68 resultados para Binary alloys
Resumo:
We present a temperature- dependent Hartree- Fock- Bogoliubov- Popov theory to analyze the properties of the equilibrium states of an homogeneous mixture of bosonic atoms in two different hyperfine states and in the presence of an internal Josephson coupling. In our calculation we show that the bistable structure of the equilibrium states at zero temperature changes when we increase the temperature of the system. We investigate two mechanisms of the disappearance of bistability. In one, near the collapse of one of the equilibrium states, the acoustical branch becomes unstable and the gap of the optical branch goes to zero. In the other, there is no divergent behavior of the system and bistability disappears at a temperature in which the two equilibrium states merge at a zero- population fraction imbalance. When we further increase the temperature, this state remains as a unique equilibrium configuration.
Resumo:
The addition of transition metals to III-V semiconductors radically changes their electronic, magnetic, and structural properties. We show by ab initio calculations that in contrast to the conventional semiconductor alloys, the lattice parameter in magnetic semiconductor alloys, including those with diluted concentration, strongly deviates from Vegard's law. We find a direct correlation between the magnetic moment and the anion-transition metal bond lengths and derive a simple and general formula that determines the lattice parameter of a particular magnetic semiconductor by considering both the composition and magnetic moment. This dependence can explain some experimentally observed anomalies and stimulate other kind of investigations.
Resumo:
Magnetoresistance measurements in p-type Pb(1-x)Eu(x)Te alloys, for x varying from 0% up to 5%, have been used to investigate localization and antilocalization effects. These are attributed to both the spin-orbit scattering and to the large Zeeman splitting present in these alloys due to the large values of the effective Lande g factor. The magnetoresistance curves are analyzed using the model of Fukuyama and Hoshino, which takes into account the spin-orbit and Zeeman scattering mechanisms. The spin-orbit scattering time is found to be independent of the temperature, while the inelastic-scattering time increases with decreasing temperature suggesting the electron-phonon interaction as the main scattering mechanism.
Resumo:
The generation of a large recoil velocity from the inspiral and merger of binary black holes represents one of the most exciting results of numerical-relativity calculations. While many aspects of this process have been investigated and explained, the ""antikick,"" namely, the sudden deceleration after the merger, has not yet found a simple explanation. We show that the antikick can be understood in terms of the radiation from a deformed black hole where the anisotropic curvature distribution on the horizon correlates with the direction and intensity of the recoil. Our analysis is focused on Robinson-Trautman spacetimes and allows us to measure both the energies and momenta radiated in a gauge-invariant manner. At the same time, this simpler setup provides the qualitative and quantitative features of merging black holes, opening the way to a deeper understanding of the nonlinear dynamics of black-hole spacetimes.
Resumo:
We present parameter-free calculations of electronic properties of InGaN, InAlN, and AlGaN alloys. The calculations are based on a generalized quasichemical approach, to account for disorder and composition effects, and first-principles calculations within the density functional theory with the LDA-1/2 approach, to accurately determine the band gaps. We provide precise results for AlGaN, InGaN, and AlInN band gaps for the entire range of compositions, and their respective bowing parameters. (C) 2011 American Institute of Physics. [doi:10.1063/1.3576570]
Resumo:
The thermo-solvatochromism of 2,6-dibromo-4-[(E)-2-(1-methylpyridinium-4-yl)ethenyl] phenolate, MePMBr(2), has been studied in mixtures of water, W, with ionic liquids, ILs, in the temperature range of 10 to 60 degrees C, where feasible. The objectives of the study were to test the applicability of a recently introduced solvation model, and to assess the relative importance of solute-solvent solvophobic interactions. The ILs were 1-allyl-3-alkylimidazolium chlorides, where the alkyl groups are methyl, 1-butyl, and 1-hexyl, respectively. The equilibrium constants for the interaction of W and the ILs were calculated from density data; they were found to be linearly dependent on N(C), the number of carbon atoms of the alkyl group; van't Hoff equation (log K versus 1/T) applied satisfactorily. Plots of the empirical solvent polarities, E(T) (MePMBr(2)) in kcal mol(-1), versus the mole fraction of water in the binary mixture, chi(w), showed non-linear, i.e., non-ideal behavior. The dependence of E(T) (MePMBr(2)) on chi(w), has been conveniently quantified in terms of solvation by W, IL, and the ""complex"" solvent IL-W. The non-ideal behavior is due to preferential solvation by the IL and, more efficiently, by IL-W. The deviation from linearity increases as a function of increasing N(C) of the IL, and is stronger than that observed for solvation of MePMBr(2) by aqueous 1-propanol, a solvent whose lipophilicity is 12.8 to 52.1 times larger than those of the ILs investigated. The dependence on N(C) is attributed to solute-solvent solvophobic interactions, whose relative contribution to solvation are presumably greater than that in mixtures of water and 1-propanol.
