215 resultados para thrombocyte adhesion


Relevância:

10.00% 10.00%

Publicador:

Resumo:

This study evaluated the influence of the dental substrates obtained after the use of different caries removal techniques on bonding of a self-etching system. Forty, extracted, carious, human molars were ground to expose flat surfaces containing caries-infected dentine surrounded by sound dentine. The caries lesions of the specimens were removed or not (control-G1) either by round steel burs and water-cooled, low speed, handpiece (G2), or by irradiation with an erbium, chromium:yttrium scandium gallium garnet (Er,Cr:YSGG) laser (2W, 20 Hz, 35.38 J/cm(2), fiber G4 handpiece with 0.2826 mm(2), non-contact mode at a 2 mm distance, 70% air/20% water-G3) or using a chemo-mechanical method (Carisolv-G4). Caries-infected, caries-affected and sound dentines were submitted to a bonding system followed by construction of a resin-based composite crown. Hour-glass shaped samples were obtained and submitted to a micro-tensile bond test. The bond strength data were compared by analysis of variance (ANOVA), complemented by Tukey`s test (P <= 0.05). The samples of sound dentine presented higher bond strengths than did samples of caries-affected dentine, except for the groups treated with the Er,Cr:YSGG laser. The highest bond strengths were observed with the sound dentine treated with burs and Carisolv. The bond strengths to caries-affected dentine were similar in all groups. Additionally, bonding to caries-affected dentine of the Er,Cr:YSGG laser and Carisolv groups was similar to bonding to caries-infected dentine. Thus, caries-affected dentine is not an adequate substrate for adhesion. Moreover, amongst the caries removal methods tested, the Er,Cr:YSGG laser irradiation was the poorest in providing a substrate for bonding with the tested self-etching system.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This study tested if dentin adhesion is affected by Er:YAG laser. Ninety dentin disks were divided in groups (n=10): G1, control; G2, Er:YAG laser 150 mJ, 90 degrees contact, 38.8 J/cm(2); G3, Er:YAG laser 70 mJ, 90 degrees contact, 18.1 J/cm(2); G4, Er:YAG laser 150 mJ, 90 degrees non-contact, 1.44 J/cm(2); G5, Er:YAG laser 70 mJ, 90 degrees non-contact, 0.67 J/cm(2); G6, Er:YAG laser 150 mJ, 45 degrees contact, 37.5 J/cm(2); G7, Er:YAG laser 70 mJ, 45 degrees contact, 17.5 J/cm(2); G8, Er:YAG laser 150 mJ, 45 degrees non-contact, 1.55 J/cm(2); and G9, Er:YAG laser 70 mJ, 45 degrees non-contact, 0.72 J/cm(2). Bonding procedures were carried out and the micro-shear-bond strength (MSBS) test was performed. The adhesive surfaces were analyzed under SEM. Two-way ANOVA and multiple comparison tests revealed that MSBS was significantly influenced by the laser irradiation (p < 0.05). Mean values (MPa) of the MSBS test were: G1 (44.97 +/- 6.36), G2 (23.83 +/- 2.46), G3 (30.26 +/- 2.57), G4 (35.29 +/- 3.74), G5 (41.90 +/- 4.95), G6 (27.48 +/- 2.11), G7 (34.61 +/- 2.91), G8 (37.16 +/- 1.96), and G9 (41.74 +/- 1.60). It was concluded that the Er:YAG laser can constitute an alternative tool for dentin treatment before bonding procedures.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The adhesive performance on deproteinized dentin of different self-adhesive resin cements was evaluated through microtensile bond strength (mu TBS) analysis and scanning electron microscopy (SEM). Occlusal dentin of human molars were distributed into different groups, according to the categories: adhesive cementation with two-step bonding systems-control Groups (Adper Single Bond 2 + RelyX ARC/3M ESPE; One Step Plus + Duolink/Bisco; Excite + Variolink I/Ivoclar Vivadent) and self-adhesive cementation-experimental groups (Rely X Unicem/3M ESPE; Biscem/Bisco; MultiLink Sprint/Ivoclar Vivadent). Each group was subdivided according to the dentin approach to: alpha, maintenance of collagen fibers and beta, deproteinization. The mean values were obtained, and submitted to ANOVA and Tukey test. Statistical differences were obtained to the RelyX Unicem groups (alpha = 13.59 MPa; beta = 30.19 MPa). All the BIS Group specimens failed before the mechanical tests. Dentinal deproteinization provided an improved bond performance for the self-adhesive cement Rely X Unicem, and had no negative effect on the other cementing systems studied. (C) 2011 Wiley Periodicals, Inc. J Biomed Mater Res Part B: Appl Biomater 98B: 387-394, 2011.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

