23 resultados para tensile testing

em Instituto Politécnico do Porto, Portugal


Relevância:

60.00% 60.00%

Publicador:

Resumo:

n the last decades the biocomposites have been widely used in the construction, automobile and aerospace industries. Not only the interface transition zone (ITZ) but also the heterogeneity of natural fibres affects the mechanical behaviour of these composites. This work focuses on the numerical and experimental analyses of a polymeric composite fabricated with epoxy resin and unidirectional sisal and banana fibres. A three-dimensional model was set to analyze the composites using the elastic properties of the individual phases. In addition, a two-dimensional model was set taking into account the effective composite properties obtained by micromechanical models. A tensile testing was performed to validate the numerical analyses and evaluating the interface condition of the constitutive phases.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A crescente evolução na tecnologia das juntas coladas conferiu um potencial atractivo às ligações adesivas, com aplicações nas mais variadas indústrias. Isto deve-se não só aos aspetos económicos, tais como a melhoria da cadência de produção mas também à resistência mecânica que estas proporcionam. A possibilidade de ligar facilmente materiais distintos, a distribuição mais uniforme das tensões, a melhor resistência à fadiga e a elevada capacidade de amortecimento de vibrações estão entre as principais vantagens da utilização deste tipo de ligação. Estas propriedades transformam as juntas coladas numas das preferidas no momento de seleção de meios de união. O trabalho desenvolvido nesta dissertação enquadra-se no âmbito das ligações adesivas e tem como principais objetivos a produção de uma ferramenta para a produção de provetes de adesivo, assim como a determinação das propriedades mecânicas à tração dos mesmos para testar o desempenho do molde fabricado. Para tal, utilizou-se um adesivo frágil (Araldite® AV 138), um dúctil (Araldite® 2015) e um muito dúctil (SikaForce® 7888). Paralelamente é selecionado o método mais adequado na obtenção destes provetes, designadamente escolhendo entre a moldação em molde aberto e a injeção em molde fechado. Com vista à obtenção dos provetes, foi projetado e construído um molde em aço. Recorrendo à máquina de tração Shimadzu AG – X 100, realizaram-se os respetivos ensaios de tração, para a determinação de todas as propriedades mecânicas dos adesivos. Para efeitos de comparação de resultados foram utilizados dois tipos de extensómetros, um mecânico e um ótico. Os resultados experimentais permitiram observar que a presença de vazios afetou especialmente a deformação de rotura e a tensão de rotura. Detetaram-se pequenas discordâncias, comparativamente com os estudos publicados, de algumas características mecânicas obtidas dos diversos adesivos utilizados. Constatou-se também um ligeiro desfasamento entre os valores adquiridos com os dois tipos de extensómetros utilizados.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A tecnologia de ligação por adesivos estruturais tem vindo a ser utilizada ao longo de várias décadas, permitindo solucionar diversos problemas associados a técnicas chamadas "tradicionais" de ligação, como a soldadura, a rebitagem ou a ligação aparafusada. Esta é uma alternativa viável para substituir as ligações mecânicas, devido a diversos fatores como o menor peso estrutural, menor custo de fabricação e capacidade de união de diferentes materiais. O crescente recurso a materiais compósitos em diversas indústrias, nomeadamente a aeronáutica e naval, levaram ao consequente aumento da aplicação de ligações adesivas, por serem indicadas como forma de união destes materiais, onde é de enaltecer a sua elevada resistência à fadiga. Uma junta adesiva está maioritariamente sujeita a esforços de corte e arrancamento e portanto o conhecimento dos módulos de elasticidade à tração (E) ou corte (G) do adesivo, e ainda as resistências máximas à tração e ao corte, não é suficiente quando se pretende prever o comportamento da mesma. Na verdade, torna-se necessário abranger na análise a plastificação progressiva verificada nas juntas adesivas antes da rotura, sendo necessário o conhecimento de parâmetros tais como a taxa crítica de libertação de energia de deformação à tração (GIc) e corte (GIIc). Este trabalho pretende estudar um adesivo estrutural recentemente lançado no mercado, carecendo portanto da sua caracterização, para facilitar a previsão da resistência de estruturas adesivas ligadas com o mesmo. São 4 os ensaios a realizar: ensaios à tração de provetes em bruto, ensaios ao corte com a geometria Thick Adherend Shear Test (TAST), ensaios Double-Cantilever Beam (DCB) e ensaios End-Notched Flexure (ENF). Com a realização dos ensaios referidos, serão determinadas as propriedades mecânicas e de fratura à tração e ao corte, e serão fornecidos os parâmetros para a previsão da resistência de juntas adesivas com este adesivo por uma variedade de métodos, desde métodos analíticos mais expeditos até aos métodos numéricos mais avançados existentes atualmente. Os resultados foram de encontro aos disponibilizados pelo fabricante, sempre que estes se encontravam disponíveis, obtendo-se discrepâncias bastante reduzidas nos diversos parâmetros determinados.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A necessidade de utilizar métodos de ligação entre componentes de forma mais rápida, eficaz e com melhores resultados tem causado a crescente utilização das juntas adesivas, em detrimento dos métodos tradicionais de ligação. A utilização das juntas adesivas tem vindo a aumentar em diversas aplicações industriais por estas apresentarem vantagens, das quais se destacam a redução de peso, redução de concentrações de tensões e facilidade de fabrico. No entanto, uma das limitações das juntas adesivas é a dificuldade em prever a resistência da junta após fabrico e durante a sua vida útil devido à presença de defeitos no adesivo. Os defeitos são normalmente gerados pela preparação inadequada das juntas ou degradação do adesivo devido ao ambiente (por exemplo, humidade), reduzindo a qualidade da ligação e influenciando a resistência da junta. Neste trabalho é apresentado um estudo experimental e numérico de juntas de sobreposição simples (JSS) com a inclusão de defeitos centrados na camada de adesivo para comprimentos de sobreposição (LO) diferentes. Os adesivos utilizados foram o Araldite® AV138, apresentado como sendo frágil, e o adesivo Sikaforce® 7752, intitulado como adesivo dúctil. A parte experimental consistiu no ensaio à tração das diferentes JSS permitindo a obtenção das curvas força-deslocamento (P-δ). A análise numérica por modelos de dano coesivo (MDC) foi realizada para analisar as tensões de arrancamento ((σy) e as tensões de corte (τxy) na camada adesiva, para estudar a variável de dano do MDC durante o processo de rotura e para avaliar a capacidade dos MDC na previsão da resistência da junta. Constatou-se um efeito significativo dos defeitos de diferentes dimensões na resistência das juntas, que também depende do tipo de adesivo utilizado e do valor de LO. Os modelos numéricos permitiram a descrição detalhada do comportamento das juntas e previsão de resistência, embora para o adesivo dúctil a utilização de uma lei coesiva triangular tenha provocado alguma discrepância relativamente aos resultados experimentais.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

