111 resultados para REINFORCED RUBBER COMPOSITES


Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this work, composites based on a phenolic matrix and untreated- and treated sisal fibers were prepared. The treated sisal fibers used were those reacted with NaOH 2% solution and esterified using benzophenonetetracarboxylic dianhydride (BTDA). These treated fibers were modified with the objective of improving the adhesion of the fiber-matrix interface, which in turn influences the properties of the composites. BTDA was chosen as the esterifying agent to take advantage of the possibility of introducing; the polar and aromatic groups that are also present in the matrix structure into the surface of the fiber, which could then intensify the interactions occurring in the fiber-matrix interface. The fibers were then analyzed by SEM and FTIR to ascertain their chemical composition. The results showed that the fibers had been successfully modified. The composites (reinforced with 15%, w/w of 3.0 cm length sisal fiber randomly distributed) were characterized by SEM, impact strength, and water absorption capacity. In the tests conducted, the response of the composites was affected both by properties of the matrix and the fibers, besides the interfacial properties of the fiber-matrix. Overall, the results showed that the fiber treatment resulted in a composite that was less hygroscopic although with somewhat lower impact strength, when compared with the composite reinforced with untreated sisal fibers. (C) 2009 Wiley Periodicals, Inc. J Appl Polym Sci 115: 269-276, 2010

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Pineapple leaf fiber (PALF) which is rich in cellulose, abundantly available, relatively inexpensive, low density, nonabrasive nature, high filling level possible, low energy consumption, high specific properties, biodegradability and has the potential for polymer reinforcement. The utilization of pineapple leaf fiber (PALF) as reinforcements in thermoplastic and thermosetting resins in micro and nano form for developing low cost and lightweight composites is an emerging field of research in polymer science and technology. In this paper we examines the industrial applicabiliy of PALF, mainly for production of composite materials and special papers, chemical feedstocks (bromelin enzyme) and fabrics.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

An investigation of the parameters as aniline: MnO(2) and temperature on synthesis of polyaniline/MnO(2) composites was performed. The composites were chemically prepared in H(2)SO(4) media using different aniline: MnO(2) ratios at 0 degrees C. After the ratio optimization, the syntheses were performed at 20 degrees C. The polyaniline/MnO(2) composites were characterized by scanning electron microscopy (SEM), ultraviolet-visible, near infrared and infrared spectroscopic techniques. Composites obtained with a uniform, homogeneous and thicker coating of polyaniline films under oxide was considered as the best condition for synthesis.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Composite electrodes were prepared using graphite powder and silicone rubber in different compositions. The use of such hydrophopic materials interned to diminish the swallowing observed in other cases when the electrodes are used in aqueous solutions for a long time. The composite was characterized for the response reproducibility, ohmic resistance, thermal behavior and active area. The voltammetric response in relation to analytes with known voltammetric behavior was also evaluated, always in comparison with the glassy carbon. The 70% (graphite, w/w) composite electrode was used in the quantitative determination of hydroquinone (HQ) in a DPV procedure in which a detection limit of 5.1 x 10(-8) mol L-1 was observed. HQ was determined in a photographic developer sample with errors lower then 1% in relation to the label value. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A graphite silicone-rubber composite electrode (GSR) was used for the determination of propranolol in drug formulation. Cyclic voltammetry (CV) at the GSR presented an irreversible oxidation peak at + 0.8V vs. SCE, in Britton Robinson (B-R) buffer pH 7.4. The quantitative determination was carried out using differential pulse voltammetry (DPV). Under optimized parameters a linear dynamic range from 5.0 to 80.6 mu mol L(-1) with a detection limit of 1.1 mu mol L(-1) was observed. A repeatability of 4.5 +/- 0.1 mu A (n = 10) peak current was found after 10 successive DPV voltammograms of propranolol in the same solution after surface renovations. Using the proposed electrode, propranolol was quantified in a pharmaceutical formulation with results that agreed within 95% confidence level (t-test) with those from an official method.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A new composite electrode based on multiwall carbon nanotubes (MWCNT) and silicone-rubber (SR) was developed and applied to the determination of propranolol in pharmaceutical formulations. The effect of using MWCNT/graphite mixtures in different proportions was also investigated. Cyclic voltammetry and electrochemical impedance spectroscopy were used for electrochemical characterization of different electrode compositions. Propranolol was determined using MWCNT/SR 70% (m/m) electrodes with linear dynamic ranges up to 7.0 mu molL(-1) by differential pulse and up to 5.4 mu molL(-1) by square wave voltammetry, with LODs of 0.12 and 0.078 mu molL(-1), respectively. Analysis of commercial samples agreed with that obtained by the official spectrophotometric method. The electrode is mechanically robust and presented reproducible results and a long useful life.