21 resultados para Al2o3-cao-mgo-sio2
em University of Queensland eSpace - Australia
Resumo:
A structurally-based quasi-chemical viscosity model for fully liquid slags in the Al2O3 CaO-'FeO'-MgOSiO2 system has been developed. The focus of the work described in the present paper is the analysis of the experimental data and viscosity models in the quaternary system Al2O3 CaO-MgO-SiO2 and its subsystems. A review of the experimental data, viscometry methods used and viscosity models available in the Al2O3 CaO-MgO-SiO2 and its sub-systems is reported. The quasi-chemical viscosity model is shown to provide good agreement between experimental data and predictions over the whole compositional range.
Resumo:
A structurally-based quasi-chemical viscosity model has been developed for the Al2O3 CaO-'FeO'-MgO-SiO2 system. The model links the slag viscosity to the internal structure of melts through the concentrations of various anion/cation Si0.5O, Me2/nn+O and Me1/nn+Si0.25O viscous flow structural units. The concentrations of structural units are derived from the quasi-chemical thermodynamic model. The focus of the work described in the present paper is the analysis of experimental data and the viscosity models for fully liquid slags in the Al2O3-CaO-MgO, Al2O3 MgO-SiO2 and CaO-MgO-SiO2 systems.
Resumo:
A structurally-based quasi-chemical viscosity model for fully liquid slags in the Al2O3 CaO-'FeO'-MgO-SiO2 system has been developed. The model links the slag viscosities to the internal structures of the melts through the concentrations of various Si0.5O, Me2/nn+O and Me1/nn+Si0.25O viscous flow structural units. The concentrations of these structural units are derived from a quasi-chemical thermodynamic model of the system. The model described in this series of papers enables the viscosities of liquid slags to be predicted within experimental uncertainties over the whole range of temperatures and compositions in the Al2O3 CaOMgO-SiO2 system.
Resumo:
A structurally based viscosity model for fully liquid silicate slags has been proposed and applied to the Al2O3-CaO-'FeO'-SiO2 system at metallic iron saturation. The model links the slag viscosity to the internal structure of melts through the concentrations of various anion/cation structural units (SUs). The concentrations of structural units are equivalent to the second nearest neighbor bond concentrations calculated by the quasi-chemical thermodynamic model. This viscosity model describes experimental data over the entire temperature and composition range within the Al2O3-CaO-'FeO'-SiO2 system at metallic iron saturation and can be extended to other industrial slag systems.
Resumo:
Liquidus isotherms and phase equilibria have been determined experimentally for a pseudo-ternary section of the form MnO-(CaO+MgO)-(SiO2+Al2O3) with a fixed Al-2,O-3,/SiO2, weight ratio of 0.17 and MgO/CaO weight ratio of 0.17 for temperatures in the range 1473-1673 K. The primary phase fields present for the section investigated include manganosite (Mn,Mg,Ca)O; dicalcium silicate alpha-2(Ca,Mg,Mn)O (.) SiO2; merwinite 3CaO(.) ((Mg,Mn)O.2SiO(2); wollastonite [(Ca,Mg,Mn)(OSiO2)-Si-.]; ;tephroite [2(Mn,Mg)O.SiO2]; rhodonite [(Mn,Mg)O. diopside [(CaO,MgO,MnO,Al2O3)(SiO2)-Si-.]; tridymite (SiO2), SiO2] and melilite [2CaO (.) (MgO,MnO,Al2O3).2(SiO2,Al2O3)]. The liquidus temperatures relevant to ferro-manganese and silico-manganese smelting slags have been determined. The liquiclus temperature is shown to be principally dependent on the modified basicity weight ratio (CaO+Mgo)/(SiO2+Al2O3) at low MnO concentrations, and dependent on the mole ratio (CaO+ MgO+MnO)/(SiO2+Al2O3) at higher MnO concentrations.