As juntas adesivas são uma alternativa viável para substituir ligações comuns como as mecânicas ou soldadas, devido a diversas vantagens como a possibilidade de união de materiais de natureza diferente, maior leveza, menores custos inerentes ao fabrico e ainda prevenção da corrosão galvânica que pode ocorrer nas ligações entre dois materiais metálicos diferentes. A resistência de uma junta depende, para um determinado tipo de solicitação imposta, da distribuição de tensões no interior da junta. Por outro lado, a geometria das juntas, as propriedades mecânicas dos adesivos e os componentes a ligar vão influenciar a distribuição de tensões. O carregamento nas camadas adesivas de uma junta poderá induzir tensões de tração, compressão, corte, arrancamento ou clivagem, ou ainda uma combinação de duas ou mais destas componentes. O objetivo da presente dissertação é a caraterização completa de um adesivo estrutural de alta ductilidade recentemente lançado no mercado (SikaPower® -4720), para facilitar o projeto e otimização de juntas adesivas ligadas com o mesmo. São quatro os ensaios a realizar: ensaios à tração de provetes maciços (também denominados de bulk), ensaios ao corte com a geometria Thick Adherend Shear Test, ensaios Double-Cantilever Beam e ainda ensaios End-Notched Flexure. Com a realização dos ensaios referidos, são determinadas as propriedades essenciais à caraterização mecânica e de fratura do adesivo. Os resultados obtidos para cada ensaio resultaram em propriedades medidas com elevada repetibilidade, da mesma maneira que se revelaram de acordo com os dados disponibilizados pelo fabricante, sempre que estes estavam disponíveis.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The impact of end customer quality complaints with direct relationship with automotive components has presented negative trend at European level for the entire automotive industry. Thus, this research proposal is to concentrate efforts on the most important items of Pareto chart and understand the failure type and the mechanism involved, link and impact of the project and parameters on the process, ending it with the development of one of the company’s most desired tool, that hosted this project – European methodology of terminals defects classification, and listing real opportunities for improvement based on measurement and analysis of actual data. Through the development of terminals defects classification methodology, which is considered a valuable asset to the company, all the other companies of the YAZAKI’s group will be able to characterize terminals as brittle or ductile, in order to put in motion, more efficiently, all the other different existing internal procedures for the safeguarding of the components, improving manufacturing efficiency. Based on a brief observation, nothing can be said in absolute sense, concerning the failure causes. Base materials, project, handling during manufacture and storage, as well as the cold work performed by plastic deformation, all play an important role. However, it was expected that this failure has been due to a combination of factors, in detriment of the existence of a single cause. In order to acquire greater knowledge about this problem, unexplored by the company up to the date of commencement of this study, was conducted a thorough review of existing literature on the subject, real production sites were visited and, of course, the actual parts were tested in lab environment. To answer to many of the major issues raised throughout the investigation, were used extensively some theoretical concepts focused on the literature review, with a view to realizing the relationship existing between the different parameters concerned. Should here be stated that finding technical studies on copper and its alloys is really hard, not being given all the desirable information. This investigation has been performed as a YAZAKI Europe Limited Company project and as a Master Thesis for Instituto Superior de Engenharia do Porto, conducted during 9 months between 2012/2013.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

