87 resultados para cure
Resumo:
The main goal of this paper is to investigate a cure rate model that comprehends some well-known proposals found in the literature. In our work the number of competing causes of the event of interest follows the negative binomial distribution. The model is conveniently reparametrized through the cured fraction, which is then linked to covariates by means of the logistic link. We explore the use of Markov chain Monte Carlo methods to develop a Bayesian analysis in the proposed model. The procedure is illustrated with a numerical example.
Resumo:
In this paper we extend the long-term survival model proposed by Chen et al. [Chen, M.-H., Ibrahim, J.G., Sinha, D., 1999. A new Bayesian model for survival data with a surviving fraction. journal of the American Statistical Association 94, 909-919] via the generating function of a real sequence introduced by Feller [Feller, W., 1968. An Introduction to Probability Theory and its Applications, third ed., vol. 1, Wiley, New York]. A direct consequence of this new formulation is the unification of the long-term survival models proposed by Berkson and Gage [Berkson, J., Gage, R.P., 1952. Survival cure for cancer patients following treatment. journal of the American Statistical Association 47, 501-515] and Chen et al. (see citation above). Also, we show that the long-term survival function formulated in this paper satisfies the proportional hazards property if, and only if, the number of competing causes related to the occurrence of an event of interest follows a Poisson distribution. Furthermore, a more flexible model than the one proposed by Yin and Ibrahim [Yin, G., Ibrahim, J.G., 2005. Cure rate models: A unified approach. The Canadian journal of Statistics 33, 559-570] is introduced and, motivated by Feller`s results, a very useful competing index is defined. (c) 2008 Elsevier B.V. All rights reserved.
Resumo:
The aim of this study was to assess the relation between the number of free radicals generated and the polymerization depth in two different commercial brands of resin composites with different colors and translucence. Electron paramagnetic resonance quantified the radical populations through relative intensity (I (r)) of free radicals generated, and radical decay was monitored. Sample translucence and the classical polymerization depth were measured. The analysis indicated that resin with more color pigments (MA4, I (r) = 0.73 a.u) or more opacity components (ODA2, I (r) = 0.84 a.u) generated smaller populations of free radicals and have the lower polymerization depth than clearer (M, I (r) = 1.20 a.u and MA2, I (r) = 1.02) or more translucent (OEA2, I (r) = 1.00 a.u) composites for the same light-curing time. It seems that irradiation doses have to be adequate to more colored and less translucent resins.
Resumo:
The purpose of this study was to evaluate the effect of pre-heating resin composite photo-cured with light-curing units (LCU) by FT-IR. Twenty specimens were made in a metallic mold (4 mm diameter x 2 mm thick) from composite resin-Tetric Ceram (R) (Ivoclar/Vivadent) at room temperature (25 degrees C) and pre heated to 37, 54, and 60 degrees C. The specimens were cured with halogen curing light (QTH) and light emitted by diodes (LED) during 40 s. Then, the specimens were pulverized, pressed with KBr and analyzed with FT-IR. The data were submitted to statistical analysis of variance and Kruskal-Wallis test. Study data showed no statistically significant difference to the degree of conversion for the different light curing units (QTH and LED) (p > 0.05). With the increase of temperature there was significant increase in the degree of conversion (p < 0.05). In this study were not found evidence that the light curing unit and temperature influenced the degree of conversion.
Resumo:
The aim of this study was to evaluate the hardness of a dental composite resin submitted to temperature changes before photo-activation with two light-curing unite (LCUs). Five samples (4 mm in diameter and 2 mm in thickness) for each group were made with pre-cure temperatures of 37, 54, and 60A degrees C. The samples were photo-activated with a conventional quartz-tungsten-halogen (QTH) and blue LED LCUs during 40 s. The hardness Vickers test (VHN) was performed on the top and bottom surfaces of the samples. According to the interaction between light-curing unit and different pre-heating temperatures of composite resin, only the light-curing unit provided influences on the mean values of initial Vickers hardness. The light-curing unit based on blue LED showed hardness mean values more homogeneous between the top and bottom surfaces. The hardness mean values were not statistically significant difference for the pre-cure temperature used. According to these results, the pre-heating of the composite resin provide no influence on Vickers hardness mean values, however the blue LED showed a cure more homogeneous than QTH LCU.