Resumo:
The longitudinal and transverse magnetostriction and microstructure of polycrystalline Fe(100-x)Ge(x) (x= 8, 12, 15, 20) alloys were investigated in order to correlate the magnetostriction with microstructure. In order to obtain different microstructures in the Fe(100-x)Ge(x) alloys, the samples were annealed at 600 degrees C during 2 h and at 1150 degrees C for half hour and then quenched in cold water. For Ge concentrations lower than 14 at.%, the longitudinal magnetostriction is positive and increases positively up to 22 ppm at 12 at.% Ge then decreases and vanishes at about 14 at.% Ge. For further Ge concentration increase the longitudinal magnetostriction is negative and reaches -30 ppm for Fe(80)Ge(20). This behavior, that is very similar to that reported for Fe-Si alloys, is explained by the structural changes caused by different thermal histories of the alloys. (C) 2008 Published by Elsevier B. V.
Production, microstructural characterization and mechanical properties of as-cast Ti-10Mo-xNb alloys
Resumo:
Beta titanium (Ti) alloys are one of the most promising groups of Ti alloys for biomedical applications. This work presents the production, microstructural characterization, and mechanical properties of as-cast Ti-10Mo-xNb (x = 0, 3, 6, 9, 20, and 30) alloys. They were produced via arc melting and characterized by scanning electron microscopy and X-ray diffraction. The density of each alloy was measured by the Archimedes method and the mechanical characterization was carried out by using the Vickers microhardness test and Young`s modulus measurements. The results show a near beta microstructure for niobium (Nb) contents lower or equal to 9 wt% while beta single-phase microstructure was obtained for higher Nb additions. The microhardness values decreased with the increase of Nb content in the alloys. The elastic modulus values of Ti-10Mo-3Nb and Ti-10Mo-20Nb alloys were lower than those of cp Ti and Ti-6Al-4V.
Resumo:
Accurate knowledge of several Me-B (Me - Metal) phase diagrams are important to evaluate higher order systems such as Me-Si-B ternaries. This work presents results of microstructural characterization of as-cast Cr-B alloys which are significant to assess the liquid compositions associated to most of the invariant reactions of this system. Alloys of different compositions were prepared by arc melting pure Cr and B pressed powder mixtures under argon atmosphere in a water-cooled copper crucible with non-consumable tungsten electrode and titanium getter. The phases were identified by scanning electron microscopy (SEM), using back-scattered electron (BSE) image mode and X-ray diffraction (XRD). In general, a good agreement was found between our data and those from the currently accepted Cr-B phase diagram. (c) 2006 Elsevier Inc. All rights reserved.
Resumo:
This work presents results of microstructural characterization of as-cast Cr-Si alloys. The alloys were prepared by arc melting pure Cr (min. 99.996%) and Si (min. 99.998%) powder mixtures under argon atmosphere in a water-cooled copper crucible with nonconsumable tungsten electrode and titanium getter. The phases were identified by scanning electron microscopy (SEM), using the back-scattered electron (BSE) image mode and X-ray diffraction (XRD). The results confirm the currently accepted Cr-Si phase diagram in terms of the invariant reactions and solid phases present in this system. Small corrections are proposed for the compositions of the liquid phase in the following reactions: (i) L double left right arrow Cr-ss+Cr3Si, from 15 to 16 at.% Si; (ii) L+alpha Cr5Si3 double left right arrow CrSi, from 51 at.% Si to slightly above 53 at.% Si; (iii) L double left right arrow CrSi+CrSi2, from 56 to slightly above 57 at.% Si; (iv) L double left right arrow CrSi2+Si, from 82 to slightly above 85 at.% Si. (c) 2006 Elsevier Inc. All rights reserved.
