. coli-lux cells, and when subjected to the antimicrobial agent, the diminishment of the BL signal was linked directly to the number of killed bacterial cells. The method provided a very convenient application, especially when compared to conventional plate counting assays. This novel real-time based method was utilized in both immunological and toxicological assessments. The parameters such as the activation phase, the lytic phase and the capacity of the killing of the serum complement system were specified not only in humans but also in other species. E. coli-lux was also successfully used to study the antimicrobial activities of insect haemolymph. The mechanisms of neutrophil activity, like that of a myeloperoxidase (MPO)-H2O2-halide system, were studied using the E. coli-lux approach. The fundamental role of MPO was challenged, since during the actual killing in described circumstances in phagolysosome the MPO system was inactivated and chlorination halted. The toxicological test system, assessing indoor air total toxicity, particularly suitable for suspected mold damages, was designed based on the E. coli-lux method. Susceptibility to the vast number of various toxins, both pure chemicals and dust samples from the buildings and extracts from molds, were investigated. The E. coli-lux application was found to possess high sensitivity and specificity attributes. Alongside the analysis system, the sampling kit for indoor dust was engineered based on the swipe stick and the container. The combination of practical specimen collector and convenient analysis system provided accurate toxic data from the dust sample within hours. Neutrophils are good indicators of the pathophysiological state of the individual, and they can be utilized as a toxicological probe due to their ability to emit chemiluminescence (CL). Neutrophils can either be used as probe cells, directly exposed to the agent studied, or they can act as indicators of the whole biological system exposed to the agent. Human neutrophils were exposed to the same toxins as tested with the E. coli-lux system and measured as luminol amplified CL emission. The influence of the toxins on the individuals was investigated by exposing rats with moniliniformin, the mycotoxin commonly present in Finnish grains. The activity of the rat neutrophils was found to decrease significantly during the 28 days of exposure.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In the present work electroluminescence in Si-SiO2 structures has been investigated. Electroluminescence has been recorded in the range of 250-900 nm in a system of electrolyte-insulator-semiconductor at the room temperature. The heating process of electrons in SiO2 was studied and possibility of separation it into two phases has been shown. The nature of luminescence centers and the model of its formation were proposed. This paper also includes consideration of oxide layer formation. Charge transfer mechanisms have been attended as well. The nature of electroluminescence is understood in detail. As a matter of fact, electron traps in silicon are the centers of luminescence. Electroluminescence occurs when electrons move from one trap to another. Thus the radiation of light quantum occurs. These traps appear as a result of the oxide growth. At the same time the bonds deformation of silicon atoms with SiOH groups is not excludes. As a result, dangling bonds are appeared, which are the trapping centers or the centers of luminescence.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A small carbonatite dyke swarm has been identified at Naantali, southwest Finland. Several swarms of shoshonitic lamprophyres are also known along the Archean-Proterozoic boundary in eastern Finland and northwest Russia. These intrusions, along with the carbonatite intrusion at Halpanen, eastern Finland, represent a stage of widespread low-volume mantle-sourced alkaline magmatism in the Svecofennian Domain. Using trace element and isotope geochemistry coupled with precise geochronology from these rocks, a model is presented for the Proterozoic metasomatic evolution of the Fennoscandian subcontinental lithospheric mantle. At ~2.2-2.06 Ga, increased biological production in shallow seas linked to continental rifting, resulted in increased burial rates of organic carbon. Subduction between ~1.93-1.88 Ga returned organic carbon-enriched sediments of mixed Archean and Proterozoic provenance to the mantle. Dehydration reactions supplied water to the mantle wedge, driving arc volcanism, while mica, amphibole and carbonate were brought deeper into the mantle with the subducting slab. The cold subducted slab was heated conductively from the surrounding warm mantle, while pressures continued to gradually increase as a result of crustal thickening. The sediments began to melt in a two stage process, first producing a hydrous alkaline silicate melt, which infiltrated the mantle wedge and crystallised as metasomatic veins. At higher temperatures, carbonatite melt was produced, which preferentially infiltrated the pre-existing metasomatic vein network. At the onset of post-collisional extension, deep fault structures formed, providing conduits for mantle melts to reach the upper crust. Low-volume partial melting of the enriched mantle at depths of at least 110 km led to the formation of first carbonatitic magma and subsequently lamprophyric magma. Carbonatite was emplaced in the upper crust at Naantali at 1795.7 ± 6.8 Ma; lamprophyres along the Archean-Proterozoic boundary were emplaced between 1790.1 ± 3.3 Ma and 1781 ± 20 Ma.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

