149 resultados para Konstnärsbröderna von Wrights dagböcker 1-7


Relevância:

100.00% 100.00%

Publicador:

Resumo:

The objective was to evaluate the suitability of using natural or lyophilized low density lipoproteins (LDL), in lieu of whole egg yolk, in extenders for cryopreserving ram semen. Once extragonadal sperm reserves were depleted in 10 fertile Santa Ines cross rams, two ejaculates per ram were collected for cryopreservation. Nine extenders were used: Tris-16% egg yolk extender with 5% glycerol as a control (T1), and substitution of whole egg yolk with 8, 12, 16 or 20% natural LDL (T2-T5, respectively), or with 8, 12, 16, or 20% lyophilized LDL (T6-T9). Semen was diluted to 100 X 10(6) sperm/mL, packaged into 0.25 mL straws, cooled, held at 5 C for 3 h, and then frozen in liquid nitrogen vapor. Immediately after thawing (37 degrees C for 30 s), sperm total and progressive motility, and kinetic parameters were analyzed with computer assisted semen analysis (CASA). Percentage of sperm with plasma membrane functional integrity was assessed by the hypoosmotic swelling test (HOST), sperm membrane physical integrity with propidium iodide (PI), and acrosome integrity with FITC-PSA using an epifluorescent microscope. For all sperm end points, there was no difference between the control and natural LDL treatments (P > 0.05): total motility (T1: 20.9 +/- 11.9 and average of T2-T5: 25.9 +/- 13.6%; mean SD), progressive motility (T1: 6.6 +/- 4.2 and average of T2-T5: 11.7 +/- 7.5%), HOST(+) (T1: 23.7 +/- 6.9 and average of T2-T5: 23.2 +/- 8.7%) and PI(-)/PSA(-) (T1: 13.8 +/- 7.8 and average of T2-T5: 18.1 +/- 7.8%). However, lyophilization was apparently unable to preserve the protective function of LDL; every sperm end point was significantly worse than in the control and natural LDL groups. We concluded that natural LDL was appropriate for cryopreserving ram semen, as it yielded results similar to those obtained with whole egg yolk. (C) 2011 Elsevier Inc. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Background: The aim of this study was to assess the prevalence, extent, and severity of probing depth (PD) and to investigate the associations between demographic, socioeconomic, and behavioral risk indicators and PD in a periodontally untreated and isolated population in Brazil. Methods: The target population consisted of all individuals aged >= 12 years as identified by a census. Consenting participants were submitted to a full-mouth clinical examination of six sites per tooth and were interviewed using a structured written questionnaire. Results: Among the 214 subjects who were interviewed and clinically examined, PD >= 4 mm was observed in 54% to 83% of the subjects, depending on age, whereas the age-dependent prevalence of PD :6 mm ranged from 5% among 12- to 19-year-olds to 50% among 40- to 49-year-olds, decreasing to 40% among subjects >= 50 years of age. Multivariate analyses identified supragingival calculus (odds ratio [OR] = 5.4 to 10.3; 95% confidence intervals [CIs]: 2.5 to 11.6 and 4.0 to 26.2 for 20% to 50% and > 50% of the sites, respectively) as a risk indicator for PD A mm, whereas age :40 years (OR = 9.0; 95% CI: 1.7 to 48.5), being a moderate/heavy smoker (OR = 3.7; 95% CI: 1.4 to 10. 1), and having supragingival calculus in 20% to 50% of sites (OR = 6.8; 95% CI: 1.4 to 32.4) or in >50% of sites (OR = 15.3; 95% CI: 3.2 to 73.6) were risk indicators for PD >= 6 mm. Having undergone urgency dental treatment was a protective factor for PD A and >= 6 mm (OR = 0.4; 95% CI: 0.2 to 0.8). Conclusions: Increased PD is highly prevalent in this isolated population. Behavioral factors played a significant role as risk indicators for increased PD in this isolated population.