Resumo:
AlSi7Mg0.35 alloy was cast into permanent moulds using different pouring temperatures (725 to 625degreesC). As the pouring temperature decreased, the as-cast microstructure changed from a coarse dendritic structure, through fine equiaxed grains to fine rosette-like grains. The as-cast materials were then partially remelted and isothermally held at 580degreesC prior to semisolid casting into a stepped die. The feedstock material cast from a high temperature filled only half the die, with severe segregation and other defects. The low-temperature-poured material completely filled the die with negligible porosity. The quality of semisolid castings is significantly affected by the microstructure of the semisolid feedstock material that arises from a combination of as-cast and subsequent thermal treatment conditions. The paper describes (a) the influence of pouring temperature on the microstructure of feedstock; (b) microstructure evolution through remelting and (c) the quality of semisolid castings produced with this material. For A17Si0.35Mg alloy, low temperature pouring in the range of 625-650degreesC followed by suitable isothermal holding treatment can result in good quality semisolid casting.
Resumo:
Hypoeutectic AI-Si alloys represent the most widely used alloy system for cast aluminium applications. This system has a unique behaviour with respect to grain formation where an increase in silicon content results in a transition to larger grain sizes after a minimum at an intermediate concentration. As a result of the already large solute content, grain refinement by solute additions is inefficient and nucleant particles from the common aluminium grain refiners are not as effective as in wrought alloys. However, casting conditions, such as a low pouring temperature, that promote the formation of wall crystals tie. crystals nucleated in the thermally undercooled layer at or next to mould walls) are very effective in yielding a small grain size. This paper presents results of an investigation of the effect of low superheat and mould preheat temperature on grain size. It was found that pouring temperature controls the effectiveness of the wall mechanism while mould preheat has little effect until high preheat temperatures at which a large increase in grain size occurs. The observed changes in grain size are explained in terms of the balance between nucleation rate and survival rate of crystal nuclei resulting from changes in superheat and mould temperature.
Resumo:
Objective-To examine changes in the prevalence of cigarette smoking in 35 study populations of the World Health Organisation's MONICA Project. Design-Data from two independent, community-based surveys conducted, on average, five years apart. Setting-Geographically defined populations in 21 countries mainly in eastern and western Europe. Subjects-Randomly selected men and women aged 25-64 years. Numbers of participants in each study population ranged from 586 to 2817 in each survey. Main outcome measures-Changes in proportions of current smokers, ex-smokers, and never-smokers by age and sex using data collected by standardised methods. Results-Among men, smoking prevalence decreased in most populations, by three to four percentage points over five years. In Beijing, however, it increased in all age groups-overall by 11 percentage points. Among women there were increases in smoking in about half the populations. The increases were mainly in the age group 35-54 years and often in those populations where smoking prevalence among women has been relatively low. Conclusions-Smoking initiation by middle-aged women in parts of southern and eastern Europe and among men of all ages in Beijing is a matter of concern. The various public health measures that have helped to reduce smoking among men in developed countries should be vigorously extended to these other groups now at growing risk of smoking-related disease.
Resumo:
The stress corrosion cracking (SCC) behavior and pre-exposure embrittlement of AZ31 magnesium alloy have been studied by slow strain rate tensile (SSRT) tests in this paper. It is showed that AZ31 sheet material is susceptible to SCC in distilled water, ASTM D1.387 solution, 0.01 M NaCl and 0.1 M NaCl solution. The AZ31 magnesium alloy also becomes embrittled if pre-exposed to 0.01 M NaCl solution prior to tensile testing. The degree of embrittlement increased with increasing the pre-exposure time, It is proposed that both the pre-exposure embrittlement and SCC were due to hydrogen which reduces the cohesive strength. i,e,. hydrogen embrittlement, (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Partially solid commercial Al-Si and Mg-Al alloys have been deformed in shear during solidification using vane rheometry. The dendritic mush was deformed for a short period at 29% solid and allowed to cool naturally after deformation. Both alloys exhibited yield point behaviour and deformation was highly localised at the surface of maximum shear stress. The short period of deformation was found to have a distinct impact on the as-cast microstructure leading to fragmented dendrites in the deformation region of both alloys. In the case of the Mg-Al alloy, a concentrated region of interdendritic porosity was also observed in the deformation region. Concentrated porosity was not observed in the Al-Si alloy. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Trace elements can have a significant effect on the processing and properties of aluminium alloys, including sintered alloys. As little as 0.07 wt% (100 ppm) lead, tin or indium promotes sintering in an Al-Zn-Mg-Cu alloy produced from mixed elemental powders. This is a liquid phase sintering system and thin liquid films form uniformly throughout the alloy in the presence of the trace elements, but liquid pools develop in their absence. Analytical transmission electron microscopy indicates that the trace elements are confined to the interparticle and grain boundary regions. The sintering enhancement is attributed to the segregation of the microalloying addition to the liquid-vapour interface. Because the microalloying elements have a low surface tension, they lower the effective surface tension of the liquid. This reduces the wetting angle and extends the spreading of the liquid through the matrix. An improvement in sintering results. (C) 2001 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.