In this work, an experimental study was performed on the influence of plug-filling, loading rate and temperature on the tensile strength of single-strap (SS) and double-strap (DS) repairs on aluminium structures. Whilst the main purpose of this work was to evaluate the feasibility of plug-filling for the strength improvement of these repairs, a parallel study was carried out to assess the sensitivity of the adhesive to external features that can affect the repairs performance, such as the rate of loading and environmental temperature. The experimental programme included repairs with different values of overlap length (L O = 10, 20 and 30 mm), and with and without plug-filling, whose results were interpreted in light of experimental evidence of the fracture modes and typical stress distributions for bonded repairs. The influence of the testing speed on the repairs strength was also addressed (considering 0.5, 5 and 25 mm/min). Accounting for the temperature effects, tests were carried out at room temperature (≈23°C), 50 and 80°C. This permitted a comparative evaluation of the adhesive tested below and above the glass transition temperature (T g), established by the manufacturer as 67°C. The combined influence of these two parameters on the repairs strength was also analysed. According to the results obtained from this work, design guidelines for repairing aluminium structures were

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Component joining is typically performed by welding, fastening, or adhesive-bonding. For bonded aerospace applications, adhesives must withstand high-temperatures (200°C or above, depending on the application), which implies their mechanical characterization under identical conditions. The extended finite element method (XFEM) is an enhancement of the finite element method (FEM) that can be used for the strength prediction of bonded structures. This work proposes and validates damage laws for a thin layer of an epoxy adhesive at room temperature (RT), 100, 150, and 200°C using the XFEM. The fracture toughness (G Ic ) and maximum load ( ); in pure tensile loading were defined by testing double-cantilever beam (DCB) and bulk tensile specimens, respectively, which permitted building the damage laws for each temperature. The bulk test results revealed that decreased gradually with the temperature. On the other hand, the value of G Ic of the adhesive, extracted from the DCB data, was shown to be relatively insensitive to temperature up to the glass transition temperature (T g ), while above T g (at 200°C) a great reduction took place. The output of the DCB numerical simulations for the various temperatures showed a good agreement with the experimental results, which validated the obtained data for strength prediction of bonded joints in tension. By the obtained results, the XFEM proved to be an alternative for the accurate strength prediction of bonded structures.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Adhesive bonding as a joining or repair method has a wide application in many industries. Repairs with bonded patches are often carried out to re-establish the stiffness at critical regions or spots of corrosion and/or fatigue cracks. Single and double-strap repairs (SS and DS, respectively) are a viable option for repairing. For the SS repairs, a patch is adhesively-bonded on one of the structure faces. SS repairs are easy to execute, but the load eccentricity leads to peel peak stresses at the overlap edges. DS repairs involve the use of two patches, one on each face of the structure. These are more efficient than SS repairs, due to the doubling of the bonding area and suppression of the transverse deflection of the adherends. Shear stresses also become more uniform as a result of smaller differential straining. The experimental and Finite Element (FE) study presented here for strength prediction and design optimization of bonded repairs includes SS and DS solutions with different values of overlap length (LO). The examined values of LO include 10, 20 and 30 mm. The failure strengths of the SS and DS repairs were compared with FE results by using the Abaqus® FE software. A Cohesive Zone Model (CZM) with a triangular shape in pure tensile and shear modes, including the mixed-mode possibility for crack growth, was used to simulate fracture of the adhesive layer. A good agreement was found between the experiments and the FE simulations on the failure modes, elastic stiffness and strength of the repairs, showing the effectiveness and applicability of the proposed FE technique in predicting strength of bonded repairs. Furthermore, some optimization principles were proposed to repair structures with adhesively-bonded patches that will allow repair designers to effectively design bonded repairs.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In this work, an experimental study was performed on the influence of plug filling, loading rate and temperature on the tensile strength of single-strap (SS) and double-strap (DS) repairs on aluminium structures. The experimental programme includes repairs with different values of overlap length (LO=10, 20 and 30 mm), and with and without plug filling. The influence of the testing speed on the repairs strength is also addressed (considering 0.5, 5 and 25 mm/min). Accounting for the temperature effects, tests were carried out at room temperature, 50ºC and 80ºC. This will permit a comparative evaluation of the adhesive tested below and above the Glass Transition Temperature (Tg), established by the manufacturer at 67ºC. The global tendencies of the test results concerning the plug filling and overlap length analyses are interpreted from the fracture modes and typical stress distributions for bonded repairs. According to the results obtained from this work, design guidelines for repairing aluminium structures were recommended.