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Purpose: To evaluate in vitro the microshear bond strength of adhesive systems applied to dentin according to manufacturers` instructions, associated or not with a hydrophobic layer of unfilled resin. Materials and Methods: Six self-etching adhesives (Clearfil SE Bond, Kuraray Medical; AdheSE, lvoclar Vivadent; Xeno III, Dentsply; I Bond, Heraeus-Kulzer; Bond Force, Tokuyama; Futurabond DC, Voco) were tested. The labial dentin of sixty bovine incisors was exposed, and the teeth were divided into two groups according to the application or not of an extra hydrophobic resin layer (Scotchbond Multi Purpose Plus, bottle 3). Six composite cylinders (Filtek Z250, 3M ESPE) were built up on each treated surface. Specimens were stored in distilled water at 37 C for 24 h and then subjected to the microshear bond strength test in a universal testing machine at a crosshead speed of 0.5 mm/min. Microshear bond strength values were analyzed by 2-way ANOVA and Tukey`s post-hoc test. Failure mode was determined using a stereomicroscope under 20X magnification. Results: The application of the hydrophobic resin layer did not affect bond strength, except for AdheSE. However, the bond strengths with the hydrophobic layer were similar among the six tested systems (Clearfil: 17.1 +/- 7.9; AdheSE: 14.5 +/- 7.1; Xeno III: 12.8 +/- 7.7; I Bond: 9.5 +/- 5.8; Bond Force: 17.5 +/- 4.1; Futurabond: 7.7 +/- 2.3). When used as recommended by the manufacturers, Bond Force presented statistically higher bond strength than AdheSE and I Bond (p < 0.05) (Clearfil 10.4 +/- 4.9; AdheSE 1.6 +/- 1.6; Xeno III: 9.0 +/- 3.8; I Bond: 3.0 +/- 1.5; Bond Force: 14 +/- 3.9; Futurabond: 8.8 +/- 3.8). Failure mode was predominantly adhesive. Conclusion: The bond strength of the self-etching systems tested was not significantly affected by the application of a hydrophobic layer, but a significant improvement was observed in AdheSE.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Objectives: The effects of interactions between cross-linking proanthocyanidins (PA) in polar solvents and type-I collagen of demineralized dentin were investigated. Methods: Three PA-rich extracts, two from grape seed (GSEP and GSES) and one from cocoa (COE), were dissolved (water, ethanol:water and acetone:water) and analyzed for their ability to increase the modulus of elasticity of demineralized dentin. Sound dentin beams (0.5 mm x 1.7 mm x 7 mm) were fully demineralized and divided into 12 groups according to the type of cross-linking agent and solvents used. Specimens were immersed in the respective solutions and tested at baseline, 10, 30, 60, 120 and 240 min. Results: The elastic modulus (EM) of dentin was significantly increased by the PA treatment regardless of time (p < 0.05 for all times). The extracts showed different solubility in different solvents. GSEP showed the highest increase in EM when diluted in distilled water and acetone at all exposure times. Both GSEs showed superior results when diluted in distilled water and after 4 h of treatment, while COE produced strongest enhancement when dissolved in ethanol:water. Conclusions: The results indicates that herbal extraction process and other pharmacognostic parameters have an important influence on extract solubility as well as constitution and, consequently, on the PA-dentin matrix interaction. (C) 2010 Elsevier Ltd. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Background: Low-fluoride dentifrices have been suggested as alternatives to reduce dental fluorosis risk, but there is no consensus regarding their clinical effectiveness, which has been suggested to be increased when their pH is acidic. Aims: This single-blind randomized clinical trial evaluated the caries increment during the use of a low-fluoride acidic liquid dentifrice. Methods: Four-year-old schoolchildren (n = 1,402) living in a fluoridated area (0.6-0.8 ppm F) were randomly allocated to 4 groups differing according to the type of dentifrice used over a 20-month period. Group 1 (n = 345): liquid dentifrice, 1,100 ppm F, pH 4.5. Group 2 (n = 343): liquid dentifrice, 1,100 ppm F, pH 7.0. Group 3 (n = 354): liquid dentifrice, 550 ppm F, pH 4.5. Group 4 (n = 360): toothpaste, 1,100 ppm F, pH 7.0. At baseline and after 20 months, clinical examinations were conducted (dmfs index) and caries increment was calculated. Data were analysed by GLM procedure using classrooms (cluster) as unit of analysis (p < 0.05). Results: The mean +/- SD (95% CI) net increments found were as follows. Group 1: 2.06 +/- 2.38 (1.8-2.3); group 2: 2.08 +/- 2.87 (1.7-2.4); group 3: 2.05 +/- 2.79 (1.7-2.4), and group 4: 2.08 +/- 2.34 (1.8-2.4). No significant differences were detected among the groups. Conclusion: In a population with high caries risk living in a fluoridated area, as the selected sample, and according to the present protocol, the low-fluoride acidic liquid dentifrice seems to lead to similar caries progression rates as conventional 1,100 ppm F toothpaste. Copyright (C) 2010 S. Karger AG, Basel

