14 resultados para Water absorption kinetics
em Repositório Científico do Instituto Politécnico de Lisboa - Portugal
Resumo:
The construction industry keeps on demanding huge quantities of natural resources, mainly minerals for mortars and concrete production. The depletion of many quarries and environmental concerns about reducing the dumping of construction and demolition waste in quarries have led to an increase in the procuring and use of recycled aggregates from this type of waste. If they are to be incorporated in concrete and mortars it is essential to know their properties to guarantee the adequate performance of the end products, in both mechanical and durability-related terms. Existing regulated tests were developed for natural aggregates, however, and several problems arise when they are applied to recycled aggregates, especially fine recycled aggregates (FRA). This paper describes the main problems encountered with these tests and proposes an alternative method to determine the density and water absorption of FRA that removes them. The use of sodium hexametaphosphate solutions in the water absorption test has proven to improve its efficiency, minimizing cohesion between particles and helping to release entrained air.
Physical, chemical and mineralogical properties of fine recycled aggregates made from concrete waste
Resumo:
This paper assesses the physical, chemical and mineralogical characteristics of fine recycled aggregates obtained from crushed concrete waste, comparing them with two types of natural fine aggregates from different origins. A commercial concrete was jaw crushed, and the effect of different aperture sizes on the particle size distribution of the resulting aggregates was evaluated. The density and water absorption of the recycled aggregates was determined and a model for predicting water absorption over time is proposed. Both natural and recycled aggregates were characterized regarding bulk density and fines content. Recycled aggregates were additionally characterized by XRD, SEM/EDS and DTA/TG of individual size fractions. The results show that natural and recycled fine aggregates have very different characteristics. This should be considered in potential applications, both in terms of the limits for replacing amounts and of the rules and design criteria of the manufactured products. (C) 2015 Elsevier Ltd. All rights reserved.
Resumo:
Fine recycled aggregates are seen as the last choice in recycling for concrete production. Many references quote their detrimental influence on the most important characteristics of concrete: compressive and tensile strength; modulus of elasticity; water absorption; shrinkage: carbonation and chloride penetration. These two last characteristics are fundamental in terms of the long-term durability of reinforced or prestressed concrete. In the experimental research carried out at IST, part of which has already been published, different concrete mixes (with increasing rates of substitution of fine natural aggregates sand - with fine recycled aggregates from crushed concrete) were prepared and tested. The results were then compared with those for a reference concrete with exactly the same composition and grading curve, but with no recycled aggregates. This paper presents the main results of this research for water absorption by immersion and capillarity, chloride penetration (by means of the chloride migration coefficient), and carbonation resistance, drawing some conclusions on the feasibility of using this type of aggregate in structural concrete, while taking into account any ensuing obvious positive environmental impact.
Resumo:
Na presente dissertação, o trabalho desenvolvido teve como objetivo, a avaliação de alguns parâmetros de durabilidade de argamassas com incorporação de catalisador exausto de FCC (do inglês “Fluid Catalytic Cracking”) para serem utilizadas na reparação de estruturas de betão. O catalisador exausto de FCC é um resíduo da indústria petrolífera e o utilizado neste estudo é proveniente da refinaria da Petrogal, S.A. em Sines. A presente investigação baseou-se na preparação, e avaliação de propriedades, de duas séries distintas de argamassas: a série que se denominou “RAS” e a série que se denominou “Durabilidade”, nas quais se substituiu, parcialmente entre 5, 10 e 15%, em massa de cimento por resíduo exausto de FCC. As argamassas de ambas as séries diferenciam-se entre si, sobretudo, pela utilização de areia reativa nas argamassas da série RAS e de areia inerte no caso das argamassas da série durabilidade. Nas argamassas estudadas foram realizados ensaios no estado fresco e ensaios no estado endurecido. Os ensaios no estado fresco incluíram a determinação da consistência por espalhamento, da massa volúmica e do teor de ar. Nos ensaios no estado endurecido foram avaliadas, no caso das argamassas da série RAS a extensão da reação àlcalis-sílica e no caso das argamassas da série Durabilidade as resistências mecânicas - à flexão e à compressão, a resistência à carbonatação acelerada, o módulo de elasticidade à compressão, a absorção capilar, a permeabilidade ao oxigénio, a difusão de cloretos em regime não estacionário. O trabalho desenvolvido nesta dissertação demonstrou que a incorporação de catalisador exausto de FCC, em argamassas à base de cimento, minimiza o efeito de expansão das reações álcalis-sílica, bem como contribui para reduzir a absorção capilar e coeficiente de difusão de cloretos. No entanto, este resíduo quando incorporados em argamassas contribui para a diminuição da resistência à carbonatação acelerada e para o aumento da permeabilidade ao oxigénio.
