Resumo:
The Iowa Department of Transportation (IDOT) received a Strategic Highway Research Program (SHRP) gyratory compactor in December 1994. Since then IDOT has been studying the ability of the compactor to analyze fundamental properties of aggregates such as shape, texture, and gradation by studying the volumetrics of the aggregate blends under a standard load using the SHRP gyratory compactor. This method of analyzing the volumetrics of aggregate blends is similar to SHRP's fine aggregate angularity procedure, which analyzes void levels in noncompacted aggregate blends, which in turn can be used to evaluate the texture or shape of aggregates, what SHRP refers to as angularity. Research is showing that by splitting the aggregate blend on the 2.36-mm (#8) sieve and analyzing the volumetrics or angularity of the separated blend, important fundamental properties can be determined. Most important is structure (the degree and location of aggregate interlock). In addition, analysis of the volumes of the coarse and fine portions can predict the voids in the mineral aggregate and the desired asphalt content. By predicting these properties, it can be determined whether the combined aggregate blend, when mixed with asphalt cement, will produce a mix with structural adequacy to carry the designed traffic load.
Resumo:
Quality management concrete allows the contractor to develop the mix design for the portland cement concrete. This research was initiated to gain knowledge about contractor mix designs. An experiment was done to determine the variation in cylinders, beams, and cores that could be used to test the strength of the contractor's mix. In addition, the contractor's cylinder strengths and gradations were analyzed for statistical stability and process capability. This research supports the following conclusions: (1) The mold type used to cast the concrete cylinders had an effect on the compressive strength of the concrete. The 4.5-in. by 9-in. (11.43-cm by 22.86-cm) cylinders had lower strength at a 95% confidence interval than the 4-in. by 8-in. (10.16-cm by 20.32-cm) and 6-in. by 12-in. (15.24-cm by 30.48-cm) cylinders. (2) The low vibration consolidation effort had the lowest strength of the three consolidation efforts. In particular, an interaction occurred between the low vibration effort and the 4.5-in. by 9-in. (11.43-cm by 22.86-cm) mold. This interaction produced very low compressive strengths when compared with the other consolidation efforts. (3) A correlation of 0.64 R-squared was found between the 28 day cylinder and 28 day compressive strengths. (4) The compressive strength results of the process control testing were not in statistical control. The aggregate gradations were mostly in statistical control. The gradation process was capable of meeting specification requirements. However, many of the sieves were off target. (5) The fineness modulus of the aggregate gradations did not correlate well with the strength of the concrete. However, this is not surprising considering that the gradation tests and the strength tests did not represent the same material. In addition, the concrete still has many other variables that will affect its strength that were not controlled.
Resumo:
Many reports have been written concerning investigations of concrete sealants. The primary concern of most investigators is the protection of bridge decks from de-icing chemicals which cause surface scaling and, when allowed to permeate to reinforcing steel, result in deep spalling and general concrete deterioration. The problem of protecting abutments and pier tops from salt solutions entails a significantly different approach than the problem of protecting bridge decks. The epoxy resins become eligible as a protective material since one need not be concerned with slipperiness or its abrasive characteristics. Protection with linseed oil at regular intervals would prove bothersome because of the inaccessibility of pier tops after the deck is placed. The primary purpose of this investigation was to evaluate various commercial products in terms of their ability to prevent concrete scaling of bridge abutments and pier tops which are subject to salt water deterioration.
Resumo:
The Iowa State Highway Commission purchased a Conrad automatic freeze and thaw machine and placed it in operation during October 1961. There were a few problems, but considering, the many electrical and mechanical devices used in the automatic system it has always functioned quite well. Rapid freezing and thawing of 4"x4"xl8" concrete beams has been conducted primarily in accordance with ASTM C-29l (now ASTM C-666 procedure B) at the rate of one beam per day. Over 4000 beams have been tested since 1961, with determination of the resulting durability factors. Various methods of curing were used and a standard 90 day moist cure was selected. This cure seemed to yield durability factors that correlated very well with ratings of coarse aggregates based on service records. Some concrete beams had been made using the same coarse aggregate and the durability factors compared relatively well with previous tests. Durability factors seemed to yield reasonable results until large variations in durability factors were noted from beams of identical concrete mix proportions in research projects R-234 and R-247. This then presents the question "How reliable is the durability as determined by ASTM C-666?" This question became increasingly more important when a specification requiring a minimum durability factor for P.C. concrete made from coarse aggregates was incorporated into the 1972 Standard Specification for coarse aggregates for concrete.