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Periodontal diseases are infectious diseases, in which periodontopathogens trigger chronic inflammatory and immune responses that lead to tissue destruction. It occurs through the generation of metalloproteinases and the activation of bone resorption mechanisms. Anti-inflammatory cytokines such as IL-10 seem to attenuate periodontal tissue destruction through the induction of tissue inhibitors of metalloproteinases (TIMPs) and the inhibitor of osteoclastogenesis osteoprotegerin (OPG). A high individual variation in levels of IL-10 mRNA is verified in periodontitis patients, which is possibly determined by genetic polymorphisms. In this study, the IL-10 promoter -592C/A single nucleotide polymorphism ( SNP), which is associated with a decrease in IL-10 production, was analyzed by RFLP in 116 chronic periodontitis (CP) patients and 173 control (C) subjects, and the IL-10, TIMPs, and OPG mRNA expression levels in diseased gingival tissues were determined by real-time-PCR. The IL-10-592 SNP CA (P=0.0012/OR=2.4/CI:1.4-4.1), AA (P=0.0458/OR=2.3/CI:1.1-4.9), and CA+AA (P=0.0006/OR=2.4/CI: 1.4-3.4) genotypes and the allele A (P=0.0036/OR=1.7/CI:1.2-2.4) were found to be significantly more prevalent in the CP group when compared with control subjects. Both CA and AA genotypes were associated with lower levels of IL-10, TIMP-3, and OPG mRNA expression in diseased periodontal tissues and were also associated with disease severity as mean pocket depth. Taken together, the results presented here demonstrate that IL10-592 SNP is functional in CP, being associated with lower levels of IL-10 mRNA expression, which is supposed to consequently decrease the expression of the downstream genes TIMP-3 and OPG, and influence periodontal disease outcome. J. Leukoc. Biol. 84: 1565-1573; 2008.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Statement of the Problem: Adhesive systems can spread differently onto a substrate and, consequently, influence bonding. Purpose: The purpose of this study was to evaluate the effect of differently oriented dentin surfaces and the regional variation of specimens on adhesive layer thickness and microtensile bond strength (MTBS). Materials and Methods: Twenty-four molars were sectioned mesiodistally to expose flat buccal and lingual halves. Standardized drop volumes of adhesive systems (Single Bond [SB] and Prime & Bond 2.1 [PB2.1]) were applied to dentin according to the manufacturer`s instructions. Teeth halves were randomly divided into groups: 1A-SB/parallel to gravity; 1B-SB/perpendicular to gravity; 2A-PB2.1/parallel to gravity; and 2B-PB2.1/perpendicular to gravity. The bonded assemblies were stored in 37 degrees C distilled water for 24 hours and then sectioned to obtain dentin sticks (0.8 mm(2)). The adhesive layer thickness was determined in a light microscope (x200), and after 48 hours the specimens were subjected to MTBS test. Data were analyzed by one-way and two-way analysis of variance and Student-Newman-Keuls tests. Results: Mean values (MPa +/- SD) of MTBS were: 39.1 +/- 12.9 (1A); 32.9 +/- 12.4 (1B); 52.9 +/- 15.2 (2A); and 52.3 +/- 16.5 (2B). The adhesive systems` thicknesses (mu m +/- SD) were: 11.2 +/- 2.9 (1A); 18.1 +/- 7.3 (1B); 4.2 +/- 1.8 (2A); and 3.9 +/- 1.3 (2B). No correlation between bond strength and adhesive layer thickness for both SB and PB2.1 (r = -0.224, p = 0.112 and r = 0.099, p = 0.491, respectively) was observed. Conclusions: The differently oriented dentin surfaces and the regional variation of specimens on the adhesive layer thickness are material-dependent. These variables do not influence the adhesive systems` bond strength to dentin. CLINICAL SIGNIFICANCE Adhesive systems have different viscosities and spread differently onto a substrate, influencing the bond strength and also the adhesive layer thickness. Adhesive thickness does not influence dentin bond strength, but it may impair adequate solvent evaporation, polymer conversion, and may also determine water sorption and adhesive degradation over time. In the literature, many studies have shown that the adhesive layer is a permeable membrane and can fail over timebecause ofits continuous plasticizing and degradation when in contact with water. Therefore, avoiding thick adhesive layers may minimize these problems and provide long-term success for adhesive restorations.