50 resultados para Interface Toughness
em Biblioteca Digital da Produção Intelectual da Universidade de São Paulo (BDPI/USP)
Resumo:
Objective: To describe the ultrastructure of the interface between periodontal tissues and titanium mini-implants in rat mandibles. Materials and Methods: A titanium mini-implant was placed between the buccal roots of the mandibular first molar of 24 adult rats. After 21, 30, 45, 60, 90, and 120 days of implantation, the mandibular portion was removed and fixed in cacodylate-buffered 2% glutaraldehyde + 2.5% formaldehyde. The material was decalcified and processed for scanning and transmission electron microscopy. Results: Ultrastructural analysis revealed a thin cementum-like layer at longer times after implantation at the areas in which the periodontal ligament was in contact with the implant. Conclusions: The alveolar bone and the periodontal ligament reorganized their constituents around the implant, and a thin cementum-like layer was formed at longer times after implantation at the areas in which the periodontal ligament was in contact with the implant. (Angle Orthod. 2010;80:459-435.)
Resumo:
We use the density functional theory/local-density approximation (DFT/LDA)-1/2 method [L. G. Ferreira , Phys. Rev. B 78, 125116 (2008)], which attempts to fix the electron self-energy deficiency of DFT/LDA by half-ionizing the whole Bloch band of the crystal, to calculate the band offsets of two Si/SiO(2) interface models. Our results are similar to those obtained with a ""state-of-the-art"" GW approach [R. Shaltaf , Phys. Rev. Lett. 100, 186401 (2008)], with the advantage of being as computationally inexpensive as the usual DFT/LDA. Our band gap and band offset predictions are in excellent agreement with experiments.
Resumo:
We model interface formation by metal deposition on the conjugated polymer poly-para-phenylene vinylene, studying direct aluminum and layered aluminum-calcium structures Al/PPV and Al/Ca/PPV. To do that we use classical molecular dynamics simulations, checked by ab initio density-functional theory calculations, for selected relevant configurations. We find that Al not only migrates easily into the film, with a strong charge transfer to the neighboring chains, but also promotes rearrangement of the polymer in the interfacial region to the hexagonal structure. On the other hand, our results indicate that a thin Ca layer is sufficient to protect the film and maintain a well-defined metal/polymer interface, and that also a thin Al capping layer may protect the whole from environmental degradation.
Resumo:
We study trapping and propagation of a matter-wave soliton through the interface between uniform medium and a nonlinear optical lattice. Different regimes for transmission of a broad and a narrow solitons are investigated. Reflections and transmissions of solitons are predicted as a function of the lattice phase. The existence of a threshold in the amplitude of the nonlinear optical lattice, separating the transmission and reflection regimes, is verified. The localized nonlinear surface state, corresponding to the soliton trapped by the interface, is found. Variational approach predictions are confirmed by numerical simulations for the original Gross-Pitaevskii equation with nonlinear periodic potentials.
Resumo:
The importance of interface effects for organic devices has long been recognized, but getting detailed knowledge of the extent of such effects remains a major challenge because of the difficulty in distinguishing from bulk effects. This paper addresses the interface effects on the emission efficiency of poly(p-phenylene vinylene) (PPV), by producing layer-by-layer (LBL) films of PPV alternated with dodecylbenzenesulfonate. Films with thickness varying from similar to 15 to 225 nm had the structural defects controlled empirically by converting the films at two temperatures, 110 and 230 degrees C, while the optical properties were characterized by using optical absorption, photoluminescence (PL), and photoluminescence excitation spectra. Blueshifts in the absorption and PL spectra for LBL films with less than 25 bilayers (<40-50 nm) pointed to a larger number of PPV segments with low conjugation degree, regardless of the conversion temperature. For these thin films, the mean free-path for diffusion of photoexcited carriers decreased, and energy transfer may have been hampered owing to the low mobility of the excited carriers. The emission efficiency was then found to depend on the concentration of structural defects, i.e., on the conversion temperature. For thick films with more than 25 bilayers, on the other hand, the PL signal did not depend on the PPV conversion temperature. We also checked that the interface effects were not caused by waveguiding properties of the excited light. Overall, the electronic states at the interface were more localized, and this applied to film thickness of up to 40-50 nm. Because this is a typical film thickness in devices, the implication from the findings here is that interface phenomena should be a primary concern for the design of any organic device. (C) 2011 American Institute of Physics. [doi:10.1063/1.3622143]
Resumo:
Electron mobility was studied in lattice-matched short-period InGaAs/InP superlattices as a function of the width of the wells. The decreasing mobility with decreasing well width was shown to occur due to the interface roughness. The roughnesses of InGaAs/InP and GaAs/AlGaAs interfaces were compared. Much smoother InGaAs/InP interfaces resulted in higher electron mobility limited by interface roughness.