Resumo:
This report is a supplement to one issued in late summer 1986 which covered construction on U.S. 71, in Buena Vista County Iowa. The work involved rehabilitation of an older 20 feet wide pavement by placing a four inch thick bonded concrete overlay monolithically with two feet of widening on each side. The work was performed on one lane at a time while construction traffic and limited public traffic used the adjacent traffic lane. When work on the first lane was complete traffic was moved onto it and rehabilitation was completed on the second lane. This report covers the condition of the rehabilitated roadway in May 1987 after the first winter. The condition is described by visual observations, core conditions, and various test results including core compressive strength, direct shear tests on cores for bond strength, profilometer results and delamtect test results.
Resumo:
The large concrete placements at the Burlington Bridge were expected to cause great temperature differentials within the individual placements. In an attempt to reduce cracking due to the large temperature differentials, the Iowa Department of Transportation required that contractors continuously monitor the temperatures and temperature differentials in the concrete placement to assure that the temperature differentials did not exceed 35 deg F. It was felt that if temperature differentials remained below 35 deg F, cracking would be minimized. The following is a summary of the background of the project, and what occurred during individual concrete placements. The following conclusions were drawn: 1) Side temperatures are cooler and more greatly affected by ambient air temperatures; 2) When the 35 deg F limit was exceeded, it was almost exclusively the center to side differential; 3) The top temperature increases substantially when a new pour is placed; 4) The use of ice and different cement types did seem to affect the overall temperature gain and the amount of time taken for any one placement to reach a peak, but did not necessarily prevent the differentials from exceeding the 35 deg F limit, nor prevent cracking in any placement; and 5) Larger placements have a greater tendency to exceed the differential limit.
Resumo:
The major objective of this research project was to investigate how Iowa fly ashes influenced the chemical durability of portland cement based materials. Chemical durability has become an area of uncertainty because of the winter application of deicer salts (rock salts) that contain a significant amount of sulfate impurities. The sulfate durability testing program consisted of monitoring portland cement-fly ash paste, mortar and concrete test specimens that had been subjected to aqueous solutions containing various concentrations of salts (both sulfate and chloride). The paste and mortar specimens were monitored for length as a function of time. The concrete test specimens were monitored for length, relative dynamic modulus and mass as a function of time. The alkali-aggregate reactivity testing program consisted of monitoring the expansion of ASTM C311 mortar bar specimens that contained three different aggregates (Pyrex glass, Oreapolis and standard Ottawa sand). The results of the sulfate durability study indicated that the paste and concrete test specimens tended to exhibit surface spalling but only very slow expansive tendencies. This suggested that the permeability of the test specimens was controlling the rate of deterioration. Concrete specimens are still being monitored because the majority of the test specimens have expanded less than 0.05%; hence, this makes it difficult to estimate the service life of the concrete test specimens or to quantify the performance of the different fly ashes that were used in the study. The results of the mortar bar studies indicated that the chemical composition of the various fly ashes did have an influence on their sulfate resistance. Typically, Clinton and Louisa fly ashes performed the best, followed by the Ottumwa, Neal 4 and then Council Bluffs fly ashes. Council Bluffs fly ash was the only fly ash that consistently reduced the sulfate resistance of the many different mortar specimens that were investigated during this study. None of the trends that were observed in the mortar bar studies have yet become evident in the concrete phase of this project. The results of the alkali-aggregate study indicated that the Oreapolis aggregate is not very sensitive to alkali attack. Two of the fly ashes, Council Bluffs and Ottumwa, tended to increase the expansion of mortar bar specimens that contained the Oreapolis aggregate. However, it was not clear if the additional expansion was due to the alkali content of the fly ash, the periclase content of the fly ash or the cristobalite content of the fly ash, since all three of these factors have been found to influence the test results.