New luminometric particle-based methods were developed to quantify protein and to count cells. The developed methods rely on the interaction of the sample with nano- or microparticles and different principles of detection. In fluorescence quenching, timeresolved luminescence resonance energy transfer (TR-LRET), and two-photon excitation fluorescence (TPX) methods, the sample prevents the adsorption of labeled protein to the particles. Depending on the system, the addition of the analyte increases or decreases the luminescence. In the dissociation method, the adsorbed protein protects the Eu(III) chelate on the surface of the particles from dissociation at a low pH. The experimental setups are user-friendly and rapid and do not require hazardous test compounds and elevated temperatures. The sensitivity of the quantification of protein (from 40 to 500 pg bovine serum albumin in a sample) was 20-500-fold better than in most sensitive commercial methods. The quenching method exhibited low protein-to-protein variability and the dissociation method insensitivity to the assay contaminants commonly found in biological samples. Less than ten eukaryotic cells were detected and quantified with all the developed methods under optimized assay conditions. Furthermore, two applications, the method for detection of the aggregation of protein and the cell viability test, were developed by utilizing the TR-LRET method. The detection of the aggregation of protein was allowed at a more than 10,000 times lower concentration, 30 μg/L, compared to the known methods of UV240 absorbance and dynamic light scattering. The TR-LRET method was combined with a nucleic acid assay with cell-impermeable dye to measure the percentage of dead cells in a single tube test with cell counts below 1000 cells/tube.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Persistent luminescence materials can store energy from solar radiation or artificial lighting and release it over a period of several hours without a continuous excitation source. These materials are widely used to improve human safety in emergency and traffic signalization. They can also be utilized in novel applications including solar cells, medical diagnostics, radiation detectors and structural damage sensors. The development of these materials is currently based on methods based on trial and error. The tailoring of new materials is also hindered by the lack of knowledge on the role of their intrinsic and extrinsic lattice defects in the appropriate mechanisms. The goal of this work was to clarify the persistent luminescence mechanisms by combining ab initio density functional theory (DFT) calculations with selected experimental methods. The DFT approach enables a full control of both the nature of the defects and their locations in the host lattice. The materials studied in the present work, the distrontium magnesium disilicate (Sr2MgSi2O7) and strontium aluminate (SrAl2O4) are among the most efficient persistent luminescence hosts when doped with divalent europium Eu2+ and co-doped with trivalent rare earth ions R3+ (R: Y, La-Nd, Sm, Gd-Lu). The polycrystalline materials were prepared with the solid state method and their structural and phase purity was confirmed by X-ray powder diffraction. Their local crystal structure was studied by high-resolution transmission electron microscopy. The crystal and electronic structure of the nondoped as well as Eu2+, R2+/3+ and other defect containing materials were studied using DFT calculations. The experimental trap depths were obtained using thermoluminescence (TL) spectroscopy. The emission and excitation of Sr2MgSi2O7:Eu2+,Dy3+ were also studied. Significant modifications in the local crystal structure due to the Eu2+ ion and lattice defects were found by the experimental and DFT methods. The charge compensation effects induced by the R3+ co-doping further increased the number of defects and distortions in the host lattice. As for the electronic structure of Sr2MgSi2O7 and SrAl2O4, the experimental band gap energy of the host materials was well reproduced by the calculations. The DFT calculated Eu2+ and R2+/3+ 4fn as well as 4fn-15d1 ground states in the Sr2MgSi2O7 band structure provide an independent verification for an empirical model which is constructed using rather sparse experimental data for the R3+ and especially the R2+ ions. The intrinsic and defect induced electron traps were found to act together as energy storage sites contributing to the materials’ efficient persistent luminescence. The calculated trap energy range agreed with the trap structure of Sr2MgSi2O7 obtained using TL measurements. More experimental studies should be carried out for SrAl2O4 to compare with the DFT calculations. The calculated and experimental results show that the electron traps created by both the rare earth ions and vacancies are modified due to the defect aggregation and charge compensation effects. The relationships between this modification and the energy storage properties of the solid state materials are discussed.