Resumo:
Mass balance calculations were performed to model the effect of solution treatment time on A356 and A357 alloy microstructures. Image analysis and electron probe microanalysis were used to characterise microstructures and confirm model predictions. In as-cast microstructures, up to 8 times more Mg is tied up in the pi-phase than in Mg2Si. The dissolution of pi is accompanied by a corresponding increase in the amount of beta-phase. This causes the rate of pi dissolution to be limited by the rate of beta formation. It is predicted that solution treatments of the order of tens of minutes at 540degreesC produce near-maximum T6 yield strengths, and that Mg contents in excess of 0.52 wt% have no advantage.
Resumo:
The immunoregulatory signaling (IRS) family includes several molecules, which play major roles in the regulation of the immune response. The CMRF-35A and CMRF-35H molecules are two new members of the IRS family of molecules, that are found on a wide variety of haemopoietic lineages. The extracellular functional interactions of these molecules is presently unknown, although CMRF-35H on initiate an inhibitory signal and is internalized when cross-linked. In this paper, we described the gene structure for the CMRF-35A gene and its localization to human chromosome 17. The gene consists of four exons spanning approximately 4.5 kb. Exon 1 encodes the 5' untranslated region and leader sequence, exon 2 encodes the immunoglobulin (Ig)-like domain, exon 3 encodes the membrane proximal region and exon 4 encodes the transmembrane region, the cytoplasmic tail and the 3' untranslated region. A region in the 5' flanking sequence of the CMRF-35A gene, that promoted expression of a reporter gene was identified. The genes for the CMRF-35A and CMRF-35H molecules are closely linked on chromosome 17. Similarity between the Ig-like exons and the preceding intron of the two genes suggests exon duplication was involved in their evolution. We also identified a further member of the CMRF-35 family, the CMRF-35J pseudogene. This gene appears to have arisen by gene duplication of the CMRF-35A gene. These three loci-the CMRF-35A, CMRF-35J and CMRF-35H genes-form a new complex of IRS genes on chromosome 17.
Resumo:
The forging characteristics of an Al-Cu-Mg-Si-Sn alloy are examined using it new testing strategy which incorporates a double truncated cone specimen and finite element modelling. This sample geometry produces controlled strain distributions within a single specimen and can readily identify the specific strain required to achieve a specific microstructural event by matching the metallographic data with the strain profiles calculated from finite element software, The friction conditions were determined using the conventional friction ring test, which was evaluated using finite element software. The rheological properties of the alloy, evaluated from compression testing of right cylinders, are similar to the properties of conventional aluminium forgings. A hoop strain develops at the outer diameter of the truncated cones and this leads to pore opening at the outer few millimetres. The porosity is effectively removed when the total strain equals the net compressive strain. The strain profiles that develop in the truncated cones are largely independent of the processing temperature and the strain rate although the strain required for pore closure increases as the forging temperature is reduced. This suggests that the microstructure and the strain rate sensitivity may also be important factors controlling pore behaviour. (C) 2002 Elsevier Science B.V. All rights reserved.
Resumo:
A new technique of surface modification by diffusion coating for AZ91D alloy was developed. A 1.0-2.0-mm alloy layer, which has hardness four to five times higher than the substrate metal, was formed after the treatment. Consequent solution treatment and aging could further improve the hardness of the alloy layer. Microstructure and chemical composition were investigated using optical microscope and electron probe.