Resumo:
The exploitation of aqueous biphasic extraction is proposed for the first time in flow analysis This extraction strategy stands out for being environmentally attractive since it is based in the utilization of two immiscible phases that are intrinsically aqueous The organic solvents of the traditional liquid-liquid extractions ale no longer used, being replaced by non-toxic, non-flammable and non-volatile ones. A single interface flow analysis (SIFA) system was implemented to carry out the extraction process due to its favourable operational characteristics that include the high automation level and simplicity of operation, the establishment of a dynamic interface where the mass transfer occurred between the two immiscible aqueous phases, and the versatile control over the extraction process namely the extraction time The application selected to demonstrate the feasibility of SIFA to perform this aqueous biphasic extraction was the pre-concentration of lead. After extraction, lead reacted with 8-hydroxyquinoline-5-sulfonic acid and the resulting product was determined by a fluorimetric detector included in the flow manifold. Therefore, the SIFA single interface was used both as extraction (enrichment) and reaction interface. (C) 2010 Elsevier B.V All rights reserved.
Resumo:
Single interface flow systems (SIFA) present some noteworthy advantages when compared to other flow systems, such as a simpler configuration, a more straightforward operation and control and an undemanding optimisation routine. Moreover, the plain reaction zone establishment, which relies strictly on the mutual inter-dispersion of the adjoining solutions, could be exploited to set up multiple sequential reaction schemes providing supplementary information regarding the species under determination. In this context, strategies for accuracy assessment could be favourably implemented. To this end, the sample could be processed by two quasi-independent analytical methods and the final result would be calculated after considering the two different methods. Intrinsically more precise and accurate results would be then gathered. In order to demonstrate the feasibility of the approach, a SIFA system with spectrophotometric detection was designed for the determination of lansoprazole in pharmaceutical formulations. Two reaction interfaces with two distinct pi-acceptors, chloranilic acid (CIA) and 2,3-dichloro-5,6-dicyano-p-benzoquinone (DDQ) were implemented. Linear working concentration ranges between 2.71 x 10(-4) to 8.12 x 10(-4) mol L(-1) and 2.17 x 10(-4) to 8.12 x 10(-4) mol L(-1) were obtained for DDQ and CIA methods, respectively. When compared with the results furnished by the reference procedure, the results showed relative deviations lower than 2.7%. Furthermore. the repeatability was good, with r.s.d. lower than 3.8% and 4.7% for DDQ and CIA methods, respectively. Determination rate was about 30 h(-1). (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
A fully automated methodology was developed for the determination of the thyroid hormones levothyroxine (T4) and liothyronine (T3). The proposed method exploits the formation of highly coloured charge-transfer (CT) complexes between these compounds, acting as electron donors, and pi-acceptors such as chloranilic acid (CIA) and 2,3-dichloro-5,6-dicyano-p-benzoquinone (DDQ). For automation of the analytical procedure a simple, fast and versatile single interface flow system (SIFA)was implemented guaranteeing a simplified performance optimisation, low maintenance and a cost-effective operation. Moreover, the single reaction interface assured a convenient and straightforward approach for implementing job`s method of continuous variations used to establish the stoichiometry of the formed CT complexes. Linear calibration plots for levothyroxine and liothyronine concentrations ranging from 5.0 x 10(-5) to 2.5 x 10(-4) mol L(-1) and 1.0 x 10(-5) to 1.0 x 10(-4) mol L(-1), respectively, were obtained, with good precision (R.S.D. <4.6% and <3.9%) and with a determination frequency of 26 h(-1) for both drugs. The results obtained for pharmaceutical formulations were statistically comparable to the declared hormone amount with relative deviations lower than 2.1%. The accuracy was confirmed by carrying out recovery studies, which furnished recovery values ranging from 96.3% to 103.7% for levothyroxine and 100.1% for liothyronine. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
A single reaction interface flow analysis (SIFA) system for the monitoring of mannitol in pharmaceutical formulations and human urine is presented. The developed approach takes advantage of the mannitol scavenger aptitude to inhibit the chemiluminescent reaction between luminol and myoglobin in the absence of H(2)O(2). The SIFA system facilitated the fully automation of the developed methodology, allowing the in-line reproducible handling of chemical species with a very short lifetime as is the case of the hydroxyl radical generated in the abovementioned luminol/myoglobin reaction. The proposed methodology allowed the determination of mannitol concentrations between 25 mmol L(-1) and 1 mol L(-1), with good precision (R.S.D. < 4.7%, n = 3) and a sampling frequency of about 60 h(-1). The procedure was applied to the determination of mannitol in pharmaceuticals and in human urine samples Without any pretreatment process. The results obtained for pharmaceutical formulations were statistically comparable to those provided by the reference method (R.D. < 4.6%); recoveries values obtained in the analysis of spiked urine samples (between 94.9 and 105.3% of the added amount) were also satisfactory. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
The objective of the present work is to evaluate the effect of surface modification of cellulose pulp fibres on the mechanical and microstructure of fibre-cement composites. Surface modification of the cellulose pulps was performed with Methacryloxypropyltri-methoxysilane (MPTS) and Aminopropyltri-ethoxysilane (APTS) in an attempt to improve their durability into fibre-cement composites. The surface modification showed significant influence on the microstructure of the composites on the fibre-matrix interface and in the mineralization of the fibre lumen as seen by scanning electron microscopy (SEM) with back-scattered electron (BSE) detector. Accelerated ageing cycles decreased modulus of rupture (MOR) and toughness (TE) of the composites. Composites reinforced with MPTS-modified fibres presented fibres free from cement hydration products, while APTS-modified fibres presented accelerated mineralization. Higher mineralization of the fibres led to higher embrittlement of the composite after accelerated ageing cycles. These observations are therefore very useful for understanding the mechanisms of degradation of fibre-cement composites. (C) 2009 Elsevier Ltd. All rights reserved.
