204 resultados para Fuji II LC cement
Resumo:
Adhesive mortars are widely used to set porcelain stoneware tiles on buildings because their bond strength and flexibility properties increase the cladding serviceability. However, their long-term performance is not well understood, mainly the degradation of the polymeric matrix. The influence of moisture content on the flexibility of six adhesive mortars is investigated, based on standard EN 12002. Four of them have defined formulations and the other two are commercial and are widely used to set porcelain stoneware tiles on building facades in Brazil. The results show that moisture content above 6% is sufficient to reduce 50% of the mortar deformability, but that the drying process allows it to recover to a value similar to that prior to saturation; a logarithmic function best fits the correlation between moisture content and flexibility; water immersion increases matrix rigidity. It is suggested that standards should consider flexibility tests on both dried and wet samples as a requirement for polymer-modified mortars. (C) 2010 Elsevier Ltd. All rights reserved.
Resumo:
Several studies using vegetable fibers as the exclusive reinforcement in fiber-cement composites have shown acceptable mechanical performance at the first ages. However, after the exposure to accelerated aging tests, these composites have shown significant reduction in the toughness or increase in embrittlement. This was mainly attributed to the improved fiber-matrix adhesion and fiber mineralization after aging process. The objective of the present research was to evaluate composites produced by the slurry dewatering technique followed by pressing and air curing, reinforced with combinations of polypropylene fibers and sisal kraft pulp at different pulp freeness. The physical properties, mechanical performance, and microstructural characteristics of the composites were evaluated before and after accelerated and natural aging. Results showed the great contribution of pulp refinement on the improvement of the mechanical strength in the composites. Higher intensities of refinement resulted in higher modulus of rupture for the composites with hybrid reinforcement after accelerated and natural aging. The more compact microstructure was due to the improved packing of the mineral particles with refined sisal pulp. The toughness of the composites after aging was maintained in relation to the composites at 28 days of cure.
Resumo:
Three formulations of fiber cement were evaluated for fungal colonization and color change after five years of exposure in aging stations located in urban (Sao Paulo), rural (Pirassununga) and coastal (Rio Grande) zones in Brazil. The lowest color change and fungal colonization were registered in Rio Grande, which has a temperate climate, as opposed to Sao Paulo and Pirassununga, which are tropical. The highest fungal colonization was recorded in Sao Paulo, one of the most air polluted cities in Brazil. Pirassununga samples had an intermediate fungal colonization, in spite of showing the highest color change with visible dark spots on the surfaces. These spots were identified as cyanobacteria, which significantly contributed to the darkening of the specimens. The fiber cement formulation, varying in proportion of organic fibers such as poly (vinyl alcohol) and cellulose, was less significant for fungal bioreceptivity than the characteristics of the exposure site. The most frequent fungal genus found in the tropical climate, in both urban and rural zones, and the main one responsible for the higher records in Sao Paulo, was Scytalidiurn sp. which was registered for the first time on this building material in Brazil. (C) 2010 Elsevier Ltd. All rights reserved.
Exploring the potential of functionally graded materials concept for the development of fiber cement
Resumo:
In this study we establish the concept of functionally graded fiber cement. We discuss the use of statistical mixture designs to choose formulations and present ideas for the production of functionally graded fiber cement components for Hatschek machines. The feasibility of producing functionally graded fiber cement by grading PVA fiber content has been experimentally evaluated. Thermogravimetric analysis (TG) was employed to assess fiber distribution profiles and four-point bending tests were applied to evaluate the mechanical performance of both conventional and graded composites. The results show that grading PVA fiber content is an effective way to produce functionally graded fiber cement, which allows for a reduction of the total fiber volume without a significant reduction on modulus of rupture of composite. TG tests were found adequate to assess the fiber content at different points in functionally graded fiber cements. (C) 2009 Elsevier Ltd. All rights reserved.