Resumo:
Ti-rich Ti-Si-B alloys can be considered for structural applications at high temperatures (max. 700 degrees C), however, phase equilibria data is reported only for T = 1250 degrees C. Thus, in this work the phase stability of this system has been evaluated at 700 degrees C. In order to attain equilibrium conditions in shorter time, rapid solidified samples have been prepared and carefully characterized. The microstructural characterization of the produced materials were based on X-ray diffraction (XRD), scanning electron microscopy (SEM-BSE), high resolution transmission electron microscopy (HRTEM), High Temperature X-ray diffraction with Synchrotron radiation (XRDSR) and Differential Scanning Calorimetry (DSC). Amorphous and amorphous with embedded nanocrystals have been observed after rapid solidification from specific alloy compositions. The values of the crystallization temperature (Tx) of the alloys were in the 509-647 degrees C temperature range. After Differential Scanning Calorimetry and High Temperature X-ray Diffraction with Synchrotron radiation, the alloys showed crystalline and basically formed by two or three of the following phases: alpha Ti, Ti(6)Si(2)B; Ti(5)Si(3); Ti(3)Si and TiB. It has been shown the stability of the Ti(3)Si and Ti(6)Si(2)B phases at 700 degrees C and the proposition of an isothermal section at this temperature. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
In the Mo-Si binary system. Mo(5)Si(3) crystallizes in the W(5)Si(3) (T(1) phase) structure type. However, when boron replaces silicon in this compound, a structural transition occurs from the W(5)Si(3) prototype structure to the Cr(5)B(3) prototype structure (T(2) phase) at the composition Mo(5)SiB(2). Mo(5)SiB(2) has received much attention in the literature as a candidate for structural application in high-temperature turbines, but its electronic and magnetic behavior has not been explored. In this work, we show that Mo(5)SiB(2) is a bulk superconducting material with critical temperature close to 5.8 K. The specific-heat, resistivity and magnetization measurements reveal that this material is a conventional type II BCS superconductor. (C) 2011 Elsevier Ltd. All rights reserved.
Resumo:
A set of stacked ribbon samples with the compositions Fe(85)Ga(15), Fe(78)Ni(7)Ga(15) and Fe(78)Co(7)Ga(15) were prepared. XRD on these ribbons show that the binary Fe(85)Ga(15) ribbon exhibits the disordered A2 structure where as the addition of Co and Ni leads to the appearance of an additional ordered DO(3) structure. A comparison of the ratio of the XRD-line intensities gave strong evidence of a (100) texture perpendicular to the ribbon surface. The optical studied microstructure supports these results because it shows a columnar grain growth parallel to the solidification direction-which is parallel to ribbon thickness. The highest magnetostriction was found for Fe(78)Ni(7)Ga(15) (370 ppm), while the Fe(78)Co(7)Ga(15) a smaller magnetostriction of 270 ppm was found. The enhancement of the magnetostriction is attributed to the (100) texture in these ribbons. (C) 2009 Elsevier B.V. All rights reserved.
Resumo:
Fe(100-x)Ti(x) alloys (x = 10, 15, 20) were studied with respect to their microstructure and magnetostriction. Depending on heat treatment temperature and composition, the sample retained either the alpha-phase (A2 structure) or the alpha-phase plus the TiFe(2) Laves phase (C14 structure). The saturation magnetostriction measured at 238K is negative, about -11 ppm. However, for fields up to 0.4 T the magnetostriction is barely zero, a very interesting result. High values of magnetostriction are of interest for applications mainly in sensors and actuators, but zero magnetostriction is also a remarkable property, desirable for many applications such as electric transformers and fluxgate sensor cores. Therefore, the Fe(100-x)Ti(x) (x < 20 at%) are an attractive option to be considered for these applications.
Resumo:
Longitudinal and transverse magnetostriction measurements were performed on polycrystalline Fe(100-x)Ti(x) alloys, for a large Ti concentration range, from x = 8.8 to 34.7 at.%. Our results showed that substituting Fe by Ti does not significantly enhance the magnetostriction. For all Ti concentrations in the magnetically saturated state, the longitudinal magnetostriction values vary from -2 x 10(-6) to 6 x 10(-6). On the other hand, Fe(100-x)Ti(x) alloys exhibit a large forced volume magnetostriction, which increases with increasing Ti-concentration. The magnetostriction behavior could be explained considering investigations of the hyteresis loops and the microstructure.