Resumo:
Dissertação de natureza Científica para obtenção do grau de Mestre em Engenharia Civil na Área de Especialização em Edificações
Resumo:
Trabalho Final de Mestrado para obtenção do grau de Mestre em Engenharia Civil na Área de Especialização de Edificações
Resumo:
The aim of this paper is to evaluate the influence of the crushing process used to obtain recycled concrete aggregates on the performance of concrete made with those aggregates. Two crushing methods were considered: primary crushing, using a jaw crusher, and primary plus secondary crushing (PSC), using a jaw crusher followed by a hammer mill. Besides natural aggregates (NA), these two processes were also used to crush three types of concrete made in laboratory (L20, L45 e L65) and three more others from the precast industry (P20, P45 e P65). The coarse natural aggregates were totally replaced by coarse recycled concrete aggregates. The recycled aggregates concrete mixes were compared with reference concrete mixes made using only NA, and the following properties related to the mechanical and durability performance were tested: compressive strength; splitting tensile strength; modulus of elasticity; carbonation resistance; chloride penetration resistance; water absorption by capillarity; water absorption by immersion; and shrinkage. The results show that the PSC process leads to better performances, especially in the durability properties. © 2014 RILEM
Resumo:
Self-compacting concrete (SCC) can soon be expected to replace conventional concrete due to its many advantages. Its main characteristics in the fresh state are achieved essentially by a higher volume of mortar (more ultrafine material) and a decrease of the coarse-aggregates. The use of over-large volumes of additions such as fly ash (FA) and/or limestone filler (LF) can substantially affect the concrete's pore structure and consequently its durability. In this context, an experimental programme was conducted to evaluate the effect on the concrete's porosity and microstructure of incorporating FA and LF in binary and ternary mixes of SCC. For this, a total of 11 SIX mixes were produced; 1 with cement only (C); 3 with C + FA in 30%, 60% and 70% substitution (fad); 3 with C + LF in 30%, 60% and 70% fad; 4 with C + FA + LF in combinations of 10-20%, 20-10%, 20-40% and 40-20% f(ad), respectively. The results enabled conclusions to be established regarding the SCC's durability, based on its permeability and the microstructure of its pore structure. The properties studied are strongly affected by the type and quantity of additions. The use of ternary mixes also proves to be extremely favourable, confirming the beneficial effect of the synergy between these additions. (C) 2015 Elsevier Ltd. All rights reserved.
Resumo:
Abstract Self-compacting concrete (SCC) can soon be expected to replace conventional concrete due to its many advantages. Its main characteristics in the fresh state are achieved essentially by a higher volume of mortar (more ultrafine material) and a decrease of the coarse-aggregates. The use of over-large volumes of additions such as fly ash (FA) and/or limestone filler (LF) can substantially affect the concrete's pore structure and consequently its durability. In this context, an experimental programme was conducted to evaluate the effect on the concrete's porosity and microstructure of incorporating FA and LF in binary and ternary mixes of SCC. For this, a total of 11 SCC mixes were produced: 1 with cement only (C); 3 with C + FA in 30%, 60% and 70% substitution (fad); 3 with C + LF in 30%, 60% and 70% fad; 4 with C + FA + LF in combinations of 10-20%, 20-10%, 20-40% and 40-20% fad, respectively. The results enabled conclusions to be established regarding the SCC's durability, based on its permeability and the microstructure of its pore structure. The properties studied are strongly affected by the type and quantity of additions. The use of ternary mixes also proves to be extremely favourable, confirming the beneficial effect of the synergy between these additions. © 2015 Elsevier Ltd. All rights reserved.
Resumo:
The aim of this paper is to evaluate the influence of the crushing process used to obtain recycled concrete aggregates on the performance of concrete made with those aggregates. Two crushing methods were considered: primary crushing, using a jaw crusher, and primary plus secondary crushing (PSC), using a jaw crusher followed by a hammer mill. Besides natural aggregates (NA), these two processes were also used to crush three types of concrete made in laboratory (L20, L45 e L65) and three more others from the precast industry (P20, P45 e P65). The coarse natural aggregates were totally replaced by coarse recycled concrete aggregates. The recycled aggregates concrete mixes were compared with reference concrete mixes made using only NA, and the following properties related to the mechanical and durability performance were tested: compressive strength; splitting tensile strength; modulus of elasticity; carbonation resistance; chloride penetration resistance; water absorption by capillarity; water absorption by immersion; and shrinkage. The results show that the PSC process leads to better performances, especially in the durability properties.
Resumo:
Dissertação de Natureza Científica para obtenção do grau de Mestre em Engenharia Civil na Área de Especialização de Edificações
Resumo:
This work intends to evaluate the (mechanical and durability) performance of concrete made with coarse recycled concrete aggregates (CRCA) obtained using two crushing processes: primary crushing (PC) and primary plus secondary crushing (PSC). This analysis intends to select the most efficient production process of recycled aggregates (RA). The RA used here resulted from precast products (P), with strength classes of 20 MPa, 45 MPa and 65 MPa, and from laboratory-made concrete (L) with the same compressive strengths. The evaluation of concrete was made with the following tests: compressive strength; splitting tensile strength; modulus of elasticity; carbona-tion resistance; chloride penetration resistance; capillary water absorption; and water absorption by immersion. These findings contribute to a solid and innovative basis that allows the precasting industry to use without restrictions the waste it generates. © (2015) Trans Tech Publications, Switzerland.
Resumo:
The objective of this research is the production of concrete with recycled aggregates (RA) from various CDW plants around Portugal. The influence of the RA collection location and consequently of their composition on the characteristics of the concrete produced was analysed. In the mixes produced in this research RA from five plants (Valnor, Vimajas, Ambilei, Europontal and Retria) were used: in three of them coarse and fine RA were analysed and in the remaining ones only coarse RA were used. The experimental campaign comprised two tests in fresh concrete (cone of Abrams slump and density) and eight in hardened concrete (compressive strength in cubes and cylinders, splitting tensile strength, modulus of elasticity, water absorption by immersion and capillarity, carbonation and chloride penetration resistance). It was found that the use of RA causes a quality decrease in concrete. However, there was a wide results scatter according to the plant where the RAs were collected, because of the variation in composition of the RA. It was also found that the use of fine RA causes a more significant performance loss of the concrete properties analysed than the use of coarse RA. © (2015) Trans Tech Publications, Switzerland.
Resumo:
Trabalho Final de Mestrado para obtenção do grau de Mestre em Engenharia Química