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Objective. We compared the anesthetic efficacy of inferior alveolar nerve block (IANB) plus buccal infiltration (BI) and IANB plus periodontal ligament (PDL) articaine injections in patients with irreversible pulpitis in the mandibular first molar. Study design. Fifty-seven volunteers, patients with irreversible pulpitis in the mandibular first molar admitted to the Department of Stomatology, Second Affiliated Hospital, Sun Yat-Sen University, randomly received conventional IANB, containing 1.7 mL 4% articaine/HCl with 1:100,000 epinephrine, plus either BI or PDL injections containing 0.4 mL articaine/HCl with 1: 100,000 epinephrine. The patients recorded the pain of the injections and endodontic access on a Heft-Parker visual analog scale (VAS). Results. According to the VAS scores, all patients experienced no or mild pain with BI and PDL injections after the application of IANB. Anesthetic success occurred in 81.48% for IANB plus BI (IANB/BI) compared with 83.33% for IANB plus PDL injection (IANB/PDL injection). None of the observed differences between the 2 groups was significant (P > .05). Conclusion. Both injection combinations resulted in high anesthetic success in patients with irreversible pulpitis in the mandibular first molar. (Oral Surg Oral Med Oral Pathol Oral Radiol Endod 2009;108:e89-e93)

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Background: The systemic renin-angiotensin system (RAS) promotes the plasmatic production of angiotensin (Ang) II, which acts through interaction with specific receptors. There is growing evidence that local systems in various tissues and organs are capable of generating angiotensins independently of circulating RAS. The aims of this study were to investigate the expression and localization of RAS components in rat gingival tissue and evaluate the in vitro production of Ang II and other peptides catalyzed by rat gingival tissue homogenates incubated with different Ang II precursors. Methods: Reverse transcription - polymerase chain reaction assessed mRNA expression. Immunohistochemical analysis aimed to detect and localize renin. A standardized fluorimetric method with tripeptide hippuryl-histidyl-leucine was used to measure tissue angiotensin-converting enzyme (ACE) activity, whereas high performance liquid chromatography showed products formed after the incubation of tissue homogenates with Ang I or tetradecapeptide renin substrate (TDP). Results: mRNA for renin, angiotensinogen, ACE, and Ang II receptors (AT(1a), AT(1b), and AT(2)) was detected in gingival tissue; cultured gingival fibroblasts expressed renin, angiotensinogen, and AT(1a) receptor. Renin was present in the vascular endothelium and was intensely expressed in the epithelial basal layer of periodontally affected gingival tissue. ACE activity was detected (4.95 +/- 0.89 nmol histidyl-leucine/g/minute). When Ang I was used as substrate, Ang 1-9 (0.576 +/- 0.128 nmol/mg/minute), Ang II (0.066 +/- 0.008 nmol/mg/minute), and Ang 1-7 (0.111 +/- 0.017 nmol/mg/minute) were formed, whereas these same peptides (0.139 +/- 0.031, 0.206 +/- 0.046, and 0.039 +/- 0.007 nmol/mg/minute, respectively) and Ang 1 (0.973 +/- 0.139 nmol/mg/minute) were formed when TDP was the substrate. Conclusion: Local RAS exists in rat gingival tissue and is capable of generating Ang II and other vasoactive peptides in vitro. J Periodontol 2009;80:130-139.