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Adhesive bonding is nowadays a serious candidate to replace methods such as fastening or riveting, because of attractive mechanical properties. As a result, adhesives are being increasingly used in industries such as the automotive, aerospace and construction. Thus, it is highly important to predict the strength of bonded joints to assess the feasibility of joining during the fabrication process of components (e.g. due to complex geometries) or for repairing purposes. This work studies the tensile behaviour of adhesive joints between aluminium adherends considering different values of adherend thickness (h) and the double-cantilever beam (DCB) test. The experimental work consists of the definition of the tensile fracture toughness (GIC) for the different joint configurations. A conventional fracture characterization method was used, together with a J-integral approach, that take into account the plasticity effects occurring in the adhesive layer. An optical measurement method is used for the evaluation of crack tip opening and adherends rotation at the crack tip during the test, supported by a Matlab® sub-routine for the automated extraction of these quantities. As output of this work, a comparative evaluation between bonded systems with different values of adherend thickness is carried out and complete fracture data is provided in tension for the subsequent strength prediction of joints with identical conditions.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Background: Temporal lobe epilepsy (TLE) is a neurological disorder that directly affects cortical areas responsible for auditory processing. The resulting abnormalities can be assessed using event-related potentials (ERP), which have high temporal resolution. However, little is known about TLE in terms of dysfunction of early sensory memory encoding or possible correlations between EEGs, linguistic deficits, and seizures. Mismatch negativity (MMN) is an ERP component – elicited by introducing a deviant stimulus while the subject is attending to a repetitive behavioural task – which reflects pre-attentive sensory memory function and reflects neuronal auditory discrimination and perceptional accuracy. Hypothesis: We propose an MMN protocol for future clinical application and research based on the hypothesis that children with TLE may have abnormal MMN for speech and non-speech stimuli. The MMN can be elicited with a passive auditory oddball paradigm, and the abnormalities might be associated with the location and frequency of epileptic seizures. Significance: The suggested protocol might contribute to a better understanding of the neuropsychophysiological basis of MMN. We suggest that in TLE central sound representation may be decreased for speech and non-speech stimuli. Discussion: MMN arises from a difference to speech and non-speech stimuli across electrode sites. TLE in childhood might be a good model for studying topographic and functional auditory processing and its neurodevelopment, pointing to MMN as a possible clinical tool for prognosis, evaluation, follow-up, and rehabilitation for TLE.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The hidden-node problem has been shown to be a major source of Quality-of-Service (QoS) degradation in Wireless Sensor Networks (WSNs) due to factors such as the limited communication range of sensor nodes, link asymmetry and the characteristics of the physical environment. In wireless contention-based Medium Access Control protocols, if two nodes that are not visible to each other transmit to a third node that is visible to the formers, there will be a collision – usually called hidden-node or blind collision. This problem greatly affects network throughput, energy-efficiency and message transfer delays, which might be particularly dramatic in large-scale WSNs. This technical report tackles the hidden-node problem in WSNs and proposes HNAMe, a simple yet efficient distributed mechanism to overcome it. H-NAMe relies on a grouping strategy that splits each cluster of a WSN into disjoint groups of non-hidden nodes and then scales to multiple clusters via a cluster grouping strategy that guarantees no transmission interference between overlapping clusters. We also show that the H-NAMe mechanism can be easily applied to the IEEE 802.15.4/ZigBee protocols with only minor add-ons and ensuring backward compatibility with the standard specifications. We demonstrate the feasibility of H-NAMe via an experimental test-bed, showing that it increases network throughput and transmission success probability up to twice the values obtained without H-NAMe. We believe that the results in this technical report will be quite useful in efficiently enabling IEEE 802.15.4/ZigBee as a WSN protocol.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