Resumo:
The structural and thermal properties of three different dental composite resins, Filtek (TM) Supreme XT, Filtek (TM) Z-250 and TPHA (R)(3) were investigated in this study. The internal structures of uncured and cured resins with blue light-emitting diodes (LEDs) were examined by Micro-Raman spectroscopy. Thermal analysis techniques as DSC, TG and DTG methods were used to investigate the temperature characteristics, as glass transition (T (g) ), degradation, and the thermal stability of the resins. The results showed that the TPHA (R)(3) and Filtek (TM) Supreme XT presented very similar T (g) values, 48 and 50A degrees C, respectively, while the Filtek (TM) Z-250 composite resin presented a higher one, 58A degrees C. AFM microscope was utilized in order to analyze the sample morphologies, which possess different fillers. The composed resin Filtek (TM) Z-250 has a well interconnected more homogeneous morphology, suggesting a better degree of conversion correlated to the glass phase transition temperature. The modes of vibration of interest in the resin were investigated using Raman spectroscopy. It was possible to observe the bands representative for the C=C (1630 cm(-1)) and C=O(1700 cm(-1)) vibrations were studied with respect to their compositions and polymerization. It was observed that the Filtek (TM) Z -250 resin presents the best result related to the thermal properties and polymerization after light curing among the other resins.
Resumo:
The different parameters used for the photoactivation process provide changes in the degree of conversion (DC%) and temperature rise (TR) of the composite resins. Thus, the purpose of this study was to evaluate the DC (%) and TR of the microhybrid composite resin photoactivated by a new generation LED. For the KBr pellet technique, the composite resin was placed into a metallic mould (1-mm thickness and 4-mm diameter) and photoactivated as follows: continuous LED LCU with different power density values (50-1000 mW/cm(2)). The measurements for the DC (%) were made in a FTIR Spectrometer Bomen (model MB-102, Quebec-Canada). The spectroscopy (FTIR) spectra for both uncured and cured samples were analyzed using an accessory for the diffuse reflectance. The measurements were recorded in the absorbance operating under the following conditions: 32 scans, 4-cm(-1) resolution, and a 300 to 4000-cm(-1) wavelength. The percentage of unreacted carbon-carbon double bonds (% C=C) was determined from the ratio of the absorbance intensities of aliphatic C=C (peak at 1638 cm(-1)) against an internal standard before and after the curing of the specimen: aromatic C-C (peak at 1608 cm-1). For the TR, the samples were made in a metallic mould (2-mm thickness and 4-mm diameter) and photoactivated during 5, 10, and 20 s. The thermocouple was attached to the multimeter to allow the temperature readings. The DC (%) and TR were calculated by the standard technique and submitted to ANOVA and Tukey`s test (p < 0.05). The degree of conversion values varied from 35.0 (+/- 1.3) to 45.0 (+/- 2.4) for 5 s, 45.0 (+/- 1.3) to 55.0 (+/- 2.4) for 10 s, and 47.0 (+/- 1.3) to 52.0 (+/- 2.4) for 20 s. For the TR, the values ranged from 0.3 (+/- 0.01) to 5.4 (+/- 0.11)degrees C for 5 s, from 0.5 (+/- 0.02) to 9.3 (+/- 0.28)degrees C for 10 s, and from 1.0 (+/- 0.06) to 15.0 (+/- 0.95)degrees C for 20 s. The power densities and irradiation times showed a significant effect on the degree of conversion and temperature rise.
Resumo:
Dental composite resins possess good esthetic properties, and are currently among the most popular dental restorative materials. Both organic and inorganic phases might influence the material behavior, the filler particle features and rate are the most important factors related to improvement of the mechanical properties of resin composites. Thus, the objective of this study was to evaluate the effect of three different composite resins on the polymerization process by Vickers hardness test. The samples were prepared using three different composite resins, as follow: group I-P-60 (3M/ESPE); group II-Herculite XRV (Kerr), and group III-Durafill (Heraeus-Kulzer). The samples were made in a polytetrafluoroethylene mould, with a rectangular cavity measuring 7 mm in length, 4 mm in width, and 3 mm in thickness. The samples were photo-activated by one light-curing unit based on blue LEDs (Ultrablue III-DMC/Brazil) for 20 and 40 s of irradiation times. The Vickers hardness test was performed 24 h after the photo-activation until the standardized depth of 3 mm. The Vickers hardness mean values varied from 158.9 (+/- 0.81) to 81.4 (+/- 1.94) for P-60, from 138.7 (+/- 0.37) to 61.7 (+/- 0.24) for Herculite XRV, and from 107. 5 (+/- 0.81) to 44.5 (+/- 1.36) for Durafill composite resins photo-activated during 20 s for the 1st and 2nd mm, respectively. During 40 s of photo-activation, the Vickers hardness mean values were: from 181.0 (+/- 0.70) to 15.6 (+/- 0.29) for P-60, and from 161.8 (+/- 0.41) to 11.2 (+/- 0.17) for Herculite XRV composite resins, for the 1st and 3th mm, respectively. For Durafill composite resin the mean values varied from 120.1 (+/- 0.66) to 61.7 (+/- 0.20), for the 1st and 2nd mm, respectively. The variation coefficient (CV) was in the most of the groups lower than 1%, then the descriptive statistic analysis was used. The Vickers hardness mean values for Durafill were lower than P-60 and Herculite XRV composite resins for 20 and 40 s of irradiation time. The polymerization process was greatly affected by the composition of the composite resins.