Resumo:
The purpose of Research Project HR-182 was to identify those aggregate types which would perform satisfactorily as seal coat aggregates. Aggregates were chosen from across the State to represent the various types normally encountered and were used with two different types of binder bitumens. A water spray treatment was also included to simulate the effects of rainfall. The evaluation was based upon aggregate retention. Due to the influence of unexpected variables upon the field samples, the laboratory data are reliable for only the most general observations. Namely, that gravels as a group appear to be retained better than carbonates and rain-fall shortly after seal coat placement can affect aggregate retention. The subsequent field observations and analysis of skid resistance data permit the following conclusions: 1. Aggregate retention is influenced by lithologic type with the gravels, quartzite, haydite, dolomites, and medium grained limestones performing best. 2. Aggregate retention is not influenced by binder bitumen type. 3. Friction values of seal coats are influ-enced by aggregate retention and/or lithologic type. The following recommendations have been determined: The aggregate used for cover aggregate/seal coat projects should be Type 4 or better skid resistance as identified in Iowa DOT Materials Instructional Memorandum T-203. This will result in maximizing the possibility of good aggregate retention and skid resistance.
Resumo:
This report presents the results of research on the influence of trace compounds from rock salt deicers on portland cement mortar and concrete. An evaluation of the deicers in stock throughout the state showed that about ninety-five percent contained enough sulfate to cause accelerated deterioration of concrete. Of the impurities found in rock salts, sulfate compounds of calcium and magnesium were found to be equally deleterious. Magnesium chloride was found to be innocuous. Introduction of fly ash eliminated the damage to portland cement mortar caused by sulfates. When used with frost resistant Alden aggregate in fly ash concrete and exposed to a variety of deicer brine compositions, the concrete did not deteriorate after exposure. With the exception of a high calcium brine, the behavior of the frost-prone Garrison aggregate was independent of deicer treatment; the high calcium brine reduced frost damage with this aggregate. Two approaches to reducing sulfate deterioration from deicers are suggested as (1) limiting the amount of sulfate to about 0.28 percent, and (2) making concrete sulfate-resistant by using fly ash. Techniques for making existing concrete deicer-sulfate-resistant are essential to a practical solution.
Resumo:
Fast Track concrete has proven to be successful in obtaining high early strengths. This benefit does not come without cost. Special Type III cement and insulating blankets to accelerate the cure add to its expense when compared to conventional paving. This research was intended to determine the benefit derived from the use of insulating blankets to accelerate strength gain in three concrete mixes using Type I cement. The goal was to determine mixes and curing procedures that would result in a range of opening times. This determination would allow the most economical design for a particular project by tailoring it to a specific time restraint. Three mixes of various cement content were tested in the field. Flexural beams were cast for each mix and tested at various ages. Two test sections were placed for each mix, one section being cured with the addition of insulating blankets and the other being cured with only conventional curing compound. Iowa Department of Transportation specifications require 500 psi flexural strength before a pavement can be opened to traffic. Concrete with Fast Track proportions (nominal 7 1/2 bag), Type I cement, and insulating blankets reached that strength in approximately 36 hr, a standard mix (nominal 6 1/2 bag) using the blankets in approximately 48 hr, and the Fast Track proportions with Type I cement without blankets in about 60 hr. The results showed a significant improvement in early strength gain with the use of insulating blankets.
Resumo:
Discarded tires have become a major disposal problem in the U.S. Different techniques of recycling these discarded tires have been tried. The state of Iowa is currently evaluating the use of discarded tires ground into crumb rubber and blending it with asphalt to make asphalt rubber cement (ARC}. This was the sixth project this process has been used in. This project is located on US 169 from the east junction of IA 175 west and north to US 20. Only the binder course was placed this year with the surface course to be let at a later date. There are four test sections, two sections with conventional mixtures and two with ARC mixtures.
Resumo:
A water reducing and retarding type admixture in concrete is commonly used on continuous bridge deck pours in Iowa. The concrete placed in the negative moment areas must remain plastic until all the dead load deflection due to the new deck's weight occurs. If the concrete does not remain plastic until the total deflection has occurred, structural cracks will develop in these areas. Retarding type admixtures will delay the setting time of concrete and prevent structural cracks if added in the proper amounts. In Section 2412.02 of the Standard Specifications, 1972, Iowa State Highway Commission, it states, "The admixture shall be used in amounts recommended by the manufacturer for conditions which prevail on the project and as approved by the engineer." The conditions which prevail on the project depend on temperature, humidity, wind conditions, etc. Each of these factors will affect the setting rate of the plastic concrete. The purpose of this project is to provide data that will be useful to field personnel concerning the retardation of concrete setting times, and how the of sets will vary with different addition rates and curing temperatures holding all other atmospheric variables constant.
