65 resultados para Security-critical software
Resumo:
The selection of housekeeping genes is critical for gene expression studies. To address this issue, four candidate housekeeping genes, including several commonly used ones, were investigated in oral squamous cell carcinoma cell lines. A simple quantitative RT-PCR approach was employed by comparing relative expression of the four candidate genes within two cancerous cell tines (HN6 and HN31) and one noncancerous cell tine (HaCaT) treated or not with EGF and TGF-beta 1. Data were analyzed using ANOVA followed by the NormFinder software program. On this basis, stability of the candidate housekeeping genes was ranked and non statistical differences were found using ANOVA test. On the other hand, the NormFinder was able to show that GAPD and TUBB presented the less variable results, representing appropriated housekeeping genes for the samples and conditions anatyzed. In conclusion, this study suggests that the GAPD and the TUBB represent adequate normalizers for gene profiting studies in OSCC cell. tines, covering, respectively, high and low expression levels genes. (C) 2008 Elsevier Ltd. All rights reserved.
Resumo:
Objective. The goal of this paper is to undertake a literature search collecting all dentin bond strength data obtained for six adhesives with four tests ( shear, microshear, tensile and microtensile) and to critically analyze the results with respect to average bond strength, coefficient of variation, mode of failure and product ranking. Method. A PubMed search was carried out for the years between 1998 and 2009 identifying publications on bond strength measurements of resin composite to dentin using four tests: shear, tensile, microshear and microtensile. The six adhesive resins were selected covering three step systems ( OptiBond FL, Scotch Bond Multi-Purpose Plus), two-step (Prime & Bond NT, Single Bond, Clear. l SE Bond) and one step (Adper Prompt L Pop). Results. Pooling results from 147 references showed an ongoing high scatter in the bond strength data regardless which adhesive and which bond test was used. Coefficients of variation remained high (20-50%) even with the microbond test. The reported modes of failure for all tests still included high number of cohesive failures. The ranking seemed to be dependant on the test used. Significance. The scatter in dentin bond strength data remains regardless which test is used confirming Finite Element Analysis predicting non-uniform stress distributions due to a number of geometrical, loading, material properties and specimens preparation variables. This reopens the question whether, an interfacial fracture mechanics approach to analyze the dentin - adhesive bond is not more appropriate for obtaining better agreement among dentin bond related papers. (C) 2009 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Resumo:
Objective. To evaluate the biaxial and short-beam uniaxial strength tests applied to resin composites based upon their Weibull parameters, fractographic features and stress distribution. Methods. Disk- (15 mm x 1 mm) and beam-shaped specimens (10 mm x 2 mm x 1 mm) of three commercial composites (Concept/Vigodent, CA; Heliomolar/Ivoclar-Vivadent, HE; Z250/3M ESPE, FZ) were prepared. After 48h dry storage at 37 degrees C, disks and beams were submitted to piston-on-three-balls (BI) and three-point bending (UNI) tests, respectively. Data were analyzed by Weibull statistics. Fractured surfaces were observed under stereomicroscope and scanning electron microscope. Maximum principal stress (sigma(1)) distribution was determined by finite element analysis (FEA). Maximum sigma(1-BI) and sigma(1-UNI) were compared to FZ strengths calculated by applying the average failure loads to the analytical equations (sigma(a-BI) and sigma(a-UNI)). Results. For BI, characteristic strengths were: 169.9a (FZ), 122.4b (CA) and 104.8c (HE), and for UNI were: 160.3a (FZ), 98.2b (CA) and 91.6b (HE). Weibull moduli ( m) were similar within the same test. CA and HE presented statistically higher m for BI. Surface pores ( BI) and edge flaws ( UNI) were the most frequent fracture origins. sigma(1-BI) was 14% lower than sigma(a-BI.) sigma(1-UNI) was 43% higher than sigma(a-UNI). Significance. Compared to the short-beam uniaxial test, the biaxial test detected more differences among composites and displayed less data scattering for two of the tested materials. Also, biaxial strength was closer to the material`s strength estimated by FEA. (C) 2009 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
Resumo:
Our purpose was to evaluate the osteoconduction potential of mixed bovine bone (MBB) xenografts as an alternative for bone grafting of critical-size defects in the calvaria of rats. After surgery, in the time intervals of 1, 3, 6, and 9 months, rats were killed and their skulls collected, radiographed and histologically prepared for analysis. The data obtained from histological analysis reported that the particles of MBB did not promote an intense immunological response, evidencing its biocompatibility in rats. Our results clearly showed the interesting evidence that MBB was not completely reabsorbed at 9 months while a small amount of newly formed bone was deposited by osteoprogenitor cells bordering the defect. However, this discrete bone-forming stimulation was unable to regenerate the bone defect. Overall, our results suggest that the properties of MBB are not suitable for stimulating intense bone regeneration in critical bone defects in rats.
Resumo:
Objective: To evaluate the repair of critical-size bone defects in rats treated with demineralized bovine bone (DBB) compared with autogenous bone (AB). Material and method: A bone defect of 8 mm in diameter was created in the calvaria of 50 Rattus norvegicus, treated either with DBB or AB. Sub-groups of five rats of each group were killed at 7, 14, 21, 30 and 90 days post-operatively, and the skulls were removed and processed histologically. Histological sections were stained with hematoxylin and eosin. Result: Histological analysis showed complete closure of the defects with new bone at 90 days in group AB, and substitution of the biomaterial by fibrotic connective tissue in the DBB group at 21 days. Morphometric analysis showed that DBB was rapidly absorbed at 14 days, with its volume density decreasing from 47%+/- 0.8% at 7 days to 1.2%+/- 0.41% at 14 days. Subsequently, volume densities of the connective tissue and neoformed bone increased from 51.1%+/- 11.17% to 86.8%+/- 7.92% and from 1.9%+/- 1.13% to 12%+/- 8.02%, respectively, for the same time interval. The volume density of AB particles did not change throughout the experimental periods, but the amount of new bone increased markedly between 7 and 90 days, from 4.5%+/- 1.57% to 53.5%+/- 6.42% (P < 0.05). Conclusion: DBB did not provide complete repair of the defects, with significantly less new bone formation than in the AB group.