Resumo:
This paper presents results of laboratory testing of unrestrained drying shrinkage during a period of 154 days of different concrete mixtures from the Brazilian production line that utilize ground granulated blast-furnace slag in their compositions. Three concrete mixtures with water/cement ratio of 0.78(M1), 0.41(M2), and 0.37(M3) were studied. The obtained experimental data were compared with the analytical results from prediction models available in the literature: the ACI 209 model (ACI), the B3 model (B3), the Eurocode 2 model (EC2), the GL 2000 model (GL), and the Brazilian NBR 6118 model (NBR), and an analysis of the efficacy of these models was conducted utilizing these experimental data. In addition, the development of the mechanical properties (compressive strength and modulus of elasticity) of the studied concrete mixtures was also measured in the laboratory until 126 days. From this study, it could be concluded that the ACI and the GL were the models that most approximated the experimental drying shrinkage data measured during the analyzed period of time.
Resumo:
The effectiveness of environmental reclamation measures implemented in limestone mines is reviewed. An assessment procedure developed by Neri and Sanchez (2008) was used. This tool comprises else! of statements of good practice grouped in three categories (essential, important and accessory practices) which are assessed through (i) carrying outfield technical inspections guided by a series of protocols especially designed for this put pose; (ii) classifying inspection evidences according to previously defined categories (totally applied or satisfactorily adapted, partially applied, not applied or not applicable); and (iii) calculating conformity indexes.. The results showed that: planning activities featured the lowest performance (low conformity indexes), operational practices reached the most satisfactory results and management practices medium conformity indexes. A general conclusion is that in these mines, current practices are partially effective in establishing favorable conditions for long-term success of rehabilitation. Improvements in planning practices could significantly enhance performance and reduce risks.
Resumo:
A procedure to evaluate mine rehabilitation practices during the operational phase was developed and validated. It is based on a comparison of actually observed or documented practices with internationally recommended best practices (BP). A set of 150 BP statements was derived from international guides in order to establish the benchmark. The statements are arranged in six rehabilitation programs under three categories: (1) planning (2) operational and (3) management, corresponding to the adoption of the plan-do-check-act management systems model to mine rehabilitation. The procedure consists of (i) performing technical inspections guided by a series of field forms containing BP statements; (ii) classifying evidences in five categories; and (iii) calculating conformity indexes and levels. For testing and calibration purposes, the procedure was applied to nine limestone quarries and conformity indexes were calculated for the rehabilitation programs in each quarry. Most quarries featured poor planning practices, operational practices reached high conformity levels in 50% of the cases and management practices scored moderate conformity. Despite all quarries being ISO 14001 certified, their management systems pay low attention to issues pertaining to land rehabilitation and biodiversity. The best results were achieved by a quarry whose expansion was recently submitted to the environmental impact assessment process, suggesting that public scrutiny may play a positive role in enhancing rehabilitation practices. Conformity indexes and levels can be used to chart the evolution of rehabilitation practices at regular intervals, to establish corporate goals and for communication with stakeholders. (C) 2010 Elsevier Ltd. All rights reserved.
Resumo:
Urban rainfall-runoff residuals contain metals such as Cr, Zn, Cu, As, Pb and Cd and are thus reasonable candidates for treatment using Portland cement-based solidification-stabilization (S/S). This research is a study of S/S of urban storm water runoff solid residuals in Portland cement with quicklime and sodium bentonite additives. The solidified residuals were analyzed after 28 days of hydration time using X-ray powder diffraction (XRD) and solid-state Si-29 nuclear magnetic resonance (NMR) spectroscopy. X-ray diffraction (XRD) results indicate that the main cement hydration products are ettringite, calcium hydroxide and hydrated calcium silicates. Zinc hydroxide and lead and zinc silicates are also present due to the reactions of the waste compounds with the cement and its hydration products. Si-29 NMR analysis shows that the coarse fraction of the waste apparently does not interfere with cement hydration, but the fine fraction retards silica polymerization.
