The Mg-Ni metastable alloys (with amorphous or nanocrystalline structures) are promising candidates for anode application in nickel-metal hydride rechargeable batteries due to its large hydrogen absorbing capacity, low weight, availability, and relative low price. In spite of these interesting features, improvement on the cycle life performance must be achieved to allow its application in commercial products. In the present paper, the effect of mechanical coating of a Mg-50 at.% Ni alloy with Ni and Ni-5 at.% Al on the structure, powder morphology, and electrochemical properties is investigated. The coating additives, Mg-Ni alloy and resulting nanocomposites (i.e., Mg-Ni alloy + additive) were investigated by means of X-ray diffraction and scanning electron microscopy. The Mg-Ni alloy and nanocomposites were submitted to galvanostatic cycles of charge and discharge to evaluate their electrode performances. The mechanical coating with Ni and Ni-5% Al increased the maximum discharge capacity of the Mg-Ni alloy from of 221 to 257 and 273 mA h g(-1), respectively. Improvement on the cycle life performance was also achieved by mechanical coating.

Relevância:

90.00% 90.00%

Publicador:

Resumo:

In recent years, Mg-Ni-based metastable alloys have been attracting attention due to their large hydrogen sorption capacities, low weight, low cost, and high availability. Despite the large discharge capacity and high activity of these alloys, the accelerated degradation of the discharge capacity after only few cycles of charge and discharge is the main shortcoming against their commercial use in batteries. The addition of alloying elements showed to be an effective way of improving the electrode performance of Mg-Ni-based alloys. In the present work, the effect of Ti and Pt alloying elements on the structure and electrode performance of a binary Mg-Ni alloy was investigated. The XRD and HRTEM revealed that all the investigated alloy compositions had multi-phase nanostructures, with crystallite size in the range of 6 nm. Moreover, the investigated alloying elements demonstrated remarkable improvements of both maximum discharge capacity and cycling life. Simultaneous addition of Ti and Pd demonstrated a synergetic effect on the electrochemical properties of the alloy electrodes. Among the investigated alloys, the best electrochemical performance was obtained for the Mg(51)Ti(4)Ni(43)Pt(2) composition (in at.%), which achieved 448 mAh g(-1) of maximum discharge capacity and retained almost 66% of this capacity after 10 cycles. In contrast, the binary Mg(55)Ni(45) alloy achieved only 248 mAh g(-1) and retained 11% of this capacity after 10 cycles. (C) 2010 Elsevier By. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Background: This study aimed to compare the cytotoxicity of base-metal dental alloys and to evaluate if the casting method could influence their cytotoxicity. Methods: Disks of base-metal dental alloys were cast by two methods: plasma, under argon atmosphere, injected by vacuum-pressure; and oxygen-gas flame, injected by centrifugation, except Ti-6Al-4V and commercially pure titanium (cpTi), cast only by plasma. SCC9 cells were cultured in culture media D-MEM/Ham`s F12 supplemented, at 37 degrees C in a humidified atmosphere of 5% carbon dioxide and 95% air, on the previously prepared disks. At subconfluence in wells without disks (control), cell number and viability were evaluated. Results: In plasma method, cpTi and Ti-6Al-4V were similar to control and presented higher number of cells than all other alloys, followed by Ni-Cr. In oxygen-gas name method, all alloys presented fewer cells than control. Ni-Cr presented more cells than any other alloy, followed by Co-Cr-Mo-W which presented more cells than Ni-Cr-Ti, Co-Cr-Mo, and Ni-Cr-Be. There were no significant differences between casting methods related to cell number. Cell viability was not affected by either chemical composition or casting methods. Conclusion: cpTi and Ti-6Al-4V were not cytotoxic while Ni-Cr-Be was the most cytotoxic among tested alloys. The casting method did not affect cytotoxicity of the alloys. (c) 2007 Wiley Periodicals, Inc.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This study compared the vertical misfit of 3-unit implant-supported nickel-chromium (Ni-Cr) and cobalt-chromium (Co-Cr) alloy and commercially pure titanium (cpTi) frameworks after casting as 1 piece, after sectioning and laser welding, and after simulated porcelain firings. The results on the tightened side showed no statistically significant differences. On the opposite side, statistically significant differences were found for Co-Cr alloy (118.64 mu m [SD: 91.48] to 39.90 mu m [SD: 27.13]) and cpTi (118.56 mu m [51.35] to 27.87 mu m [12.71]) when comparing 1-piece to laser-welded frameworks. With both sides tightened, only Co-Cr alloy showed statistically significant differences after laser welding. Ni-Cr alloy showed the lowest misfit values, though the differences were not statistically significantly different. Simulated porcelain firings revealed no significant differences.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