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Considering the increase in esthetic restorative materials and need for improvement in unsatisfactory restoration substitution with minimal inadvertent removal of healthy tissues, this study assessed the efficacy of erbium:yttrium-aluminum-garnet (Er:YAG) laser for composite resin removal and the influence of pulse repetition rate on the morphological analyses of the cavity by scanning electron microscope. Composite resin fillings were placed in cavities (1.0 mm deep) prepared in bovine teeth, and the 75 specimens were randomly assigned to five groups according to the technique used for composite filling removal (high-speed diamond bur, group I, as a control, and Er:YAG laser, 250 mJ output energy and 80 J/cm(2) energy density, using different pulse repetition rates: group II, 2 Hz; group III, 4 Hz; group IV, 6 Hz; group V, 10 Hz). After the removal, the specimens were split in the middle, and we analyzed the surrounding and deep walls to check for the presence of restorative material. The estimation was qualitative. The surfaces were examined with a scanning electron microscope. The results revealed that the experimental groups presented bigger amounts of remaining restorative material. The scanning electron microscopy (SEM) analyses showed irregularities of the resultant cavities of the experimental groups that increased proportionally with increase in repetition rate.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

To evaluate several protocols for the application of ultrasound during removal of cast posts with varying core configurations cemented with zinc phosphate. Sixty maxillary canines were distributed into three groups (n = 20): group 1 - core with 5 mm diameter/height and post diameter of 1.3 mm; groups 2 and 3 - core with the same diameter as the post (1.3 mm) and heights of 5 mm and 3 mm, respectively. Posts/cores were cemented using a standard technique with zinc phosphate cement. Each group was divided into two subgroups according to the ultrasonic vibration mode: point vibration - ultrasonic vibration applied to the core surface for 5 s, on each face totalling 25 s; alternate vibration - intermittent application of ultrasonic vibration for 10 s to the labial and lingual surfaces, 10 s to the mesial and distal surfaces and 5 s to the incisal surface, totalling 25 s. The specimens were submitted to the tensile test using an Instron machine (1 mm min(-1)) and results were analysed by anova and t-test. The failure type was also analysed. Statistical analysis showed significant differences between groups relating to the core preparations (P < 0.05). The lowest mean values of traction force were obtained for group 3 (46.1 +/- 7.7 N), followed by group 2 (89.0 +/- 2.7 N) and group 1 (160.4 +/- 7.5 N). Regarding ultrasonic vibration, the lowest mean was observed with alternate vibration (81.1 +/- 10.1 N), which was significantly lower than the point vibration (115.9 +/- 9.5 N) (P < 0.05). Cohesive failure occurred in all cases. A reduction in core diameter/height and intermittent ultrasonic application improved the removal of cast posts cemented with zinc phosphate.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Purpose: To evaluate the bond strength of glass fiber posts to intraradicular dentin when cemented with self-etching and self-adhesive resin cements. Materials and Methods: Forty-eight single-rooted human teeth were decoronated, endodontically treated, post-space prepared and divided into 8 groups (n = 6). The glass fiber posts used were: Exacto (EA) (Angelus) and everStick (ES) (StichTeck), which were cemented with two self-adhesive resin cements: BisCem (BIS) (Bisco) and Rely-X Unicem (UNI) (3M/ESPE), and two self-etching resin cements: Esthetic Cementing System NAC100 (NAC) (Kuraray) and Panavia-F (PAN) (Kuraray). Specimens were thermocycled between 5 degrees C and 55 degrees C for 1000 cycles and stored in water at 37 degrees C for 1 month. Four 1-mm-thick (in cross section) rods were obtained from the cervical region of the roots. Specimens were then subjected to microtensile testing in a special machine (BISCO; Schaumburg, IL, USA) at a crosshead speed of 0.5 mm/min. Microtensile bond strength (mu TBS) data were analyzed with two-way ANOVA and Tukey`s tests. Results: Means (and SD) of mu TBS (MPa) were: EA/PAN: 10.3 (4.1), EA/NAC: 14 (5.1) EA/BIS: 16.4 (4.8), EA/UNI: 19.8 (5.1), ES/PAN: 25.9 (6.1), ES/NAC: 29.1 (7), ES/BIS: 28.9 (6), ES/UNI: 30.5 (6.6). ANOVA indicated significant differences among the groups (p < 0.001). Mean mu TBS values obtained with ES post were significantly higher than those obtained with EA (p < 0.001). For EA, Tukey`s test indicated that higher mu TBS means were obtained with the self-adhesive resin cements (BIS and UNI), which were statistically significantly different (p < 0.05) from values obtained with the self-etching resin cements (PAN and NAC). Different cements had no significant effects on the bond strength values of ES post (p > 0.05). mu TBS values obtained with ES post were significantly higher than those obtained with EA post irrespective of the resin cement used. Conclusion: everStick posts resulted in the highest mean mu TBS values with all cements. Self-adhesive cements performed well in terms of bond strength.