Resumo:
The purpose of this study was to evaluate the effectiveness of different light-curing units on the bond strength (push-out) of glass fiber posts in the different thirds of the root (cervical, middle and apical) with different adhesive luting resin systems (dual-cure total-etch; dual-cured and self-etch bonding system; and dual-cure self-adhesive cements), Disks of the samples (n = 144) were used, with approximately 1 mm of thickness of 48 bovine roots restored with glass fiber posts, that were luted with resin cements photo-activated by halogen LCU (QTH, Optilux 501) and blue LED (Ultraled), with power densities of 600 and 550 mW/cm(2), respectively. A universal testing machine (MTS 810 Material Test System) was used with a 1 mm diameter steel rod at cross-head speed of 0.5 mm/min until post extrusion, with load cell of 50 kg, for evaluation of the push-out strength in the different thirds of each sample. The push-out strength values in kgf were converted to MPa and analyzed through Analysis of Variance and Tukey`s test, at significance level of 5%. The results showed that there were no statistical differences between the QTH and LED LCUs. The self-adhesive resin cement had lower values of retention. The total-etch and self-adhesive system resin cements seem to be a possible alternative for glass fiber posts cementation into the radicular canal and the LED LCU can be applied as an alternative to halogen light on photo-activation of dual-cured resin cements.
Resumo:
Dental composites can be improved by heat treatment, as a possible way to increase mechanical properties due to additional cure (post-cure). Direct dental composites are essentially similar to the indirect ones, supposing they have the same indication. Therefore, to establish a heat treatment protocol for direct composites, using as indirect (photoactivated by continuous and pulse-delay techniques), a characterization (TG/DTG and DSC) is necessary to determine parameters, such as mass loss by thermal decomposition, heat of reaction and glass transition temperature (T (g)). By the results of this study, a heat treatment could be carried out above 160 A degrees C (above T (g), and even higher than the endset exothermic event) and under 180 A degrees C (temperature of significant initial mass loss).
Resumo:
Objective: To evaluate the flexural strength, microleakage, and degree of conversion of a microhybrid resin polymerized with argon laser and halogen lamp. Method and Materials: For both flexural test and degree of conversion analysis, 5 bar samples of composite resin were prepared and polymerized according to ISO 4049. The halogen light-curing unit was used with 500 MW/cm(2) for 20 seconds and the argon laser with 250 mW for 10 and 20 seconds. Samples were stored in distilled water in a dark environment at 37 degrees C for 24 hours. The flexural property was quantified by a 3-point loading test. For the microleakage evaluation, 60 bovine incisors were used to prepare standardized Class 5 cavities, which were restored and polished. Specimens were stored in distilled water for 24 hours at 37 degrees C and thermocycled 500 times (6 degrees C to 60 degrees C). Specimens were then immersed in art aqueous solution of basic fuchsin for 24 hours. Longitudinal sections of each restoration were obtained and examined with a stereomicroscope for qualitative evaluation of microleakage. Fourier transform (FT)-Raman RFS 100/S spectrometer (Bruker) was used to analyze the degree of conversion. Results: ANOVA showed no statistically significant differences of flexural strength between the photoactivation types evaluated in the flexural study. Microleakage data were statistically analyzed by Mann-Whitney and Kruskal-Wallis tests. Enamel margins resulted in a statistically lower degree of leakage than dentin margins. No statistically significant difference was found among the 3 types of photocuring studied. ANOVA also showed no statistically significant difference in the degree of conversion among the studied groups. Conclusion: According to the methodology used in this research, the argon laser is a possible alternative for photocuring, providing the same quality of polymerization as the halogen lamp. None of the photocured units tested in this study completely eliminated microleakage.
Resumo:
Lignocellulosic materials can significantly contribute to the development of biobased composites. In this work, glyoxal-phenolic resins for composites were prepared using glyoxal, which is a dialdehyde obtained from several natural resources. The resins were characterized by (1)H, (13)C, (2)D, and (31)P NMR spectroscopies. Resorcinol (10%) was used as an accelerator for curing the glyoxal-phenol resins in order to obtain the thermosets. The impact-strength measurement showed that regardless of the cure cycle used, the reinforcement of thermosets by 30% (w/w) sisal fibers improved the impact strength by one order of magnitude. Curing with cycle 1 (150 degrees C) induced a high diffusion coefficient for water absorption in composites, due to less interaction between the sisal fibers and water. The composites cured with cycle 2 (180 degrees C) had less glyoxal resin coverage of the cellulosic fibers, as observed by images of the fractured interface observed by SEM. This study shows that biobased composites with good properties can be prepared using a high proportion of materials obtained from natural resources. (C) 2009 Elsevier Ltd. All rights reserved.