Resumo:
In Part I [""Fast Transforms for Acoustic Imaging-Part I: Theory,"" IEEE TRANSACTIONS ON IMAGE PROCESSING], we introduced the Kronecker array transform (KAT), a fast transform for imaging with separable arrays. Given a source distribution, the KAT produces the spectral matrix which would be measured by a separable sensor array. In Part II, we establish connections between the KAT, beamforming and 2-D convolutions, and show how these results can be used to accelerate classical and state of the art array imaging algorithms. We also propose using the KAT to accelerate general purpose regularized least-squares solvers. Using this approach, we avoid ill-conditioned deconvolution steps and obtain more accurate reconstructions than previously possible, while maintaining low computational costs. We also show how the KAT performs when imaging near-field source distributions, and illustrate the trade-off between accuracy and computational complexity. Finally, we show that separable designs can deliver accuracy competitive with multi-arm logarithmic spiral geometries, while having the computational advantages of the KAT.
Resumo:
Activated slag cement (ASC) shows significantly higher shrinkage than ordinary Portland cement agglomerates. Cracking generated by shrinkage is one of the most critical drawbacks for broader applications of this promising alternative binder. This article investigates the relationship between ASC hydration, unrestrained drying and autogenous shrinkage of mortar specimens. The chemical and microstructure evolution due to hydration were determined on pastes by thermogravimetric analysis, conduction calorimetry and mercury porosimetry. Samples were prepared with ground blast furnace slag (BFS) activated with sodium silicate (silica modulus of 1.7) with 2.5, 3.5 and 4.5% of Na2O, by slag mass. The amount of activator is the primary influence on drying and autogenous shrinkage, and early hydration makes a considerable contribution to the total result, which increases with the amount of silica. Drying shrinkage occurred in two stages, the first caused by extensive water loss when the samples were exposed to the environment, and the second was associated with the hydration process and less water loss. Due to the refinement of ASC porous system, autogenous shrinkage is responsible for a significant amount of the total shrinkage. (C) 2007 Elsevier Ltd. All rights reserved.
Resumo:
This paper studies the performance of fiber-cement corrugated sheets exposed to long-term weathering, exploring the effect of different environments on fiber-cement degradation. Fiber-cement corrugated sheets that had been exposed to weathering, and in place for more than 30-years, were collected from two different Brazilian cities (Sao Paulo and Criciuma). Mechanical properties (MOR, MOE and fracture toughness) were tested on samples removed from the corrugated sheets. Microstructure was evaluated by X-ray diffraction, SEM with EDS analysis, MIP and TG. The results show that the 37-year-old asbestos-cement corrugated sheets from Sao Paulo presented similar characteristics to those of the non-aged asbestos-cement readily available on the market place. Conversely, deterioration of the asbestos-cement from the industrial area of Criciuma is related to acidic attack, along with carbonation and leaching as a consequence of continued exposition to acid rain during several decades. This process resulted in higher porosity and lower mechanical strength, revealing that leaching mechanisms can have important effect on the performance of thin fiber-cement sheets. (c) 2007 Elsevier Ltd. All rights reserved.
Resumo:
At present, the cement industry generates approximately 5% of the world`s anthropogenic CO(2) emissions. This share is expected to increase since demand for cement based products is forecast to multiply by a factor of 2.5 within the next 40 years and the traditional strategies to mitigate emissions, focused on the production of cement, will not be capable of compensating such growth. Therefore, additional mitigation strategies are needed, including an increase in the efficiency of cement use. This paper proposes indicators for measuring cement use efficiency, presents a benchmark based on literature data and discusses potential gains in efficiency. The binder intensity (bi) index measures the amount of binder (kg m(-3)) necessary to deliver 1 MPa of mechanical strength, and consequently express the efficiency of using binder materials. The CO(2) intensity index (ci) allows estimating the global warming potential of concrete formulations. Research benchmarks show that bi similar to 5 kg m(-3) MPa(-1) are feasible and have already been achieved for concretes >50 MPa. However, concretes with lower compressive strengths have binder intensities varying between 10 and 20 kg m(-3) MPa(-1). These values can be a result of the minimum cement content established in many standards and reveal a significant potential for performance gains. In addition, combinations of low bi and ci are shown to be feasible. (c) 2010 Elsevier Ltd. All rights reserved.