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Purpose: This study evaluated the effect of the incorporation of the antimicrobial monomer methacryloyloxyundecylpyridinium bromide (MUPB) on the hardness, roughness, flexural strength, and color stability of a denture base material. Materials and Methods: Ninety-six disk-shaped (14-mm diameter x 4-mm thick) and 30 rectangular (65 x 10 x 3.3 mm(3)) heat-polymerized acrylic resin specimens were divided into three groups according to the concentration of MUPB (w/w): (A) 0%, (B) 0.3%, (C) 0.6%. Hardness was assessed by a hardness tester equipped with a Vickers diamond penetrator. Flexural strength and surface roughness were tested on a universal testing machine and a surface roughness tester, respectively. Color alterations (Delta E) were measured by a portable spectrophotometer after 12 and 36 days of immersion in water, coffee, or wine. Variables were analyzed by ANOVA/Tukey HSD test (alpha = 0.05). Results: The following mean results (+/-SD) were obtained for hardness (A: 15.6 +/- 0.6, B: 14.6 +/- 1.7, C: 14.8 +/- 0.8 VHN; ANOVA: p = 0.061), flexural strength (A: 111 +/- 17, B: 105 +/- 12, C: 88 +/- 12 MPa; ANOVA: p = 0.008), and roughness (A: 0.20 +/- 0.11, B: 0.20 +/- 0.11, C: 0.24 +/- 0.08 mu m; ANOVA: p = 0.829). Color changes of immersed specimens were significantly influenced by solutions and time (A: 9.1 +/- 3.1, B: 14.8 +/- 7.5, C: 13.3 +/- 6.1 Delta E; ANOVA: p < 0.05). Conclusions: The incorporation of MUPB affects the mechanical properties of a denture base acrylic resin; however, the only significant change was observed for flexural strength and may not be critical. Color changes were slightly higher when resin containing MUPB was immersed in wine for a prolonged time; however, the difference has debatable clinical relevance.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Purpose: This study evaluated the effect of different microwave polymerization cycles on the color changes of a microwave-processed denture base resin after accelerated aging and immersion in beverages. Materials and Methods: Specimens of light pink acrylic resin were divided into three groups according to polymerization cycle: (A) 500 W for 3 minutes, (B) 90 W for 13 minutes + 500 W for 90 seconds, and (C) 320 W for 3 minutes + 0 W for 4 minutes + 720 W for 3 minutes. Control groups were a heat-processed acrylic resin (T) and a chemically activated denture repair resin (Q). Eight specimens per group were aged in an artificial aging chamber and evaluated at 20, 192, and 384 hours. Another series of 40 specimens per group were immersed in water, coffee, tea, cola, or red wine and evaluated at 1, 12, and 36 days. Color was measured by a spectrophotometer before and after aging or immersion. Color changes (Delta E) were analyzed by ANOVA/Bonferroni t-test (alpha = 0.05). Results: Mean Delta E (+/- SD) after 384 hours of accelerated aging were (A) 2.51 +/- 0.50; (B) 3.16 +/- 1.09; (C) 2.89 +/- 1.06; (T) 2.64 +/- 0.34; and (Q) 9.03 +/- 0.40. Group Q had a significantly higher Delta E than the other groups. Color changes of immersed specimens were significantly influenced by solutions and time, but the five groups showed similar values. Mean Delta E at 36 days were (water) 1.4 +/- 0.8; (coffee) 1.3 +/- 0.6; (tea) 1.7 +/- 0.5; (cola) 1.4 +/- 0.7; and (red wine) 10.2 +/- 2.7. Results were similar among the five test groups. Conclusions: Color changes of the microwave-polymerized denture base resin tested were not affected by different polymerization cycles after accelerated aging or immersion in beverages. These changes were similar to the conventional heat-polymerized acrylic resin test, but lower than the repair resin after accelerated aging.