Resumo:
Phase equilibria have been determined experimentally for pseudo-ternary sections of the form “MnO”- (CaO+MgO)-(SiO2+Al2O3) with a fixed Al2O3/SiO2 weight ratio of 0.17 and MgO/CaO weight ratios of 0.25 and 0.17 respectively for temperatures in the range 1473-1673 K. The primary phase fields present for the MgO/CaO weight ratio of 0.17 include manganosite (Mn,Mg,Ca)O; dicalcium silicate α-2(Ca,Mg,Mn)O·SiO2; merwinite 3CaO⋅(Mg,Mn)O⋅2SiO2; wollastonite [(Ca,Mg,Mn)O·SiO2]; diopside [(CaO,MgO,MnO,Al2O3)·SiO2]; tridymite (SiO2); tephroite [2(Mn,Mg)O·SiO2]; rhodonite [(Mn,Mg)O·SiO2] and melilite [2CaO·(MgO,MnO,Al2O3)·2(SiO2,Al2O3)]. For the section with MgO/CaO weight ratio of 0.25 the anorthite phase (CaO⋅Al2O3⋅2SiO2) is also present. The liquidus temperatures of ferro- and silico-manganese smelting slags have been determined. The liquidus temperatures at low MnO concentrations are shown to be principally dependent on the modified basicity weight ratio (CaO+MgO)/(SiO2+Al2O3).
Resumo:
The development of new experimental techniques for the determination of phase equilibria in complex slag systems, chemical thermodynamic, and viscosity models is reported. The new experimental data, and new thermodynamic and viscosity models, have been combined in a custom-designed computer software package to produce limiting operability diagrams for slag systems. These diagrams are used to describe phase equilibria and physicochemical properties in complex slag systems. The approach is illustrated with calculations on the system FeO-Fe2O3-CaO-SiO-Al2O3 at metallic iron saturation, slags produced in coal slagging gasifiers, and in the reprocessing of nonferrous smelting slags. This article was presented at the Mills Symposium Molten Metals, Slags and Glasses-Characterisation of Properties and Phenomena held in London in August 2000.
Resumo:
Research techniques and a methodology have been developed that enable the reduction kinetics of molten lead smelting slags with solid carbon to be studied. The rates of reduction of PbO-FeO-Fe2O3-CaO-SiO2 slags with carbon have been measured for a range of slag compositions for PbO concentrations between 3 and 100 weight percent, and temperatures between 1423 and 1573 K. The reduction rates were determined for both graphite and coke. Within the range of process conditions examined, it has been shown that the reaction rates are almost independent of carbon reactivity, SiO2/CaO and SiO2/Fe ratio in the range of compositions investigated and are not influenced by the presence of sulphur in the slag.The apparent first order rate constants for oxygen removal increase with increasing PbO concentration and oxygen activity in the slag. The data indicate that the rate limiting reaction step for the reduction of lead slags with solid carbon is the chemical reaction at the gas/slag interface.
Resumo:
Highly ordered mesoporous bioactive glasses (MBGs) with different compositions have been synthesized by a combination of surfactant templating, sol-gel method and evaporation-induced self-assembly (EISA) processes. The texture properties and compositional homogeneity of MBGs have been characterized and compared with conventional bioactive glasses (BGs) synthesized in the absence of surfactants by evaporation method. The formation mechanism (pore - composition dependence) and compositional homogeneity in the case of MBG materials are different from those in conventional BGs. Unlike conventional sol-gel-derived BGs that shows a direct correlation between their composition and pore architecture, MBGs with different compositions may possess similar pore volume and uniformly distributed pore size when the same structure-directing agent is utilized. The framework of MBG is homogeneously distributed in composition at the nanoscale and the inorganic species generally exists in the form of amorphous phase. MBGs calcined at temperatures
Resumo:
Ordered mesoporous bioactive glasses (MBGs) with different compositions were prepared by using nonionic block copolymer surfactants as structure-directing agents through an evaporation-induced self-assembly process. Their in-vitro bioactivities were studied in detail by electron microscopy, Fourier-transform infrared spectroscopy, and inductively coupled plasma (ICP) atomic emission spectroscopy. The ICP element analysis results were further calculated in terms of the total consumption of Ca and P, Delta[Ca]/Delta[P] ratios, and ionic activity product (IP) of hydroxyapatite. Through the above analysis, it is clear that MBGs show a different structure-bioactivity correlation compared to conventional sol-gel-derivcd BGs. The in vitro bioactivity of MBGs is dependent on the Si/Ca ratio in the network when the other material parameters such as the mesostructure and texture properties (pore size, pore volume) are controlled. MBG 80S15C with relatively lower calcium content exhibits the best in vitro bioactivity, in contrast to conventional sol-gel-derived BGs where usually higher calcium percentage BGs (e.g. 60S35C) show better bioactivity. Calcination temperature is another important factor that influences the in vitro bioactivity. According to our results, MBGs calcined at 973 K may possess the best in vitro bioactivity. The influences of the composition and calcination temperature upon bioactivity are explained in terms of the unique structures of MBGs. (c) 2006 Elsevier Ltd. All rights reserved.