7 resultados para Types of optical fibres
em Universidad de Alicante
Resumo:
The changes in mechanical properties of portland cement mortars due to the addition of carbon fibres (CF) to the mix have been studied. Compression and flexural strengths have been determined in relation to the amount of fibres added to the mix, water/binder ratio, curing time and porosity. Additionally, the corrosion level of reinforcing steel bars embedded in portland cement mortars containing CF and silica fume (SF) have also been investigated and reinforcing steel corrosion rates have been determined. As a consequence of the large concentration of oxygen groups in CF surface, a good interaction between the CF and the water of the mortar paste is to be expected. A CF content of 0.5% of cement weight implies an optimum increase in flexural strength and an increase in embedded steel corrosion.
Resumo:
The stabilisation of pitch fibres (PFs) is the most important step for their subsequent use in the preparation of carbon fibres (CFs) and their resulting characteristics. The present work studies the influence that the stabilisation time has on the porosity of the CFs, and on the subsequent properties as carbon molecular sieve (CMS). The increase of the stabilisation time carried out at 573 K, from 2 to 8 h favours their CMS properties producing a decrease in the microposity accessible to N2, which gets completely blocked after 6 and 8 h, while the narrow microporosity (V-DR CO2) remains accessible. Adsorption kinetic studies with CH4 and CO2 were performed to assess the possibility of using these CFs as CMS by comparing them with Takeda 3A CMS. The results suggest that there is an optimal stabilisation time which allows the preparation of CFs from an abundant raw precursor with properties similar to Takeda 3A CMS.
Resumo:
Support for this work was provided by the Generalitat Valenciana (Spain) with projects PROMETEO/2009/043/FEDER, and by the Spanish MCT CTQ2008-05520.
Resumo:
Combustion runs at 700 °C in a horizontal laboratory furnace were carried out on two different electric wires (PVC and halogen-free wire). Tests were performed in the presence and in the absence of the metal conductor of the wires. The analyses of the polycyclic aromatic hydrocarbons (PAHs), chlorobenzenes (CBzs), chlorophenols (CPhs), mono- to octa-chlorodibenzo-p-dioxin and dibenzofurans (PCDD/Fs), and dioxin-like PCBs are shown. Regarding semivolatile compounds, PAHs production decreases in the presence of metal, while a higher amount of chlorinated compounds are emitted. Respect to the PCDD/Fs, the PVC wire in the presence of metal presents the highest emission, with a much more emission of furans than dioxins. The maximum emission is with 2 or 3 chlorine atom PCDD/Fs. PCBs emission correlates with PCDD/F production and represents 3–4% of total toxicity, determined by using WHO2005 factors.
Resumo:
A method using iodine has been developed for the stabilisation of low softening point (SP) pitch fibres that avoids air stabilisation in the production of carbon fibres (CF). The interaction between iodine and petroleum pitches has been studied by following the changes in the hydrogen content, aromatic or aliphatic, during the heat treatment of iodine-treated pitch fibres. Two low SP petroleum pitches were used and the iodine-treated pitch fibres were analysed by TGA, DSC, DRIFT, XPS and SEM. The results confirm that using this novel method pitches with low SP can be used to prepare CF with two advantages, compared with conventional methods. The stabilisation time is considerably reduced and treatments to increase the SP, usually required when low SP pitches are used to prepare CF, can be avoided.
Resumo:
We have investigated the spin preparation efficiency by optical pumping of individual Mn atoms embedded in CdTe/ZnTe quantum dots. Monitoring the time dependence of the intensity of the fluorescence during the resonant optical pumping process in individual quantum dots allows to directly probe the dynamics of the initialization of the Mn spin. This technique presents the convenience of including preparation and readout of the Mn spin in the same step. Our measurements demonstrate that Mn spin initialization, at zero magnetic field, can reach an efficiency of 75% and occurs in the tens of nanoseconds range when a laser resonantly drives at saturation one of the quantum-dot transition. We observe that the efficiency of optical pumping changes from dot-to-dot and is affected by a magnetic field of a few tens of millitesla applied in Voigt or Faraday configuration. This is attributed to the local strain distribution at the Mn location which predominantly determines the dynamics of the Mn spin under weak magnetic field. The spectral distribution of the spin-flip-scattered photons from quantum dots presenting a weak optical pumping efficiency reveals a significant spin relaxation for the exciton split in the exchange field of the Mn spin.