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The drug discovery process is facing new challenges in the evaluation process of the lead compounds as the number of new compounds synthesized is increasing. The potentiality of test compounds is most frequently assayed through the binding of the test compound to the target molecule or receptor, or measuring functional secondary effects caused by the test compound in the target model cells, tissues or organism. Modern homogeneous high-throughput-screening (HTS) assays for purified estrogen receptors (ER) utilize various luminescence based detection methods. Fluorescence polarization (FP) is a standard method for ER ligand binding assay. It was used to demonstrate the performance of two-photon excitation of fluorescence (TPFE) vs. the conventional one-photon excitation method. As result, the TPFE method showed improved dynamics and was found to be comparable with the conventional method. It also held potential for efficient miniaturization. Other luminescence based ER assays utilize energy transfer from a long-lifetime luminescent label e.g. lanthanide chelates (Eu, Tb) to a prompt luminescent label, the signal being read in a time-resolved mode. As an alternative to this method, a new single-label (Eu) time-resolved detection method was developed, based on the quenching of the label by a soluble quencher molecule when displaced from the receptor to the solution phase by an unlabeled competing ligand. The new method was paralleled with the standard FP method. It was shown to yield comparable results with the FP method and found to hold a significantly higher signal-tobackground ratio than FP. Cell-based functional assays for determining the extent of cell surface adhesion molecule (CAM) expression combined with microscopy analysis of the target molecules would provide improved information content, compared to an expression level assay alone. In this work, immune response was simulated by exposing endothelial cells to cytokine stimulation and the resulting increase in the level of adhesion molecule expression was analyzed on fixed cells by means of immunocytochemistry utilizing specific long-lifetime luminophore labeled antibodies against chosen adhesion molecules. Results showed that the method was capable of use in amulti-parametric assay for protein expression levels of several CAMs simultaneously, combined with analysis of the cellular localization of the chosen adhesion molecules through time-resolved luminescence microscopy inspection.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Sequestration of carbon dioxide in mineral rocks, also known as CO2 Capture and Mineralization (CCM), is considered to have a huge potential in stabilizing anthropogenic CO2 emissions. One of the CCM routes is the ex situ indirect gas/sold carbonation of reactive materials, such as Mg(OH)2, produced from abundantly available Mg-silicate rocks. The gas/solid carbonation method is intensively researched at Åbo Akademi University (ÅAU ), Finland because it is energetically attractive and utilizes the exothermic chemistry of Mg(OH)2 carbonation. In this thesis, a method for producing Mg(OH)2 from Mg-silicate rocks for CCM was investigated, and the process efficiency, energy and environmental impact assessed. The Mg(OH)2 process studied here was first proposed in 2008 in a Master’s Thesis by the author. At that time the process was applied to only one Mg-silicate rock (Finnish serpentinite from the Hitura nickel mine site of Finn Nickel) and the optimum process conversions, energy and environmental performance were not known. Producing Mg(OH)2 from Mg-silicate rocks involves a two-staged process of Mg extraction and Mg(OH)2 precipitation. The first stage extracts Mg and other cations by reacting pulverized serpentinite or olivine rocks with ammonium sulfate (AS) salt at 400 - 550 oC (preferably < 450 oC). In the second stage, ammonia solution reacts with the cations (extracted from the first stage after they are leached in water) to form mainly FeOOH, high purity Mg(OH)2 and aqueous (dissolved) AS. The Mg(OH)2 process described here is closed loop in nature; gaseous ammonia and water vapour are produced from the extraction stage, recovered and used as reagent for the precipitation stage. The AS reagent is thereafter recovered after the precipitation stage. The Mg extraction stage, being the conversion-determining and the most energy-intensive step of the entire CCM process chain, received a prominent attention in this study. The extraction behavior and reactivity of different rocks types (serpentinite and olivine rocks) from different locations worldwide (Australia, Finland, Lithuania, Norway and Portugal) was tested. Also, parametric evaluation was carried out to determine the optimal reaction temperature, time and chemical reagent (AS). Effects