beta-Catenin is a bifunctional protein related to cell adhesion and gene transcription when activated by Wnt pathway. Altered expression of beta-catenin was related to loss of differentiation, more aggressive phenotype, increase of tumor invasion, and poor prognosis in a number of different cancers. Actinic cheilitis is caused by excessive exposure to ultraviolet radiation and has a high potential to suffer malignant transformation into squamous cell carcinoma (SCC) of the lip, the most frequent oral malignancy. Studies of oral cancer have shown the correlation of beta-catenin expression and oral SCC prognosis, and loss of membrane expression may be considered as a potential marker for early tumor recurrence. Thirty-five cases of actinic cheilitis and 12 cases of SCC of the lip were select and submitted to immunohistochemical staining using beta-catenin antibody. beta-Catenin was positive on the membrane for all cases. Eighty-five percent of actinic cheilitis cases showed cytoplasmatic staining, and 22% nuclear staining. Eighty-three percent of SCC was positive for beta-catenin, and none of them had nuclear staining. Cytoplasmatic and nuclear staining of beta-catenin on studied cases point to pathway alterations. Results demonstrated that beta-catenin expression is altered on epithelial dysplasia, and it is related to degree of alterations. (C) 2011 Elsevier Inc. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Aims Claudins are integral transmembrane proteins of the tight junctions, critical for maintaining cell adhesion and polarity. Alterations in the expression of individual claudins have been detected in carcinomas and appear to correlate with tumour progression. Methods In this study, a panel of anti-claudin antibodies (anti-claudins 1, 2, 3, 4, 5 and 7) was employed to map claudin expression in 136 cases of oral squamous cell carcinoma (OSCC) organised in a tissue microarray. Results Claudins were expressed in a reticular pattern up to the prickle layer in normal mucosal epithelium. In OSCC, claudins were strongly present in well-differentiated tumours, they presented mild and low expression in moderately differentiated OSCC, and were negative in poorly differentiated OSCC; the absences of claudin 1 (p = 0.002) and claudin 4 (p<0.001) were associated with moderately/poorly differentiated tumours. Strong expression of claudin 4 was associated with decreased perineural infiltration (p = 0.024). Claudins 5 and 7 were mostly negative or weakly expressed in all cases studied. Expression of claudin 7 was associated with the early clinical stages of the disease, whereas loss of claudin 7 tended to be more frequent in advanced stages of OSCC (p = 0.054). Absence of claudin 7 was also associated with absent vascular infiltration (p = 0.045) and with presence of recurrence (p = 0.052). Conclusions Claudin expression patterns showed a strong correlation with histological type of OSCC; claudin expression was decreased in areas of invasion, and negative in poorly differentiated tumours. This pattern may be related to evolution and prognosis of these tumours, especially in the case of claudin 7, which seems to be associated with a poor prognosis in OSCC.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The formation of salivary glands entails the proliferation of epithelial cells from the stomatodeum into the underlying ectomesenchyme, culminating in a complex network of ducts and acinar bulbs. The extent to which mucins regulate this process is unknown, but they appear to mediate luminal space formation and maturation. Our aim was to examine mucin expression patterns during the morphogenesis of human salivary glands. Mucin expression - MUC1, 2, 3, 4, 5AC, 5B, 6, and 16 - was analyzed in specimens of developing human salivary glands, obtained from fetuses at 4-24 weeks` gestation, and fully developed salivary glands by immunohistochemistry. Expression patterns were analyzed qualitatively according to the development stage of the salivary glands. Mucins 1, 3, 4, 5B, and 16 were expressed during salivary gland development - being stronger in all ductal segments by the final phases of branching morphogenesis and in mature glands. Acinar cells were negative for most mucins, including MUC1 in mature salivary glands. Mucins 2, 5AC, and 6 were not expressed. Mucins MUC1, 3, 4, 5B, and 16 are expressed in developing human salivary glands and in mature glands, suggesting important roles in the maturation and maintenance of the ductal network.