Resumo:
The concrete admixture Ipanex (Registered trademark) manufactured by IPA Systems Inc. was submitted to the Iowa Department of Transportation (Iowa DOT) New Products Committee on April 15, 1998. The New Products Committee requested that the Iowa DOT Materials Laboratory evaluate the durability, corrosion inhibiting and concrete permeability reduction effects of this admixture. This report is intended to present the results of testing in Iowa DOT materials laboratories, review a Pennsylvania State University report, as well as review the IPA Systems Inc. marketing literature. The objective is to provide the New Products Committee with a recommendation concerning approval of this product based on the information gathered. The portland cement concrete admixture Ipanex (Registered trademark) did not show any significant benefit in terms of improvement in areas of permeability, chloride resistance and strength in the testing performed at the Iowa DOT. The literature and reports reviewed did not provide enough credible evidence to refute this conclusion. Additionally, the benefits ascribed to this product can be more economically achieved using other currently available products such as slag and silica fume. The recommendation is that this product not be approved for use on State projects in Iowa.
Resumo:
The objective of this research project was to service load test a representative sample of old reinforced concrete bridges (some of them historic and some of them scheduled for demolition) with the results being used to create a database so the performance of similar bridges could be predicted. The types of bridges tested included two reinforced concrete open spandrel arches, two reinforced concrete filled spandrel arches, one reinforced concrete slab bridge, and one two span reinforced concrete stringer bridge. The testing of each bridge consisted of applying a static load at various locations on the bridges and monitoring strains and deflections in critical members. The load was applied by means of a tandem axle dump truck with varying magnitudes of load. At each load increment, the truck was stopped at predetermined transverse and longitudinal locations and strain and deflection data were obtained. The strain data obtained were then evaluated in relation to the strain values predicted by traditional analytical procedures and a carrying capacity of the bridges was determined based on the experimental data. The response of a majority of the bridges tested was considerably lower than that predicted by analysis. Thus, the safe load carrying capacities of the bridges were greater than those predicted by the analytical models, and in a few cases, the load carrying capacities were found to be three or four times greater than calculated values. However, the test results of one bridge were lower than those predicted by analysis and thus resulted in the analytical rating being reduced. The results of the testing verified that traditional analytical methods, in most instances, are conservative and that the safe load carrying capacities of a majority of the reinforced concrete bridges are considerably greater than what one would determine on the basis of analytical analysis alone. In extrapolating the results obtained from diagnostic load tests to levels greater than those placed on the bridge during the load test, care must be taken to ensure safe bridge performance at the higher load levels. To extrapolate the load test results from the bridges tested in this investigation, the method developed by Lichtenstein in NCHRP Project 12-28(13)A was used.
Resumo:
The characterization and categorization of coarse aggregates for use in portland cement concrete (PCC) pavements is a highly refined process at the Iowa Department of Transportation. Over the past 10 to 15 years, much effort has been directed at pursuing direct testing schemes to supplement or replace existing physical testing schemes. Direct testing refers to the process of directly measuring the chemical and mineralogical properties of an aggregate and then attempting to correlate those measured properties to historical performance information (i.e., field service record). This is in contrast to indirect measurement techniques, which generally attempt to extrapolate the performance of laboratory test specimens to expected field performance. The purpose of this research project was to investigate and refine the use of direct testing methods, such as X-ray analysis techniques and thermal analysis techniques, to categorize carbonate aggregates for use in portland cement concrete. The results of this study indicated that the general testing methods that are currently used to obtain data for estimating service life tend to be very reliable and have good to excellent repeatability. Several changes in the current techniques were recommended to enhance the long-term reliability of the carbonate database. These changes can be summarized as follows: (a) Limits that are more stringent need to be set on the maximum particle size in the samples subjected to testing. This should help to improve the reliability of all three of the test methods studied during this project. (b) X-ray diffraction testing needs to be refined to incorporate the use of an internal standard. This will help to minimize the influence of sample positioning errors and it will also allow for the calculation of the concentration of the various minerals present in the samples. (c) Thermal analysis data needs to be corrected for moisture content and clay content prior to calculating the carbonate content of the sample.