of reactor types and configuration, mixing and scale-up possibilities were also studied. The Mg(OH)2 produced can be used to convert CO2 to thermodynamically stable and environmentally benign magnesium carbonate. Therefore, the process energy and life cycle environmental performance of the ÅAU CCM technique that first produces Mg(OH)2 and the carbonates in a pressurized fluidized bed (FB) were assessed. The life cycle energy and environmental assessment approach applied in this thesis is motivated by the fact that the CCM technology should in itself offer a solution to what is both an energy and environmental problem. Results obtained in this study show that different Mg-silicate rocks react differently; olivine rocks being far less reactive than serpentinite rocks. In summary, the reactivity of Mg-silicate rocks is a function of both the chemical and physical properties of rocks. Reaction temperature and time remain important parameters to consider in process design and operation. Heat transfer properties of the reactor determine the temperature at which maximum Mg extraction is obtained. Also, an increase in reaction temperature leads to an increase in the extent of extraction, reaching a maximum yield at different temperatures depending on the reaction time. Process energy requirement for producing Mg(OH)2 from a hypothetical case of an iron-free serpentine rock is 3.62 GJ/t-CO2. This value can increase by 16 - 68% depending on the type of iron compound (FeO, Fe2O3 or Fe3O4) in the mineral. This suggests that the benefit from the potential use of FeOOH as an iron ore feedstock in iron and steelmaking should be determined by considering the energy, cost and emissions associated with the FeOOH by-product. AS recovery through crystallization is the second most energy intensive unit operation after the extraction reaction. However, the choice of mechanical vapor recompression (MVR) over the “simple evaporation” crystallization method has a potential energy savings of 15.2 GJ/t-CO2 (84 % savings). Integrating the Mg(OH)2 production method and the gas/solid carbonation process could provide up to an 25% energy offset to the CCM process energy requirements. Life cycle inventory assessment (LCIA) results show that for every ton of CO2 mineralized, the ÅAU CCM process avoids 430 - 480 kg CO2. The Mg(OH)2 process studied in this thesis has many promising features. Even at the current high energy and environmental burden, producing Mg(OH)2 from Mg-silicates can play a significant role in advancing CCM processes. However, dedicated future research and development (R&D) have potential to significantly improve the Mg(OH)2 process performance.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Binary probes are oligonucleotide probe pairs that hybridize adjacently to a complementary target nucleic acid. In order to detect this hybridization, the two probes can be modified with, for example, fluorescent molecules, chemically reactive groups or nucleic acid enzymes. The benefit of this kind of binary probe based approach is that the hybridization elicits a detectable signal which is distinguishable from background noise even though unbound probes are not removed by washing before measurement. In addition, the requirement of two simultaneous binding events increases specificity. Similarly to binary oligonucleotide probes, also certain enzymes and fluorescent proteins can be divided into two parts and used in separation-free assays. Split enzyme and fluorescent protein reporters have practical applications among others as tools to investigate protein-protein interactions within living cells. In this study, a novel label technology, switchable lanthanide luminescence, was introduced and used successfully in model assays for nucleic acid and protein detection. This label technology is based on a luminescent lanthanide chelate divided into two inherently non-luminescent moieties, an ion carrier chelate and a light harvesting antenna ligand. These form a highly luminescent complex when brought into close proximity; i.e., the label moieties switch from a dark state to a luminescent state. This kind of mixed lanthanide complex has the same beneficial photophysical properties as the more typical lanthanide chelates and cryptates - sharp emission peaks, long emission lifetime enabling time-resolved measurement, and large Stokes’ shift, which minimize the background signal. Furthermore, the switchable lanthanide luminescence technique enables a homogeneous assay set-up. Here, switchable lanthanide luminescence label technology was first applied to sensitive, homogeneous, single-target nucleic acid and protein assays with picomolar detection limits and high signal to background ratios. Thereafter, a homogeneous four-plex nucleic acid array-based assay was developed. Finally, the label technology was shown to be effective in discrimination of single nucleotide mismatched targets from fully matched targets and the luminescent complex formation was analyzed more thoroughly. In conclusion, this study demonstrates that the switchable lanthanide luminescencebased label technology can be used in various homogeneous bioanalytical assays.