78 resultados para Planning of the landscape pattern in general
Resumo:
Our objective was to compare the polymerization stress (sigma(pol)) of a series of composites obtained using poly(methyl methacrylate) (PMMA) or glass as bonding substrates, and to compare the results with those from in vitro microleakage of composite restorations. The tested hypothesis was that stress values obtained in a less rigid testing system (i.e. using PMMA) would show a better relationship with microleakage data. Five dental composites were tested: Filtek Z250 (FZ), Z100 (Z1), Concept (CO), Durafill (DU) and Heliomolar (HM). sigma(pol) was determined in 1 mm high specimens inserted between two rods (empty set = 5 mm) of either PMMA or glass. The composite elastic modulus (E) was obtained by three-point bending. sigma(pol) and E data were submitted to a one-way analysis of variance/Tukey test (alpha = 0.05). For the microleakage test (MI), bovine incisors received cylindrical cavities (empty set = 5 mm, h = 2 mm), which were restored in bulk. After storage for 24 h in water, specimens were subjected to dye penetration using AgNO(3) as tracer. Specimens were sectioned twice, perpendicularly, and microleakage was measured (in millimeters) under 20x magnification. Data from MI were submitted to the Kruskal-Wallis test. Means (SD) of sigma(pol) (MPa) using glass/PMMA were FZ: 7.5(1.8)(A)/2.5(0.2)(bc); Z1: 7.3(0.5)(A)/2.8(0.3)(ab); CO: 6.8(1.1)(A)/3.2(0.5)(a); DU: 4.5(0.7)(B)/2.0(0.2)(bc); HM: 3.5(0.2)(B)/2.3(0.3)(c). sigma(pol) obtained using PMMA rods were 34-67% lower than with glass. Means (SD) for tooth average/tooth maximum microleakage were FZ: 0.92(0.19)(B)/1.53(0.30)(a); Z1: 1.19(0.21)(A)/1.75(0.20)(a); CO: 1.26(0.25)(A)/1.78(0.24)(a); DU: 0.83(0.30)(B)/1.68(0.46)(a): HM: 0.81(0.27)(B)/1.64(0.54)(a). The tested hypothesis was confirmed, as the composites showed the same ordering both in the polymerization stress test using PMMA rods and in the microleakage test. (C) 2009 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
The aim of this study was to evaluate the development of the osteoblastic phenotype in human alveolar bone-derived cells grown on collagen type I-coated titanium (Ti) surface (Col-Ti) obtained by plasma deposition acrylic acid grafting compared with machined Ti (M-Ti). Osteoblastic cells were cultured until subconfluence and subcultured on Col-Ti and M-Ti for periods of up to 21 days. Cultures grown on Col-Ti and M-Ti exhibited similar cell morphology. Cell adhesion, total protein content, and alkaline phosphatase (ALP) activity were not affected by Ti surface modification in all evaluated periods. Growth analyses indicated that there were significantly more cells in cultures grown on Col-Ti at day 3. Runt-related transcription factor 2 (Runx2), osteopontin (OPN), and osteoprotegerin (OPG) mRNA expression of cells subcultured on Col-Ti was higher, whereas collagen type I (COL) was lower compared with M-Ti. Ti surface modification neither affected the osteocalcin (OC), ALP and receptor activator of NF-kappa B ligand (RANKL) mRNA expression nor the calcium content extracted from mineralized matrix. These results demonstrated that Col-Ti favours cell growth during the proliferative phase (day 3) and osteoblastic differentiation, as demonstrated by changes in mRNA expression profile during the matrix mineralization phase (day 14), suggesting that this Ti surface modification may affect the processes of bone healing and remodelling. To cite this article:Assis AF, Beloti MM, Crippa GE, de Oliveira PT, Morra M, Rosa AL. Development of the osteoblastic phenotype in human alveolar bone-derived cells grown on a collagen type I-coated titanium surface.Clin. Oral Impl. Res. 20, 2009; 240-246.doi: 10.1111/j.1600-0501.2008.01641.x.
Resumo:
Strategies to promote bone repair have included exposure of cells to growth factor (GF) preparations from blood that generally include proteins as part of a complex mixture. This study aimed to evaluate the effects of such a mixture on different parameters of the development of the osteogenic phenotype in vitro. Osteoblastic cells were obtained by enzymatic digestion of human alveolar bone and cultured under standard osteogenic conditions until subconfluence. They were subcultured on Thermanox coverslips up to 14 days. Treated cultures were exposed during the first 7 days to osteogenic medium supplemented with a GFs + proteins mixture containing the major components found in platelet extracts [plate I et-derived growth factor-BB, transforming growth factor (TGF)-beta 1, TGF-beta 2, albumin, fibronectin, and thrombospondin] and to osteogenic medium alone thereafter. Control cultures were exposed only to the osteogenic medium. Treated cultures exhibited a significantly higher number of adherent cells from day 4 onward and of cycling cells at days 1 and 4, weak alkaline phosphatase (ALP) labeling, and significantly decreased levels of ALP activity and mRNA expression. At day 14, no Alizarin red-stained nodular areas were detected in cultures treated with GFs + proteins. Results were confirmed in the rat calvaria-derived osteogenic cell culture model. The addition of bone morphogenetic protein 7 or growth and differentiation factor 5 to treated cultures upregulated Runx2 and ALP mRNA expression, but surprisingly, ALP activity was not restored. These results showed that a mixture of GFs + proteins affects the development of the osteogenic phenotype both in human and rat cultures, leading to an increase in the number of cells, but expressed a less differentiated state.