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Transforming growth factor-beta (TGF-beta) is a multifunctional growth factor that has several biological effects in vivo including control of cell growth and differentiation, cell migration, lineage determination, motility, adhesion, apoptosis, and synthesis and degradation of extracellular matrix, and TGF-beta plays an important role in regulating tissue repair and regeneration. Our study analyzed the participation of TGF-beta 1, -beta 2, and -beta 3 in the different stages of morphogenesis and differentiation of human developing dental organ using immunobistochemistry. The maxillae and mandibles of 10 human embryos ranging from 8 to 23 weeks of gestation were employed, according to the approval of the ethical committee. Our study revealed that the TGF-beta subunits-beta 1, beta 2, and beta 3 were present in the various stages of tooth development, but the expression varied according to the differentiation stage, tissue, and TGF-beta subunit. Our results indicated that TGF-beta 1 is closely related to differentiation of enamel organ and initiation of matrix secretion, TGF-beta 2 to cellular differentiation, and TGF-beta 3 to mineral maturation matrix.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The aim of this in vitro study was to investigate the effect of erbium:yttrium-aluminum-garnet (Er:YAG) laser irradiation on dentinal collagen by transmission electron microscopy and to analyze the resin-dentin interface by scanning electron microscopy. A tensile bond strength test was also applied. Specimens from 69 sound human third molars were randomly divided into three groups: control (no laser), and two irradiated groups, laser 250 (250 mJ/2 Hz) and laser 400 (400 mJ/4 Hz). Then, specimens were restored with two adhesive systems, an etch-and-rinse or a self-etch system. Although ultrastructural examination showed a modified surface in the irradiated dentin, there was no statistical difference in bond strength values between the laser groups and controls (P < 0.05). In conclusion, the use of Er:YAG laser for ablating human dentin did not alter the main adhesion parameters when compared with those obtained by conventional methods, thus reinforcing its use in restorative dentistry.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Objective. The goal of this paper is to undertake a literature search collecting all dentin bond strength data obtained for six adhesives with four tests ( shear, microshear, tensile and microtensile) and to critically analyze the results with respect to average bond strength, coefficient of variation, mode of failure and product ranking. Method. A PubMed search was carried out for the years between 1998 and 2009 identifying publications on bond strength measurements of resin composite to dentin using four tests: shear, tensile, microshear and microtensile. The six adhesive resins were selected covering three step systems ( OptiBond FL, Scotch Bond Multi-Purpose Plus), two-step (Prime & Bond NT, Single Bond, Clear. l SE Bond) and one step (Adper Prompt L Pop). Results. Pooling results from 147 references showed an ongoing high scatter in the bond strength data regardless which adhesive and which bond test was used. Coefficients of variation remained high (20-50%) even with the microbond test. The reported modes of failure for all tests still included high number of cohesive failures. The ranking seemed to be dependant on the test used. Significance. The scatter in dentin bond strength data remains regardless which test is used confirming Finite Element Analysis predicting non-uniform stress distributions due to a number of geometrical, loading, material properties and specimens preparation variables. This reopens the question whether, an interfacial fracture mechanics approach to analyze the dentin - adhesive bond is not more appropriate for obtaining better agreement among dentin bond related papers. (C) 2009 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Stress distributions in torsion and wire-loop shear tests were compared using three-dimensional (3-D) linear-elastic finite element method, in an attempt to predict the ideal conditions for testing adhesive strength of dental resin composites to dentin. The torsion test presented lower variability in stress concentration at the adhesive interface with changes in the proportion adhesive thickness/resin composite diameter, as well as lower variability with changes in the resin composite elastic modulus. Moreover, the torsion test eliminated variability from changes in loading distance, and reduced the cohesive fracture tendency in the dentin. The torsion test seems to be more appropriate than wire-loop shear test for testing the resin composite-tooth interface strength. (c) Koninklijke Brill NV, Leiden, 2009