Resumo:
The inclined plane test (IPT) is commonly performed to measure the interface shear strength between different materials as those used in cover systems of landfills. The test, when interpreted according to European test Standards provides the static interface friction angle, usually assumed for 50 mm displacement and denoted as phi(stat)(50). However, if interpreted considering the several phases of the sliding process, the test is capable of yielding more realistic information about the interface shear strength such as differentiating interfaces which exhibit the same value of phi(stat)(50) but different behavior for displacement less than 50 mm. In this paper, the IPT is used to evaluate the interface shear strength of some materials usually present in cover liner systems of landfill. The results of the tests were analyzed for both, the static and the dynamic phases of the sliding and were interpreted based on the static initial friction angle, phi(0), and the limit friction angle, phi(lim). It is shown that depending on the sliding behavior of the interfaces, phi(stat)(50), which is usually adopted as the designing parameter in stability analysis, can be larger than phi(0) and phi(lim). (C) 2009 Elsevier Ltd. All rights reserved.
Resumo:
In this paper, a computational tool concerning the computation of flexural and fracture toughness of cement based composites is presented. Firstly, RILEM`s (Reunion Internationale des Laboratoires d`Essais de Materiaux) recommendations related to the analysis of FRC in three-point bend tests are discussed in their relevant aspects regarding the computational implementations. The determination of other mechanical properties such as the Young modulus has been added to the program. Taking this into account, a new formulation based on displacements is used. In the second part of the paper, the determination of fracture properties of concrete, such as the fracture energy, G(F) , and the fracture toughness, K-IC(S), is discussed regarding the computational strategies used in the implementations. Several features whereby anterior data can be reanalyzed, obtained from other standards and recommendations, have been incorporated into the program, therefore allowing comparative studies and back analysis activities.
Resumo:
Nanomaterials have triggered excitement in both fundamental science and technological applications in several fields However, the same characteristic high interface area that is responsible for their unique properties causes unconventional instability, often leading to local collapsing during application Thermodynamically, this can be attributed to an increased contribution of the interface to the free energy, activating phenomena such as sintering and grain growth The lack of reliable interface energy data has restricted the development of conceptual models to allow the control of nanoparticle stability on a thermodynamic basis. Here we introduce a novel and accessible methodology to measure interface energy of nanoparticles exploiting the heat released during sintering to establish a quantitative relation between the solid solid and solid vapor interface energies. We exploited this method in MgO and ZnO nanoparticles and determined that the ratio between the solid solid and solid vapor interface energy is 11 for MgO and 0.7 for ZnO. We then discuss that this ratio is responsible for a thermodynamic metastable state that may prevent collapsing of nanoparticles and, therefore, may be used as a tool to design long-term stable nanoparticles.
Resumo:
The effects of temperature on the fast fracture behavior of aluminum nitride with 5 wt% Y(2)O(3) ceramic were investigated. Four-point flexural strength and fracture toughness were measured in air at several temperatures (30-1,300 A degrees C). The flexural strength gradually decreased with the increase of temperature up to 1,000 A degrees C due to the change in the fracture mode from transgranular to intergranular, and then became almost constant up to 1,300 A degrees C. Two main flaw types as fracture origin were identified: small surface flaw and large pores. The volume fraction of the large pores was only 0.01%; however, they limited the strength on about 50% of the specimens. The fracture toughness decreased slightly up to 800 A degrees C controlled by the elastic modulus change, and then decreased significantly at 1,000 A degrees C due to the decrease in the grain-boundary toughness. Above 1,000 A degrees C, the fracture toughness increased significantly, and at 1,300 A degrees C, its value was close to that measured at room temperature.