An evaluation was made of the influence of calcination temperatures on the structure, morphology and eletromagnetic properties of Ni-Zn ferrite powders. To this end, Ni(0.5)Zn(0.5)Fe(2)O(4) ferrite powders were prepared by combustion reaction and calcined at temperatures of 800, 1000 and 1200 degrees C/2 h. The resulting powders were characterized by XRD, SEM and reflectivity measurements in the frequency bands of 8-12 GHz. The results demonstrated that raising the calcination temperature increased the particle sizes of the powders of all the systems in question, improving the reflectivity of the materials. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Ni(II)GGH (GGH, glycylglycyl-L-histidine) reacts rapidly with S(IV), in air-saturated solution, to produce Ni(III)GGH. A mechanism is proposed where Ni(III) oxidizes SO(3)(2-) to SO(3)(center dot-), which reacts with dissolved oxygen to produce SO(5)(center dot-), initiating radical chain reactions. DNA strand breaks and 8-oxo-7,8-dihydro-20-deoxyguanosine (8-oxodGuo) formation were observed in air-saturated solutions containing micromolar concentrations of nickel(II) and S(IV). The efficacies of melatonin, (-)-epigallocatechin-gallate (from green tea), resveratrol, tannic, and ascorbic acids in terms of their inhibitory activities of DNA strand breaks and 8-oxodGuo formation were evaluated.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The reaction Of Cu(ClO(4))(2)center dot 6H(2)O with dimethylglyoxime (H(2)dmg) in a 1:1 mole ratio in aqueous methanol at room temperature affords the dinuclear complex [Cu(2)(mu-Hdmg)(4)] (1). Reaction of 1 with [Cu(bpy)(H(2)O)(2)](ClO(4))(2) (bpy = 2,2`-bipyridine) in a 1:1 mole ratio in aqueous methanol at room temperature yields the tetranuclear complex [Cu(2)(mu-HdMg)(2)(mu-dMg)(2)(bpy)(2)(H(2)O)(2)](ClO(4))(2) (2). The direct reaction of Cu(ClO(4))(2)center dot 6H(2)O with H(2)dmg and bpy in a 2:21 mole ratio in aqueous methanol at room temperature also yields 2 quantitatively. The complexes 1 and 2 were structurally characterized by X-ray crystallography. Unlike the binding in Ni/Co-dmg, two different types of N-O bridging modes during the oxime based metallacycle formation and stacking of square planar units have been identified in these complexes. The neutral dinuclear complex 1 has CuN(4)O coordination spheres and complex 2 consists of a dicationic [Cu(2)(mu-HdMg)(2)(mu-dMg)(2)(bpy)(2)(H(2)O)(2)](2+) unit and two uncoordinated ClO(4)(-) anions having CuN(4)O and CuN(2)O(3) coordination spheres. The two copper(II) ions are at a distance of 3.846(8) angstrom in 1 for the trans out of plane link and at 3.419(10) and 3.684(10) angstrom in 2 for the trans out of plane and cis in plane arrangements, respectively. The average Cu-N(oxime) distances are 1.953 and 1.935 angstrom, respectively. The average basal and apical Cu-N(oxime) distances are 1.945, 2.295 and 2.429 angstrom. The UV-Vis spectra of 2 is similar to the spectrum of the reaction mixture of 1 and [Cu(bpy)(H(2)O)(2)](2+). Variable temperature magnetic properties measurement shows that the interaction between the paramagnetic copper centers in complex I is antiferromagnetic in nature. The EPR spectra of frozen solution of the complexes at 77 K consist of axially symmetric fine-structure transitions (Delta M(S) = 1) and half-field signals (Delta M(S) = 2) at ca. 1600 G, suggesting the presence of appreciable Cu-Cu interactions. (C) 2009 Elsevier Ltd. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Titanium alloys, alloys, especially beta-type alloys containing beta-stabilizing elements, constitute a highly versatile category of metallic materials that have been under constant development for application in orthopedics and dentistry. This type of alloy generally presents a high mechanical strength-to-weight ratio, excellent corrosion resistance and low elastic modulus. The purpose of this study is to evaluate the cytotoxicity and adhesion of fibroblast cells on titanium alloy substrates containing Nb, Ta, Zr, Cu, Sn and Mo alloying elements. Cells cultured on polystyrene were used as controls. In vitro results with Vero cells demonstrated that the tested materials, except Cu-based alloy, presented high viability in short-term testing. Adhesion of cells cultured on disks showed no differences between the materials and reference except for the Ti-Cu alloy, which showed reduced adhesion attributed to poor metabolic activity. Titanium alloys with the addition of Nb, Ta, Zr, Sn and Mo elements show a promising potential for biomedical applications. (C) 2011 Elsevier B.V. All rights reserved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The performance of La((1-y))Sr(y)Ni(x)Co((1-x))O(3) perovskites for the water gas shift reaction (WGSR) was investigated. The samples were prepared by the co- precipitation method and were performed by the BET method, XRD, TPR, and XPS. The catalytic tests were performed at 300 and 400 A degrees C and H(2)O(v)/CO = 2.3/1 (molar ratio). The sample with the highest surface area is La(0.70)Sr(0.30)NiO(3). The XRD results showed the formation of perovskite structure for all samples, and the La(0.70)Sr(0.30)NiO(3) sample also presented peaks corresponding to La(2)NiO(4) and NiO, indicating that the solubility limit of Sr in the perovskite lattice was surpassed. The replacement of Co by Ni favored the reduction of the species at lower temperatures, and the sample containing Sr presented the highest amount of reducible species, as identified by TPR results. All samples were active, the Sr containing perovskite appearing the most active due to the highest surface area, presence of the La(2)NiO(4) phase, and higher content of Cu in the surface, as detected by XPS. Among the samples containing Co, the most active one was that with x = 0.70 (60% of CO conversion).