This work addresses both experimental and numerical analyses regarding the tensile behaviour of CFRP single-strap repairs. Two fundamental geometrical parameters were studied: overlap length and patch thickness. The numerical model used ABAQUS® software and a developed cohesive mixed-mode damage model adequate for ductile adhesives, and implemented within interface finite elements. Stress analyses and strength predictions were carried out. Experimental and numerical comparisons were performed on failure modes, failure load and equivalent stiffness of the repair. Good correlation was found between experimental and numerical results, showing that the proposed model can be successfully applied to bonded joints or repairs.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Bonded joints are gaining importance in many fields of manufacturing owing to a significant number of advantages to the traditional methods. The single lap joint (SLJ) is the most commonly used method. The use of material or geometric changes in SLJ reduces peel and shear peak stresses at the damage initiation sites. In this work, the effect of adherend recessing at the overlap edges on the tensile strength of SLJ, bonded with a brittle adhesive, was experimentally and numerically studied. The recess dimensions (length and depth) were optimized for different values of overlap length (LO), thus allowing the maximization of the joint’s strength by the reduction of peak stresses at the overlap edges. The effect of recessing was also investigated by a finite element (FE) analysis and cohesive zone modelling (CZM), which allowed characterizing the entire fracture process and provided joint strength predictions. For this purpose, a static FE analysis was performed in ABAQUS1 considering geometric nonlinearities. In the end, the experimental and FE results revealed the accuracy of the FE analysis in predicting the strength and also provided some design principles for the strength improvement of SLJ using a relatively simple and straightforward technique.