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Finite element analysis (FEA) utilizing models with different levels of complexity are found in the literature to study the tendency to vertical root fracture caused by post intrusion (""wedge effect""). The objective of this investigation was to verify if some simplifications used in bi-dimensional FEA models are acceptable regarding the analysis of stresses caused by wedge effect. Three plane strain (PS) and two axisymmtric (Axi) models were studied. One PS model represented the apical third of the root entirely, in dentin (PS-nG). The other models included gutta-percha in the apical third, and differed regarding dentin-post relationship: bonded (PS-B and Axi-B) or nonbonded (PS-nB and Axi-nB). Mesh discretization and material properties were similar for all cases. Maximum principal stress (sigma(max)) was analyzed as a response to a 165 N longitudinal load. Stress magnitude and orientation varied widely (PS-nG: 10.3 MPa; PS-B: 0.8 MPa; PS-nB: 10.4 MPa; Axi-13: 0.2 MPa, Axi-nB: 10.8 MPa). Axi-nB was the only model where all (sigma(max) vectors at the apical third were perpendicular to the model plane. Therefore, it is adequate to demonstrate the tendency to vertical root fractures caused by wedge effect. Axi-13 showed only part of the (sigma(max) perpendicular to the model plane while PS models showed sigma(max) on the model plane. In these models, sigma(max) orientation did not represent a situation where vertical root fracture would occur due to wedge effect. Adhesion between post and dentin significantly reduced (c) 2007 Wiley Periodicals, Inc.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Hydroxyapatite (HA), a stable and biocompatible material for bone tissue therapy, may present a variable stoichiometry and accept a large number of cationic substitutions. Such substitutions may modify the chemical activity of HA surface, with possible impact on biocompatibility. In this work, we assessed the effects of calcium substitution with diverse divalent cations (Pb(2+), Sr(2+), Co(2+), Zn(2+), Fe(2+), Cu(2+), or Mg(2+)) on the biological behavior of HA. Physicochemical analyses revealed that apatite characteristics related to crystallinity and calcium dissolution/uptake rates are very sensitive to the nature of cationic substitution. Cytocompatibility was evaluated by mitochondrial activity, membrane integrity, cell density, proapoptotic potential, and adhesion tests. With the exception of Zn-HA, all the substituted HAs induced some level of apoptosis. The highest apoptosis levels were observed for Mg-HA and Co-HA. Cu-HA was the only material to impair simultaneously mitochondrial activity, membrane integrity, and cell density. The highest relative cell densities after exposure to the modified HAs were observed for Mg-HA and Zn-HA, while Co-HA significantly improved cell adhesion onto HA surface. These results show that changes on surface dissolution caused by cationic substitution, as well as the increase of metal species released to biological media, were the main responsible factors related to alterations on HA biocompatibility. (C) 2011 Wiley Periodicals, Inc. J Biomed Mater Res Part A: 98A: 351-358, 2011.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Tartrate-resistant acid phosphatase (TRAP) is a well-known marker of osteoclasts and bone resorption. Here we have investigated whether osteoblast-like cells (hFOB 1.19) present TRAP activity and how would be its pattern of expression during osteoblastic differentiation. We also observed how the osteoblastic differentiation affected the reduced glutathione levels. TRAP activity was measured using the p-nitrophenylphosphate substrate. The osteogenic potential of hFOB 1.19 cells was studied by measuring alkaline phosphatase activity and mineralized nodule formation. Oxidative stress was determined by HPLC and DNTB assays. TRAP activity and the reduced glutathione-dependent microenvironment were modulated during osteoblastic differentiation. During this phase, TRAP activity, as well as alkaline phosphatase and glutathione increased progressively up to the 21st day, decreasing thereafter. We demonstrate that TRAP activity is modulated during osteoblastic differentiation, possibly in response to the redox state of the cell, since it seemed to depend on suitable levels of reduced glutathione.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Our purpose was to evaluate the osteoconduction potential of mixed bovine bone (MBB) xenografts as an alternative for bone grafting of critical-size defects in the calvaria of rats. After surgery, in the time intervals of 1, 3, 6, and 9 months, rats were killed and their skulls collected, radiographed and histologically prepared for analysis. The data obtained from histological analysis reported that the particles of MBB did not promote an intense immunological response, evidencing its biocompatibility in rats. Our results clearly showed the interesting evidence that MBB was not completely reabsorbed at 9 months while a small amount of newly formed bone was deposited by osteoprogenitor cells bordering the defect. However, this discrete bone-forming stimulation was unable to regenerate the bone defect. Overall, our results suggest that the properties of MBB are not suitable for stimulating intense bone regeneration in critical bone defects in rats.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Objectives: To evaluate the effect of chemical degradation on bond strength of resin-modified glass-ionomer cements bonded to primary and permanent dentin. Methods: Class I cavities of permanent and primary extracted human molars were restored with two resin-modified glass-ionomer cements: Fuji 11 LC and Vitremer, and stored in water for 24 h. Half samples were immersed in 10% NaOCl aqueous solution for 5 h. Teeth were sectioned into beams and tested for microtensile bond strengths. Results were analyzed with multiple ANOVA and Tukey`s tests (p < 0.05). Analysis of debonded surfaces was performed by SEM. Results: 24 h bond strengths for Vitremer and Fuji 11 LC were similar. For Fuji 11, bond strength values were higher for primary than for permanent dentin. Vitremer bond strength was similar for both. Chemical degradation did not affect Fuji I] LC bond strength to dentin. However, decreases in bond strength were found for Vitremer groups after NaOCl immersion. Signs of glass ionomer-dentin interaction were evident by SEM analysis for Fuji 11 LC specimens. Conclusions: Vitremer and Fuji II presented similar bond strength at 24. Vitremer dentin bonds were prone to chemical degradation. Fuji II LC-dentin bonds showed typical features of glass-ionomer dentin interaction at the bonded interfaces, and were resistant to in vitro degradation. (C) 2009 Elsevier Ltd. All rights reserved.