Resumo:
Ethylene/vinyl acetate (EVA) copolymer. as latex or redispersable powder, is added to mortars and concrete to improve the fracture toughness, impermeability and bond strength to various substrates. The physical and chemical interactions were already proved after one day of hydration but during the first hour just the physical interaction was identified and some evidences of a chemical interaction. The aim of this paper was to evaluate the chemical interaction between EVA and Portland cement during the first hours of hydration in the thermogravimetric analysis. The results confirmed that the EVA hydrolyses in pH alkaline and consumes calcium ions from the solution, forming an organic salt (calcium acetate). reducing the calcium hydroxide content. And, its interaction occurred in the first 15 min of hydration. (C) 2009 Elsevier Ltd. All rights reserved.
Resumo:
Mature pregnant crossbred ewes (n = 90) were used in a randomized complete block design experiment and were assigned to 1 of 3 winter-feeding systems differing in primary feed source: haylage (HL), limit-fed corn (CN), or limit-fed dried distillers grains (DDGS). Effects of these winter-feeding strategies on postweaning progeny performance were determined. Lamb progeny (n = 96) were weaned at 61 +/- 4 d of age and fed a common high-concentrate diet. Lambs were assigned to feedlot pen (n = 18) based on dam mid-gestation pen. Growth rate, DMI, and ADG were determined for the first 40 d of the finishing period. At 96 +/- 4 d of age, 1 wether lamb was randomly selected from each pen (n = 18) for a glucose tolerance test. The experiment was terminated, and lambs were slaughtered individually when they were determined to have achieved 0.6-cm 12th-rib fat thickness. After a 24-h chill, carcass data were collected and a 2.54-cm chop was removed from each lamb from the LM posterior to the 12th rib for ether extract analysis. Additional carcass measurements of bone, muscle, and fat from the shoulder, rack, loin, and leg were collected on 35 carcasses. At weaning, lamb BW was not different among treatments, whereas final BW tended to be greater (P = 0.09) for lambs from ewes fed DDGS and CN during gestation than from those fed HL. Overall lamb growth rate from birth to slaughter was not different among treatments. Lambs from ewes fed DDGS vs. CN or HL tended to have a greater initial insulin response (P = 0.09). Dressing percent was less (P = 0.04) in lambs from ewes fed DDGS, but no difference (P = 0.16) was detected in HCW among treatments. As expected, 12th rib fat thickness was similar among treatments, whereas LM area was largest to smallest (P = 0.05) in lambs from ewes fed CN, HL, and DDGS, respectively. Proportion of internal fat tended to be greatest to smallest (P = 0.06) in lambs from ewes fed DDGS, CN, and HL, respectively. Calculated boneless trimmed retail cuts percentage was less (P = 0.04) in lambs from ewes fed DDGS than CN or HL. Loin muscle weight as a percentage of wholesale cut tended (P = 0.10) to be greater in lambs from ewes fed CN and HL than DDGS, whereas other muscle, bone, and fat weights and proportions were similar (P > 0.24) among treatments. Prepartum diet during mid to late gestation of ewes altered postnatal fat and muscle deposition and may be associated with alterations in insulin sensitivity of progeny.
Resumo:
The behaviour of cis isomers of selected mono- and di-acyl chlorogenic acids produced by UV-irradiation has been investigated by LC-MSn. cis Isomers fragment identically to the more common trans isomers. cis-5-Acyl chlorogenic acids are more hydrophobic and elute later than their mono- or di-trans counterparts whereas the reverse is true for cis-3-acyl and cis-4-acyl chlorogenic acids. The cis isomers of 1,3-dicaffeoylquinic acid, the only I-acyl chlorogenic acid investigated, are also more hydrophobic than the di-trans isomer. Coffee leaves had a proportionately greater content of cis isomers relative to trans isomers compared with coffee beans suggesting that UV-irradiation in vivo may also cause geometric isomerisation. (c) 2007 Elsevier Ltd. All rights reserved.